Up for sale is my 16s 20ah A123 pack with custom case and built in BMS for charging. These cells are the original USA cells and the pack has an estimated ~300 cycles on it (cycle life is ~2000). The pack has a 200a fuse internally at the high current connector and a 30a BMS for charging and balancing on a separate lead.
These cells are legendary for their robustness, current handling, and cycle life. When I bought these I ordered an extra cell and tested it to 200 amps continuous.
External balance leads in addition to the leads to the internal bms. This gives you the ability to check cells or use your own balance charger.
Testing at 800w load extracted 17.85ah and 901wh.
6x7x11in
22lbs
Located in 94517 for local pick up or shipped for $35
Up for sale is my 16s 20ah A123 pack with custom case and built in BMS for charging. These cells are the original USA cells and the pack has an estimated ~300 cycles on it (cycle life is ~2000). The pack has a 200a fuse internally at the high current connector and a 30a BMS for charging and balancing on a separate lead.
These cells are legendary for their robustness, current handling, and cycle life. When I bought these I ordered an extra cell and tested it to 200 amps continuous.
External balance leads in addition to the leads to the internal bms. This gives you the ability to check cells or use your own balance charger.
Testing at 800w load extracted 17.85ah and 901wh.
6x7x11in
22lbs
Located in 94517 for local pick up or shipped for $35