Tesla Cells for sale as wrapped or welded packs

Got something to sell? Have extra parts that need a good home? Have something that others would need to complete their kits? Post it up here and see if anyone else is searching for what you are selling.
eric1565   10 W

10 W
Posts: 89
Joined: Feb 28 2015 4:50pm

Re: Tesla Cells for sale as wrapped or welded packs

Post by eric1565 » Jul 04 2018 2:23pm

The plastic is "lexan" with sticky goo on the bottom. I bought from amazon I think.

the nylon is sticking really well. But I do have it pretty torn up. I have rough sanded the lexan top to get more mechanical adhesion. I use an ice pick to pry off the parts, and that does some more tearing up of the plastic.

Overall very happy with the prints. My benchie came out really well. the Hull was VERY smooth... smoke stack... not so good, but that may have been because it was so quick to print, and it needed more time to cool between layers.

eric1565   10 W

10 W
Posts: 89
Joined: Feb 28 2015 4:50pm

Re: Tesla Cells for sale as wrapped or welded packs

Post by eric1565 » Jul 05 2018 9:13am

X2flier wrote:
Jul 04 2018 11:16am
kriskros wrote:
May 16 2018 2:24am
can you build a 54.4 [48.1v nominal]30ah pack? what would dimensions be?? I domt know the specs of Tesla cells
Eric,

Same question, with USA shipping. I would need to get a 48 Vdc (with 30~40 Ah) battery pack. Your printed cell holders look fine to me, but I would have to know the number of cells that I would need for my pack(s). I could CAD something up if you want, if I had the dimensions of your cell holders, maybe across five cells.

Hopefully I can figure out a decent BMS and charger set-up. I have some electronics experience, but not much experience with batteries.

Total noob to ebikes here, so please bear with me.

Thanks,

I can build any type of pack. For the dim's of the holders, look at the picture I put up of the triangle pack. you can count the cells and the dims are in mm's. I did measure 5 cells in a pack, and the outside to ouside dim of the CELLS is 96.07mm. The hex holder wall is right about .8mm to 1mm.

I will only ship to the US so if you are in canada, I can ship to a PO box or similar so you can pic up in the US and take across the border.
pack.jpg
pack.jpg (78.18 KiB) Viewed 1170 times
on the pack size, that is a generic size. I can do pretty much anything, so you need to give me your limiting dims, and I work around that. I have been working with a guy on a triangle pack, and there was a TON of back and forth. after about 30 msgs we are both happy and moving forward on the pack. I am sure it gets a bit annoying me always asking what you want, but I WANT to make sure what I am spending my time making, is what the other person on the other end of the computer is EXPECTING.

If you want to put on your own balance leads, and main leads you can take that price off. I have bought a Bluetooth and UART BMS and I was very happy with one, I was less happy with another (both were similar, one was a 4S (not happy) and a 7S (very happy). I was only using them as balancer.

If you have any questions let me know.

Eric

jkj   1 mW

1 mW
Posts: 13
Joined: Nov 27 2015 11:05am

Re: Tesla Cells for sale as wrapped or welded packs

Post by jkj » Jul 12 2018 3:06pm

Really dumb question and I've only had a battery with BMS before. How difficult would this be to charge and use safely?

User avatar
DanGT86   10 kW

10 kW
Posts: 604
Joined: Sep 06 2012 9:18pm
Location: Saint Louis MO

Re: Tesla Cells for sale as wrapped or welded packs

Post by DanGT86 » Jul 12 2018 8:56pm

That all depends on what you are using to monitor them and how much effort you are willing to put into being the human BMS. Most good cells stay pretty well balanced. If you are willing to monitor them and occasionally balance them you could get by. It really depends on how you want to use them and how much you are willing to interact with the pack.

For instance:
If you want to charge the pack totally full while its unattended and then ride it till its totally dead then you really want a bms.
If you are letting other people charge or borrow the bike that know nothing about it then you want a BMS.
If you are pulling relatively low current where the BMS is $30-50 then you probably want a BMS
If you don't know or care to learn much about batteries then you want a bms
If you don't want to have multiple ugly balance taps hanging out of the pack then you probably want a bms
If you don't own any RC balance chargers, alarms, cell logs etc. then its cheaper to just get a BMS

I use an RC charger to balance my 20s pack every few months. When I use a normal bulk charger I stop at 4.15v per cell. I also plug a cell log into each balance cable when its close to done on the bulk charger or before a ride just to make sure everything is stable and balanced. I also use low voltage alarms when I'm on a long ride where I'm getting into the last 10-20% of my capacity. The bummer part is that cell logs and LV alarms will pull the pack out of balance if you leave them connected. They would be almost as good as a BMS if they could be left connected.

For what its worth I would never give someone else a setup that required this much tinkering. It's a bit of a hassle but the bike is a hotrod and not daily transportation. I'm a hobbyist and find it interesting getting to know my battery packs.My packs get moved around on my fleet of FrankenBikes and I'm pulling 80-100amps from the pack. It was hard to justify a $100+ BMS on $250 worth of LiPo.

These Tesla cells are way safer than LiPo so you don't have to be as paranoid as I am but you still don't want to trash a nice pack. Even if it's not going to burn your house down.

Hope that helps illuminate some of the factors involved in the decision.

eric1565   10 W

10 W
Posts: 89
Joined: Feb 28 2015 4:50pm

Re: Tesla Cells for sale as wrapped or welded packs

Post by eric1565 » Jul 12 2018 10:20pm

I have an icharger. I also use a cell logger to monitor my packs. Tesla cells stay pretty balanced if not abused (dragged down to far).

BMS 's are good but not required if u can be the human BMS. If u can monitor the voltages and not drag the packs down to far u can work just fine. But u also NEED a balance charger. You NEED a way to monitor ur pack.
Eric

jkj   1 mW

1 mW
Posts: 13
Joined: Nov 27 2015 11:05am

Re: Tesla Cells for sale as wrapped or welded packs

Post by jkj » Jul 14 2018 10:47am

The bike is mainly used by my dad and I want it to be pretty easy to maintain. So I guess that puts me in the BMS camp for this project. If I buy a BMS to send your way would you be into doing a BMS pack?

eric1565   10 W

10 W
Posts: 89
Joined: Feb 28 2015 4:50pm

Re: Tesla Cells for sale as wrapped or welded packs

Post by eric1565 » Jul 17 2018 1:29pm

Yeah, I can do that. I can also print a case for the BMS if it needs one.

Eric

eric1565   10 W

10 W
Posts: 89
Joined: Feb 28 2015 4:50pm

Re: Tesla Cells for sale as wrapped or welded packs

Post by eric1565 » Jul 19 2018 10:22pm

Pack went out today. Took me a while to build it (sorry about that). But I am VERY happy with those nylon holders.

If anybody wants nylon holders let me know. I sell them for .15$ per cell. you need a set top and bottom, so you need to double your cell count. They are 7mm thick.

The nylon is so strong I can hold the entire pack by sticking 2-3 fingers in the empty cells on the ends and carry the pack that way. If I did that with the cast urethane then I would drop a pack :(!!!

You can see the process of this one.
IMG_20180711_191347988.jpg
IMG_20180711_191347988.jpg (249.06 KiB) Viewed 1038 times
IMG_20180711_193119577_HDR.jpg
IMG_20180711_214704821_HDR.jpg
IMG_20180711_214708341_HDR.jpg
IMG_20180711_214756954.jpg
IMG_20180719_182109542.jpg
IMG_20180719_182109542.jpg (200.75 KiB) Viewed 1038 times
IMG_20180719_182138742.jpg
IMG_20180719_182138742.jpg (208.31 KiB) Viewed 1038 times

999zip999   100 GW

100 GW
Posts: 8427
Joined: Jan 10 2010 1:40pm
Location: Dana Point So. Cal

Re: Tesla Cells for sale as wrapped or welded packs

Post by 999zip999 » Jul 20 2018 3:33pm

? What is it . How about a Plastic ruler on top. Also what do you think it weighs ? Good power-sharing.

eric1565   10 W

10 W
Posts: 89
Joined: Feb 28 2015 4:50pm

Re: Tesla Cells for sale as wrapped or welded packs

Post by eric1565 » Jul 20 2018 11:11pm

It is a battery.... Lol... Each cell weighs about 53 grams all said and done 168 cells so ... Ugh math. Who uses this? 8.7kg

The thing is SOLID. I was surprised at how stiff it was with the new nylon holders..

It took me a number of designs to get there.

It fits in the triangle of a bike. Guy said 3C max pull. That nickle can take about 30amps per cell MAX. 15 amp per cell continuious is probably a good number

User avatar
Ultraman   1 W

1 W
Posts: 60
Joined: Apr 10 2009 11:25pm
Location: Toronto, Canada

Re: Tesla Cells for sale as wrapped or welded packs

Post by Ultraman » Jul 30 2018 11:01pm

Impressive work. PM sent regarding cell holders.
Vector frame, Adaptto Mid-E, MXUS 3k.
Tidal Force IO Cruiser, Lightning Rods mid drive.

999zip999   100 GW

100 GW
Posts: 8427
Joined: Jan 10 2010 1:40pm
Location: Dana Point So. Cal

Re: Tesla Cells for sale as wrapped or welded packs

Post by 999zip999 » Jul 31 2018 11:17am

I meant S and P and ah ect.

eric1565   10 W

10 W
Posts: 89
Joined: Feb 28 2015 4:50pm

Re: Tesla Cells for sale as wrapped or welded packs

Post by eric1565 » Aug 04 2018 8:27pm

Ah it was a 14S12P.

A pretty big boy. My charging battery 8S3P of 20ah pouch cells could not cycle half that battery. I may need to make a bigger cycle battery for big packs.

Eric

999zip999   100 GW

100 GW
Posts: 8427
Joined: Jan 10 2010 1:40pm
Location: Dana Point So. Cal

Re: Tesla Cells for sale as wrapped or welded packs

Post by 999zip999 » Aug 06 2018 7:58pm

168 cells ? What size is that thing how about putting a 12 oz beer can to it , or maybe a bottle of wine give us a clue. Or even a gallon of milk...

eric1565   10 W

10 W
Posts: 89
Joined: Feb 28 2015 4:50pm

Re: Tesla Cells for sale as wrapped or welded packs

Post by eric1565 » Aug 08 2018 4:32pm

Look at the cells they are 18mm in dia... There is your scale.

Yes 168 cells. Each cell is 11wh, so it is 1.8kwh pack. Big...

999zip999   100 GW

100 GW
Posts: 8427
Joined: Jan 10 2010 1:40pm
Location: Dana Point So. Cal

Re: Tesla Cells for sale as wrapped or welded packs

Post by 999zip999 » Aug 08 2018 9:37pm

Well I want a 160 cell triangle pack and since one is in front of you I thought you could put a tape measure on it so I wouldn't have to guess. It would need to fit my bike for me to be interested .Thank you for your support.

eric1565   10 W

10 W
Posts: 89
Joined: Feb 28 2015 4:50pm

Re: Tesla Cells for sale as wrapped or welded packs

Post by eric1565 » Aug 09 2018 1:59pm

Yes it was at the time of the picture taking, but is has been sent away.

See pic for dims... all in mm.
Solaire_design9.jpg
Eric

papabless   10 µW

10 µW
Posts: 6
Joined: Aug 05 2018 1:56pm

Re: Tesla Cells for sale as wrapped or welded packs

Post by papabless » Aug 10 2018 11:46pm

I'm interested in a 52v 40ah triangle battery pack to fit inside a 2018 trek ds 2. How much would it cost and weigh?

eric1565   10 W

10 W
Posts: 89
Joined: Feb 28 2015 4:50pm

Re: Tesla Cells for sale as wrapped or welded packs

Post by eric1565 » Aug 11 2018 10:38am

Printing cell holders for a guy. He gave me the specs and its printing. Also slowly improving my engraving looks...
IMG_20180811_103138402.jpg
I have another triangle pack to do

stephan_holders.jpg

eric1565   10 W

10 W
Posts: 89
Joined: Feb 28 2015 4:50pm

Re: Tesla Cells for sale as wrapped or welded packs

Post by eric1565 » Aug 19 2018 9:53pm

Another battery pack for a guy. This one is a 20S7P. It was difficult to come up with the right layout on this one. No real good way to get lots of nickel between the cells. I will have to solder a copper wire to the center of each one to help with electrical flow. The 25mm wide nickel maxes out at 38 amps... and that is MAX MAX MAX, like a 10 second pull. And he says he will have a 45 amp continuous, so I need more. A 16 Ga wire MAX's out at 58 amps... so that will work.

Below are pics of the progress.

Printing the holders... NYLON IS DA BOMB... SO much bettery than the cast urathane... SO SO SO much better!!!
IMG_20180818_185831757.jpg
IMG_20180819_092256106.jpg
IMG_20180819_091614191_HDR.jpg
IMG_20180819_213913886_HDR.jpg
IMG_20180819_213853635.jpg
IMG_20180819_210425975_HDR.jpg
IMG_20180819_201635861_HDR.jpg
Attachments
holders.jpg

eric1565   10 W

10 W
Posts: 89
Joined: Feb 28 2015 4:50pm

Re: Tesla Cells for sale as wrapped or welded packs

Post by eric1565 » Sep 09 2018 7:27pm

I got a module in this week. I am going to remove the cells and I will have 444 cells ready for sale late next week if anybody needs them, or packs made.

Eric

Solaire   1 mW

1 mW
Posts: 15
Joined: Apr 01 2018 8:22am

Re: Tesla Cells for sale as wrapped or welded packs

Post by Solaire » Sep 16 2018 9:26pm

are these new cells the 3200 or 3400 cells. thanks

eric1565   10 W

10 W
Posts: 89
Joined: Feb 28 2015 4:50pm

Re: Tesla Cells for sale as wrapped or welded packs

Post by eric1565 » Sep 17 2018 6:51am

The cells are from a 2016 70. So I don't know right now. My Icharger blew up last week, and I just sent it off to get fixed. Once I get it back I will check.

Eric

eric1565   10 W

10 W
Posts: 89
Joined: Feb 28 2015 4:50pm

Re: Tesla Cells for sale as wrapped or welded packs

Post by eric1565 » Oct 12 2018 6:13pm

I checked the capacity on the cells.

I cycled them from 4.1 to 3.0V and the capacity was 2800mah. So I think that is on par for 18650BE 3200mah cell with a realistic capacity of 3000mah.

If I had gone to 4.2 and 2.5, it would be much closer to 3000-3200mah, but I don't like to push the cells like that.

I will sell these cells for 3.85 each. I have over 300 if anybody is interested.

The cells come wrapped and washered.
IMG_20181012_181027715.jpg
Eric

eric1565   10 W

10 W
Posts: 89
Joined: Feb 28 2015 4:50pm

Re: Tesla Cells for sale as wrapped or welded packs

Post by eric1565 » Dec 21 2018 2:03pm

Here is the latest pack build. This is for a guy who will be putting a Magic Pie hub motor on his bike.

This was a 14S9P build. luckily he was in Houston so we could test fit. We found an interference and had to change the design a bit.
IMG_20181103_114730217.jpg
IMG_20181115_120708783.jpg
5.jpg
3.jpg
2.jpg


Here I am going thru each bank, 4 at a time and making sure there are no bad banks.
Usually they are all good. But one time one bank was down about 2600 mah, and it had a bad cell, or a bad weld job, not sure.
This pack had no issues so i was happy about that. When i cycle test them, I do 4.1V down to about 3.3V (under load) So this is an easy load on the batteries, and I usually get about 2600 mah per cell with that. I could go to 4.2V down to 3V, or 2.8V (under load) to get more mah, but I don't see a reason to stress the cells, it is a check to make sure all banks are very similar.