Post by x.l.r.8 » Feb 22 2018 12:45am

Okay, I have a tesla roadster that has the well documented PEM failure
The answer seems to be replacement of the thermal layer under the IGBT's
https://teslamotorsclub.com/tmc/threads ... ure.88028/
But there is little conclusion as to what that may be.
I'm hoping the collective minds would have a good idea as to what would be a good replacement
Aluminium Nitrate is an expensive 'hope it works' material
Aluminium oxide seems way to brittle for long term results.
Paste seems to either crumble and loose its electrical conductive properties.
Any ideas??
Intelligence is distributed nearly evenly, with only the occasional concentration in one person. The total quantity of Intelligence is a constant: as more people come into being, fewer and fewer get a sufficient amount for themselves.
Some say this has already reached homeopathic levels.

Buk___   10 kW

10 kW
Posts: 750
Joined: Jul 28 2017 5:59pm

Re: Tesla PEM heat sink material required

Post by Buk___ » Feb 22 2018 1:36am

x.l.r.8 wrote:
Feb 22 2018 12:45am
Okay, I have a tesla roadster that has the well documented PEM failure
The answer seems to be replacement of the thermal layer under the IGBT's
https://teslamotorsclub.com/tmc/threads ... ure.88028/
But there is little conclusion as to what that may be.
I'm hoping the collective minds would have a good idea as to what would be a good replacement
Aluminium Nitrate is an expensive 'hope it works' material
Aluminium oxide seems way to brittle for long term results.
Paste seems to either crumble and loose its electrical conductive properties.
Any ideas??
With no opinion on its suitability for your application, here is a product I've been considering for an entirely different purpose that might be suitable: Flexible Thermally Conductive Adhesive Electrically Insulating Epoxy Low Thermal Expansion ....

Please note: I highly recommend that you do your own research, perhaps contact the vendor and ask, and arrive at your own judgement as to suitability.

Hillhater   100 GW

100 GW
Posts: 10531
Joined: Aug 03 2010 10:33pm
Location: Sydney ..(Hilly part !) .. Australia/ Down under !

Re: Tesla PEM heat sink material required

Post by Hillhater » Feb 22 2018 8:27pm

Is this an issue confined solely to the Roadster PEM for some unique combination of material and component choice ?
If it is common as it appears from that forum, I would have thought Tesla would be all over this with a upgrade program before they end up with a fleet of static cars !
This forum owes its existence to Justin of ebikes.ca

User avatar
x.l.r.8   100 W

100 W
Posts: 117
Joined: Jul 30 2017 12:13pm
Location: Toronto and Cambridge

Re: Tesla PEM heat sink material required

Post by x.l.r.8 » Feb 23 2018 3:41am

The problem appears around 40,000 or 5 years. The answer is a remanufactured PEM at $10,000 that has a 3 year warranty. They simply replace the compound. The goal for them it seems is to get people to upgrade to the 3.0 battery pack with an upgraded PEM that uses better quality IGBT’s. If a solution can be found that is cost effective and lasts at least 3 years I would be more than happy to do it, but you seem to get one chance at repair, the solid plates allow the IGBT’s to short and then you need to start replacing them. The compound seems to not last very long causing a lot of heat damage. Something with the same thermal properties that is an elastic or a gel may do well. The better heat transfer the better for the components. There is enough problems keeping the exterior cooling system working without having to worry to much about the inside of it.
Intelligence is distributed nearly evenly, with only the occasional concentration in one person. The total quantity of Intelligence is a constant: as more people come into being, fewer and fewer get a sufficient amount for themselves.
Some say this has already reached homeopathic levels.