If I wanted to put two of these batteries in parallel should i use an XT90 Y harness or an XT60 Y harness?
http://www.ebay.com/itm/281865122600

User avatar
millzy555   100 W

100 W
Posts: 175
Joined: Aug 14 2011 9:48pm
Location: Melbourne, Victoria, Australia

Re: Parallel Harness

Post by millzy555 » Apr 07 2016 1:59am

How many amps you pulling?

saul   1 W

1 W
Posts: 64
Joined: Apr 02 2015 12:46am
Location: Los Angeles, CA

Re: Parallel Harness

Post by saul » Apr 07 2016 3:04am

that battery has a xt60, but i would use a xt90 with it for an anitspark key.

also get those batteries straight from hobbyking, half price! but i would look at the 8 or 10 ah packs, about the same price, but thinner and of course more capacity.
Builds:
97mm Fly wheels + tiny 85kv + 12s Vesc
https://endless-sphere.com/forums/viewt ... 35&t=76450

more to come...

nowind   100 W

100 W
Posts: 160
Joined: Nov 10 2014 2:52am

Re: Parallel Harness

Post by nowind » Apr 08 2016 12:05am

Hey.

The linked batteries are crap... Go with something with higher C Rating

I would use XT90 Connectors too.

Greetz

bbcane78   1 W

1 W
Posts: 55
Joined: Nov 06 2015 6:24pm

Re: Parallel Harness

Post by bbcane78 » Apr 11 2016 4:55am

nowind wrote:Hey.

The linked batteries are crap... Go with something with higher C Rating

I would use XT90 Connectors too.

Greetz
If i wanted to use two 9s batteries in parallel would i need XT90s? The batteries would be 3 3S1P in series with 20-30C output.

User avatar
izeman   100 GW

100 GW
Posts: 5048
Joined: Jun 21 2011 8:25am
Location: Vienna, Austria
Contact:

Re: Parallel Harness

Post by izeman » Apr 11 2016 5:01am

XT60 can do 60A for a long time - my personal experience. They are much smaller if space is an issue. If not, xt90 is always nice and you can get them with anti spark resistor included.
The batteries are ok if you don't need to pull too many amps. Saying they are crap generally is bs. It depends on your power needs and on how many you want to put in parallel.

bbcane78   1 W

1 W
Posts: 55
Joined: Nov 06 2015 6:24pm

Re: Parallel Harness

Post by bbcane78 » Apr 12 2016 3:08pm

izeman wrote:XT60 can do 60A for a long time - my personal experience. They are much smaller if space is an issue. If not, xt90 is always nice and you can get them with anti spark resistor included.
The batteries are ok if you don't need to pull too many amps. Saying they are crap generally is bs. It depends on your power needs and on how many you want to put in parallel.
If I setup those in batteries in parallel I would have 20-30C for 10000mAh, so I would be pulling 200-300A right? Is the VESC able to handle this or am i thinking about this wrong? I dont want to do this and end up screwing my board up. Even with the XT90 connectors for parallel, it would go to my watt meter and VESC which both have XT60s.

torqueboards   100 MW

100 MW
Posts: 2940
Joined: May 27 2013 10:02pm
Location: San Francisco, CA
Contact:

Re: Parallel Harness

Post by torqueboards » Apr 12 2016 3:12pm

Technically, you can pull 20-30C but the rating is never the actual rating.. Besides, we don't use that much power anyways. You'd knock yourself off.

Typically, we only use about 10-80amps.

VESC can be limited by current per motor which is usually about 50-60amps.

XT90's are fine if you want more durability. XT60's will work too and are capable of higher than 60amps.

The reason to go bigger I suppose is due to having a bigger output. I always prefer bigger as well.
DIYElectricSkateboard.com Electric Skateboard Kits

nowind   100 W

100 W
Posts: 160
Joined: Nov 10 2014 2:52am

Re: Parallel Harness

Post by nowind » Apr 13 2016 12:16am

izeman wrote:XT60 can do 60A for a long time - my personal experience. They are much smaller if space is an issue. If not, xt90 is always nice and you can get them with anti spark resistor included.
The batteries are ok if you don't need to pull too many amps. Saying they are crap generally is bs. It depends on your power needs and on how many you want to put in parallel.