JP spot welder

Place for dealers to post items for sale.
User avatar
riba2233   1 MW

1 MW
Posts: 1846
Joined: Jun 30 2013 10:23am
Location: Croatia

Re: JP spot welder

Post by riba2233 » Aug 10 2016 5:09am

Thanks, I'm also glad that you are satisfied with welder :)

I also want to thank you guys for being cooperative and not sending me PM's, I haven't received a single one while I was in hospital, thank you for understanding! 8)
My electric moped: http://www.evalbum.com/4966

My electric car: http://www.evalbum.com/5364

r3volved   100 kW

100 kW
Posts: 1452
Joined: Jul 24 2013 4:01pm
Location: Waterloo, Ontario, Canada

Re: JP spot welder

Post by r3volved » Aug 10 2016 7:19am

Welcome back! Glad to hear everything went well and you're on the road to recovery!

User avatar
bigbore   10 kW

10 kW
Posts: 524
Joined: Sep 25 2009 7:43am
Location: Italy

Re: JP spot welder

Post by bigbore » Aug 10 2016 8:47am

Great news riba!
I'm very satisfied with welder too but now the only thing that count is your health. ... than we will talk about your nice welder again :D

User avatar
arek_arecki   1 mW

1 mW
Posts: 14
Joined: Jun 15 2011 1:47pm
Location: Poland
Contact:

Re: JP spot welder

Post by arek_arecki » Aug 14 2016 5:56am

Very nice to hear that you're back to health.
I am also satisfied with the welding machine.

Sometimes it happens that the transistors shoot.
generally when the battery voltage drops below 12.5V
I use Yuasa 110Ah 900A + diode. Time set to 6-7ms nickel 0.18mm.
welding points are very good.
sometimes adheres to the positive electrode of nickel, the solution can be the use of molybdenum electrodes?

Image
Image
Image

I greet all users JP Spot
KARIWA, KARIWA LITE, KARIWA ECO, Teleport Prime, Ekross, Qulbix, ebike frame
Custom ebike, monster ebike
Battery pack Li-ion, BMS, connector, etc
email: info@cyklonebike.com, phone: +48516081337
:bolt: :flame: http://www.cyklonebike.com :flame: :bolt:
http://www.facebook.com/cyklonebike :thumb:
http://www.instagram.com/cyklonebike :thumb:

atarijedi   100 W

100 W
Posts: 239
Joined: Jul 18 2016 7:16am

Re: JP spot welder

Post by atarijedi » Aug 16 2016 3:38am

Here's hoping riba will post all the information, so we can make our own, maybe modify it to have the diode on the PCB. Do group runs to PCB manufacturers, etc...

ScooterMan101   1 MW

1 MW
Posts: 1902
Joined: Oct 06 2012 4:45pm
Location: South of San Jose, California.

Re: JP spot welder

Post by ScooterMan101 » Aug 23 2016 5:14pm

What has happened to this / to the builder-seller riba2233 ?

Is anyone selling the JP Spot Welder ?

if not,

Is there anyone in the U.S. ( North America ) selling one ?

and/or any plans on where to buy all the parts to build a spot welder ?

Thanks
My first conversion ... Sold

viewtopic.php?f=3&t=71378&p=1077497&hil ... 1#p1077497

It's 2018 already, ( now 2019 ) lets get some real , improved e-bike / e-velomobile / e-motorcycle designs .

User avatar
riba2233   1 MW

1 MW
Posts: 1846
Joined: Jun 30 2013 10:23am
Location: Croatia

Re: JP spot welder

Post by riba2233 » Aug 24 2016 12:59am

Hi, a lot has happened to me lol

As I wrote few posts back, I'm not making and selling them anymore.
My electric moped: http://www.evalbum.com/4966

My electric car: http://www.evalbum.com/5364

User avatar
Overclocker   10 kW

10 kW
Posts: 634
Joined: Mar 17 2014 5:48am
Location: Philippines

Re: JP spot welder

Post by Overclocker » Sep 05 2016 12:46am

Image

it welds CR2032 as well :mrgreen:

User avatar
Doctorbass   100 GW

100 GW
Posts: 7433
Joined: Apr 08 2007 2:24am
Location: Quebec, Canada East
Contact:

Re: JP spot welder

Post by Doctorbass » Sep 07 2016 11:20pm

riba2233 wrote:Hi, a lot has happened to me lol

As I wrote few posts back, I'm not making and selling them anymore.

Riba,

I have spent about 120 hours building my JP spotwelder in a beautifull and powerfull project.

I now need the PIC to repair mine that is blown.. i dont want to bother you with that but you seem to be teh only person to be able to help me.... My welder have been waiting months now and it is useless without the PIC.

Could you do me a favor and send me one or two spare i will PAY$$ what it require but i really need that! I have many project that i planed to use it for that are also waiting.

Personally i get alot of request from various people from all around the world every week and i spend hiours of time to help them. I very rarely ask for help but now i need it.

Thanks for your patience and understanding.

Doc
Attachments
20160620_211306 (Personnalisé).jpg
20160620_211306 (Personnalisé).jpg (134.89 KiB) Viewed 3494 times
20160508_002150 (Personnalisé).jpg
20160508_002150 (Personnalisé).jpg (165.1 KiB) Viewed 3494 times
20160420_233719 (Personnalisé).jpg
20160420_233719 (Personnalisé).jpg (158.87 KiB) Viewed 3494 times
CURRENT PROJECT: 2WD duo MXUS/Max-E ebike 32kW
http://endless-sphere.com/forums/viewto ... =3&t=65764
-Fastest speed record 117 km/h on flat
-Fastest 1/4 mile@ 114km/h on flat and 16.316 sec
-Succeded to haul a 19200 pounds schoolbus!
113kmh Gianthttp://www.evalbum.com/3406
Mongoosehttp://www.evalbum.com/1947
YOUTUBE---https://m.youtube.com/user/Doctorbasss
http://twitter.com/DocbassMelancon
I speak FRENCH and english

okashira   10 kW

10 kW
Posts: 957
Joined: Nov 17 2014 6:45pm
Location: Houston, TX

Re: JP spot welder

Post by okashira » Sep 08 2016 1:11am

I'm about to program two of these PIC's for a special project. If Riba can''t or he prefers, I can send you a programmed one
"Peace out - I'm done."
-- Bernhard Riemann, 1859

edisonmotors.net
Tesla Model S 18650 cells - like new - and custom packs from Tesla cells for sale. Any shape Any power Any capacity.
PM me or search my threads.

User avatar
riba2233   1 MW

1 MW
Posts: 1846
Joined: Jun 30 2013 10:23am
Location: Croatia

Re: JP spot welder

Post by riba2233 » Sep 08 2016 12:20pm

Yeah doc sorry for the wait, please just PM me your address and you'll get it soon :)
My electric moped: http://www.evalbum.com/4966

My electric car: http://www.evalbum.com/5364

User avatar
fechter   100 GW

100 GW
Posts: 14526
Joined: Dec 31 2006 3:23pm
Location: California Bay Area, USA

Re: JP spot welder

Post by fechter » Sep 08 2016 6:32pm

If you install a socket for the PIC, it will never blow :wink: Some kind of reverse Murphy's Law corollary.
"One test is worth a thousand opinions"

User avatar
riba2233   1 MW

1 MW
Posts: 1846
Joined: Jun 30 2013 10:23am
Location: Croatia

Re: JP spot welder

Post by riba2233 » Sep 09 2016 1:04am

Yeah, that's not far from true :)
My electric moped: http://www.evalbum.com/4966

My electric car: http://www.evalbum.com/5364

mudflap5   10 W

10 W
Posts: 90
Joined: Jul 28 2013 8:24am
Location: DFW Area Texas

Re: JP spot welder

Post by mudflap5 » Sep 09 2016 9:29am

Finally got my spot welder up and running!
Now it is an issue of electrodes. Bought a 709A and made welding leads using the 709A tips. Well, after a few hundred welds, they are done.
Any recommendations on new electrodes? Is there a source for the ones used on Riba's unit?
Would any of these work?

http://sunstoneengineering.com/products ... lectrodes/


Thanks.

User avatar
riba2233   1 MW

1 MW
Posts: 1846
Joined: Jun 30 2013 10:23am
Location: Croatia

Re: JP spot welder

Post by riba2233 » Sep 09 2016 9:35am

There is no source of my electrodes other than myself, they are custom engineered and made :) From raw parts. Sunstone electrodes will work, they are great, but very expensive (unreasonably, they must have extreme mark-up on them).
My electric moped: http://www.evalbum.com/4966

My electric car: http://www.evalbum.com/5364

mudflap5   10 W

10 W
Posts: 90
Joined: Jul 28 2013 8:24am
Location: DFW Area Texas

Re: JP spot welder

Post by mudflap5 » Sep 09 2016 3:39pm

Picked up some 4, 6, and 8 gauge solid ground wire from the electrical supply store today. Maybe I can make some electrodes out of that....

User avatar
riba2233   1 MW

1 MW
Posts: 1846
Joined: Jun 30 2013 10:23am
Location: Croatia

Re: JP spot welder

Post by riba2233 » Sep 10 2016 4:24am

You can yeah, my first electrodes were from 6 mm2 solid wire, and 10 mm2 solid wire (before I've switched to 5 mm solid copper bar).
My electric moped: http://www.evalbum.com/4966

My electric car: http://www.evalbum.com/5364

User avatar
ohzee   1 MW

1 MW
Posts: 1715
Joined: Jul 20 2011 1:13pm
Location: Columbus Ohio USA

Re: JP spot welder

Post by ohzee » Sep 10 2016 9:39am

Glad to hear riba you are out and doing well.

User avatar
Doctorbass   100 GW

100 GW
Posts: 7433
Joined: Apr 08 2007 2:24am
Location: Quebec, Canada East
Contact:

Re: JP spot welder

Post by Doctorbass » Sep 12 2016 12:01pm

riba2233 wrote:Yeah doc sorry for the wait, please just PM me your address and you'll get it soon :)

Thanks all for your help offer :mrgreen: , I will contact Riba.
CURRENT PROJECT: 2WD duo MXUS/Max-E ebike 32kW
http://endless-sphere.com/forums/viewto ... =3&t=65764
-Fastest speed record 117 km/h on flat
-Fastest 1/4 mile@ 114km/h on flat and 16.316 sec
-Succeded to haul a 19200 pounds schoolbus!
113kmh Gianthttp://www.evalbum.com/3406
Mongoosehttp://www.evalbum.com/1947
YOUTUBE---https://m.youtube.com/user/Doctorbasss
http://twitter.com/DocbassMelancon
I speak FRENCH and english

User avatar
Offroader   10 MW

10 MW
Posts: 2479
Joined: Sep 08 2013 9:03pm
Location: USA

Re: JP spot welder

Post by Offroader » Oct 31 2016 11:48pm

Hi Riba,

Are you 100% absolutely done with selling welders?

markz   100 GW

100 GW
Posts: 7939
Joined: Jan 09 2014 11:38pm
Location: Alberta Canada

Re: JP spot welder

Post by markz » Nov 01 2016 12:30am

Ya I'd need the programmed chip atleast.

User avatar
riba2233   1 MW

1 MW
Posts: 1846
Joined: Jun 30 2013 10:23am
Location: Croatia

Re: JP spot welder

Post by riba2233 » Nov 01 2016 2:57am

Offroader wrote:Hi Riba,

Are you 100% absolutely done with selling welders?
Hi, I have something coming up, you'll be notified once I make a decision :)

markz wrote:Ya I'd need the programmed chip atleast.
Yeah sorry I wont be selling that.
My electric moped: http://www.evalbum.com/4966

My electric car: http://www.evalbum.com/5364

liamcaff   1 kW

1 kW
Posts: 418
Joined: Feb 17 2013 6:21pm
Location: Dublin

Re: JP spot welder

Post by liamcaff » Nov 01 2016 6:46am

Am interested in your decision too :)

User avatar
riba2233   1 MW

1 MW
Posts: 1846
Joined: Jun 30 2013 10:23am
Location: Croatia

Re: JP spot welder

Post by riba2233 » Nov 01 2016 7:15am

Ok, just please be patient and don't ask me when it's going to happen, because I don't know at this moment! :)
My electric moped: http://www.evalbum.com/4966

My electric car: http://www.evalbum.com/5364

User avatar
fechter   100 GW

100 GW
Posts: 14526
Joined: Dec 31 2006 3:23pm
Location: California Bay Area, USA

Re: JP spot welder

Post by fechter » Nov 01 2016 8:06am

I'm interested too.

A while back I suggested the idea of licensing the design to somebody who wants to build and sell the boards and cut riba2233 in for a percentage of the profit. Even better if we can find people on both sides of the ocean.
"One test is worth a thousand opinions"

Post Reply