Hello,
Did anybody disassemble original Yamaha battery?
There are three connectors coming from battery, when fully charged 0V, 40V and 42V. Seems they are using 10s4p 2900 Li ion cells.
Could be possible to replace them?
Thanks.

Edit:
https://www.pedelecforum.de/forum/index ... ing.39480/
Attachments
IMG_20150612_171220.jpg
IMG_20150612_171353.jpg
Yamaha_X94_Manual.pdf
(2.41 MiB) Downloaded 284 times
Last edited by dusan on Nov 15 2017 5:29am, edited 2 times in total.

User avatar
Nobuo   10 kW

10 kW
Posts: 839
Joined: Nov 21 2014 3:38am
Location: Madrid

Re: Custom Bosch / Yamaha battery

Post by Nobuo » Jun 12 2015 1:18pm

the pack inside it will be highly probably spot welded, so you need to open and figures how the pack is mounted. Then you could take the BMS you will find connected inside to the pack and even use it in the new pack if you will dispose the cells.

As that cases are some times sealed, maybe you can't open and close again as it was before, so you maybe have to seal the pack again.

Be very careful opening the case, is too easy to short cells and conudctors if you use some like a screw driver
* Lithium + Air = Fire * <-----> ** Lithium + Chemical-Additives + Air = ZERO Fire **
<Battery and EV works>
https://facebook.com/evmadrid1
<Battery building resources>
http://www.endless-sphere.com/forums/vi ... 14&t=68005

dusan   100 W

100 W
Posts: 153
Joined: Aug 31 2014 2:10pm
Location: Slovakia

Re: Custom Bosch / Yamaha battery

Post by dusan » Jun 12 2015 2:45pm

Thank you Nobuo,
Can you please confirm my previous guesswork?
Are there really 10s4p 2900mah Li ion cells?
I'm using only Economy mode, so my current requirements are only up to 8 Amps. I additionally geared previous configuration with 42t rear sprocke, so 38t front and 42t rear within 29" wheels.
https://www.e-bikeshop.co.uk/Haibike-sD ... ne-RC-2015
I am very happy with bike at all but I can't achieve over 80km in XC terrain with Economy mode.
I was thinking to change 2900mah with Panasonic 3400mAh.
Also, why is there third connector pin with only 40V? To balance battery voltage drop? Actually I didn't notice voltage drop on output power.

Punx0r   100 GW

100 GW
Posts: 5514
Joined: May 03 2012 8:16am
Location: England

Re: Custom Bosch / Yamaha battery

Post by Punx0r » Jun 13 2015 5:23am

Unfortunately you have experienced the normal marketing (lies) for ebike range specification ;) Your battery is of modest capacity and the 80Km range will be based on flat, smooth ground, low speed and very minimal assist from the motor (basically, nearly all pedalling).

Upgrading to 3500mAh cells might work. This would give you ~500Wh of capacity, which should increase your range by 25%. Would this be enough?

dusan   100 W

100 W
Posts: 153
Joined: Aug 31 2014 2:10pm
Location: Slovakia

Re: Custom Bosch / Yamaha battery

Post by dusan » Jun 16 2015 1:23pm

Punx0r wrote:Unfortunately you have experienced the normal marketing (lies) for ebike range specification ;) Your battery is of modest capacity and the 80Km range will be based on flat, smooth ground, low speed and very minimal assist from the motor (basically, nearly all pedalling).

Upgrading to 3500mAh cells might work. This would give you ~500Wh of capacity, which should increase your range by 25%. Would this be enough?
yes, that would help
as i wrote, i don't need much current, just to increase capacity
I've understood, speak about assistance below 5Wh/km is nonsense.

Punx0r   100 GW

100 GW
Posts: 5514
Joined: May 03 2012 8:16am
Location: England

Re: Custom Bosch / Yamaha battery

Post by Punx0r » Jun 16 2015 3:33pm

nkon.nl is a good EU supplier of genuine 18650 cells, they have several in the 3400-3500mAh range.

What is the maximum power (watts) or current (amps) draw of your bike?

silentflight   100 W

100 W
Posts: 142
Joined: May 07 2007 5:42pm
Location: cloud 9.5

Re: Custom Bosch / Yamaha battery

Post by silentflight » Jun 16 2015 4:37pm

That looks like a very nice bike. I've ridden a 2014 Bosch Haibike and thought it was great, just wish it wouldn't stop the assist when you ride even somewhat fast. I found myself "riding over the top of the motor" if that makes sense to you. Essentially 90% leg power and 10% motor power just above the speed cutoff. I still thought it was a great bike, and will consider buying one when I know that I can disable the speed limiter.

How much did you pay for your bike and where did you buy it? Would be interested if it were available at better than list prices.

I've thought about how I would handle the battery situation, as I ride long distances. I ride a large cargo bike and average 7.5 Wh/km with a hub motor. With a lighter bike like yours and a mid-drive motor running in its sweet spot for efficiency I might get 6 Wh/km, but not much below that. I obviously like to pedal. I think I would buy a second battery to start with if I were you, but I know they are expensive. I wouldn't replace the cells in the battery that came with it- for another option I might make a second 10S 18650 pack to connect to it in parallel and keep it on a rear rack or in a pannier bag with a wire running up to the original battery on the down tube. This would involve opening the battery to solder on wires to connect to it in parallel and a hope that the BMS would tolerate the extra amp hours during discharge. I would charge them separately. Good luck with whatever route you choose, and have a blast riding it.

dusan   100 W

100 W
Posts: 153
Joined: Aug 31 2014 2:10pm
Location: Slovakia

Re: Custom Bosch / Yamaha battery

Post by dusan » Jun 23 2015 4:35pm

Thanks silent, it's great idea to have another battery in parallel but I ride XC. I am using Economy mode and I can tell, I usually support 50W, rest coming from motor. It's pretty enough after 38t / 42t upgrade. Yeah, I think to upgrade cells with more capacitive, 3500mAh or more. I will probably do it after battery warranty.
Max power should be around 700W, but I very unusually used it. I am riding up to 100% assistance, up to 250W, below 7 Amp.

Syonyk   10 kW

10 kW
Posts: 527
Joined: May 16 2015 12:41am

Re: Custom Bosch / Yamaha battery

Post by Syonyk » Jun 23 2015 6:36pm

Without opening the pack, you can't tell what the configuration is. It will be 10S almost certainly, but the parallel configuration will depend on the cells used. It could be 4P, it could be 5P with 2200mah cells (which, if I had to guess, I'd say is more likely - most commercial packs use the cheap cells, which are usually lower capacity).

Most packs can be rebuilt with higher capacity, but it's a somewhat involved project, involving spot welders, soldering irons, and a non-trivial bit of skill.

One thing to be aware of is that at least some of the higher capacity 18650s are not 4.2v cells - they're fully charged at 4.35v, which means if you charge to 4.2 per cell, you're not getting the full rated capacity. If you're coming from 2200mah cells, it's still a nice improvement in capacity, but check the discharge curves to see how much you're actually getting at 4.2v/cell.
Battery packs, Sunkko Welders, and more. http://syonyk.blogspot.com/

Malloot   10 mW

10 mW
Posts: 22
Joined: Jun 17 2015 8:16am

Re: Custom Bosch / Yamaha battery

Post by Malloot » Jun 24 2015 5:56am

Syonyk wrote:Without opening the pack, you can't tell what the configuration is. It will be 10S almost certainly, but the parallel configuration will depend on the cells used. It could be 4P, it could be 5P with 2200mah cells (which, if I had to guess, I'd say is more likely - most commercial packs use the cheap cells, which are usually lower capacity).

Most packs can be rebuilt with higher capacity, but it's a somewhat involved project, involving spot welders, soldering irons, and a non-trivial bit of skill.

One thing to be aware of is that at least some of the higher capacity 18650s are not 4.2v cells - they're fully charged at 4.35v, which means if you charge to 4.2 per cell, you're not getting the full rated capacity. If you're coming from 2200mah cells, it's still a nice improvement in capacity, but check the discharge curves to see how much you're actually getting at 4.2v/cell.
Not all 3500 or 3200 cells are 4.35V
http://www.dampfakkus.de/akkutest.php?id=577
http://www.dampfakkus.de/akkutest.php?id=537

I have opened Bosch packs they are 4p 2900 cells from Samsung, i am guessing that Yamaha uses the same cells. Both brands do not seem to want to go bigger size physically because of marketing and cleaner looks. Problem is that many customers do want bigger packs for higher range. Bosch actually makes high speed versions up to 45kmh support. Its a shame Yamaha doesn't do that as i like there systems support from 0 rpm more.

BTW i removed the speed sensor from one of the Yamaha bikes in the shop, unlike Bosch it still works and I was hoping to get unlimited support. However I was surprised to find support still stops at roughly 25kmh, no idea how they figure the speed out because the cadence is not a give away...

The best bet you have on increasing you range is just buying another pack and taking it with you, i would be hesitant to risk destroying your expensive pack and removing warranty of 500 charge cycle's. It might be expensive but thats the problem of buying the brand stuff, they overcharge you for that shit. LG MH1 cells alone would give you 1kwh for about 300 dollar but then you'd have to make the pack yourself

Syonyk   10 kW

10 kW
Posts: 527
Joined: May 16 2015 12:41am

Re: Custom Bosch / Yamaha battery

Post by Syonyk » Jun 24 2015 8:19am

If it is a 4p pack using 2900mah cells, there's really not much additional capacity you can cram in. Going from 2200mah cells to 3200-3500mah cells is a significant upgrade, but going from 2900mah to 3200-3500 is probably not worth the effort.
Battery packs, Sunkko Welders, and more. http://syonyk.blogspot.com/

dusan   100 W

100 W
Posts: 153
Joined: Aug 31 2014 2:10pm
Location: Slovakia

Re: Custom Bosch / Yamaha battery

Post by dusan » Sep 24 2015 2:56pm

Now I am not sure.
Yamaha battery is 500g heavier and warranty cycles are 700, two times more than Bosch.
There actually could be 10s5p configuration as 10 cells with 50g are 500g over.
Then it could really make a sense to buff it with 3500mAh cells. But I still worrying about warranty, I would probably need to buy spare one for service / warranty purposes.
So far I have 3.000km done, there is some capacity loosed but still fine. I guess, I could charge it around 50 times.

dusan   100 W

100 W
Posts: 153
Joined: Aug 31 2014 2:10pm
Location: Slovakia

Re: Custom Bosch / Yamaha battery

Post by dusan » Dec 04 2015 1:27pm

Regarding speed limit, there is a cheap solution
https://youtu.be/K8yF6mzg2aw
I didn't try since I'm riding mostly XC and don't feel need to ride faster but for road it could be definitely first approach I would try.

I looked at battery, because warranty said 1 year or 700 cycles and still over 50% original capacity, waiting for 50% of capacity is wasting of weight and time for me. I will probably go for another pack and experiment with current one. Looks like well assembled and after unsoldering PBC, cells could be replaced.

After around 4.000km, battery has started to be weak at 15% of remaining capacity. I did maybe around 100 cycles.
Attachments
IMG_20151204_191712.jpg
IMG_20151204_191747.jpg
IMG_20151204_192025.jpg
IMG_20151204_192042.jpg
IMG_20151204_192100.jpg
IMG_20151204_192116.jpg
IMG_20151204_192132.jpg
IMG_20151204_192154.jpg

dusan   100 W

100 W
Posts: 153
Joined: Aug 31 2014 2:10pm
Location: Slovakia

Re: Custom Bosch / Yamaha battery

Post by dusan » Jan 15 2016 2:47pm

So, it seems, my problem was solved by neoprene cover for battery and charging at room temp.
Last edited by dusan on Feb 28 2016 5:32am, edited 1 time in total.

User avatar
spinningmagnets   100 GW

100 GW
Posts: 11539
Joined: Dec 21 2007 10:27pm
Location: Ft Riley, NE Kansas

Re: Custom Bosch / Yamaha battery

Post by spinningmagnets » Jan 15 2016 4:58pm

Thank you for posting this, please take many pictures of all the details...

mwerme   1 µW

1 µW
Posts: 2
Joined: Mar 21 2017 9:44am
Location: Stockholm

Re: Custom Bosch / Yamaha battery

Post by mwerme » Mar 27 2017 3:52am

Dusan, did you by any chance take any additional pictures of the external connectors and how they connect inside the battery pack? Trying to use an identical pack to power a different e-bike but need to know which connectors to use.

User avatar
tumich   100 W

100 W
Posts: 209
Joined: May 28 2014 3:28am
Location: EU

Re: Custom Bosch / Yamaha battery

Post by tumich » May 10 2017 9:15am

Did anybody try to make 'custom additional battery' compatible with Bosch CX?
My ebikes:
1. Sur ron

Cheap, new, oryginal li-ion cells 18650 up to 3500mAh --> viewtopic.php?f=31&t=61608

Voltron   10 MW

10 MW
Posts: 2172
Joined: May 02 2013 4:53pm
Location: Santa Barbara CA

Re: Custom Bosch / Yamaha battery

Post by Voltron » May 10 2017 11:09am

Bosch pack internals fwiw..
bosch.jpg
bosch.jpg (71.74 KiB) Viewed 8168 times
packopen.jpg
packopen.jpg (56.18 KiB) Viewed 8168 times
boschbms.jpg
boschbms.jpg (53.87 KiB) Viewed 8168 times

User avatar
gamerpaddy   1 µW

1 µW
Posts: 4
Joined: Apr 26 2017 9:57am
Location: Germany

Re: Custom Bosch / Yamaha battery

Post by gamerpaddy » Jul 05 2017 3:16pm

sorry for late post.
but i reverse engineered the yamaha battery a year ago.


in case you want to build your own.
Just get a Arduino compatible board and a few discrete components.

Add a 5V source, i usually use a LM2596HV dc dc converter for this. A USB powerbank or even running it from two or three Cells on the pack (VIN pin of the arduino) will work.

Optional: To monitor the voltage add a voltage divider set to a ratio of 7.401 (42v in 5v out) and connect it to the A0 pin of the Arduino.

Edit this code https://pastebin.com/34SdehGt
>Edit line 35 to match your voltage divider. calculate or test to find out ADC values.
>Change line 44 and 45 (the number 20) to a value you want. 20 means it averages the current voltage 20 times to smooth it out. 20 is 5 seconds.
>Remove line 50 if you dont want your indicator to stay at 10% even if its lower. this prevent turning the motor off when voltage drops driving up a hill.

After that, Flash it in Arduino IDE

Wire it up like this.
Image

Some people including me allready did it to the haibikes, works great. See german pedelecforum.
If its too much for you, a guy called Cosas in pedelecforum is selling modules based off my code that does exactly this, basically dongles you put on the Battery connector and can connect any ordinary 36V Battery onto it.


Havent done anything on Bosch so far, i dont have Bosch.
###############################Signature##############################
i successfully reverse engineered the Yamaha DriveUnit Battery Protocol http://goo.gl/R1RWAc
>Haibike SDURO Hardnine SL 400Wh + 600Wh + SB SpeedBox

Daniel...   1 µW

1 µW
Posts: 1
Joined: Nov 24 2017 4:30am

Re: Custom Bosch / Yamaha battery

Post by Daniel... » Nov 24 2017 4:39am

hi guys i have problem. i dont know wich wire from charger fits to wire in battery. i change destroyed connector but i dont check it. there is four connectors from battery : white/blue and red/black from charger: black/yellow and red/blue ....somebody helps wich one from battery fits to wich one from charger thanks

ulikus   1 µW

1 µW
Posts: 2
Joined: Sep 19 2017 3:13pm

Re: Custom Bosch / Yamaha battery

Post by ulikus » Apr 28 2018 3:41am

gamerpaddy wrote:
Jul 05 2017 3:16pm
Havent done anything on Bosch so far, i dont have Bosch.
Hi! Got a Bosch Classic battery.
Want to make a replaceable BMS for it, but don't know where to start. (got programming knowledge and abit of EE-can wire and program arduino) just need to understand how to read data from battery )

Rumberopie   10 mW

10 mW
Posts: 22
Joined: Aug 12 2011 9:34pm

Re: Custom Bosch / Yamaha battery

Post by Rumberopie » May 20 2018 9:06am

Hi!
I try this circuit but don't work!
can you tell me the exact components you used?
Thanks

Joachim   1 kW

1 kW
Posts: 435
Joined: Jul 30 2015 1:02pm
Contact:

Re: Custom Bosch / Yamaha battery

Post by Joachim » May 20 2018 1:25pm

the rackpack Yamaha 500wh battery is a hel of a job :shock: a no go for hobby builders trust me :wink:

attila   1 µW

1 µW
Posts: 1
Joined: Dec 02 2018 10:21am

Re: Custom Bosch / Yamaha battery

Post by attila » Dec 02 2018 10:47am

gamerpaddy wrote:
Jul 05 2017 3:16pm
sorry for late post.
but i reverse engineered the yamaha battery a year ago.


in case you want to build your own.
Just get a Arduino compatible board and a few discrete components.

Add a 5V source, i usually use a LM2596HV dc dc converter for this. A USB powerbank or even running it from two or three Cells on the pack (VIN pin of the arduino) will work.

Optional: To monitor the voltage add a voltage divider set to a ratio of 7.401 (42v in 5v out) and connect it to the A0 pin of the Arduino.

Edit this code https://pastebin.com/34SdehGt
>Edit line 35 to match your voltage divider. calculate or test to find out ADC values.
>Change line 44 and 45 (the number 20) to a value you want. 20 means it averages the current voltage 20 times to smooth it out. 20 is 5 seconds.
>Remove line 50 if you dont want your indicator to stay at 10% even if its lower. this prevent turning the motor off when voltage drops driving up a hill.

After that, Flash it in Arduino IDE

Wire it up like this.
Image

Some people including me allready did it to the haibikes, works great. See german pedelecforum.
If its too much for you, a guy called Cosas in pedelecforum is selling modules based off my code that does exactly this, basically dongles you put on the Battery connector and can connect any ordinary 36V Battery onto it.


Havent done anything on Bosch so far, i dont have Bosch.
Please help me with the Yamaha 500 wh battery. It has 3 pins connecting it to the engine, I do not understand why. I would like to build a bigger battery than the yamaha 500 wh without a bms, but I do not understand how to connect it.

Pwnlord187   10 W

10 W
Posts: 73
Joined: Jul 27 2016 8:18pm

Re: Custom Bosch / Yamaha battery

Post by Pwnlord187 » Mar 22 2019 12:52am

If you bypass the discharge on your Yamaha battery pcb (cut the thick red/black wires going to the board from the discharge port, and solder them to the main leads of the pack, which are oval shaped solder pads on each end, the one closest to the port is positive) if you do this you won't be restricted by yamahas discharge limits, which are set to be overly conservative compared to how the cells can actually perform