LG Chem 10S2P battery modules - 37V30Ah - 1100 wh [EU] [SOLD]
Re: LG Chem 10S2P battery modules - 37V30Ah - 1100 wh [EU] [SOLD]
Looks like I could use 1 or 2. Building a E-trailbike that is almost ready but with out a good battery the bike is useless.
Pm. send. Living in the same country.
Pm. send. Living in the same country.
Re: LG Chem 10S2P battery modules - 37V30Ah - 1100 wh [EU] [SOLD]
Here is a guide on how I remove the Cells from the packs.
https://imgur.com/a/rvJkNPw
I might make another one where I solder the Cells in different configs.
https://imgur.com/a/rvJkNPw
I might make another one where I solder the Cells in different configs.
Re: LG Chem 10S2P battery modules - 37V30Ah - 1100 wh [EU] [SOLD]
I am looking for LG 10S2P battery it is stil to buy. I am like to buy some for 48 volt power wall.


Re: LG Chem 10S2P battery modules - 37V30Ah - 1100 wh [EU] [SOLD]
There are better options for a 48v power wall
Re: LG Chem 10S2P battery modules - 37V30Ah - 1100 wh [EU] [SOLD]
I will like some help. Wat is beter prius hybryd baterry of hybryd Civic. Ah is lower buy hybryd and prijs. I dont know wat is beter?



- louis raaijmakers 100 W
- Posts: 159
- Joined: Oct 09 2013 3:22pm
Re: LG Chem 10S2P battery modules - 37V30Ah - 1100 wh [EU] [SOLD]
cheap hollander incomming.
nog wat accus te koop? zoek een setje accu's voor tijdelijk lieft 48v 4/500a piek
leuk om meer hollanders te zien hier!
ps: @boekel ik zou graag een keer komen kijken. als je weer zon interessant projectje hebt!
zag dat je tesla packs gedemonteerd had?

nog wat accus te koop? zoek een setje accu's voor tijdelijk lieft 48v 4/500a piek
leuk om meer hollanders te zien hier!
ps: @boekel ik zou graag een keer komen kijken. als je weer zon interessant projectje hebt!
zag dat je tesla packs gedemonteerd had?
-
- Posts: 9
- Joined: May 09 2019 6:21am
Re: LG Chem 10S2P battery modules - 37V30Ah - 1100 wh [EU] [SOLD]
I have 20pcs of these modules in Sweden.
I just shipped 2 to a happy customer in Romania.
Let me know your zip code for a shipping quote.
130 euros per module
Victor
I just shipped 2 to a happy customer in Romania.
Let me know your zip code for a shipping quote.
130 euros per module
Victor
Re: LG Chem 10S2P battery modules - 37V30Ah - 1100 wh [EU] [SOLD]
I have 2 of those modules for sale.
Velokraft Batmobile
KMX Cobra with Xlyte 5403
Go-One Evo with Cromotor
BATMOBILE - in progress
Giant CRS Alliance - SOLD
3Element Espire - SOLD
Custom built Specialized BigHit with BBS02
Velokraft e-VK3
Velokraft Vk2
Steintrike Mungo Sport HS3540
Scorpion FS HS3540
Kona Dawg BMC v2
KMX Cobra with Xlyte 5403
Go-One Evo with Cromotor
BATMOBILE - in progress
Giant CRS Alliance - SOLD
3Element Espire - SOLD
Custom built Specialized BigHit with BBS02
Velokraft e-VK3
Velokraft Vk2
Steintrike Mungo Sport HS3540
Scorpion FS HS3540
Kona Dawg BMC v2