Post by Mick48 » Apr 26 2018 1:50pm

Just received my new QS motor and was wondering if within the motor case itself, is there
a place where they list the motor winding? I ordered the 3.5 winding and am pretty certain
they sent me the 5T.

User avatar
amberwolf   100 GW

100 GW
Posts: 25460
Joined: Aug 17 2009 6:43am
Location: Phoenix, AZ, USA, Earth, Sol, Local Bubble, Orion Arm, Milky Way, Local Group
Contact:

Re: QS 205 V3 50H Winding Stamp?

Post by amberwolf » Apr 26 2018 8:36pm

Sometimes they write it on the stator inside teh motor. You can test the speed at a particular voltage to see what RPM it gets, this lets you calculate the kV (RPM per volt). Then you can compare that with the manufacturers specs for the winding you think it should be, and if its not close, then they may have sent you the wrong one.

Mick48   1 mW

1 mW
Posts: 12
Joined: Sep 20 2011 3:12pm

Re: QS 205 V3 50H Winding Stamp?

Post by Mick48 » Apr 27 2018 2:35pm

Thanks, amberwolf.
Yeah I'm not about to take it apart but did bench test it yesterday and not only
found the rpm low but heard a grinding noise coming from the motor. I guess its
time to send this one back. :cry: