Re: Watt meter connected to E-skateboard.

Post by buzztiaan » Jun 18 2015 2:47am

FYI on SLA , you get less than original capacity if you discharge above ~0.1C, which i guess you are doing?
HK150 - 5055 SK3 280kv - 6S 5000mAh - 90mm bigfoots
https://nurdspace.nl/RobertLongboard

User avatar
bandaro   10 kW

10 kW
Posts: 526
Joined: Jun 01 2010 2:17am
Location: Canberra, Australia

Re: Watt meter connected to E-skateboard.

Post by bandaro » Jun 18 2015 6:26am

I had my solid state relay burn out so connected my watt meter (pictured) in line to replace the length the relay took, and haven't yet had a chance to test different settings and their effect on the draw, but I'm making about 1600 watts, and burning through about 15wh/km (25/mile), so not a great efficiency compared to some of you guys! Also running dual motors (custom 42mm ones) on 6s. I'm not getting to full power as the motor starts screeching something horrible about 3/4 throttle and on brake. Not sure why, but trying to fix it so if anyone has clues...

T-wattmeter.jpg
T-wattmeter.jpg (95.26 KiB) Viewed 491 times

FVT esc, and the timing is on 'high'. Any lower and the throttle would cut out and coast at higher unput levels, this setting is the lowest that still gives me full range. Haven't had heat problem yet either.

Barndom   10 W

10 W
Posts: 95
Joined: Jul 11 2013 6:24am
Location: Sweden

Re: Watt meter connected to E-skateboard.

Post by Barndom » Jun 18 2015 9:53am

buzztiaan wrote:FYI on SLA , you get less than original capacity if you discharge above ~0.1C, which i guess you are doing?
Yes, the more you load it the less the capacity. I top out at 5C and use 1C on everage. Of the 7 Ah i get out about 4 to 5 Ah wich was more than I expected.

User avatar
buzztiaan   1 W

1 W
Posts: 52
Joined: Mar 09 2015 4:57am
Location: Netherlands

Re: Watt meter connected to E-skateboard.

Post by buzztiaan » Jun 18 2015 12:18pm

Oh yeah, that is a lot more than expected! I wasn't so lucky with trying out SLA's..