Was given this broken scooter to fix up and sell, but as I put more work into it I think I'm better off keeping compared to what I could possibly sell it for.
Image

The batteries were shot of course, but I just happened to have a pair of unused 12V 9Ah SLA batteries laying around to get it going. Front inner tube needed to be patched, the battery harness needed the wires replaced, still needs a charger port and probably a kickstand (I'm 22 and having to lean it up is bothering me, can't imagine what a possible parent buying the thing would think about that).

The chain was making an awful noise (even after lubricating it), turns out the rear sprocket was bent pretty bad. Took a few hours of swearing but eventually I got that stupid thing off the wheel.
Image

So I'll start off with getting a freewheel and slightly smaller sprocket for the rear wheel, plus a new chain, just to get it going again.

Future stuff will be lithium-ion batteries (duh), different motor and controller, and maybe disc brakes. I don't intend to make a rocketship here, just a little something to get around town in other than my car.

MWisBest   1 µW

1 µW
Posts: 4
Joined: May 08 2018 1:06pm

Re: Currie IZIP I-500-CD Project

Post by MWisBest » May 18 2018 12:38pm

Got my parts in yesterday!

Image Image

Scooter is whisper quiet now, night and day difference. I had to put a couple washers between the wheel sprocket and the freewheel to get the correct alignment with the motor sprocket, but other than that it went together pretty good. BTW, for anybody installing something onto these threaded wheel hubs, I highly recommend putting some anti-seize on there. Good luck removing it later if you don't.

User avatar
fechter   100 GW

100 GW
Posts: 13302
Joined: Dec 31 2006 3:23pm
Location: California Bay Area, USA

Re: Currie IZIP I-500-CD Project

Post by fechter » May 18 2018 2:18pm

Nice work. Now you need to update the batteries with some lithium cells.
"One test is worth a thousand opinions"

MWisBest   1 µW

1 µW
Posts: 4
Joined: May 08 2018 1:06pm

Re: Currie IZIP I-500-CD Project

Post by MWisBest » May 18 2018 6:22pm

fechter wrote:
May 18 2018 2:18pm
Nice work. Now you need to update the batteries with some lithium cells.
Thanks! Yeah it definitely needs lithium batteries, but I'll have to save up for a while to buy them. Got other more important things to pay for!

MWisBest   1 µW

1 µW
Posts: 4
Joined: May 08 2018 1:06pm

Re: Currie IZIP I-500-CD Project

Post by MWisBest » May 24 2018 9:19am

I didn't like the power wiring on the scooter very much, so I kinda redid it. I have a bit of a wiring fetish so this is kinda overkill, but having 12 AWG wire fused at 40A was kinda ridiculous I think.

Got some goodies from Littelfuse to try out:
Image

That's a MAXI fuse holder, an inline low-profile JCASE fuse holder with 8 AWG leads, and some extra fuses. The MAXI fuse is available in a 58V version (although I could only get samples of the 32V fuse, which is fine for now at least). The LP JCASE fuse is rated to 58V as well. ATO fuses (like what the scooter used stock) are only rated to 32V, so again another sketchy thing with the stock wiring since I assume they use that on the 36V scooters too...

12 oz can for size reference on the MAXI fuse holder, thing's huge!
Image

Decided to go with the MAXI fuse holder as the controller fuse, and it's going to double as an on/off switch, rather than the sketchy "DPST switch in parallel for double the current handling" thing.

8 AWG wires crimped to the included connectors:
Image

All put together. Quite the ignition key! Lol.
Image

This is how it all mounts. The power wires come in and out through what used to be the charger port cutout, with a grommet added so they seal up and don't cut on the metal. The fuse holder is attached to a rubber plug that fit into the switch cutout well enough. I'll go around this all with silicone when I'm satisfied it's all good.
Image

So now I just gotta get this connected to the battery and the controller and I'll be good to go.

Surfingjeff   10 W

10 W
Posts: 81
Joined: Feb 27 2018 11:43pm
Location: San Diego

Re: Currie IZIP I-500-CD Project

Post by Surfingjeff » Jul 19 2018 10:58pm

I’ve modified Schwinns and Lashouts and I noticed your trying to add disc brakes . My suggestion would be to pick up some available machined parts from EV deals . I sent protypes to Scott there and now you can buy them cheap these will allow you to add the discs .
Attachments
scooter.JPG
scooter.JPG (107.97 KiB) Viewed 302 times
scooter adapter.jpg
scooter adapter.jpg (102.67 KiB) Viewed 302 times
scooter rear.jpg
scooter rear.jpg (137.16 KiB) Viewed 302 times
avid and adapter.jpg
avid and adapter.jpg (71.43 KiB) Viewed 302 times

Surfingjeff   10 W

10 W
Posts: 81
Joined: Feb 27 2018 11:43pm
Location: San Diego

Re: Currie IZIP I-500-CD Project

Post by Surfingjeff » Jul 19 2018 11:27pm

Also you mentioned you needed parts kick stands, I also have custom battery trays for your scooter . If you need them let me know. Just cover the freight and handling its yours. just show them on a post so I know they are being used for your project.
schwinn parts.jpg
schwinn parts.jpg (63.74 KiB) Viewed 302 times

Post Reply