I built this some time back but only just finished it. It's a 14s7p battery built using Panasonic NCR18650GA cells spotwelded with nickel. It's got fly-wires for a balance port, but I've left it in case a specific BMS is wanted.
The battery has been potted in West Systems epoxy resin, so you can drop it from a height and it would just break the ground.
There's AUD$500 worth of cells in it, so I'll sell for ~$400. Can ship to anywhere in Australia. I'll put whatever connector on it you want, depending on the end goal.
Voltage: 48 V nominal (charge to 58.6 V)
Capacity: 24 Ah
Mass: 5.85 kg
Cells: Panasonic NCR18650GA (3500 mAh) 10 A max.
Arrangement: 14s7p
Max discharge current: Probably 50 A, but not for long.
The battery has been potted in West Systems epoxy resin, so you can drop it from a height and it would just break the ground.
There's AUD$500 worth of cells in it, so I'll sell for ~$400. Can ship to anywhere in Australia. I'll put whatever connector on it you want, depending on the end goal.
Voltage: 48 V nominal (charge to 58.6 V)
Capacity: 24 Ah
Mass: 5.85 kg
Cells: Panasonic NCR18650GA (3500 mAh) 10 A max.
Arrangement: 14s7p
Max discharge current: Probably 50 A, but not for long.