project: no-car

General Discussion about electric vehicles.
User avatar
efMX Trials Electric Freeride   1 MW

1 MW
Posts: 1735
Joined: Feb 15 2013 4:43pm

Re: project: no-car

Post by efMX Trials Electric Freeride » Feb 02 2014 8:24pm

joepah wrote:
angelo212 wrote:subbed. Looking forward to seeing this.
How do you subscribe? I just keep it on my list of articles, doesn't notify me of new comments.
if you view a thread when logged in there is a "Subscribe topic" link at the bottom of the page..
im guessing if you click this subscribe button the you will receive (email) notifications upon thread activity??..
some ride & sk8 videos:
metacafe.com/channels/NATAS666DAMIEN
http://www.youtube.com/natas666damien
i have nothing for sale.. :)

joepah   10 W

10 W
Posts: 93
Joined: Aug 28 2011 8:02pm

Re: project: no-car

Post by joepah » Feb 05 2014 5:40am

efMX Trials Electric Freeride wrote:
joepah wrote:
angelo212 wrote:subbed. Looking forward to seeing this.
How do you subscribe? I just keep it on my list of articles, doesn't notify me of new comments.
if you view a thread when logged in there is a "Subscribe topic" link at the bottom of the page..
im guessing if you click this subscribe button the you will receive (email) notifications upon thread activity??..
oh duhhhhhhhhhh

Rambo Ruckus   10 mW

10 mW
Posts: 30
Joined: Jan 12 2014 10:50pm
Location: nj

Re: project: no-car

Post by Rambo Ruckus » Feb 05 2014 10:49am

so, i made my deadline. been riding it and tweaking a little. next need upgrades. new rear shock, smaller pegs, front fork, rear brake, more batteries. a couple of other things. need to redo my "battery box" wich is a 50cal 100 round ammo can. and need 8mm bullets for my phase wires. and an ignition switch. need to run the resistors in 2s2p for my precharger, it only lets it reach 72v... and gets REAL warm. so when i get more bullets ill do that, and ill tidy up my harnesses and shorten them. find a spot for all my "control" wires. and get new bars. new front tire and rim... not exatly sure what size... but either a 17 or 19" rim... for sure. marzocchi front forks. maybe an old school fox vanilla rear shock. need to determine travel and ride height.. but yeah, heres the attrocious beast... some specs thus far...


as of now:

weight: 99.8 lbs
front: 40lbs
rear: 59.8
batteries: 5x zippy flightmax 6s1p 8000mah, resulting in 30s1p 111v nominal 126v hvc 96lvc (my setting) 8hr (so far, 16ah soon)
controller settings: reprogramed to 40amp rated 100 phase, pulling 5096watts (then i screwed up and set it to 80/200 pulling 9600watts. lmao. what a blast!!!)
speed 1: 35% seems to put me right around 20, im happy
speed 2: havent really used it tbh.
speed 3: 99% the tire spins to 60mph (via ca) going to have to run gps on this one to be sure... but its fast. i hit atleast 50 on this setting and it was still going :)

im going to restet the controller to 50rated 110 phase and see how i like it for now. so i dont beat my batteries up too much. untill i get more batteries in a couple weeks.

heres some pics:
ebikers.jpg
working on it
ebikers.jpg (71.64 KiB) Viewed 190 times
1888450_10202336250761890_744862617_n.jpg
125v hoc :)
1888450_10202336250761890_744862617_n.jpg (49.3 KiB) Viewed 190 times
1507912_10202336251041897_1420871152_n.jpg
1507912_10202336251041897_1420871152_n.jpg (52.82 KiB) Viewed 190 times
1620841_10202336251321904_2138033598_n.jpg
1620841_10202336251321904_2138033598_n.jpg (59.35 KiB) Viewed 441 times
1888754_10202336251761915_106404894_n.jpg
1888754_10202336251761915_106404894_n.jpg (55.52 KiB) Viewed 441 times
1891010_10202336252241927_579560994_n.jpg
1891010_10202336252241927_579560994_n.jpg (76.29 KiB) Viewed 441 times
1891046_10202336252521934_704159960_n.jpg
1891046_10202336252521934_704159960_n.jpg (72.15 KiB) Viewed 441 times
1606986_10202336252961945_1471840176_n.jpg
1606986_10202336252961945_1471840176_n.jpg (105.88 KiB) Viewed 441 times
sorry i havent updated in forever. ive been soo busy. i think we had 13 or so inches of snow in the past week, and work and then getting this up and running.... pulling long hours. im so happy its "done" and ready to go!!! cant wait to upgrade it.

Post Reply