Post by Allex » Oct 31 2018 4:32am

Give us some more pictures of that display. Also more inputs would be good, wh/km, amps, volt sag, battery impedance and so on. a good display should have all that by default.
Can you answer my pm please?

evolutiongts   10 kW

10 kW
Posts: 777
Joined: Dec 31 2013 5:13pm
Location: Alhambra, CA

Re: Accelerated Systems ASI BAC 4000 & BAC 8000 FOC BT Controllers

Post by evolutiongts » Nov 02 2018 7:36am

I will take more pictures tomorrow.

Display has a clock, odometer, tripmeter, speedometer, Watts, battery voltage or %. Adjustable assist level which can be configurated with the model app. It can show AH (Capacity well). Fully digital color gauges for speedo and watts
http://www.electricrt.com
Electric Race Technologies

Schwinn 405 2WD Track Bike 18KW
EDGE 1500W Hub / MXUS 3K Turbo
ASI BAC 2000 / BAC 4000 Bluetooth
viewtopic.php?f=6&t=93079

10Kw KMX death trike
MUXUS 3K Turbo
Sabvoton 72V150A
Moto Wheels all around
Front Suspension Kit
viewtopic.php?f=6&t=83423

Giant Trance 4 Full Suspension
Cyclone 3000W
74V 3000W
http://endless-sphere.com/forums/viewto ... =6&t=59005

999zip999   100 GW

100 GW
Posts: 10766
Joined: Jan 10 2010 1:40pm
Location: Dana Point So. Cal

Re: Accelerated Systems ASI BAC 4000 & BAC 8000 FOC BT Controllers

Post by 999zip999 » Nov 02 2018 2:09pm

Does it have temperature ?

User avatar
Doctorbass   100 GW

100 GW
Posts: 7491
Joined: Apr 08 2007 2:24am
Location: Quebec, Canada East
Contact:

Re: Accelerated Systems ASI BAC 4000 & BAC 8000 FOC BT Controllers

Post by Doctorbass » Nov 05 2018 2:54pm

These BAC controller are very nice. Plus these are from ASI, a Canadian company 8)

It would be VERY interesting to get every possible adjustment on the screen and get rid of the computer for programming...

The Adaptto platform allow that and even can communicate with the BMS.. ...Well all settings and advance setting and info are availlable thru the display, as well as the Boost converter function to recharge the battery from any power source. I am a big fan of the Adaptto and their innovations, as well these are not perfect and the support is not as good as it should... However these are very advanced and the interface that allow both communication with BMS and controller is awsome!

so... why not have that kind of programming and monitoring possibility on ASI display?

I am one like many here that would be ready to pay extra to have that on the display!!

It make the use and the programming in the field much more easy than to have to cary a laptop with you!!

Doc
CURRENT PROJECT: 2WD duo MXUS/Max-E ebike 32kW
http://endless-sphere.com/forums/viewto ... =3&t=65764
-Fastest speed record 117 km/h on flat
-Fastest 1/4 mile@ 114km/h on flat and 16.316 sec
-Succeded to haul a 19200 pounds schoolbus!
113kmh Gianthttp://www.evalbum.com/3406
Mongoosehttp://www.evalbum.com/1947
YOUTUBE---https://m.youtube.com/user/Doctorbasss
http://twitter.com/DocbassMelancon
I speak FRENCH and english

evolutiongts   10 kW

10 kW
Posts: 777
Joined: Dec 31 2013 5:13pm
Location: Alhambra, CA

Re: Accelerated Systems ASI BAC 4000 & BAC 8000 FOC BT Controllers

Post by evolutiongts » Nov 05 2018 7:37pm

You dont even need a display, just use your mobile phone with the BacDoor app via bluetooth. You can change any of your settings there, and monitor everything.
http://www.electricrt.com
Electric Race Technologies

Schwinn 405 2WD Track Bike 18KW
EDGE 1500W Hub / MXUS 3K Turbo
ASI BAC 2000 / BAC 4000 Bluetooth
viewtopic.php?f=6&t=93079

10Kw KMX death trike
MUXUS 3K Turbo
Sabvoton 72V150A
Moto Wheels all around
Front Suspension Kit
viewtopic.php?f=6&t=83423

Giant Trance 4 Full Suspension
Cyclone 3000W
74V 3000W
http://endless-sphere.com/forums/viewto ... =6&t=59005

leffex   1 kW

1 kW
Posts: 329
Joined: Apr 08 2012 4:39pm
Location: Sweden

Re: Accelerated Systems ASI BAC 4000 & BAC 8000 FOC BT Controllers

Post by leffex » Nov 14 2018 2:08pm

I need a controller :flame:

Why should I get this one (ASI BAC 4000) ? I'm also looking at Kelly and Sabvoton rated at 150A battery current. I want plug and play, so to say. As long as I know what is what I can make it work and crimp my own cables together. (plug and play means, connect usual phase wires and or phase halls, plus ignition on, throttle, three-speed and battery connectors, brake signal switch needed ) (very happy if I can use an app and set foc overspeed values etcetera to make it work with my system))

What is the minimum connections that are "necessary to be connected" for the controller to work its magic on the motor its connected to?

Thanks

Its going to be heart transplanted to a Super Soco TS1200. With a hub motor 17" that I estimated to be 5T( 90v = 65-70km/h, tested from a 24fet 80a foc, jerky start, scrambling controller)
Last edited by leffex on Nov 18 2018 12:25pm, edited 1 time in total.
Salestech in an ebike store

evolutiongts   10 kW

10 kW
Posts: 777
Joined: Dec 31 2013 5:13pm
Location: Alhambra, CA

Re: Accelerated Systems ASI BAC 4000 & BAC 8000 FOC BT Controllers

Post by evolutiongts » Nov 14 2018 8:01pm

Plug and play, depending on which motor you are using.

I have motor profiles for QS 205, QS273 40H, QS273 50H, MXUS 3K Turbo, EDGE 1500W, 1000W Hub, 750W Hub.

If you are using any of the above motors, It will be plug and play ready to run out of the box. I also have various mid drive motor profiles.

Even if you are not using any of the above motors, my controllers are setup with throttle, variable regen etc and can configure the controller for you prior to shipping it out.

The minimum connections other than battery, phase, halls (optional). Are just throttle and ignition. Everything else is optional like regen brake, 2-mode power switch, reverse, cruise, display, PAS.
http://www.electricrt.com
Electric Race Technologies

Schwinn 405 2WD Track Bike 18KW
EDGE 1500W Hub / MXUS 3K Turbo
ASI BAC 2000 / BAC 4000 Bluetooth
viewtopic.php?f=6&t=93079

10Kw KMX death trike
MUXUS 3K Turbo
Sabvoton 72V150A
Moto Wheels all around
Front Suspension Kit
viewtopic.php?f=6&t=83423

Giant Trance 4 Full Suspension
Cyclone 3000W
74V 3000W
http://endless-sphere.com/forums/viewto ... =6&t=59005

flat tire   1 MW

1 MW
Posts: 1970
Joined: Feb 26 2014 12:20am

Re: Accelerated Systems ASI BAC 4000 & BAC 8000 FOC BT Controllers

Post by flat tire » Nov 14 2018 9:41pm

Electric Race Technology review:

I've received a BAC4000 controller and it works great. Not out of the box, it did require me to adjust some parameters despite having filled out the customer setup form. Furthermore, I found out that phase current was set to maximum (456 amps) which is higher than I requested and too much for a QS205, the motor indicated on my setup form. Power was set to 16000 watts or ~250 battery amps while I had requested 150. Motor inductance and resistance were totally incorrect, and the temp sensor wasn't setup right. I didn't mind reprogramming the controller and would have done it anyway so this wasn't a problem for me, but it may be relevant to you if you are looking for a no-hassle setup.

Next issue is you don't actually get a login to use the ASI smartphone app, which not only requires login but validates your right to use every few days. At the very best, you would have to request a login from someone else who already has one to use the app, and be at the mercy of their account remaining valid and not getting banned after ASI discovers 2 dozen people are logged in at once from across the country (uhh...).

Next issue is ERT's harness is very low quality with hobby-grade JST connectors and comes with the cheapest possible Chinese shunt which does work but looks very low quality and came with mismatched fastners, a uneven amount of washers and a couple Hanzi. Do you know what those are? When purchasing a expensive controller which itself uses decent waterproof automotive-grade connectors, you expect more. I threw away the ERT harness and used my own.

I needed more controllers (4000 and 8000) but after waiting over a month after ERT said my order would ship before I received it (experience detailed above) there was no way I could make another order from them. I bought instead from ASI and not only did my order ship ONE day after purchase, I get a login to use their smartphone app, the most current version of their PC software as well as an hour of tech support. There is no comparison. Also, I get to make the harness myself which is a major plus since I can use high quality wire and connectors.

The only positive thing I can say about ERT is Alan, the CEO, seems like a nice guy who is very passionate about ebikes. He makes cool youtube videos, and I don't think he's out to be a crook, but the present condition of his business is so unprofessional it's the last place I'd look for a expensive, highly configurable controller. I would consider buying again in the future, but only if they demonstrably turn a new leaf.

FINAL RATINGS:
Controller itself: 9/10
ERT: 1/10

district9prawn   1 kW

1 kW
Posts: 338
Joined: Jul 20 2013 10:46pm
Location: Sydney

Re: Accelerated Systems ASI BAC 4000 & BAC 8000 FOC BT Controllers

Post by district9prawn » Nov 15 2018 7:19am

flat tire wrote:
Nov 14 2018 9:41pm
I needed more controllers (4000 and 8000) but after waiting over a month after ERT said my order would ship before I received it (experience detailed above) there was no way I could make another order from them. I bought instead from ASI and not only did my order ship ONE day after purchase, I get a login to use their smartphone app, the most current version of their PC software as well as an hour of tech support.
I've been waiting a few weeks for a controller from ERT. A week ago I was told to expect the controller in two weeks by Alan so hopefully he comes through. To be fair, he's been more helpful and responsive than ASI. That doesn't say much as ASI's response to my enquiry was "Sorry we don't sell to end users". Initially I considered purchasing the evaluation kit as well but I didn't see $150 USD of value in 1 hour of support and the login.
Neu 8057 6kW left hand drive hardtail with 18 fet Vesc: viewtopic.php?f=6&t=96754

flat tire   1 MW

1 MW
Posts: 1970
Joined: Feb 26 2014 12:20am

Re: Accelerated Systems ASI BAC 4000 & BAC 8000 FOC BT Controllers

Post by flat tire » Nov 18 2018 1:53am

district9prawn wrote:
Nov 15 2018 7:19am
I've been waiting a few weeks for a controller from ERT. A week ago I was told to expect the controller in two weeks by Alan so hopefully he comes through. To be fair, he's been more helpful and responsive than ASI. That doesn't say much as ASI's response to my enquiry was "Sorry we don't sell to end users". Initially I considered purchasing the evaluation kit as well but I didn't see $150 USD of value in 1 hour of support and the login.
Well I bought them using my actual company email, but you can do the same whether you have a company or not. ASI is legit they just don't want to deal with idiots which end users tend to be.

I agree, ERT's price for the BAC4000 is a lot better. Even so, that doesn't excuse the fact that you aren't even "allowed" to use ASI's smartphone app when buying thru ERT. I will pay whatever to ensure that I can whip out my phone and adjust the controller whenever I want without having to worry if I can find someone else to share a login that could get shut down at literally any time.

xenodius   10 kW

10 kW
Posts: 549
Joined: Sep 03 2012 6:55pm
Location: Florida

Re: Accelerated Systems ASI BAC 4000 & BAC 8000 FOC BT Controllers

Post by xenodius » Nov 21 2018 4:28pm

larsb wrote:
Oct 18 2018 1:59pm
Are you for real? I would recommend you to look at the first post before asking what the voltage limit is. It's right there before your eyes.

If you cannot find it then i think this controller isn't for you. :D
Yeah the first post does say 90v. But the latest brochure from ASI says 72v 'nominal'; http://accelerated-systems.com/wp-conte ... NE2018.pdf

Other folks on here alluded to 20s max. If its 72v "nominal" then I assume 84V is the highest they care anyone to go. I'd like to go 21 or perhaps 22s but could live with 20s.

I simply wanted to verify because of the discrepancy and the obvious importance of this spec, so hold the sass, thanks.

larsb   100 MW

100 MW
Posts: 2646
Joined: Dec 10 2014 5:12am
Location: Gothenburg, Sweden

Re: Accelerated Systems ASI BAC 4000 & BAC 8000 FOC BT Controllers

Post by larsb » Nov 21 2018 5:19pm

sorry, see your point, could've done the same seeing 90v and 72v nominal on the same sheet.

i guess they have 100v FETs, pretty common, so a max used voltage of 90 is reasonable but not 90v nominal..

User avatar
liveforphysics   100 GW

100 GW
Posts: 14468
Joined: Oct 29 2008 1:48am
Location: Manhattan Beach, CA, USA
Contact:

Re: Accelerated Systems ASI BAC 4000 & BAC 8000 FOC BT Controllers

Post by liveforphysics » Nov 21 2018 5:42pm

22s explodes (at least on the 4000 model a few years ago at Joby).

21s can be tuned to be stable.
Each carcinogen vapor exposure includes a dice roll for cancer.

Each mutagen vapor exposure includes a dice roll for reproductive genetic defects in your children.

Each engine start sprays them into a shared atmosphere which includes beings not offered an opportunity to consent accepting these cancer experiences and defective genetics life experiences.

Every post is a free gift to the collective of minds composing the living bleeding edge of LEV development on our spaceship.

litespeed   1 MW

1 MW
Posts: 1635
Joined: Aug 11 2010 4:42pm
Location: O’Fallon, Missouri

Re: Accelerated Systems ASI BAC 4000 & BAC 8000 FOC BT Controllers

Post by litespeed » Apr 23 2019 9:20pm

So my MaxE took a dirt nap and I’m looking for a replacement. I’m thinking the BAC 4000 would be the equivalent of what I had and the 8000 way overkill. I have a QS205 3.5T I bought from you guys a couple few years ago. Always thinking about going to a 273 which may or may not happen one day.

What recommendations do you have? Any sales coming up?

Thanks,

Tom
I'm married so you know I'm no stranger to pain!

SnoGoer   100 µW

100 µW
Posts: 9
Joined: Mar 23 2019 6:36am

Re: Accelerated Systems ASI BAC 4000 & BAC 8000 FOC BT Controllers

Post by SnoGoer » Apr 24 2019 3:21pm

How long does it typically take to get a 4000 from ERT? I ordered mine a month ago and have not heard any updates?

It should come all set up for the stock Sur Ron battery and be ready to plug and play!

flat tire   1 MW

1 MW
Posts: 1970
Joined: Feb 26 2014 12:20am

Re: Accelerated Systems ASI BAC 4000 & BAC 8000 FOC BT Controllers

Post by flat tire » Apr 29 2019 5:31pm

It takes a very very long time because the owner of the business is a dishonest buffoon and extremely unprofessional. Alan runs ERT like a hobby he resents not a business. Aside from the very long wait after purchase, you are at the mercy of using his shared login to ASI's app against their TOS to program your controller. The quality of the harness and connectors he supplies is very low. I don't think anyone would order from ERT if they this stuff in advance.

ASI sells to anyone, by the way. You just have to email them from something that looks vaguely like a company email. And they will give a discount on orders after your first since you don't have to get a eval kit with every one.

soldham   10 W

10 W
Posts: 73
Joined: May 09 2013 9:38pm
Location: Nashville Tn.

Re: Accelerated Systems ASI BAC 4000 & BAC 8000 FOC BT Controllers

Post by soldham » Jul 20 2019 12:01pm

I have been waiting for almost two months for a A.S.I 8000WATT CONTROLLER and had a family emergency come up my brother was in a bad car wreck so I asked the owner to just refund my money so I could buy A plane ticket to see my brother. And that I would buy a controller after they come in. At first he emailed me back and said that the controller had just so happened to show up the same day that I was asking for a refund. And that he would fill my order or refund my money. So I sent him as n email asking for a refund so I might be able to see my brother. But he sent no refund and stopped replying to all my emails. So I am having to file a case threw PayPal to get my money back never ever do business with this guy he is a crook.

flat tire   1 MW

1 MW
Posts: 1970
Joined: Feb 26 2014 12:20am

Re: Accelerated Systems ASI BAC 4000 & BAC 8000 FOC BT Controllers

Post by flat tire » Jul 20 2019 6:47pm

Hmm, if only people had bothered to report the exact same problems months ago in this very thread!

SnoGoer   100 µW

100 µW
Posts: 9
Joined: Mar 23 2019 6:36am

Re: Accelerated Systems ASI BAC 4000 & BAC 8000 FOC BT Controllers

Post by SnoGoer » Jul 22 2019 9:29am

I’m getting no reply from him as well!! At first he was quick and responsive!!! Now after 3 months no reply or update!! Should have just waited for Luna!!

Genchichik   1 mW

1 mW
Posts: 18
Joined: Aug 23 2019 3:19pm

Re: Accelerated Systems ASI BAC 4000 & BAC 8000 FOC BT Controllers

Post by Genchichik » Aug 23 2019 3:22pm

Hi to everyone who encountered the problem, the fact that the controller does not save the parameters? :evil:

SnoGoer   100 µW

100 µW
Posts: 9
Joined: Mar 23 2019 6:36am

Re: Accelerated Systems ASI BAC 4000 & BAC 8000 FOC BT Controllers

Post by SnoGoer » Aug 26 2019 7:49pm

There must be a way to save new parameters? I would assume that updates can also be provided as they fine tune the programming ability and additional features.

I’m still waiting on mine. I am getting updates from him once a month or so saying that I’ll get the controller in a week..?? Nothing mentioned the updates on the battery 72v I ordered shortly after I ordered the ASI 4000...

I’m being optimistic and patient...!!!

Genchichik   1 mW

1 mW
Posts: 18
Joined: Aug 23 2019 3:19pm

Re: Accelerated Systems ASI BAC 4000 & BAC 8000 FOC BT Controllers

Post by Genchichik » Aug 27 2019 12:36am

I'm considering selling my plug and play kit bought from ert

User avatar
The Toecutter   100 kW

100 kW
Posts: 1144
Joined: Feb 08 2015 4:02pm

Re: Accelerated Systems ASI BAC 4000 & BAC 8000 FOC BT Controllers

Post by The Toecutter » Aug 28 2019 1:26am

How much do these controllers, the BAC4000 and 8000 weigh? I did not see that spec listed in this topic.
Custom electric velomobile, 2500W: viewtopic.php?f=6&t=110298

SnoGoer   100 µW

100 µW
Posts: 9
Joined: Mar 23 2019 6:36am

Re: Accelerated Systems ASI BAC 4000 & BAC 8000 FOC BT Controllers

Post by SnoGoer » Aug 31 2019 11:00pm

Genchichik wrote:
Aug 27 2019 12:36am
I'm considering selling my plug and play kit bought from ert
Why are you selling? Is it a performance issue?

Are you not happy with their kit?

Genchichik   1 mW

1 mW
Posts: 18
Joined: Aug 23 2019 3:19pm

Re: Accelerated Systems ASI BAC 4000 & BAC 8000 FOC BT Controllers

Post by Genchichik » Sep 01 2019 6:40pm

because I can’t change the settings, bac is configured for 16 s battery only, but I want to use 20s, ERT does not support