I am working on a project to 3D print a large EDF (electric ducted fan). Currently there are no specific applications but I have VTOL in mind. That's why it is large for better disc loading and the pitch is low for better static performance. However changing the blades to a higher pitch for forward flight is a simple task.

I use 3D printing (FDM PETG) in order to lower costs because an EDF this large would cost many thousands to machine out of aluminium or make out of carbon fibre. An aim of this project is simply to show it's feasibility because it is popularly thought that a 3D printed EDF this large would simply explode.

It has a gearbox in order to further reduce costs by enabling the use of a cheap, off-the-shelf inrunner instead of an expensive, custom wound low Kv inrunner or a bulky and heavy outrunner. Originally the gearbox was also 3D printed but I had to abandon that and now it is machined out of steel.

Image

Image

Image



Here are videos of the performance so far (all thrust is recorded in kilograms).






User avatar
charlesmcnall   1 mW

1 mW
Posts: 17
Joined: Jul 12 2016 1:05pm
Location: SLC, UT

Re: 3D printed 400mm EDF project

Post by charlesmcnall » May 26 2021 11:24am

Well I'll reply back. This is awesome. great job.
Could you put into the text the performance you have seen so far?
It's harder for me to tease out the values on the gauges at work with no headphones.
Electric Ninja 250 http://evalbum.com/preview.php?vid=5243
Lemond Etape 1400W hub motor 48V 15ah - need to make EValbum
6hp Electric snowblower conversion http://evalbum.com/preview.php?vid=5250

SlowCo   1 MW

1 MW
Posts: 1986
Joined: Jan 05 2015 5:43pm
Location: The Netherlands

Re: 3D printed 400mm EDF project

Post by SlowCo » May 26 2021 2:06pm

Nice project :thumb:

Jordan325ic   10 W

10 W
Posts: 81
Joined: Aug 05 2020 6:44am

Re: 3D printed 400mm EDF project

Post by Jordan325ic » May 27 2021 7:19am

400mm! I know nothing about turbines but they do look good. Great work, what printer are you using and how many parts are in that build as shown?

SkyersJet   1 mW

1 mW
Posts: 19
Joined: May 11 2021 2:41pm

Re: 3D printed 400mm EDF project

Post by SkyersJet » May 28 2021 10:08pm

charlesmcnall wrote:
May 26 2021 11:24am
Well I'll reply back. This is awesome. great job.
Could you put into the text the performance you have seen so far?
It's harder for me to tease out the values on the gauges at work with no headphones.
Hi, thanks for your interest! All of the data is summarised at the end of my videos. In the first video (thrust test 6) I recorded 20kg thrust at 7712W. In the second video (thrust test 8 ) I recorded 18.7kg @ 7471W. NB: Different scales were used for both tests + I think that the batteries were sagging by the time I switched scales so I don't know which result is more valid.
Last edited by SkyersJet on May 28 2021 10:12pm, edited 1 time in total.

SkyersJet   1 mW

1 mW
Posts: 19
Joined: May 11 2021 2:41pm

Re: 3D printed 400mm EDF project

Post by SkyersJet » May 28 2021 10:12pm

Jordan325ic wrote:
May 27 2021 7:19am
400mm! I know nothing about turbines but they do look good. Great work, what printer are you using and how many parts are in that build as shown?
Hi thank you! I use a Creality CR-20 printer to print the parts in PETG. There are 62 parts in the build.

Jordan325ic   10 W

10 W
Posts: 81
Joined: Aug 05 2020 6:44am

Re: 3D printed 400mm EDF project

Post by Jordan325ic » May 29 2021 8:49am

SkyersJet wrote:
May 28 2021 10:12pm
Jordan325ic wrote:
May 27 2021 7:19am
400mm! I know nothing about turbines but they do look good. Great work, what printer are you using and how many parts are in that build as shown?
Hi thank you! I use a Creality CR-20 printer to print the parts in PETG. There are 62 parts in the build.
How do you like that printer?
I assume the impeller blades are all printed as one piece, so the limiting factor is the 220x220 build plate?
What methos did you use to bond the petg parts together?

SkyersJet   1 mW

1 mW
Posts: 19
Joined: May 11 2021 2:41pm

Re: 3D printed 400mm EDF project

Post by SkyersJet » May 29 2021 9:04am

Jordan325ic wrote:
May 29 2021 8:49am
SkyersJet wrote:
May 28 2021 10:12pm
Jordan325ic wrote:
May 27 2021 7:19am
400mm! I know nothing about turbines but they do look good. Great work, what printer are you using and how many parts are in that build as shown?
Hi thank you! I use a Creality CR-20 printer to print the parts in PETG. There are 62 parts in the build.
How do you like that printer?
I assume the impeller blades are all printed as one piece, so the limiting factor is the 220x220 build plate?
What methos did you use to bond the petg parts together?
I love it. I don't know why it wasn't more popular than the Ender 3. It is not much more expensive while being far easier to assemble and is an all round better printer. Yes the print bed size is the only limiting factor. Most of the parts are screwed together except the intake ring which is glued together to save weight.

User avatar
spinningmagnets   100 GW

100 GW
Posts: 12560
Joined: Dec 21 2007 10:27pm
Location: Ft Riley, NE Kansas

Re: 3D printed 400mm EDF project

Post by spinningmagnets » May 29 2021 11:36am

Here is a pic of a "segmented" stator, which allows each stator-tooth to be wound individually before the stator is assembled, which can increase copper-fill, and the speed at which robotic assemblers can wind the coils.

Image

I really like how you made a much larger assembly from segmented parts. This kind of thinking allows smaller and more affordable 3D printers to be used for a much broader scope of products. I also don't like the tunnel-vision some builders who are new to 3D printing, and they want to make 100% of a product out of plastic in one single print. I am a fan of combining multiple materials, such as laser-cut / water-jetted metal plates as reinforcement (aluminum, stainless steel, etc). Several 3D parts can be wrapped in fiberglass/carbon fiber cloth. An assembly os smaller parts can be sized so that the completed assembly can fit inside a section of large-diameter PVC pipe, etc...

Beautiful work.

SkyersJet   1 mW

1 mW
Posts: 19
Joined: May 11 2021 2:41pm

Re: 3D printed 400mm EDF project

Post by SkyersJet » Jul 28 2021 11:01am

spinningmagnets wrote:
May 29 2021 11:36am
Here is a pic of a "segmented" stator, which allows each stator-tooth to be wound individually before the stator is assembled, which can increase copper-fill, and the speed at which robotic assemblers can wind the coils.

Image

I really like how you made a much larger assembly from segmented parts. This kind of thinking allows smaller and more affordable 3D printers to be used for a much broader scope of products. I also don't like the tunnel-vision some builders who are new to 3D printing, and they want to make 100% of a product out of plastic in one single print. I am a fan of combining multiple materials, such as laser-cut / water-jetted metal plates as reinforcement (aluminum, stainless steel, etc). Several 3D parts can be wrapped in fiberglass/carbon fiber cloth. An assembly os smaller parts can be sized so that the completed assembly can fit inside a section of large-diameter PVC pipe, etc...

Beautiful work.
Hi, thank you. Yes it's faster to print this way as well in addition to not needing expensive large volume printers.

SkyersJet   1 mW

1 mW
Posts: 19
Joined: May 11 2021 2:41pm

Re: 3D printed 400mm EDF project

Post by SkyersJet » Jul 28 2021 11:03am

It needs some more work before I can put it on an EV.

User avatar
fechter   100 GW

100 GW
Posts: 15599
Joined: Dec 31 2006 3:23pm
Location: California Bay Area, USA

Re: 3D printed 400mm EDF project

Post by fechter » Jul 28 2021 2:15pm

Too bad it exploded. But great that you got it on video! I'm very impressed anyway. Now you just need stronger material. Knowing at what point it blows up is pretty important if you want to fly with it. You also need some safety factor for bugs, hail, small birds, etc.

What if you printed a mold and used that to mold some carbon fiber?
"One test is worth a thousand opinions"

User avatar
nicobie   1 GW

1 GW
Posts: 3425
Joined: Aug 07 2008 1:48pm
Location: Central Coast CA, USA

Re: 3D printed 400mm EDF project

Post by nicobie » Jul 28 2021 2:30pm

People are starting to use 3D printers to make molds for pouring aluminum using a lost plastic process. However it would probably be a nightmare balancing the finished product.
Ask for it by name.

my eTownie build thread: http://endless-sphere.com/forums/viewto ... =6&t=23701
Magazine article https://www.electricbike.com/nicks-etownie/

Grantmac   10 kW

10 kW
Posts: 888
Joined: Oct 22 2018 12:43pm
Location: Victoria, BC

Re: 3D printed 400mm EDF project

Post by Grantmac » Jul 28 2021 2:47pm

Continuous fiber filament printing I believe can produce parts with almost the strength of aluminum now. Prices are coming way down too.

SkyersJet   1 mW

1 mW
Posts: 19
Joined: May 11 2021 2:41pm

Re: 3D printed 400mm EDF project

Post by SkyersJet » Jul 28 2021 6:13pm

I think 3D printed blades can work so long as I stop them from hitting the duct wall.

User avatar
nicobie   1 GW

1 GW
Posts: 3425
Joined: Aug 07 2008 1:48pm
Location: Central Coast CA, USA

Re: 3D printed 400mm EDF project

Post by nicobie » Jul 28 2021 6:21pm

Grantmac wrote:
Jul 28 2021 2:47pm
Continuous fiber filament printing
Now that sounds interesting. I didn't know that they did continuous fiber. All I knew about was the infused fiber filament.

It would take a hell of a slicer to do the g code for continuous fiber to get the fiber located in the proper place for maximum strength.
Ask for it by name.

my eTownie build thread: http://endless-sphere.com/forums/viewto ... =6&t=23701
Magazine article https://www.electricbike.com/nicks-etownie/

User avatar
stan.distortion   1 kW

1 kW
Posts: 308
Joined: Jun 12 2019 12:53pm

Re: 3D printed 400mm EDF project

Post by stan.distortion » Jul 28 2021 6:55pm

nicobie wrote:
Jul 28 2021 6:21pm
Grantmac wrote:
Jul 28 2021 2:47pm
Continuous fiber filament printing
Now that sounds interesting. I didn't know that they did continuous fiber. All I knew about was the infused fiber filament.

It would take a hell of a slicer to do the g code for continuous fiber to get the fiber located in the proper place for maximum strength.
Next wave of 3d printer tech but its big benefits might be out of the reach to hobbyists on anything but a really small scale, being able to weave thousands of strands simultaneously in a tightly controlled environment would beat any alternative process for strength to weight. Yep, one hell of a slicer!
Projects indirectly sponsored by https://www.dash.org/

Grantmac   10 kW

10 kW
Posts: 888
Joined: Oct 22 2018 12:43pm
Location: Victoria, BC

Re: 3D printed 400mm EDF project

Post by Grantmac » Jul 28 2021 7:45pm


SkyersJet   1 mW

1 mW
Posts: 19
Joined: May 11 2021 2:41pm

Re: 3D printed 400mm EDF project

Post by SkyersJet » Jul 29 2021 9:06am

Grantmac wrote:
Jul 28 2021 7:45pm
https://markforged.com/3d-printers/mark ... NQQAvD_BwE

It's almost hobby level now.
Don't those things cost £10k?

Grantmac   10 kW

10 kW
Posts: 888
Joined: Oct 22 2018 12:43pm
Location: Victoria, BC

Re: 3D printed 400mm EDF project

Post by Grantmac » Jul 29 2021 10:31am

SkyersJet wrote:
Jul 29 2021 9:06am
Grantmac wrote:
Jul 28 2021 7:45pm
https://markforged.com/3d-printers/mark ... NQQAvD_BwE

It's almost hobby level now.
Don't those things cost £10k?
Yes. But compare that with getting the tools to machine 6061 or to produce carbon fiber parts in the traditional way, costs are similar or a bit less.

User avatar
stan.distortion   1 kW

1 kW
Posts: 308
Joined: Jun 12 2019 12:53pm

Re: 3D printed 400mm EDF project

Post by stan.distortion » Jul 29 2021 5:03pm

Slicer software alone (or weaver software?) could justifiably cost 100 times that, it would be possible to design in far more than simple strength. How an object deforms for example, build a crumple zone into perfectly straight and even tube or modify its heat pathways, all sorts beyond aligning with stresses. $10k to get hands on experience is a bargain, not an easy reach for most but well within the reach of schools and collages.
Projects indirectly sponsored by https://www.dash.org/

User avatar
Greendog   100 W

100 W
Posts: 119
Joined: Jun 15 2021 5:27pm

Re: 3D printed 400mm EDF project

Post by Greendog » Jul 31 2021 6:53am

Well that is testing to destruction, looked beautiful just before it rapidly self disassembled, :wink: sounded like there was a bit of interference between the duct and the prop, ? Suspect one of the blades came off,
Maybe could reinforce blades by laying on some carbon mat and epoxy or an aluminum rod /spar fiberglassed on to make a strengthening rib, or a cavity for a piece of alloy to go in, balancing very important too, 10g on a car wheel equals approx 10t at 840rpm , maybe a car wheel balancer is sensitive enough could use to balance prop if you made adaptor to fit it to balancer this would be good as gives dynamic balance back to front as well as up down , but old fashioned balance method good, spin then note which part facing down when stops, add weight to top until stops at different spot every time , are you balancing now ? NASA has some interesting blade designs for some of there landers maybe some strengthening ideas you could borrow :mrgreen:
“If you want to find the secrets of the universe, think in terms of energy, frequency and vibration.”

my ride , viewtopic.php?f=6&t=112483.
olive, camo bike viewtopic.php?f=6&t=112696
kona commuter viewtopic.php?f=6&t=235&start=2000#p1675516
“You create your own universe as you go along.” Churchill


I hope nothing. I fear nothing. I am free.
N Kazantzakis

SkyersJet   1 mW

1 mW
Posts: 19
Joined: May 11 2021 2:41pm

Re: 3D printed 400mm EDF project

Post by SkyersJet » Jul 31 2021 8:17am

I will make more attempt to balance the next one yes. I will probably do it by sanding.

User avatar
stan.distortion   1 kW

1 kW
Posts: 308
Joined: Jun 12 2019 12:53pm

Re: 3D printed 400mm EDF project

Post by stan.distortion » Jul 31 2021 8:38am

Older (dynamic) wheel balancers where fairly simple, not much more than a flexible mounting, a switch/trigger and a strobe light that would light up a degree wheel on the shaft. And a motor to drive it of course but it probably wouldn't be too hard to print something up to mount the whole unit flexibly.
Projects indirectly sponsored by https://www.dash.org/

User avatar
Dui, ni shuo de dui   10 kW

10 kW
Posts: 644
Joined: Jan 29 2016 3:21am

Re: 3D printed 400mm EDF project

Post by Dui, ni shuo de dui » Aug 03 2021 12:58am

Awesome project
Do you have some pictures of what the gearbox assembly looks like?
:bolt: New Build in Progress: Electric Roadster, 30 000W Kelly KLS72701, 24S2P A123 cells :bolt:
viewtopic.php?f=12&t=109246

:bolt: My electric Ninja 250 clone: 16 000W Sabvoton 72200 Unlocked, 23S2P A123 cells : :bolt:
viewtopic.php?f=12&t=90032

:bolt: My electric Scooter: 16 000W Sabvoton 72200 Unlocked, 72V 20Ah 24S1P A123 cells: :bolt:
viewtopic.php?f=12&t=75912

Post Reply