kWeld from Keenlab now available in the US

Place for dealers to post items for sale.
Hummina Shadeeba   100 MW

100 MW
Posts: 2601
Joined: Apr 25 2014 10:26pm
Location: sausalito cali..up the hill in front of the cruising club.

Re: kWeld from Keenlab now available in the US

Post by Hummina Shadeeba » Feb 02 2021 10:48am

spinningmagnets wrote:
Aug 10 2019 11:11am
Keith at "18650 Heat Shrink & Cell Holders, Inc"

The purchase website can be found here
https://www.facebook.com/18650Shrink/?e ... L0ZuGIkhgW


The forum can be found here
https://www.facebook.com/groups/KWeldNorthAmerica/
I don’t see where to buy. I ordered from Germany by mistake, should I cancel and reorder from u?

User avatar
spinningmagnets   100 GW

100 GW
Posts: 11870
Joined: Dec 21 2007 10:27pm
Location: Ft Riley, NE Kansas

Re: kWeld from Keenlab now available in the US

Post by spinningmagnets » Feb 02 2021 11:11am

Contact Keith at his Facebook page. Ask him. He might be able to ship one and cancel the order from Germany.

Hummina Shadeeba   100 MW

100 MW
Posts: 2601
Joined: Apr 25 2014 10:26pm
Location: sausalito cali..up the hill in front of the cruising club.

Re: kWeld from Keenlab now available in the US

Post by Hummina Shadeeba » Feb 02 2021 7:58pm

aha i see they have a forum thanks for the link!!!



anyone know where i can get one of these or another welder that can do .2mm copper while i figure out how to fix mine?
Last edited by Hummina Shadeeba on Feb 02 2021 9:51pm, edited 1 time in total.

User avatar
tatus1969   1 kW

1 kW
Posts: 350
Joined: Mar 17 2017 7:36am
Location: Germany
Contact:

Re: kWeld from Keenlab now available in the US

Post by tatus1969 » Feb 03 2021 3:34am

spinningmagnets wrote:
Feb 02 2021 11:11am
Contact Keith at his Facebook page. Ask him. He might be able to ship one and cancel the order from Germany.
No problem, just tell me your keenlab order number and I'll cancel+refund. Just important to mention, both me and all my resellers are out of stock at the moment. That's all your fault because you're all ordering quicker than I can resupply. Just kidding :-) I'm expecting replenishment this week.
Resistance is futile - We Are The Watt.

Hummina Shadeeba   100 MW

100 MW
Posts: 2601
Joined: Apr 25 2014 10:26pm
Location: sausalito cali..up the hill in front of the cruising club.

Re: kWeld from Keenlab now available in the US

Post by Hummina Shadeeba » Feb 03 2021 11:02am

tatus1969 wrote:
Feb 03 2021 3:34am
spinningmagnets wrote:
Feb 02 2021 11:11am
Contact Keith at his Facebook page. Ask him. He might be able to ship one and cancel the order from Germany.
No problem, just tell me your keenlab order number and I'll cancel+refund. Just important to mention, both me and all my resellers are out of stock at the moment. That's all your fault because you're all ordering quicker than I can resupply. Just kidding :-) I'm expecting replenishment this week.
I’ll email u. I found one I can use so not in a rush anymore and will wait for them to get to USA instead of paying shipping from Germany which seems like 40$ more. Thanks.

User avatar
amberwolf   100 GW

100 GW
Posts: 31693
Joined: Aug 17 2009 6:43am
Location: Phoenix, AZ, USA, Earth, Sol, Local Bubble, Orion Arm, Milky Way, Local Group
Contact:

Re: kWeld from Keenlab now available in the US

Post by amberwolf » Feb 07 2021 1:45am

spinningmagnets wrote:
Nov 16 2018 8:24am
A 3D printing file of an electrode holder is available and free to use, designed by Shannon Williams. The probes in the picture below are the stock probes from keenlab in Germany.

https://secondlifestorage.com/t-Easy-to ... sing-files


kWeldHolder1.png
The picture has vamoosed...can you reupload it?