Samsung 30Q INR18650-30Q 3000mah 15a cell

Batteries, Chargers, and Battery Management Systems.
Post Reply
jk1   1 kW

1 kW
Posts: 339
Joined: Feb 27 2009 6:04am

Re: Samsung 30Q INR18650-30Q 3000mah 15a cell

Post by jk1 » Feb 04 2016 8:46pm

It will be interesting to see what the NCR18650GA's will do at 7a they should be ok at that since they are 10 a rated cells.

Pajda   1 kW

1 kW
Posts: 353
Joined: Jan 24 2016 3:45am
Location: Czech Republic

Re: Samsung 30Q INR18650-30Q 3000mah 15a cell

Post by Pajda » Feb 05 2016 3:43pm

jk1 wrote:It will be interesting to see what the NCR18650GA's will do at 7a they should be ok at that since they are 10 a rated cells.
The holy trinity of Samsung INR18650-35E, Sanyo NCR18650GA and LG INR18650 MJ1 as a highest capacity cells available on the market are good performers up to 3C discharge rate but they hate faster charging than standard 0,5C (this value of CHG current is recommended in datasheets of all three cells). Here you can see the results of cycle life tested at 1C-1C:

Image

I can tell you that Sanyo NCR18650GA have the lowest DCIR, but LG have superior cycle life under all conditions. I have also very bad experience with "High capacity" Samsung cells ("E" and "A" series) like 35E and 32A, they all have very poor cycle life. So I am a little surprised that "High power" ("Q" and "R" series) Samsungs cells are such a good performers.

okashira   10 kW

10 kW
Posts: 957
Joined: Nov 17 2014 6:45pm
Location: Houston, TX

Re: Samsung 30Q INR18650-30Q 3000mah 15a cell

Post by okashira » Feb 05 2016 3:46pm

Pajda wrote:
jk1 wrote:It will be interesting to see what the NCR18650GA's will do at 7a they should be ok at that since they are 10 a rated cells.
The holy trinity of Samsung INR18650-35E, Sanyo NCR18650GA and LG INR18650 MJ1 as a highest capacity cells available on the market are good performers up to 3C discharge rate but they hate faster charging than standard 0,5C (this value of CHG current is recommended in datasheets of all three cells). Here you can see the results of cycle life tested at 1C-1C:

Image

I can tell you that Sanyo NCR18650GA have the lowest DCIR, but LG have superior cycle life under all conditions. I have also very bad experience with "High capacity" Samsung cells ("E" and "A" series) like 35E and 32A, they all have very poor cycle life. So I am a little surprised that "High power" ("Q" and "R" series) Samsungs cells are such a good performers.
You're charging too fast. Run again charging the GA at 1.5A not 3.5A (!!!)
"Peace out - I'm done."
-- Bernhard Riemann, 1859

edisonmotors.net
Tesla Model S 18650 cells - like new - and custom packs from Tesla cells for sale. Any shape Any power Any capacity.
PM me or search my threads.

okashira   10 kW

10 kW
Posts: 957
Joined: Nov 17 2014 6:45pm
Location: Houston, TX

Re: Samsung 30Q INR18650-30Q 3000mah 15a cell

Post by okashira » Feb 05 2016 3:47pm

okashira wrote:
Pajda wrote:
jk1 wrote:It will be interesting to see what the NCR18650GA's will do at 7a they should be ok at that since they are 10 a rated cells.
The holy trinity of Samsung INR18650-35E, Sanyo NCR18650GA and LG INR18650 MJ1 as a highest capacity cells available on the market are good performers up to 3C discharge rate but they hate faster charging than standard 0,5C (this value of CHG current is recommended in datasheets of all three cells). Here you can see the results of cycle life tested at 1C-1C:

Image

I can tell you that Sanyo NCR18650GA have the lowest DCIR, but LG have superior cycle life under all conditions. I have also very bad experience with "High capacity" Samsung cells ("E" and "A" series) like 35E and 32A, they all have very poor cycle life. So I am a little surprised that "High power" ("Q" and "R" series) Samsungs cells are such a good performers.
You're charging too fast. Run again charging the GA at 1.5A not 3.5A (!!!)
ALl of those cycle life's are terrible. It's nice that the MJ1 outperformed in this test, but it's still unacceptable performance so these results can be mostly discounted. You need to reduce charge current substantially
"Peace out - I'm done."
-- Bernhard Riemann, 1859

edisonmotors.net
Tesla Model S 18650 cells - like new - and custom packs from Tesla cells for sale. Any shape Any power Any capacity.
PM me or search my threads.

Pajda   1 kW

1 kW
Posts: 353
Joined: Jan 24 2016 3:45am
Location: Czech Republic

Re: Samsung 30Q INR18650-30Q 3000mah 15a cell

Post by Pajda » Feb 05 2016 4:54pm

okashira wrote: ALl of those cycle life's are terrible. It's nice that the MJ1 outperformed in this test, but it's still unacceptable performance so these results can be mostly discounted. You need to reduce charge current substantially
Yes, I was doing those tests with this expectation. In short the meaning of this test was to determine what impact will have a fast charging in BEVs for those industrial grade cells in comparsion to the Tesla cells. And as you have already mentioned the impact is "devastating".
okashira wrote: You're charging too fast. Run again charging the GA at 1.5A not 3.5A (!!!)
As you wish :wink: 0,5C equals to 1700 mA (datasheet value of "Standard" charging current for both cells):

Image

Science Faction   1 W

1 W
Posts: 59
Joined: May 18 2009 10:23pm

Re: Samsung 30Q INR18650-30Q 3000mah 15a cell

Post by Science Faction » Feb 10 2016 11:46pm

Hi All, Great work and data in this thread.
Where are we upto in terms of suppliers?
What is the most reliable/cheapest supplier? especially for small units as I am doing a quadcopter project.
If anyone has bought them in bulk and wants to sell me 4 for testing I would be most appreciative.
Actualy I wouldn't mind 4 x 25R's as well.
Cheers
Paul

User avatar
ridethelightning   1 MW

1 MW
Posts: 1905
Joined: Jul 21 2013 9:48pm

Re: Samsung 30Q INR18650-30Q 3000mah 15a cell

Post by ridethelightning » Feb 11 2016 6:56am

best supplier for small quantities that I know is fasttech, 2x30Q ~$12(?) free shipping.
others have cheaper prices but you need to buy larger quantities to get a discount and to make the expensive shipping worthwhile

User avatar
TheBeastie   10 MW

10 MW
Posts: 2042
Joined: Jul 28 2012 12:31am
Location: Melbourne Australia

Re: Samsung 30Q INR18650-30Q 3000mah 15a cell

Post by TheBeastie » Feb 11 2016 8:10am

Pajda wrote:
okashira wrote: ALl of those cycle life's are terrible. It's nice that the MJ1 outperformed in this test, but it's still unacceptable performance so these results can be mostly discounted. You need to reduce charge current substantially
Yes, I was doing those tests with this expectation. In short the meaning of this test was to determine what impact will have a fast charging in BEVs for those industrial grade cells in comparsion to the Tesla cells. And as you have already mentioned the impact is "devastating".
okashira wrote: You're charging too fast. Run again charging the GA at 1.5A not 3.5A (!!!)
As you wish :wink: 0,5C equals to 1700 mA (datasheet value of "Standard" charging current for both cells):
Pajda, Quite fascinating to see how much poor performance you get with your cells when you charge them at a high rate..
I am wondering if other people get the same results if they charge at such a high rate...

I can see how its a worth while test because so many posts on on ES in general people buy/use/talk about massive high amp power supplies/charger setup so I can't help but assume they do in fact charge at these high rates.. I am guessing that its due to the logic that they feel its a better way to go if they bulk charge etc as they can be fully around with little waiting while its charging instead of very slowly charging overnight while they sleep or when not around at all..

Also the increase in resting time between chargers showing a larger increase in capacity is also very interesting, I remember in the final 6 months of using my last lipo pack that when I had left it on its ideal storage voltage for a good few months and came back to use it as a once off it had great performance for that single cycle and I figured leaving it rest a long time was some how internally 'recharging its batteries' so to speak but I never bothered mentioning it to anyone in the past.

Okashira, when I look at your charts/posts I haven't been able to see what charge rate you charge at?
http://i.imgur.com/LVpBOH3.jpg

okashira   10 kW

10 kW
Posts: 957
Joined: Nov 17 2014 6:45pm
Location: Houston, TX

Re: Samsung 30Q INR18650-30Q 3000mah 15a cell

Post by okashira » Feb 11 2016 2:38pm

TheBeastie wrote:
Pajda wrote:
okashira wrote: ALl of those cycle life's are terrible. It's nice that the MJ1 outperformed in this test, but it's still unacceptable performance so these results can be mostly discounted. You need to reduce charge current substantially
Yes, I was doing those tests with this expectation. In short the meaning of this test was to determine what impact will have a fast charging in BEVs for those industrial grade cells in comparsion to the Tesla cells. And as you have already mentioned the impact is "devastating".
okashira wrote: You're charging too fast. Run again charging the GA at 1.5A not 3.5A (!!!)
As you wish :wink: 0,5C equals to 1700 mA (datasheet value of "Standard" charging current for both cells):
Pajda, Quite fascinating to see how much poor performance you get with your cells when you charge them at a high rate..
I am wondering if other people get the same results if they charge at such a high rate...

I can see how its a worth while test because so many posts on on ES in general people buy/use/talk about massive high amp power supplies/charger setup so I can't help but assume they do in fact charge at these high rates.. I am guessing that its due to the logic that they feel its a better way to go if they bulk charge etc as they can be fully around with little waiting while its charging instead of very slowly charging overnight while they sleep or when not around at all..

Also the increase in resting time between chargers showing a larger increase in capacity is also very interesting, I remember in the final 6 months of using my last lipo pack that when I had left it on its ideal storage voltage for a good few months and came back to use it as a once off it had great performance for that single cycle and I figured leaving it rest a long time was some how internally 'recharging its batteries' so to speak but I never bothered mentioning it to anyone in the past.

Okashira, when I look at your charts/posts I haven't been able to see what charge rate you charge at?
http://i.imgur.com/LVpBOH3.jpg
I've been using ~2A until 3.8V, 1.5A to 4.15V for the 30Q

1.6A until 3.77V then 0.9A until 4.15V for the Model S cell
"Peace out - I'm done."
-- Bernhard Riemann, 1859

edisonmotors.net
Tesla Model S 18650 cells - like new - and custom packs from Tesla cells for sale. Any shape Any power Any capacity.
PM me or search my threads.

cwah   10 GW

10 GW
Posts: 4216
Joined: Jul 24 2011 5:42am
Location: Between paris and london

Re: Samsung 30Q INR18650-30Q 3000mah 15a cell

Post by cwah » Feb 11 2016 2:45pm

Yes i noticed that that's why i charge them as low as possible rate
Help me find my stolen electric brompton: http://bit.ly/1a0vbBC and Bosch Sinus B3 http://bit.ly/1eV0WQz

Pajda   1 kW

1 kW
Posts: 353
Joined: Jan 24 2016 3:45am
Location: Czech Republic

Re: Samsung 30Q INR18650-30Q 3000mah 15a cell

Post by Pajda » Feb 11 2016 3:31pm

okashira wrote:
I've been using ~2A until 3.8V, 1.5A to 4.15V for the 30Q

1.6A until 3.77V then 0.9A until 4.15V for the Model S cell
and cut-off currents pls?

Did you find any significant benefit by using "Tesla AVC" instead of standard CC-CV method? I hope I can start "2 stage AVC" tests for LG MJ1 cell samples this week ("Only" 2 stage AVC because the chinese tester ZKE EBC-A10 is limited to program 6 steps only). I think I can start with "1C-1C" equivalent at 100% DoD, so the time to full charge with 100mA cut-off is 1h 35min. I have already tried this settings:

1) CC-CV: 5,0A to 3,9V with 2,5A cut-off
2) CC-CV: 2,5A to 4,2V with 100mA cut-off

With this AVC setting the cell reach 4,2V within 45min (almost the same time as CC phase with 1C at 3,4A) but the finishing CV phase starting on 2,5A is much longer so the total charging time is 1h 50min.

okashira   10 kW

10 kW
Posts: 957
Joined: Nov 17 2014 6:45pm
Location: Houston, TX

Re: Samsung 30Q INR18650-30Q 3000mah 15a cell

Post by okashira » Feb 11 2016 3:42pm

Pajda wrote:
okashira wrote:
I've been using ~2A until 3.8V, 1.5A to 4.15V for the 30Q

1.6A until 3.77V then 0.9A until 4.15V for the Model S cell
and cut-off currents pls?

Did you find any significant benefit by using "Tesla AVC" instead of standard CC-CV method? I hope I can start "2 stage AVC" tests for LG MJ1 cell samples this week ("Only" 2 stage AVC because the chinese tester ZKE EBC-A10 is limited to program 6 steps only). I think I can start with "1C-1C" equivalent at 100% DoD, so the time to full charge with 100mA cut-off is 1h 35min. I have already tried this settings:

1) CC-CV: 5,0A to 3,9V with 2,5A cut-off
2) CC-CV: 2,5A to 4,2V with 100mA cut-off

With this AVC setting the cell reach 4,2V within 45min (almost the same time as CC phase with 1C at 3,4A) but the finishing CV phase starting on 2,5A is much longer so the total charging time is 1h 50min.
0.15A cut off for Model S cell
0.2A cut off for 30Q
"Peace out - I'm done."
-- Bernhard Riemann, 1859

edisonmotors.net
Tesla Model S 18650 cells - like new - and custom packs from Tesla cells for sale. Any shape Any power Any capacity.
PM me or search my threads.

okashira   10 kW

10 kW
Posts: 957
Joined: Nov 17 2014 6:45pm
Location: Houston, TX

Re: Samsung 30Q INR18650-30Q 3000mah 15a cell

Post by okashira » Feb 11 2016 3:43pm

Pajda wrote:
okashira wrote:
I've been using ~2A until 3.8V, 1.5A to 4.15V for the 30Q

1.6A until 3.77V then 0.9A until 4.15V for the Model S cell
and cut-off currents pls?

Did you find any significant benefit by using "Tesla AVC" instead of standard CC-CV method? I hope I can start "2 stage AVC" tests for LG MJ1 cell samples this week ("Only" 2 stage AVC because the chinese tester ZKE EBC-A10 is limited to program 6 steps only). I think I can start with "1C-1C" equivalent at 100% DoD, so the time to full charge with 100mA cut-off is 1h 35min. I have already tried this settings:

1) CC-CV: 5,0A to 3,9V with 2,5A cut-off
2) CC-CV: 2,5A to 4,2V with 100mA cut-off

With this AVC setting the cell reach 4,2V within 45min (almost the same time as CC phase with 1C at 3,4A) but the finishing CV phase starting on 2,5A is much longer so the total charging time is 1h 50min.
I have not done any comparisons to see if there is a benefit to the AVC method, however as you can see it's exactly what I am using.

I did cycle test using a supercharge algorithm, my tester does 10 steps so I am able to emulate it closely. I got really bad cycle life doing that.
"Peace out - I'm done."
-- Bernhard Riemann, 1859

edisonmotors.net
Tesla Model S 18650 cells - like new - and custom packs from Tesla cells for sale. Any shape Any power Any capacity.
PM me or search my threads.

okashira   10 kW

10 kW
Posts: 957
Joined: Nov 17 2014 6:45pm
Location: Houston, TX

Re: Samsung 30Q INR18650-30Q 3000mah 15a cell

Post by okashira » Feb 11 2016 3:47pm

See this post where I tried a fast charge
https://endless-sphere.com/forums/viewt ... 0#p1058819
I was using a pretty conservative supercharge, and it was the sole reason for the poor cycle life.
Reducing charge current fixed the cycle life

I am pretty sure you will rape the cell with the 5A / 2.5A charge setup, but give it a try. :)

My guess is Tesla uses pulse charging (ie, 8A for 100ms, 0a for 100ms) to cause the cells to warm up as much as possible at the beginning
"Peace out - I'm done."
-- Bernhard Riemann, 1859

edisonmotors.net
Tesla Model S 18650 cells - like new - and custom packs from Tesla cells for sale. Any shape Any power Any capacity.
PM me or search my threads.

Pajda   1 kW

1 kW
Posts: 353
Joined: Jan 24 2016 3:45am
Location: Czech Republic

Re: Samsung 30Q INR18650-30Q 3000mah 15a cell

Post by Pajda » Feb 11 2016 4:26pm

okashira wrote:See this post where I tried a fast charge
https://endless-sphere.com/forums/viewt ... 0#p1058819
For the next time I should read the whole thread before I ask for what was already mentioned :)
okashira wrote: I was using a pretty conservative supercharge, and it was the sole reason for the poor cycle life.
Reducing charge current fixed the cycle life
hmmm...
okashira wrote: I am pretty sure you will rape the cell with the 5A / 2.5A charge setup, but give it a try. :)
I also think there will be a short end. :twisted: But the cell perform very well even at 5A charging current. The phase of 5A CC takes only 10min and after that the cell is only a barely hot (I usually have IR camera and temperature data logger but not at this time) but I can easily hold my hand on the cell. :roll:

okashira wrote: My guess is Tesla uses pulse charging (ie, 8A for 100ms, 0a for 100ms) to cause the cells to warm up as much as possible at the beginning
That is a new information for me... But I do not believe that pulse charging with average value of 4A will generate much more heat inside the cell than 4A continuously.

User avatar
parabellum   10 MW

10 MW
Posts: 2079
Joined: Nov 19 2010 9:55am
Location: Dominican Republic, north.

Re: Samsung 30Q INR18650-30Q 3000mah 15a cell

Post by parabellum » Feb 11 2016 4:38pm

Pajda wrote: But I do not believe that pulse charging with average value of 4A will generate much more heat inside the cell than 4A continuously.
Not much more, just double. :D

okashira   10 kW

10 kW
Posts: 957
Joined: Nov 17 2014 6:45pm
Location: Houston, TX

Re: Samsung 30Q INR18650-30Q 3000mah 15a cell

Post by okashira » Feb 11 2016 4:48pm

Pajda wrote:
okashira wrote:See this post where I tried a fast charge
https://endless-sphere.com/forums/viewt ... 0#p1058819
For the next time I should read the whole thread before I ask for what was already mentioned :)
okashira wrote: I was using a pretty conservative supercharge, and it was the sole reason for the poor cycle life.
Reducing charge current fixed the cycle life
hmmm...
okashira wrote: I am pretty sure you will rape the cell with the 5A / 2.5A charge setup, but give it a try. :)
I also think there will be a short end. :twisted: But the cell perform very well even at 5A charging current. The phase of 5A CC takes only 10min and after that the cell is only a barely hot (I usually have IR camera and temperature data logger but not at this time) but I can easily hold my hand on the cell. :roll:

okashira wrote: My guess is Tesla uses pulse charging (ie, 8A for 100ms, 0a for 100ms) to cause the cells to warm up as much as possible at the beginning
That is a new information for me... But I do not believe that pulse charging with average value of 4A will generate much more heat inside the cell than 4A continuously.
I did a supercharge and recorded temperature here:
https://www.youtube.com/watch?v=vFrTUlYIQww

Heat is not the problem with high charge current. Actually, the hotter the better because the lithium ions can diffuse faster.
http://lithiumbatteryresearch.com/Plating.php
"Peace out - I'm done."
-- Bernhard Riemann, 1859

edisonmotors.net
Tesla Model S 18650 cells - like new - and custom packs from Tesla cells for sale. Any shape Any power Any capacity.
PM me or search my threads.

okashira   10 kW

10 kW
Posts: 957
Joined: Nov 17 2014 6:45pm
Location: Houston, TX

Re: Samsung 30Q INR18650-30Q 3000mah 15a cell

Post by okashira » Feb 17 2016 1:58am

Updated 30Q, 7A model S.

IN RED - Also added another Model S cell. This one I charge to 4.05V with a 0.2A cut. Discharge to 2.9V with 5A. The first few cycles I set the charge cut wrong so it was high.

Image

Remind me to fix the labels and descriptions...
"Peace out - I'm done."
-- Bernhard Riemann, 1859

edisonmotors.net
Tesla Model S 18650 cells - like new - and custom packs from Tesla cells for sale. Any shape Any power Any capacity.
PM me or search my threads.

okashira   10 kW

10 kW
Posts: 957
Joined: Nov 17 2014 6:45pm
Location: Houston, TX

Re: Samsung 30Q INR18650-30Q 3000mah 15a cell

Post by okashira » Feb 28 2016 7:51pm

Updated\
Seems the Model S cell has some sort of self healing characteristic. Very interesting.
Any significant pause in cycle testing results in improved capacity.
All of the same pauses are done on the 30Q, and it only results in the same or reduced capacity.
Image
"Peace out - I'm done."
-- Bernhard Riemann, 1859

edisonmotors.net
Tesla Model S 18650 cells - like new - and custom packs from Tesla cells for sale. Any shape Any power Any capacity.
PM me or search my threads.

User avatar
Wheazel   10 kW

10 kW
Posts: 970
Joined: Nov 02 2010 2:30pm
Location: Sundsvall, Sweden

Re: Samsung 30Q INR18650-30Q 3000mah 15a cell

Post by Wheazel » Feb 29 2016 7:06am

That is very intresting indeed. Wonder what process lies behind this data...

User avatar
bigbore   10 kW

10 kW
Posts: 537
Joined: Sep 25 2009 7:43am
Location: Italy

Re: Samsung 30Q INR18650-30Q 3000mah 15a cell

Post by bigbore » Feb 29 2016 1:21pm

Is there any comparison between Model S and 30Q at 10A discharge (not cycle testing)?

User avatar
riba2233   1 MW

1 MW
Posts: 1852
Joined: Jun 30 2013 10:23am
Location: Croatia

Re: Samsung 30Q INR18650-30Q 3000mah 15a cell

Post by riba2233 » Feb 29 2016 2:16pm

I have both cells at home, but can only test up to 5 A...
My electric moped: http://www.evalbum.com/4966

My electric car: http://www.evalbum.com/5364

User avatar
bigbore   10 kW

10 kW
Posts: 537
Joined: Sep 25 2009 7:43am
Location: Italy

Re: Samsung 30Q INR18650-30Q 3000mah 15a cell

Post by bigbore » Feb 29 2016 2:53pm

riba2233 wrote:I have both cells at home, but can only test up to 5 A...
Do you want to look at my poor discharge setup? I could make a little video tomorrow :D
These days I've been checking my old zippy lipos cells to make a 3s?p pack to use with your spot welder and I can discharge single lithium cells at 10A +/- 0.100A

User avatar
riba2233   1 MW

1 MW
Posts: 1852
Joined: Jun 30 2013 10:23am
Location: Croatia

Re: Samsung 30Q INR18650-30Q 3000mah 15a cell

Post by riba2233 » Feb 29 2016 6:04pm

That's great, now you only need cells :)
My electric moped: http://www.evalbum.com/4966

My electric car: http://www.evalbum.com/5364

User avatar
hillzofvalp   1 MW

1 MW
Posts: 1878
Joined: Dec 26 2010 2:09am
Location: Los Angeles, CA

Re: Samsung 30Q INR18650-30Q 3000mah 15a cell

Post by hillzofvalp » Feb 29 2016 6:23pm

Anyone willing to cycle the HG2 at 2A charge, 7A discharge?

Post Reply