Official Web: http://www.cnqsmotor.com/en/
Facebook: https://www.facebook.com/cnqsmotor/
There are many store sale QS Motor and Electric Motor Kits on aliexpress, I would like to make it more clearly for better understanding.
SiAECOSYS (SIA in short) is the subsidiary company of QSMOTOR, who focus on electric motor & motor kits as electic powertrain of electric 2/3/4 wheelers, for internantional market.
Vito, Judy, Tessio, Jasmine in 1st sales team,
Store name: SIA Electric Powertrain Store
https://siaecosys.aliexpress.com/store/5881618
Damon, Vincent in 2nd sales team,
Store name: QS Motor Factory Store
https://qsmotorfactory.aliexpress.com/store/1389549…
Store name: SiAECOSYS Store
https://www.aliexpress.com/store/5079180…
Carrie, Summer in 3rd sales team.
Store name: QS Electric Drive Store
https://qs-motordrive.aliexpress.com/store/4393030…
Store name: SIA Tech Store
https://siatech.aliexpress.com/store/5616201…
Others are not powered by SIA, please noted.
Welcome to visit our web on aliexpress, especially SIA Electric Powertrain Store, follow us on aliexpress for lastest news. ; ) QS Motor/Taizhou Quanshun Motor Co., Ltd (not QS MOTOR LIMITED) is located in Luqiao district, Taizhou city, Zhejiang province, east well-developed China. The Registered Trademark is QSMOTOR, short for QS Motor or QSMOTOR. It is the leading manufacturer for high power & quality Electric Bike,Scooter,Motorycle,Tricycle,Car in-wheel hub motor (range from 500W to 14kW, 48V-144V, 30km/h-160km/h) in China. After 16 years of endeavor in the field of hub motor industry, QS Motor has established strong brand recognition in the hub motor markets.
SiAECOSYS
Taizhou SIA trading Co.,Ltd. (brand name “SiAECOSYS”) is the subsidiary company of QSMOTOR, who focus on electric
motor & motor kits as electic power train of electric 2/3/4 wheelers, for internantional market.
There are 205 (500W-3000W), 260 (1500W-5000W), 273 (3000W-8000W) Hub Motor, doulbe shaft or single shaft design is avaialbe, which varies with or without wheels for different electric vehicles.
205 motor means the diameter of iron ring is 205mm, for all 205 motor, e.g. 10inch & 12inch 205 e-scooter hub motor,
205 spoke hub motor, 10inch & 12inch 205 single shaft hub motor, etc., the configuration & performance is the same as 10inch 205 Hub Motor.
QS Motor participated in INTERMOT 2016, Cologne Germany
Hall: 6 Stand:A041
It's the first time for us to attend international fair. QS Motor carefully prepared, with a superb level of technology, high-performance motor. The new mid drive motor become a major highlight in the fair, together with electric bike M6 and electric scooter Turtle King, which attracted many foreign businessmen & enthusiast gathered to watch and consultation to discuss.
It is a harvest tour. We meet many appointed customer face to face according to the appoitment schedule, and hunreds of new customer visit our booth. The exhibition, sold all QS Motor exhibition samples, and we also brought back a lot of advice from end users & delaers invaluable.
For more information, refer to below link.
http://www.cnqsmotor.com/en/article_read_574.html

QS Motor Electric In Wheel Hub Motor List


Attached catalog "QS MOTOR Catalog 2015.10.20" for reference. New QSMOTOR Catalog
https://www.dropbox.com/s/0xl7xi5w0tww4 ... 8.pdf?dl=0
Distributor/Dealer of QS Motor
If you tested QS Motor, and interest to be the dealer for better price & service.
Meanwhile, able to do some maintenance of hub motor (e.g. change hall sensors).
Here are some Dealers scheme as below.
E.g. MOQ15-29pcs, Annual 100pcs
MOQ30-49pcs, Annual 120pcs
MOQ50pcs, Annual above 120pcs
MOQ50pcs, Annual above 500pcs
Please don't hesitate to contact with us if any interest!
We're looking forwarder to cooperate with distributor/dealer throughout the world.
Electric scooter/motorcycle list:
QS Motor Factory News - Racing Electric Motorcycle with QS 14kw motor 160km/h 96v
viewtopic.php?f=31&t=65972&p=1267233#p1267233
For details, please refer to the hyperlink.
Lastest Product, Most Powerful Hub Motor
QS Motor 17X4.5 12kW-14kW 273 Water Cooled Electric Scooter Hub Motor
http://www.cnqsmotor.com/en/article_rea ... r/538.html
Electric Scooter/Motorycle Hub Motor
QS Motor 10inch 500W-4000W 205 Electric Scooter Hub Motor
http://www.cnqsmotor.com/en/article_rea ... r/526.html
QS Motor 12inch 500W-3000W 205 Electric Scooter Hub Motor
http://www.cnqsmotor.com/en/article_lis ... r/112.html
QS Motor 12inch 1500W-5000W 260 Electric Scooter Hub Motor
viewtopic.php?f=31&t=65972&start=925
http://www.cnqsmotor.com/en/article_rea ... r/562.html
QS Motor 13inch 1500W-5000W 260 Electric Scooter Hub Motor
http://www.cnqsmotor.com/en/article_rea ... r/563.html
QS Motor 13inch 1500W-8000W 273 Electric Scooter Hub Motor
http://www.cnqsmotor.com/en/article_lis ... r/113.html
QS Motor 14inch 1500W-5000W 260 Electric Scooter Hub Motor
http://www.cnqsmotor.com/en/article_rea ... r/564.html
QS Motor 14inch 2000W-8000W 273 Electric Scooter Hub Motor
http://www.cnqsmotor.com/en/article_lis ... r/114.html
QS Motor 16inch 2000W-8000W 273 Electric Scooter Hub Motor
http://www.cnqsmotor.com/en/article_lis ... r/115.html
QS Motor 17inch 2000W-8000W 273 Electric Scooter Hub Motor
viewtopic.php?f=31&t=65972&p=1235434#p1235434
http://www.cnqsmotor.com/en/article_lis ... r/139.html
QS Motor 13-17inch 2000W-8000W 273 Water Cooled Electric Scooter Hub Motor
PS. 1.Above 273 hub motor could be water cooled (mass production).
2. 10-17inch 205 & 273 Hub Motor could be Single Shaft Design.
Electric Bike/Motorcycle Hub Motor
Integrated Wheel Motor
QS Motor 16inch 1500W 260 E-Bike Hub Motor
http://www.cnqsmotor.com/en/article_rea ... r/488.html
QS Motor 20inch 500-1500W 205 E-bike Hub Motor
http://www.cnqsmotor.com/en/article_rea ... r/487.html
Spoke Hub Motor
Update: QS Motor 500W-3000W 205 Electric Bike Spoke Hub Motor
viewtopic.php?f=31&t=65972&p=1235450#p1235450
http://www.cnqsmotor.com/en/article_rea ... r/536.html
Update: Link on ES, QS 205 50H V3 Electric Spoke Hub Motor
viewtopic.php?f=31&t=65972&p=1082427#p1082427
Item: Article on electricbike.com writen by spinningmagnets "Large Hot Rod Hubmotors for Street E-bikes, the Double D’s"
https://www.electricbike.com/large-hot-rod-hubmotors/
Item: QS Motor Lace in moped wheels, 19"X1.6" available 1X2 cross pattern
http://www.cnqsmotor.com/en/article_rea ... t/391.html
(Christmas Preferential promotion)QS 3000W 205 50H V3 E-bike Spoke Hub Motor & QSKLS-7245H controller
viewtopic.php?f=31&t=65972&start=925#p1250076
QS Motor 3000W-8000W 273 Electric Motorycycle Spoke Hub Motor
http://www.cnqsmotor.com/en/article_lis ... r/117.html

Electric Car In Wheel Hub Motor
QS Motor 1000W-3000W 205 Electric Car Wheel Hub Motor
http://www.cnqsmotor.com/en/article_rea ... r/565.html
QS Motor 3000W-8000W 273 Electric Car Wheel Hub Motor
http://www.cnqsmotor.com/en/article_rea ... r/566.html
Electric Single Shaft Hub Motor
QS Motor 10-17inch 500W-8000W Electric Single Shaft Hub Motor
http://www.cnqsmotor.com/en/article_lis ... or/92.html
QS Motor 13inch 1500W~6000W 273 Electric Single Shaft Detachable Wheel Hub Motor
http://www.cnqsmotor.com/en/article_rea ... r/535.html
Customized Hub Motor
QS Motor Dual Stator Electric In Wheel Hub Motor
http://www.cnqsmotor.com/en/article_lis ... r/106.html
Mid Drive Motor (under develop)
Please more information, please refer to QS Motor Official Website.(New*)
viewtopic.php?f=31&t=65972&p=1235435#p1235435
http://www.cnqsmotor.com/en/
Product & Price List base online, the offline price will be a bit cheaper.
E.g. QS Motor 10inch 500W-4000W 205 Electric Scooter Hub Motor

PS. 1. Above quotation base on 10X2.15inch wheel, for all wide tire 10X3.0inch, it's USD 3.1 more.
2. For 205 motor, the voltage is 48V~96V.
3. Above configuration is suggested for mass production,
for EV enthusiast, V2 & V3 motor could be over-voltaged to gain more speed/performance (customizable).
Recently we did some update for our 3000w 205 50H V3 spoke hub motor to improve its waterproof
1. QS make dual holes for axle glue instead of single hole which make axle glue fill up with phase wires
2. Add heat shrink tubing to lengthen PVC silicone fiberglass sleeving for better waterproof
3. QS change better side cover glue and implement glue automatically (instead by hand)
Pls check this link:
viewtopic.php?f=31&t=65972&p=1082427#p1082427
viewtopic.php?f=31&t=65972&start=1100#p1385746
E.g. QS Motor 205 500W-3000W 205 Electric Bike Spoke Hub Motor

PS. 1. Above quotation base on 205 electric bike spoke hub motor.
2. For 205 motor, the voltage is 48V~96V.
3. Above configuration is suggested for mass production,
for EV enthusiast, V2 & V3 motor could be over-voltaged to gain more speed (customizable).
For the max continuous power rating
The data should be tested in lab, which means no further temp rise at the power (e.g. 100 degree inside of motor at the power).
Unluckly, all the continuous power rating is not done before.
Due to our understanding and feedback of customer,
for 205 3000W motor, the max continuous power could be 6000W, peak power 12kW (even 18kW).
For EV enthusiastic, they could input more power to enjoy the high performance, but the motor might suffer from over heating or even burnt.
For EV Manufacture, we should notice the potential performance of motor, and keep some allowance for the whole e-scooter kits.
include motor, controller, battery. to get them as stable as possible & decress the repair rate (consider all the usage environment).
E.g. 3000W as continuous rating power.
QS Motor Specification (e.g. 3000W 205 50H V3 Electric Bike Spoke Hub Motor)
1.Motor Type: BLDC Outer Rotor In-Wheel Hub Motor With Hall Sensor
2.Brand: QS Motor,QSMOTOR
3.Motor Design: Double axle with 205mm diameter hub motor, 36 spoke holes, OD 4.2mm
4.Suitable Rim size: 24inch, 26inch E-Bike Wheel, 17inch, 18inch, 19inch moped wheel.
5.Magnet Height: 50mm, 16 pole pairs
6.Stator: Aluminmum Core
7.Rated Power: 3000W (could be 12kW peak),
8.Speed(customizable, depends on wheel size):
48v 21km/h~65km/h
60v 26km/h~80km/h
72v 32km/h~80km/h
9.Max Torque approix 182N.m
10.Thermic Probe: KTY83/122 (as default)
11.Max Efficiency above 86%
12.Brake type: Disc brake, PCD6*44mm
13.Drop-outs: 150mm~154mm
14.Dual Hall Set with water proof connectos
15.10mm² Phase Wire (not include insulation)
16.Waterproof Grade: IP54
17.Color: Black (as default)
Gross Weight 14.5kg (with freewheel)
Package: 34cmX34cmX33cm
PS. Temp Sensor Options: KTY84/130, KTY83/122, 10K@25C NTC(model MF58-103F3950).
QS Motor could work 120 ℃ in half an hour without damage.
Suggestion (Setting of Controller)
When it's 130 ℃ inside of motor (in 30s), the current should be limited 50%.
When it's 150 ℃, the controller shut down. When it drop down to 110℃, the controller work again.
Price:
USD 279.8/piece (base on 1-2pcs samples offline)
USD 276.8/piece (base on 3-4pcs)
USD 271.8/piece (base on 5~9pcs)
USD 264.8/piece (base on 10~19pcs)
USD 259.8/piece (base on 20~29pcs)
USD 254.8/piece (base on 30~49pcs)
USD 252.8/piece (base on 50~100pcs)
Payment term: Wire Transfer/TT, Money Gram,Western Union, Paypal 100% in advance
Generally, we perefer T/T, Money Gram,Western Union 100% in advance (for sample). Meanwhile, we could also accpet paypal.
There will be extra cost for transaction fee: Total cost*4.4%+0.3 Withdraw fee: USD 35.0 (We could bear USD 35.0). For over USD 700.0, we prefer TT.
Valid time: 30 days
Producing Time:
For 24X5T &30*4T Widing (Standard axle), there are some motors in store, the lead time could be 2-3 working days after receiving payment.
For other winding, 10-12 working days after receiving payment(6 working days per week).
For Winding/kV list of 205 50H V3.

More QS Motor Informaiton:
Optional Appearance
Motor Details, drawing, performance curve (refer to attachment in PDF). For more information, please feel free to contact with us (pm or send email to vito@tzquanshun.com)
Inner View of Hub Motor (e.g. QS Motor 3000W 205 50H V3 Electric Bike Spoke Hub Motor)

For samples, "QSMOTOR" logo is laser print on side cover as default.
Meanwhile, the logo could be customized with below essential document.
· Please provide high definition logo in jpg format.
· Brand Letter of Authorization.
· Certificate of Trademark Registration
· Please advise the position & Size of your logo on side cover.
How to find suitable hub motor
To customized a suitable motor, could you pls. inform below points:
1.E-scooter, E-tricycle or E-car, tire model?
2.Volt and wattage of motor, Speed(kV), and torque/climb angle ?
3.Your vehicle weight and loading weight?
4.Lithium or lead-acid Battery?
We could suggest most suitable motor accordingly, thank you for your cooperation.
PS. To calculate the speed, v(km/h)=n(r/min)*2rπ(m)*60/1000, n=load RPM, r=tire radius.
For speed less than 100KPH, consider the Windage Resistance & Rolling resistance.
the load RPM is appr 0.9 * no-load RPM. v(km/h)=0.9*n(r/min)*2rπ(m)*60/1000
For over 100KPH, V=0.85*RPM*2rπ*60/1000
Electric Motor Kits
After confirming the motor, we could try to offer suitable motor kits, e.g. controller, wheel set, charger, speedometer,
throttle, brake, DC-DC converter, etc.
PS. So far, the battery is not avaiable.
Motor Controller
Item: Sabvoton SVMC/SSC Series Brushless Sinusoidal Programable Motor Controller
http://www.cnqsmotor.com/en/article_rea ... r/537.html
Item: Cheap BLDC controller, APT Programmable Sine Wave FOC AE96600 72V 96V 8kW PM Motor Driver Controller
http://www.cnqsmotor.com/en/article_rea ... r/332.html
Bluetooth intelligent anti-theft device by VOTOL
viewtopic.php?f=31&t=65972&p=1231911#p1231911
QS Motor V1/V2/V3 Type Motor
There are three types, Normal/V1 type (low cost), Export/V2 type (Cost-effective) and Extra/V3 type (Best Performance). 1. Difference between V1 & V2
Holder: Iron(V1), Aluminum (V2)
Hall: One hall with Normal connector(V1), Two halls with Waterproof connector(V2)
Stator: V2 have a stronger configuration, more cooper, thicker section surface, energy saving in usage.
Magnetic Steel Grade: V2 ≥ V1
Efficiency: 84~87%(V1) 86~88%(V2)
In short, normal type is standard configuration, while export type is high configuration.The price differs because of the cost of raw materials.
2. Difference between V2 & V3
The raw materials are alike, main difference in inner construction.
For V3 (16 Pole Pairs): stronger configuration than V2, wider lamination,
more cooper wire /thicker Cross-sectional area section, bear more current
in usage. Higher torque at same current, lower temperature rise, more stable in high current.
Magentic Steel: V3 is wider and thicker.
Efficiency: 86~88%(V2) 88~92%(V3); Thus, V3 have best performance.
PS. for the same V1 steel/iron stator motors, QS Motor performance better on lifetime & stability becasue of good raw material. So the cost is more than normal hub motor in the market.
E.g. 1. Choose C&U bearing which is motorcycle standard, more quiet when riding.
2. High Coil space factor, better efficiency.
3. Silicon steel sheet 0.35mm instead of 0.5mm, less current consumption & low temp rise.
4. Insulation varnish outside of varnished wire, max 180 ℃ than normal 120 ℃.
5. Better magnet, demagnetizing less than 1% than normal 3%.
QS Motor Steel Seal
We could laser print it on side cover or edge of side cover.
For V3 type motors(e.g. WP20040X140607 7355)
WP= V3 type 200=2000W, 300=3000W
40 means winding X means 32 pieces magnetic steel
140607 means producting date, 07th, June, 2014. 7355, is producing serial number
For V2 type motors(e.g. QSMOTOR 48V3000W 140720 604329)
48V3000W=48V 3000W 140720 means producing date, 20th, July, 2014.
60 means rated speed, 60km/h. 4329 is producing serial number.
P.S.: We define power base on rated output power, rather than peak output power.
How to make the order
·Before-sale, please advise which motor do you prefer, and advise above expected configuration of EV if possible.
After confirming motor, we could also advise suitable motor kits (e.g. controller).
It could be paid online, e.g. QS Motor Shop on alibaba, aliexpress;
We suggest to make the deal offline, we will make PI accordingly (latest price & accurate delivery cost).
·In-sale, we will informe you once received the payment to start the order & ETD.
Before delivery, we will send some pictures for reference.
·After-sale, Once got the tracking number, will informed you immediately.
Manual and software will be sent accordingly, also we will email you after the package delivered.
Payment Term
Wire Transfer/TT, Money Gram,Western Union, Paypal 100% in advance(for sample)
Generally, we perefer T/T, Money Gram,Western Union 100% in advance (for sample).
Meanwhile, we could also accpet paypal. There will be extra cost for transaction fee: Total cost*4.4%+0.3
Withdraw fee: USD 35.0 (We could bear USD 35.0).
For Mass Production, we support 30% T/T in advance + 70% T/T the balance before shipment.
Produce Time
For normal motors, e.g. e-scooter motor, e-motorcycle, it takes 10-12 business days (6 business per week).
For customzide motor & single shaft motor, it takes 15-16 business days.
In busy season, the order might be postponed. For mass production, the produce time will be increased accordingly.
PS. For the 3000W 205 50H V3 spoke hub motor, we made some 24*5T & 30*4T motor in store.
Package
Standard export packing 1. polyfoam + carton box (for sample) 2. Or according to customer's requirements
Life Time of QS Motor & Warranty of Sample
The Life Time of motor depends on usage.
For general usage, it's about 3-5 years, and it could be 5-7 years if it work in good condition.
For testing and abusing usage, the lifetime will decrease accordingly.
E.g., For 3kW V2/V3 motor, the peak power could be 6kW (2 times of rated power).
Situation 1:
We suggest peak 70-80A battery current for general usage (72V). It's most stable configuration & longest life time.
Some EV enthusiast adjust it to be 150A, the output power is far more than 6kW peak. QS Motor could also work,
which might not as stable as former situation. For a long time in high current/power, the motor might over heat & even burnt.
We strongly suggest to install Thermic Probe (e.g. KTY 83/122), so that controller will protect motor due to the temp inside of motor.
Situation 2:
The peak speed of 1pc 3kW motor is 80KPH in 72V(for e-scooter).
Some EV enthusiast adjust it to be 96V, the max speed might be 100KPH, the continuous output power is far more than 3kW rated (maybe equal to 5-6kW).
QS Motor could also work, which might not as stable as it in 72V.
We call it over voltage/abusing usage, the life time might be shorter, and V3 will work better than V2.
Warranty period: one year and three months (sincethe date of manufacture) or after riding 15000KM.
For Sample, If it's destructive test/abusing usage due to test purpose, we could not do aftersale issue for free.
If there is some damage during your test, which we could repair.
After checking your video or pictures, we could deliver some motor parts (e.g. hall sensor) for maintenance.
Also, you could deliver them back to our factory(I'm afraid that you have to bear delivery fee, both way),
We will make maintenance as possible as we could. For repair fee, we could bear the cost for 1 year.
QS Motor Manufacture
Certification: Business License, Patent Certificatie, ISO9001 Certificate,CCC Certificate, CE Certificate, Brand Certificate.

Application


No QS Motor, No Super EVs!
Thanks and best regards,
QS Motor- Vito Ho