ive managed to blow out the side of my dual skin 20" bmx hub rim. (see pic)
needless to say, i need to replace it and would like something more durable.
im probably going to fit a disc break to the rear now aswell. (need to weld a bracket to the frame)
just wondering if a single skin steel rims as comparable strength-wise to a double skin alluminum?
needless to say, i need to replace it and would like something more durable.
im probably going to fit a disc break to the rear now aswell. (need to weld a bracket to the frame)
just wondering if a single skin steel rims as comparable strength-wise to a double skin alluminum?