Post by Animalector » Dec 03 2019 4:13pm

are you using a throttle? is it speed limited?

I'm interested to know if it's a failure because it pushing the limits or if it is just a failure.

Thanks

Map Paddy   10 mW

10 mW
Posts: 30
Joined: Oct 07 2018 4:30pm

Re: FREY eMTB with Bafang m600 is developing with your ideas!

Post by Map Paddy » Dec 03 2019 6:53pm

I was riding on a trail bike switched off Screen flashed when I restarted it then nothing had to push and wheel bike for about an hour back to where I parked my van its hilly but wasn't been overly aggressive ,so annoying was loving the bike

Map Paddy   10 mW

10 mW
Posts: 30
Joined: Oct 07 2018 4:30pm

Re: FREY eMTB with Bafang m600 is developing with your ideas!

Post by Map Paddy » Dec 03 2019 6:55pm

Normal riding in the hills no throttle 160 pound rider.i will update with there solution I still have hope never a problem with my ht 1000 other than hub which they replaced

Map Paddy   10 mW

10 mW
Posts: 30
Joined: Oct 07 2018 4:30pm

Re: FREY eMTB with Bafang m600 is developing with your ideas!

Post by Map Paddy » Feb 03 2020 12:50am

They replaced motor controller failed had to send old one back fair play to them