Need thin, non conductive, fire retardent sheets. Mica?

Post by jimbo69ny » Mar 19 2018 10:02pm

Hello,

I am looking for thin sheets that are non conductive and fire retardant for my battery box. I've heard and seen that Tesla uses mica sheets in their battery box. I looked up prices on ebay and amazon and the stuff is expensive!

Do you have any other recommendations? I need approximately 8 sheets that are roughly 36" x 20". So kind of a lot.

Thank you!

User avatar
jonescg   1 GW

1 GW
Posts: 3338
Joined: Aug 07 2009 9:22pm
Location: Perth, Western Australia

Re: Need thin, non conductive, fire retardent sheets. Mica?

Post by jonescg » Mar 19 2018 10:05pm

G10FR4 - comes in sheets as thin as 0.6 mm. It's fire retardant, and a good electrical insulator.

jimbo69ny   1 W

1 W
Posts: 52
Joined: Feb 10 2018 12:53am

Re: Need thin, non conductive, fire retardent sheets. Mica?

Post by jimbo69ny » Mar 19 2018 11:27pm

I just found this. MIght be the way to go.
https://www.electro-wind.com/rochling-g ... 48x96.html