Post by Wheazel » Jun 23 2015 6:47pm

First of all welcome to this buildthread. The purpose of this project is to create a long john style cargobike that I can use for a larger variety of needs and replace the car more.
It is going to very long, pretty dead on 3meters. This is quite abit longer than standard cargobikes.

The main reasons for this length are:
A 26" suspensionfork in the front to be able to use the best spiketyres incase i end up using it during wintertime. (also for ride comfort reasons)
The same "cargobay" length as other long john bikes. I glanced at the bullit.
A Revolt 120pro instead of a hubmotor makes the bike longer backwards since I am using bottombracket and cranks from an old donor mtb. (could have gone wider cranks and reduced some length)

The 35x1,24mm chromotubing showed to be hard to bend well, and I could not get the tube bent without waves on the inner radius.
This is no biggie for this application tho, as the tubes are superstrong anyway, and the frame feels extremely rigid.
The 25x1,24mm tubing is far easier to bend.

Some pics to start this thread, more to come.

Image
Image
Image
Image
Image
Image

User avatar
Wheazel   10 kW

10 kW
Posts: 969
Joined: Nov 02 2010 2:30pm
Location: Sundsvall, Sweden

Re: Cargobike project. Very long john from chromo tubing

Post by Wheazel » Jun 23 2015 6:47pm

Reserved

User avatar
Gregory   100 kW

100 kW
Posts: 1084
Joined: Jul 27 2007 9:18pm
Location: Perth, Western Australia

Re: Cargobike project. Very long john from chromo tubing

Post by Gregory » Jun 23 2015 7:17pm

Looking good Wheazel. Nice welds.


1) x5305 Hub Motor in a 24" Sun rim with 10G spokes, Kelly 72601 controller, 74V 10Ah Turnigy LiPo 20C Battery and CycleAnalyst
2) Mac 10T rear hub in a 700C "comfort bike" 15S 5Ah LiPo, stock 28A Xie Cheng controller
3) 38" Longboard, Turnigy 6374, CC Mamba XL2 ESC

User avatar
goodgnus   100 mW

100 mW
Posts: 49
Joined: May 14 2012 11:44am

Re: Cargobike project. Very long john from chromo tubing

Post by goodgnus » Jun 23 2015 7:42pm

Are you using a dedicated tubing bender with appropriately sized dies? Just curious.
I unlock Bionx systems! Removes all speed limits. Find my service posted on eBay or PM me.

User avatar
recumpence   100 GW

100 GW
Posts: 5301
Joined: Apr 19 2008 8:33am
Location: On Earth right now. That can change at any time, though..........

Re: Cargobike project. Very long john from chromo tubing

Post by recumpence » Jun 23 2015 7:51pm

Awesome. Best cargo chassis style around.

Love the attention to detail.

Matt
1% of the world's population can think "Outside the box". The rest are firmly stuck within the box. Where are you?

User avatar
Wheazel   10 kW

10 kW
Posts: 969
Joined: Nov 02 2010 2:30pm
Location: Sundsvall, Sweden

Re: Cargobike project. Very long john from chromo tubing

Post by Wheazel » Jun 24 2015 3:27am

goodgnus wrote:Are you using a dedicated tubing bender with appropriately sized dies? Just curious.
Yes dies of correct size and a pulling bender. Also tried sandfill in combination with the bender which improved the bends slightly, but didnt make them perfect.
I think the radius of the 35mm die I have in combination with the wall thickness of the 35mm pipe and material properties just makes a hard relationship.

User avatar
Wheazel   10 kW

10 kW
Posts: 969
Joined: Nov 02 2010 2:30pm
Location: Sundsvall, Sweden

Re: Cargobike project. Very long john from chromo tubing

Post by Wheazel » Jun 24 2015 4:52am

Some more
Image
Image
Image
Image
Image

User avatar
Wheazel   10 kW

10 kW
Posts: 969
Joined: Nov 02 2010 2:30pm
Location: Sundsvall, Sweden

Re: Cargobike project. Very long john from chromo tubing

Post by Wheazel » Jun 24 2015 6:05am

The rear swing is not made of 4130 to start with, due to simplicity and testing things out.
Might end up doing a more gracious chromo swing to replace it later on.

tahustvedt   10 kW

10 kW
Posts: 595
Joined: May 26 2014 9:31am
Location: Northern Norway

Re: Cargobike project. Very long john from chromo tubing

Post by tahustvedt » Jun 24 2015 11:01am

Looks good so far. I'm going to follow this. I like cargo bikes.

User avatar
amberwolf   100 GW

100 GW
Posts: 29861
Joined: Aug 17 2009 6:43am
Location: Phoenix, AZ, USA, Earth, Sol, Local Bubble, Orion Arm, Milky Way, Local Group
Contact:

Re: Cargobike project. Very long john from chromo tubing

Post by amberwolf » Jun 24 2015 2:11pm

I like it so far--but the cargo area seems pretty small. Is that just an illusion, or am I just used to my own stuff? :lol:

User avatar
Wheazel   10 kW

10 kW
Posts: 969
Joined: Nov 02 2010 2:30pm
Location: Sundsvall, Sweden

Re: Cargobike project. Very long john from chromo tubing

Post by Wheazel » Jun 24 2015 5:08pm

The cargo area is slightly longer than the bullitt bikes cargo area.
I figured it would be large enough for the majority of my transportation needs. Time will tell!

For reference
http://larryvsharry.com/technical-info/

User avatar
amberwolf   100 GW

100 GW
Posts: 29861
Joined: Aug 17 2009 6:43am
Location: Phoenix, AZ, USA, Earth, Sol, Local Bubble, Orion Arm, Milky Way, Local Group
Contact:

Re: Cargobike project. Very long john from chromo tubing

Post by amberwolf » Jun 25 2015 1:47am

Looks like the Bullitt is about 28" on the base of the cargo area?

It's not really small, I suppose, just I guess I'm spoiled. :lol:

I guess that's around what my CrazyBike2 could do across teh top of the cargo pods behind the seat (but then there is also the area within the pods, which is on the lefthand pod about 16" high x 17" long x 9.5" wide. The righthand pod is the same, minus the 1" styrofoam insulation against our heat, making it only 14" x 15" x 7.5". (but if I have icepacks in there on the way to the store and while shopping, to pre-chill it, icecream and other frozen stuff stays that way even on a hot day on a 30+ minute trip back home).

Anyway, sorry about the OT, I was just wondering cuz I keep looking at builds like yours and..was it 1KW? thinking I really ought to try actually building what had been called Loooooooongbike, and got renamed Barkfiet, but is still just ideas in it's thread and my head, cuz I don't know that I could actually use it unless I make it a narrow leanign trike frontend. (especially with the dog(s) riding on the platform).

User avatar
Gregory   100 kW

100 kW
Posts: 1084
Joined: Jul 27 2007 9:18pm
Location: Perth, Western Australia

Re: Cargobike project. Very long john from chromo tubing

Post by Gregory » Jun 25 2015 2:42am

You're probably thinking about 1000W aka Matt's long bike.


1) x5305 Hub Motor in a 24" Sun rim with 10G spokes, Kelly 72601 controller, 74V 10Ah Turnigy LiPo 20C Battery and CycleAnalyst
2) Mac 10T rear hub in a 700C "comfort bike" 15S 5Ah LiPo, stock 28A Xie Cheng controller
3) 38" Longboard, Turnigy 6374, CC Mamba XL2 ESC

User avatar
Wheazel   10 kW

10 kW
Posts: 969
Joined: Nov 02 2010 2:30pm
Location: Sundsvall, Sweden

Re: Cargobike project. Very long john from chromo tubing

Post by Wheazel » Jun 25 2015 3:07pm

More pics
Image
Image
Image
Image
Image
Image
Image
Image

User avatar
SkyknightJohn   100 W

100 W
Posts: 206
Joined: Jan 06 2012 8:56am
Location: Bloomington, IN USA

Re: Cargobike project. Very long john from chromo tubing

Post by SkyknightJohn » Jun 26 2015 3:39pm

Nice work. I like the use of rod ends for the swing arm pivots. I'll be watching your progress. :D

User avatar
Wheazel   10 kW

10 kW
Posts: 969
Joined: Nov 02 2010 2:30pm
Location: Sundsvall, Sweden

Re: Cargobike project. Very long john from chromo tubing

Post by Wheazel » Jun 29 2015 2:50pm

Some more pics!

Image
Image
Image
Image
Image
Image
Image

User avatar
Wheazel   10 kW

10 kW
Posts: 969
Joined: Nov 02 2010 2:30pm
Location: Sundsvall, Sweden

Re: Cargobike project. Very long john from chromo tubing

Post by Wheazel » Jul 04 2015 5:09pm

Amother update. This time around I have wasted about 15 hours on failed steering mechanism attempts. I think the current solution will be rigid enough. At least the first tests indicate that.
Spent alot of time making an arrangement for a push-pull wire commonly used with boat outboard motors. Ended up having too much slack, and was scrapped.

Image
Image
Image
Image
Last edited by Wheazel on Jul 05 2015 4:55am, edited 1 time in total.

User avatar
amberwolf   100 GW

100 GW
Posts: 29861
Joined: Aug 17 2009 6:43am
Location: Phoenix, AZ, USA, Earth, Sol, Local Bubble, Orion Arm, Milky Way, Local Group
Contact:

Re: Cargobike project. Very long john from chromo tubing

Post by amberwolf » Jul 05 2015 12:10am

FWIW, on my never-completed ReCycle, my first custom bike, I went thru a bunch of remote steering ideas, from pull cables to chain, etc...and none would actually work right (some close, but no cigar). I tried variations on some of them for my next bike, CrazyBike2, and ended up with a simple two-pivot/bearing pushrod on one side, which has evolved a little over time, but is still my preferred method. For redundancy I'd like to have one on each side, and then I could make them smaller, but it works like it is.

The present one is simply made from rod-end bearings screwed directly onto threaded rod, with double nuts and washers holding them in the right place once adjusted for length and straightness of steering. Then bolts directly run thru the bearing tubes into the 1/4" plate-steel mounts (one made from teh back of a desk chair, one from a car alternator mounting bracket), which are themselves welded to their respective ends of the steering mechanism. One is on the bottom end of the handlebar steerer pivot, and the other on a steel clamp-on stem on the fork's steerer.

There's a teensy amount of slop in it because teh bolts do not *completely* fill the bearing holes, but there's not enough slop to get any material I hve here in as shims. Close enough to not notice it while riding (especially compared to my previous version made from welded-closed eyebolts and rollerskate bearings and washers, scrwed into nuts welded to the ends of a hollow rod that used to be a weedeater handle).

User avatar
Wheazel   10 kW

10 kW
Posts: 969
Joined: Nov 02 2010 2:30pm
Location: Sundsvall, Sweden

Re: Cargobike project. Very long john from chromo tubing

Post by Wheazel » Jul 05 2015 5:03am

Ty for your insights Amberwolf, it is getting clear to me why a solid pushrod is so commonly used.
My main concern is that I have to compromise so much when using that solution.
26" wheel and suspensionfork makes the low-mount unconvenient, and my design doesnt support it well in its current state. (Would have to rebuild)
The high mount to the steertube interferes with the cargoarea.

I will give this wire steering a real testride when the time comes, and the solid rod will have to be the last resort solution.
I have beefed up some of the guidingpoints for the wire, and plan to use more tension for the real testride.

User avatar
amberwolf   100 GW

100 GW
Posts: 29861
Joined: Aug 17 2009 6:43am
Location: Phoenix, AZ, USA, Earth, Sol, Local Bubble, Orion Arm, Milky Way, Local Group
Contact:

Re: Cargobike project. Very long john from chromo tubing

Post by amberwolf » Jul 05 2015 3:38pm

Wheazel wrote:Ty for your insights Amberwolf, it is getting clear to me why a solid pushrod is so commonly used.
I didn't want to use one either, for a few reasons, but it was all I coudl get to work, and it's worked so well I stuck with it on CB2.

I know it's not the only way to do it, and I knwo cable steering and chain link steering can work, too, but as you're finding, the slop in the system has to be taken out and it's harder to do than in a solid rod.

One way is with a threaded cable adjuster, I forget exactly what they are called, but it has a threaded eyebolt in each end, with the cables tied to the eyebolts, and the adjuster when twisted one way brings the eyes together, tightening the cable, and the other way pushes them apart, loosening the cable.

I could not build tensioners like that or wheel-type tensioners (kinda like derailers) at the time, but if you can build adjustable tensioners you can secure after adjustment, like pressure rollers against the cable, you could take out any extra slack in the cable.


The high mount to the steertube interferes with the cargoarea.
There's an alternate, by bending strong tubing into a kind of L or long S shape, so that it runs along the bottom of the bike under the cargo area, until it gets to the front, past the cargo bay, then goes up to meet the steerer mount point up on the fork.

Another way is to go "around" the back of the tire, bending it outward instead of upward, and then reaching a pivot point that sticks out from the side of the fork somewhere.

I've seen both of those methods on pics of various bakfiets.


I hope you can make the cable steering work, because whatever you do for that I'd like to try out myself, when I eventually replace the tiller steering on the SB Cruiser trike. (which was meant to be temporary until I could build or get parts for the remote steering).

User avatar
ax57ax57   10 mW

10 mW
Posts: 20
Joined: Mar 16 2015 12:41pm
Location: Northern Arizona

Re: Cargobike project. Very long john from chromo tubing

Post by ax57ax57 » Jul 05 2015 4:36pm

One way is with a threaded cable adjuster, I forget exactly what they are called, but it has a threaded eyebolt in each end, with the cables tied to the eyebolts, and the adjuster when twisted one way brings the eyes together, tightening the cable, and the other way pushes them apart, loosening the cable.
AW, you're thinking of a turnbuckle. Turnbuckles allow for proper cable tensioning, and in a well-designed system you can achieve zero play with them. Cable control systems have been used as aircraft primary flight control systems since the very beginning of aviation because they are lightweight, reliable, and extraordinarily strong. In fact, even flight controls that have very large aerodynamic forces acting on them are normally only made with 1/8" (3.175mm) aircraft cable.

Wheazel, that heavy-duty cable that you're using is probably too heavy and stiff to be optimal. Some links below might give you some ideas based on cable control systems that are used in aircraft.

http://www.daerospace.com/MechanicalSys ... emDesc.php

http://avstop.com/ac/apgeneral/controlcables.html

http://luscombe.org/technicaldocs/controlcables.pdf
Rick

User avatar
Wheazel   10 kW

10 kW
Posts: 969
Joined: Nov 02 2010 2:30pm
Location: Sundsvall, Sweden

Re: Cargobike project. Very long john from chromo tubing

Post by Wheazel » Jul 05 2015 5:54pm

Hey, thanks for the inputs! I am actually using turnbuckles for the steering already, but will improve the way I bind the wire to the turnbuckles.
(Right now I have it welded directly to the turnbuckle) This makes me abit hesitant to tense the wire anymore, even if the guidsystem would handle it.
I am getting new turnbuckles tomorrow and will incorporate them with some proper wirelocks.
The reason for the 3mm wire, is to be able to increase tension without damaging the plastic guidewheels.

I will probably try a dyneema line if the 3mm wire solution is hard to get perfect. A dymeema line will be much more agile and direct, would probably lose slack at a lower tension than the wire.
However it is harder to fasten in the endwheels, would probably have to do some mods. It can be tied to forked turnbuckles, so that point is no problem.

Have also been thinking some about the flight controls in aircraft.
One main difference is that flight control surfaces are designed to be self stabilizing, most often the entire controlarea is behind the hinge axle. This makes the system more forgiving to slack.
I have built several model airplanes through the years and one I built was severely flawed on this point. The entire stabilizer was hinged, and had slightly more area infront of the rotationpoint than behind.
This ended up stripping the servos gears during a high speed pass and the plane crashed.

A front fork like this at the angle I have choosen, is not self centering at low speed. It wants to tip to the sides, and there is a small force required to steer from one side to the other and pass the straight position,
since you are basically lifting the front end of the bike slightly.

Anyways, ill report back about the results of the next mods. Got the rear brake temporarily installed, so I will just throw a casette and a chain on to try some basic biking around.
Will give a better picture than just rolling from small hills.

User avatar
Wheazel   10 kW

10 kW
Posts: 969
Joined: Nov 02 2010 2:30pm
Location: Sundsvall, Sweden

Re: Cargobike project. Very long john from chromo tubing

Post by Wheazel » Jul 08 2015 9:14am

So I made the mods to the wiresteering and it seems to work well now. Very direct and no bad behaviour. Have been doing some biking around both on and off road. Some bumpy riding and some smooth riding. A huge plus is the completely linear relation between handlebar turningangle and front wheel turningangle. (just like a regular bike) Turn radius is awesome for such a long bike as the front wheel can be turned somewhere around 70-80degrees in both directions before it bumps into the steeringstop. The tension on the wire is quite stiff, can almost be played like a guitar. I am hopeful for more tests at higher speeds etc, the bike feels very stable in general.

Image
Image
Image
Image
Image
Image

User avatar
Wheazel   10 kW

10 kW
Posts: 969
Joined: Nov 02 2010 2:30pm
Location: Sundsvall, Sweden

Re: Cargobike project. Very long john from chromo tubing

Post by Wheazel » Jul 16 2015 2:07pm

Some more progress. Getting close to start welding the battery.

Image
Image
Image
Image
Image

User avatar
Stielz   100 W

100 W
Posts: 202
Joined: May 20 2011 11:54pm
Location: Wellington, New Zealand

Re: Cargobike project. Very long john from chromo tubing

Post by Stielz » Jul 16 2015 4:58pm

Nice work. Damn thats a lot of batteries :!:

Post Reply