Post by Boekel » Dec 23 2017 9:33pm

Update: I have reduced the price!

I have at least 3 modules (= 1332) of loose cells for sale, I'm located in the Netherlands.

They come from a 2016 P85D (3000 km according to seller) this is the car:
https://www.onderdelenlijn.nl/voertuige ... el-s-2016/

Pictures of the pack:
http://boekel.nu/foto/17/2017-09_tesla_battery/

Price for clean cells:
10-50 = €3,50
51-100 = €3,25
100+ = €3,00

uncleaned:
10-50 = €3,00
51-100 = €2,75
100+ = €2,50

Price for complete module: €2,00 per cell

Price for cells with small dents: €1,-

Contact: tesla@boekel.nu
Last edited by Boekel on Feb 19 2018 3:41am, edited 2 times in total.

User avatar
Luk   100 mW

100 mW
Posts: 38
Joined: Feb 16 2014 1:01am

Re: FS: Tesla Model S cells (Europe)

Post by Luk » Dec 24 2017 9:18am

Hi Boekel .
it's 20700 cell or 18650 ?
Luk-ebike.fr

User avatar
Boekel   1 mW

1 mW
Posts: 14
Joined: Nov 26 2017 6:56pm
Location: Netherlands
Contact:

Re: FS: Tesla Model S cells (Europe)

Post by Boekel » Dec 24 2017 11:32am

18650

User avatar
Boekel   1 mW

1 mW
Posts: 14
Joined: Nov 26 2017 6:56pm
Location: Netherlands
Contact:

Re: FS: Tesla Model S cells (Europe)

Post by Boekel » Dec 25 2017 7:13am

Image
I can also sell like this. quite strong cell-holders...

Image
clean cells

Image

Image
uncleaned cells

Image

Image

User avatar
Boekel   1 mW

1 mW
Posts: 14
Joined: Nov 26 2017 6:56pm
Location: Netherlands
Contact:

Re: FS: Tesla Model S cells (Europe)

Post by Boekel » Jan 02 2018 3:01pm

I have reduced the price, I think it's a good price for 2016 cells?

mjar99   10 µW

10 µW
Posts: 6
Joined: Oct 22 2014 9:33am

Re: FS: Tesla Model S cells (Europe)

Post by mjar99 » Jan 04 2018 5:36am

What is the capacity of each cell?

User avatar
Boekel   1 mW

1 mW
Posts: 14
Joined: Nov 26 2017 6:56pm
Location: Netherlands
Contact:

Re: FS: Tesla Model S cells (Europe)

Post by Boekel » Jan 04 2018 5:40pm

A couple of cells are tested (leads soldered to them): 3050 mAh

User avatar
Boekel   1 mW

1 mW
Posts: 14
Joined: Nov 26 2017 6:56pm
Location: Netherlands
Contact:

Re: FS: Tesla Model S cells (Europe)

Post by Boekel » Jan 04 2018 6:54pm

Image

Pajda   100 W

100 W
Posts: 216
Joined: Jan 24 2016 3:45am
Location: Czech Republic

Re: FS: Tesla Model S cells (Europe)

Post by Pajda » Jan 05 2018 1:11pm

Today arrived a few cell samples from Boekel for my cycle life tests and comparsion with other industrial 18650 cells. For some time I was looking for cells with known history with the lowest possible mileage and calendar age.

I have measured nominal capacity/energy at calibrated 4-wire battery tester. I used settings for Panasonic NCR18650BM

settings: nominal capacity test (0.5C charge to 4.2V @ 60mA cut-off - 10minut rest time - 0.2C discharge to 2.5V):

new NCR18650BM: capacity: 3125 mAh, energy: 11.35 Wh
3000km Tesla P85D: capacity: 3120 mAh, energy: 11.32 Wh

settings: cycle life test (0.5C charge to 4.2V @ 100mA cut-off - 10minut rest time - 1C discharge to 2.5V):

new NCR18650BM: capacity: 3038 mAh, energy: 10.67 Wh
3000km Tesla P85D: capacity: 3081 mAh, energy: 10.79 Wh

edit: corrected units
Last edited by Pajda on Jan 06 2018 4:23am, edited 2 times in total.

User avatar
Boekel   1 mW

1 mW
Posts: 14
Joined: Nov 26 2017 6:56pm
Location: Netherlands
Contact:

Re: FS: Tesla Model S cells (Europe)

Post by Boekel » Jan 05 2018 2:22pm

Pajda wrote:
Jan 05 2018 1:11pm
Today arrived a few cell samples from Boekel for my cycle life tests and comparsion with other industrial 18650 cells. For some time I was looking for cells with known history with the lowest possible mileage and calendar age.

I have measured nominal capacity/energy at calibrated 4-wire battery tester. I used settings for Panasonic NCR18650BM (0.5C charge to 4.2V @ 60mA cut-off - 10minut rest time - 0.2C discharge to 2.5V) and here is the comparsion:

new NCR18650BM: capacity: 3.125 mAh, energy: 11.35 Wh
3000km Tesla P85D: capacity: 3.120 mAh, energy: 11.32 Wh
Wow that's good!
better results than with cheap tester...
Thank you!

Buk___   10 kW

10 kW
Posts: 750
Joined: Jul 28 2017 5:59pm

Re: FS: Tesla Model S cells (Europe)

Post by Buk___ » Jan 05 2018 4:00pm

Pajda wrote:
Jan 05 2018 1:11pm
new NCR18650BM: capacity: 3.125 mAh, energy: 11.35 Wh
3000km Tesla P85D: capacity: 3.120 mAh, energy: 11.32 Wh
Presumably, those numbers are Ah, not mAh?

Pajda   100 W

100 W
Posts: 216
Joined: Jan 24 2016 3:45am
Location: Czech Republic

Re: FS: Tesla Model S cells (Europe)

Post by Pajda » Jan 06 2018 4:19am

Buk___ wrote:
Jan 05 2018 4:00pm
Pajda wrote:
Jan 05 2018 1:11pm
new NCR18650BM: capacity: 3.125 mAh, energy: 11.35 Wh
3000km Tesla P85D: capacity: 3.120 mAh, energy: 11.32 Wh
Presumably, those numbers are Ah, not mAh?
Of course, sorry for that. I have corrected the values to mAh and add a new setting with 1C discharge for cycle life test.

eleratas   1 µW

1 µW
Posts: 2
Joined: Aug 19 2015 1:55pm

Re: FS: Tesla Model S cells (Europe)

Post by eleratas » Jan 15 2018 9:23am

Last week got my Tesla cells from comrade Boekel. Everything perfect! Very happy with his communication and service! Thanks a lot from Estonia, Boekel!

Milordas   1 µW

1 µW
Posts: 1
Joined: Jan 13 2018 3:13pm

Re: FS: Tesla Model S cells (Europe)

Post by Milordas » Jan 24 2018 6:05pm

Am Monday got cells from Boekel, excellent service, fast shipping, now disassembling and sorting. Charged 32pcs from 220, all 32 work good, found 1 cell with higher internal resistance - about 100mOm (others 32-53mOm according to my cheap charger). Will try this cell in flashlight.
Thanks from Lithuania!

mgotsop   1 µW

1 µW
Posts: 1
Joined: Jan 22 2013 7:21pm

Re: FS: Tesla Model S cells (Europe)

Post by mgotsop » Feb 18 2018 1:44am

Hi
Are there any modules?
Thanks

User avatar
Boekel   1 mW

1 mW
Posts: 14
Joined: Nov 26 2017 6:56pm
Location: Netherlands
Contact:

Re: FS: Tesla Model S cells (Europe)

Post by Boekel » Feb 18 2018 4:41am

I only have 1 complete module left (without busbars, 444 cells)

seanyt   1 mW

1 mW
Posts: 10
Joined: Oct 30 2014 4:01am

Re: FS: Tesla Model S cells (Europe)

Post by seanyt » Feb 18 2018 11:43am

PM sent

public_enemy   10 mW

10 mW
Posts: 21
Joined: Jan 04 2016 5:59am
Location: Bulgaria

Re: FS: Tesla Model S cells (Europe)

Post by public_enemy » Feb 18 2018 2:17pm

I have interest in a whole module if you have any.What will be the shipping price to Bulgaria?

User avatar
Boekel   1 mW

1 mW
Posts: 14
Joined: Nov 26 2017 6:56pm
Location: Netherlands
Contact:

Re: FS: Tesla Model S cells (Europe)

Post by Boekel » Feb 19 2018 3:41am

All are sold for now, will make a new post if I get more.

Thanks.

seanyt   1 mW

1 mW
Posts: 10
Joined: Oct 30 2014 4:01am

Re: FS: Tesla Model S cells (Europe) (sold!)

Post by seanyt » Feb 20 2018 1:54pm

Very fast delivery.
Well priced, will be after some more cells in the future

Post Reply