Show off your Ebike creation here.
-
nuvola 10 mW

- Posts: 21
- Joined: Nov 09 2009 6:11pm
Post
by nuvola » Jul 11 2010 5:35pm
Here is my ebike:
http://www.jobike.it/Public/data/nuvola ... o%201.jpeg
some technical details:
72V 15ah lifepo4 battery with 3c prismatic cell (10kg)
72V 40A controller
tyre:
front 28x1.75
Rear 26x.2.35
Front brake juicy 5 with 180mm shimano XTR disk
(it should be substituted by a Formula the one 2010 220mm front brake but I need to change front fork before)
C.A.
sigma computer
my weight 100kg
top speed 59km/h without pedaling,amazing acceleration
I'm very very happy

bike 1) 9C Rh205 28" Rear, controller 48V 27A with 51V 60ah battery, watt's up
bike 2) 5305 26" Rear, controller 72V 40A with 72V 15ah battery, CA
-
beast775 100 kW

- Posts: 1209
- Joined: Jul 05 2007 11:55am
- Location: victoria british columbia
Post
by beast775 » Jul 11 2010 6:05pm
good lookin bike,i know i always like a bigger tire up front,dont know why but i do.your batts look like a big sla slab.what type of covering is that?nothin better than the sound of a 5305.did you incorporate torque arms?
2 FINGER SALUTE TO ESSO.no buying gasoline for 14 years now.
I spent all my money on bicycles women and beer the rest i just wasted.
-
nuvola 10 mW

- Posts: 21
- Joined: Nov 09 2009 6:11pm
Post
by nuvola » Jul 11 2010 7:17pm
what type of covering is that?
If I remember it was made by chinabattery.com
did you incorporate torque arms?
still to do.
bike 1) 9C Rh205 28" Rear, controller 48V 27A with 51V 60ah battery, watt's up
bike 2) 5305 26" Rear, controller 72V 40A with 72V 15ah battery, CA
-
toft 10 W

- Posts: 84
- Joined: Jun 10 2010 5:12am
Post
by toft » Jul 12 2010 1:51pm
Look,s good, maybe you should try to put your battery pak inside the main frame triangle...? better ballance etc... the question is how wide is the battery;).
Regards toft
PS. Is this shwalbe tire confortable? Maybe in new project il tray this tires...
-
ambroseliao 100 kW

- Posts: 1221
- Joined: Apr 27 2009 3:34pm
- Location: Washington, DC, USA area
-
Contact:
Post
by ambroseliao » Jul 12 2010 3:55pm
Nice looking bike.
What are you using for rear brakes? I don't see any!
Ambrose
http://www.ebikes.ca/ is the best!
TidalForce M-750X, Tidalforce S-750 with Crystalyte HS3540, 1x TF iO-X Cruiser. E+ 1000W hybrid bike. ebikes.ca DrainBrain & Cycle Analyst meters. GoPro HD Hero2 camera. Bosch Fat Packs, 37V 10Ah LiPO pack. Turnigy Multistar batteries
My blog:
http://ebikerider.blogspot.com
Remember LiFEPo4 HVC is 3.65V and LVC is 2.7V
-
nuvola 10 mW

- Posts: 21
- Joined: Nov 09 2009 6:11pm
Post
by nuvola » Jul 13 2010 5:29am
Battery pack is too big to fit as is inside triangle, but I've no problems at all where it is now.
Balance is perfect just now.
There's no Rear brake!
I'd like to use and idraulic brake but my old 5305 hasn't way to get connected to a disk, I'm still studing an easy solution.
any proposal?
big tyre (apple) is a must to do, bike now it's very confortable.
If possibile I will use bigger tyre, but the biggest I found was just mine (26x2.35) (bigger aren't for road use)
bike 1) 9C Rh205 28" Rear, controller 48V 27A with 51V 60ah battery, watt's up
bike 2) 5305 26" Rear, controller 72V 40A with 72V 15ah battery, CA
-
Kepler 1 GW

- Posts: 3268
- Joined: Nov 08 2009 9:22pm
- Location: Eastern suburbs Melbourne Australia
Post
by Kepler » Jul 13 2010 7:17am
Nice bike. Good work. Be careful you dont do a major tank slapper with that weight so high rear biased. Especially at the sort of speed that thing does.
Couldnt see any torque arms on the back. I presume they are there.
-
nuvola 10 mW

- Posts: 21
- Joined: Nov 09 2009 6:11pm
Post
by nuvola » Jul 13 2010 5:29pm
I have no rear torque arms at the moment.
ebikes.ca seems to have discontinued their rear version.
any other website where to buy it?
bike 1) 9C Rh205 28" Rear, controller 48V 27A with 51V 60ah battery, watt's up
bike 2) 5305 26" Rear, controller 72V 40A with 72V 15ah battery, CA
-
nuvola 10 mW

- Posts: 21
- Joined: Nov 09 2009 6:11pm
Post
by nuvola » Jul 17 2010 2:16pm
some updates:
I'd a puncture in my apple, so I decided to change my tyres!
So I've bought 2 maxxis hookworm 26x2.5
Next monday, I will go to a bike shop to buy a Marzocchi Fork, so I could finally mount my formula the one 2010 220mm front brake!
And the ebike will be quite finished...

(i just need to find a solution for a rear brake)
bike 1) 9C Rh205 28" Rear, controller 48V 27A with 51V 60ah battery, watt's up
bike 2) 5305 26" Rear, controller 72V 40A with 72V 15ah battery, CA
-
Kepler 1 GW

- Posts: 3268
- Joined: Nov 08 2009 9:22pm
- Location: Eastern suburbs Melbourne Australia
Post
by Kepler » Jul 17 2010 3:32pm
Try and come up with some way to get the batteries forward and lower. A rear brake and a better COG will really finish it off then. And dont forget the torque arms. That sort of power will rip your dropout to pieces in no time and frankly is just plain dangerous. Do a search on making your own. There not too hard to make.
-
nuvola 10 mW

- Posts: 21
- Joined: Nov 09 2009 6:11pm
Post
by nuvola » Jul 17 2010 7:53pm
I've found the perfect toruqe arm from ampebikes, I will just order it when I will come back from holidays.
For rear brake I've to understand if I can just change the left cover with the new threaded 5305 cover.
I'm speaking about buying this:
my 5305 is old and doesn't have threaded cover.
batteries is perfect just where it is.
what is a COG?
bike 1) 9C Rh205 28" Rear, controller 48V 27A with 51V 60ah battery, watt's up
bike 2) 5305 26" Rear, controller 72V 40A with 72V 15ah battery, CA
-
Kepler 1 GW

- Posts: 3268
- Joined: Nov 08 2009 9:22pm
- Location: Eastern suburbs Melbourne Australia
Post
by Kepler » Jul 17 2010 8:08pm
nuvola wrote:
batteries is perfect just where it is.
what is a COG?
There is a good reason why people go to so much trouble to install the batteries further forward but its what you are happy with at the end of the day
COG "Centre of Gravity"

-
nuvola 10 mW

- Posts: 21
- Joined: Nov 09 2009 6:11pm
Post
by nuvola » Jul 20 2010 4:50pm
my new buy:
Marzocchi Marathon SL 80mm
finally I could mount my Formula 220mm front break.
For rear Brake, I'm still looking for a good and easy solution.
ps. I'v mounted 11-34 gear

bike 1) 9C Rh205 28" Rear, controller 48V 27A with 51V 60ah battery, watt's up
bike 2) 5305 26" Rear, controller 72V 40A with 72V 15ah battery, CA
-
nuvola 10 mW

- Posts: 21
- Joined: Nov 09 2009 6:11pm
Post
by nuvola » Sep 14 2010 4:42pm
here's my gallery:
http://picasaweb.google.com/nuvolamax/superbaics#
note the new 220mm front disk!
the battery position is perfect because due to very big powerful front brake it helps to don't let the rear wheel going up.
Now I'm working on a rear ebrake.
bike 1) 9C Rh205 28" Rear, controller 48V 27A with 51V 60ah battery, watt's up
bike 2) 5305 26" Rear, controller 72V 40A with 72V 15ah battery, CA
-
icecube57 1 GW

- Posts: 3072
- Joined: Apr 25 2008 8:42am
- Location: Austell GA
-
Contact:
Post
by icecube57 » Sep 14 2010 5:46pm
I got an amped bikes torque arm holding my x5303 beast in. The Tidal Force frame has the perfect notch for it. Ive been playing hard and using regen with no issue.. It hasnt wiggle nor has axle bolt moved. All I can say is kudos to the torque arm and good luck with your build.
-
chroot 100 kW

- Posts: 1284
- Joined: Nov 29 2009 4:03pm
Post
by chroot » Sep 14 2010 8:10pm
Your bike looks so finest and nice one. I have a question, You said you are using a 72v batteries and only run 36mph (59km/h) and Aren't the 72v supposed push your 5305 lot fast more than 40mph (65km/h).
Thank you Justin Lemire-Elmore - You are a HERO!
Tidalforce, Yuba Mundo V4 Cargo bike, Juiced Riders ODK V1 Cargo bike
English is my secondary language - ASL (American Sign Language) is my primary.
-
icecube57 1 GW

- Posts: 3072
- Joined: Apr 25 2008 8:42am
- Location: Austell GA
-
Contact:
Post
by icecube57 » Sep 14 2010 9:42pm
36... sounds about right. A 5304 would peak around the low 40s depending on rider.
-
nuvola 10 mW

- Posts: 21
- Joined: Nov 09 2009 6:11pm
Post
by nuvola » Sep 15 2010 6:49pm
I will check top speed this saturday, with big apple 2.3 was 59km/h, now I want to see difference with hookwoorm 2.5
I just have to understand how to set tyre size on CA!
Anyway my weight it's about 105kg plus 15kg of lifepo4, not a light one and I believe that big tyres let your max speed going down due to friction with asphalt.
bike 1) 9C Rh205 28" Rear, controller 48V 27A with 51V 60ah battery, watt's up
bike 2) 5305 26" Rear, controller 72V 40A with 72V 15ah battery, CA