Custom aluminum frame with 2.8kwh capacity

General Discussion about electric bicycles.
User avatar
Ratking   1 kW

1 kW
Posts: 499
Joined: May 20 2010 5:27am
Location: Norway

Custom aluminum frame with 2.8kwh capacity

Post by Ratking » May 10 2015 8:31am

Hello,

The time has come to build a commuter bike for commuting around the city I soon move to.
I got some requirements that I want to incorporate to the frame, but nothing is set in stone.

Specs:
-Aluminium frame
-<100v pack so I can use 4410 fets
-Large battery pack build with Enerdel cells
-The biggest hub motor with freewheel I can get my hands on
-If possible, 17" motowheels in aluminum. I want to try mc tires
-All components either downhill specs or stronger
-Power and throttle controlled by CA v3
-Good acceleration and a top speed >80km'h

The basis for the frame is an old Specialized Big Hit. They is some old parts from my other mid drive build and I wanted to recycle them.
The Enerdel cells are large. I really hoped to design a neat and good looking frame, but that did not happend. No way that it was possible to put more than one cell in one plane without making the frame bulky and large. But I wanted a large capacity bike, so I did the best I could.

Weight guesstimate:
Battery, 22s2p, 470g x 44= 20.68kg
Hub motor, commonly around 12 kg with wheel
Complete frame ex rear wheel/motor= 22kg
Total weight=55kg

I hope that I can get the weight below 55kg, but I don't care. I am a big man and I can handle 55kg. I just hope that the bike can handle my 115kg's.

Frame is built with 4mm 5052 aluminum. Easy to weld and can be bent without cracking. I found out that the aluminum was very dirty, so I had problems with getting good welds. I used a lot of gas and time just to heat up the aluminum and get the contamination out.
For the motor I hoped that QS motor could supply me with their 273mm motor, but since they don't reply to mails anymore I wont send them any money before the explain themselves. I am open to any suggestion for a big hub motor with lots of torque.

Below is a couple of pictures of what I did in one session. I think it is possible to make a frame from scratch in one day if you have enough welding gas, food and patience :lol:
Attachments
IMG_0351_640x480.jpg
IMG_0351_640x480.jpg (47.38 KiB) Viewed 6432 times
IMG_0352_640x480.jpg
IMG_0352_640x480.jpg (46.29 KiB) Viewed 6432 times
IMG_0353_640x480.jpg
IMG_0353_640x480.jpg (46.23 KiB) Viewed 6432 times
IMG_0354_640x480.jpg
IMG_0354_640x480.jpg (39.75 KiB) Viewed 6432 times
IMG_0358_640x480.jpg
IMG_0358_640x480.jpg (41.52 KiB) Viewed 6432 times
IMG_0359_640x480.jpg
IMG_0359_640x480.jpg (57.2 KiB) Viewed 6432 times
IMG_0360_640x480.jpg
IMG_0360_640x480.jpg (58.92 KiB) Viewed 6432 times
IMG_0362_640x480.jpg
IMG_0362_640x480.jpg (45.01 KiB) Viewed 6432 times
IMG_0364_640x480.jpg
IMG_0364_640x480.jpg (57.95 KiB) Viewed 6432 times
IMG_0366_640x480.jpg
IMG_0366_640x480.jpg (46.29 KiB) Viewed 6432 times
IMG_0371_640x480.jpg
IMG_0371_640x480.jpg (42 KiB) Viewed 6432 times
Last edited by Ratking on May 10 2016 3:08am, edited 2 times in total.

User avatar
beast775   100 kW

100 kW
Posts: 1208
Joined: Jul 05 2007 11:55am
Location: victoria british columbia

Re: Custom aluminum frame with 2.8kw/h capacity

Post by beast775 » May 10 2015 1:03pm

Holy smokes :shock: thats alotta work for 1 day,gonna be a great build.
2 FINGER SALUTE TO ESSO.no buying gasoline for 14 years now.
I spent all my money on bicycles women and beer the rest i just wasted.

User avatar
Ratking   1 kW

1 kW
Posts: 499
Joined: May 20 2010 5:27am
Location: Norway

Re: Custom aluminum frame with 2.8kw/h capacity

Post by Ratking » May 10 2015 4:02pm

beast775 wrote:Holy smokes :shock: thats alotta work for 1 day,gonna be a great build.
Thank you. I hope so myself :wink:

I started to calculate what the parts I needed would cost, this is an expensive hobby for sure. Just a good pair of front forks and rear shock is several hundred dollars for the absolute cheapest option. And I need a motor, controller, wheels, tires etc. I need to get a second job...

User avatar
Ratking   1 kW

1 kW
Posts: 499
Joined: May 20 2010 5:27am
Location: Norway

Re: Custom aluminum frame with 2.8kw/h capacity

Post by Ratking » Apr 25 2016 7:02am

I want to resurrect this project from the dead ;)

I have been busy with other projects this winter and started to collect parts and plans this spring.
I will just trow out some progress pictures as for now and give a better explanation later.

Final spec:

Motor QS 205 4t
Controller Sabvoton 72150
Battery Enerdel 20s 35Ah
Rims: MT-2.5 17" motorcycle(will try tubeless)
Bunch of downhill stuff that I will not bother listing, just the usual

What is pictured is a lot of hours in cleaning and welding etc. Still my welding skills such at aluminum. The parts has to be clean and use the right filler rod etc. I had problems with the types of aluminum/alloy I wanted to join, but as long as it holds together for a while ;)
Due to luck I now have access to a lathe and mill. So this project should now soon be done. I really look forward to feel the power from a QS 205 in a 17" rim. I hope it is not over hyped.
Attachments
IMG_2252 (Small).JPG
IMG_2252 (Small).JPG (60.87 KiB) Viewed 6186 times
IMG_2253 (Small).JPG
IMG_2253 (Small).JPG (71.26 KiB) Viewed 6186 times
IMG_2254 (Small).JPG
IMG_2254 (Small).JPG (71.44 KiB) Viewed 6186 times
IMG_2255 (Small).JPG
IMG_2255 (Small).JPG (64.27 KiB) Viewed 6186 times
IMG_2262 (Small).JPG
IMG_2262 (Small).JPG (68.81 KiB) Viewed 6186 times
IMG_2263 (Small).JPG
IMG_2263 (Small).JPG (55.03 KiB) Viewed 6186 times
IMG_2265 (Small).JPG
IMG_2265 (Small).JPG (64.41 KiB) Viewed 6186 times
IMG_2266 (Small).JPG
IMG_2266 (Small).JPG (61.69 KiB) Viewed 6186 times
IMG_2268 (Small).JPG
IMG_2268 (Small).JPG (70.51 KiB) Viewed 6186 times
IMG_2270 (Small).JPG
IMG_2270 (Small).JPG (62.74 KiB) Viewed 6186 times
IMG_2273 (Small).JPG
IMG_2273 (Small).JPG (72.51 KiB) Viewed 6186 times
IMG_2272 (Small).JPG
IMG_2272 (Small).JPG (56.07 KiB) Viewed 6186 times
IMG_2274 (Small).JPG
IMG_2274 (Small).JPG (51.99 KiB) Viewed 6186 times
IMG_2276 (Small).JPG
IMG_2276 (Small).JPG (72.13 KiB) Viewed 6186 times
IMG_2277 (Small).JPG
IMG_2277 (Small).JPG (38.44 KiB) Viewed 6186 times

User avatar
Ratking   1 kW

1 kW
Posts: 499
Joined: May 20 2010 5:27am
Location: Norway

Re: Custom aluminum frame with 2.8kw/h capacity

Post by Ratking » May 09 2016 4:18am

Got some more work done, the main machining and steelwork is done, so I hope to get the wheels lanced soon and try this bike out. The weather got much better, so I would have liked to have the bike done by now :/

I did see something that I don't like, the exit/gap for the phase wires between the drop out and disc brake is too small. What do people do in order to protect the wires from being chewed over by the turning parts and the drop out? I would like a permanent solution, capable of withstanding a few rolls and crashes

The QS hub motor looks nice, I hope it performs well in a 17" rim.
Attachments
IMG_2341 (Custom).JPG
IMG_2341 (Custom).JPG (55.72 KiB) Viewed 6045 times
IMG_2342 (Custom).JPG
IMG_2342 (Custom).JPG (50 KiB) Viewed 6045 times
IMG_2344 (Custom).JPG
IMG_2344 (Custom).JPG (34.42 KiB) Viewed 6045 times
IMG_2345 (Custom).JPG
IMG_2345 (Custom).JPG (62.97 KiB) Viewed 6045 times
IMG_2347 (Custom).JPG
IMG_2347 (Custom).JPG (42.45 KiB) Viewed 6045 times
IMG_2349 (Custom).JPG
IMG_2349 (Custom).JPG (70.85 KiB) Viewed 6045 times
IMG_2350 (Custom).JPG
IMG_2350 (Custom).JPG (70.78 KiB) Viewed 6045 times

User avatar
izeman   100 GW

100 GW
Posts: 5072
Joined: Jun 21 2011 8:25am
Location: Vienna, Austria
Contact:

Re: Custom aluminum frame with 2.8kw/h capacity

Post by izeman » May 09 2016 9:36am

you are CRAZY! i like it :) what alloy did you use? 6xxx or 7xxx? (and please remove the slash between 2.8kW and h in your topic :mrgreen: )
edit: reread the thread. you mention 5052 alloy. so you're mixing 6'alloy and 5'alloy? can you heat treat the frame? or do you just build it stronger?

User avatar
Ratking   1 kW

1 kW
Posts: 499
Joined: May 20 2010 5:27am
Location: Norway

Re: Custom aluminum frame with 2.8kw/h capacity

Post by Ratking » May 10 2016 1:57am

izeman wrote:you are CRAZY! i like it :) what alloy did you use? 6xxx or 7xxx? (and please remove the slash between 2.8kW and h in your topic :mrgreen: )
edit: reread the thread. you mention 5052 alloy. so you're mixing 6'alloy and 5'alloy? can you heat treat the frame? or do you just build it stronger?
I am mixing everything ;) I just hope that the frame don't break at the front crown/ head tube. The head tube is extra long and well welded. But I hope it will handle the stress without any heat treatment. Having a front fork with 200mm stroke will take some of the beating of the head tube. The frame is 6mm 5052, mated to 6000 series alloy on the big hit frame, so compared to the orignial thickness I have trippeled the wall thickness. Lets hope that is enough ;)

User avatar
ridethelightning   1 MW

1 MW
Posts: 1870
Joined: Jul 21 2013 9:48pm

Re: Custom aluminum frame with 2.8kwh capacity

Post by ridethelightning » May 10 2016 6:07am

holy crap!
one of the most fast and furious builds iv seen!

migueralliart   10 kW

10 kW
Posts: 890
Joined: Apr 08 2011 7:32pm
Location: West Palm Beach , FL
Contact:

Re: Custom aluminum frame with 2.8kwh capacity

Post by migueralliart » May 10 2016 9:43am

Great build .. excellent welding and machining skills.

Eager to see the end result.

User avatar
Merlin   10 MW

10 MW
Posts: 2015
Joined: Jan 29 2013 10:00am
Location: europe

Re: Custom aluminum frame with 2.8kwh capacity

Post by Merlin » May 12 2016 3:17am

looks badass Ratking ....

plz take a look at the statorade groupbuy :wink:

User avatar
macribs   1.21 GW

1.21 GW
Posts: 3648
Joined: Jul 22 2014 5:59pm

Re: Custom aluminum frame with 2.8kwh capacity

Post by macribs » May 16 2016 1:40pm

Kool frame. What made you choose those batteries?

User avatar
Samd   1.21 GW

1.21 GW
Posts: 3667
Joined: Jun 28 2011 11:08pm
Location: Ballarat, AU
Contact:

Re: Custom aluminum frame with 2.8kwh capacity

Post by Samd » May 16 2016 8:53pm

I've chopped a lot of frames - and this is some really cool work. Well done!
http://ballaratebikes.com/

ImageImageImage
"Knowledge is knowing that a tomato is a fruit. Wisdom is knowing that a 165mm rear shock can't deliver 220mm of rear swingarm travel." - Oprah Winfrey.

User avatar
Brake   100 W

100 W
Posts: 285
Joined: Jan 24 2014 12:58am
Location: Spokane, Wa

Re: Custom aluminum frame with 2.8kwh capacity

Post by Brake » May 17 2016 3:12am

Cool build for sure. Looking forward to watching it unfold. Nice job!

User avatar
multifrag   100 W

100 W
Posts: 120
Joined: Feb 19 2016 5:44am
Location: London, UK

Re: Custom aluminum frame with 2.8kwh capacity

Post by multifrag » May 17 2016 8:03am

Is it cost effective to use Enerdel cells over 18650s?

User avatar
izeman   100 GW

100 GW
Posts: 5072
Joined: Jun 21 2011 8:25am
Location: Vienna, Austria
Contact:

Re: Custom aluminum frame with 2.8kwh capacity

Post by izeman » May 18 2016 1:05am

multifrag wrote:Is it cost effective to use Enerdel cells over 18650s?
most probably not, but easier to build, and easier to manage. you can monitor every single cell and if one fails you will notice it immediately.

User avatar
Ratking   1 kW

1 kW
Posts: 499
Joined: May 20 2010 5:27am
Location: Norway

Re: Custom aluminum frame with 2.8kwh capacity

Post by Ratking » May 19 2016 3:26am

macribs wrote:Kool frame. What made you choose those batteries?
Thank you, I got a really good deal. Else I would have chosen the Volt or any other smaller format. To be honest, the frame is a bit bulky for my taste, but it was the only way of getting 20s2p in there ;)

User avatar
Ratking   1 kW

1 kW
Posts: 499
Joined: May 20 2010 5:27am
Location: Norway

Re: Custom aluminum frame with 2.8kwh capacity

Post by Ratking » May 19 2016 3:27am

multifrag wrote:Is it cost effective to use Enerdel cells over 18650s?
If you are lucky enough to get them cheap and you have the space. they are also delivered as OEM and that speaks volume of the quality for me. Less connections is also a big plus

User avatar
Ratking   1 kW

1 kW
Posts: 499
Joined: May 20 2010 5:27am
Location: Norway

Re: Custom aluminum frame with 2.8kwh capacity

Post by Ratking » Sep 16 2016 1:55am

After a long break, due to lack of will to measure custom spokes for the back and front wheel, I am finally back :P
This should have been done for several months ago, but it is now bought, delivered and awesome. I did actually measure the right length and the chineese company delivered nice, stainless spokes and nipples for the job.

What I got is two 17"x2.5" super motard rims that will be used with Michelin Pilot sport tires. I want to be able to drive hard and corner like a super motard and not a bike. I had to use super heavy gauge spokes, because of the nipple holes. Spokes are 9G, hope they dont break anything.

Next step is to get the wheel straight, put on some new tires and try them on the bike, can't wait to try the bike out, I feel this bike will be solid and have a large enough battery pack to be useful
Attachments
IMG_2824 (Small).JPG
IMG_2824 (Small).JPG (31.95 KiB) Viewed 5064 times
IMG_2848 (Small).JPG
IMG_2848 (Small).JPG (22.86 KiB) Viewed 5064 times
IMG_2870 (Small).JPG
IMG_2870 (Small).JPG (58.64 KiB) Viewed 5064 times
IMG_2872 (Small).JPG
IMG_2872 (Small).JPG (61.7 KiB) Viewed 5064 times
IMG_2875 (Small).JPG
IMG_2875 (Small).JPG (67.03 KiB) Viewed 5064 times

User avatar
Ratking   1 kW

1 kW
Posts: 499
Joined: May 20 2010 5:27am
Location: Norway

Re: Custom aluminum frame with 2.8kwh capacity

Post by Ratking » Sep 16 2016 4:55am

I bought a 20 mm front hub with 36 spoke holes, they don't come cheap from Hope. Did not like to bore out the hub for bigger spokes, feels wrong :/
Attachments
IMG_2890 (Small).JPG
IMG_2890 (Small).JPG (49.35 KiB) Viewed 5048 times
IMG_2891 (Small).JPG
IMG_2891 (Small).JPG (52.11 KiB) Viewed 5048 times
IMG_2892 (Small).JPG
IMG_2892 (Small).JPG (46.92 KiB) Viewed 5048 times

User avatar
Ratking   1 kW

1 kW
Posts: 499
Joined: May 20 2010 5:27am
Location: Norway

Re: Custom aluminum frame with 2.8kwh capacity

Post by Ratking » Sep 26 2016 3:15am

More work has been done, but mostly planning and tinkering around how to safely incorporate a battery pack with enough compression. When I first made the frame I had four 90 degree aluminum angles welded to the frame that was there to hold the cells in t position, but I did not like the design and cut the parts out. That did not go as planned due to an angle grinder doing more work than I wanted :cry: The disk hit the bone and they had to brush and scrape all the particles out of there. Not the best feeling when you can feel metal chew against your bone

What I have decided is to use half the plastic mounts on the Enerdel modules to make them thinner, I don't think it will do any difference regarding safety. I don't have much room to work with, so it must be like this anyway.

I also welded a new bottom bracket in place. The old one was welded with with the left threads on the right side :/
Attachments
IMG_2930 (Small).JPG
IMG_2930 (Small).JPG (60.59 KiB) Viewed 4920 times
IMG_2931 (Small).JPG
IMG_2931 (Small).JPG (53.36 KiB) Viewed 4920 times
IMG_2948 (Small).JPG
IMG_2948 (Small).JPG (61.74 KiB) Viewed 4920 times
IMG_2946 (Small).JPG
IMG_2946 (Small).JPG (57.08 KiB) Viewed 4920 times
IMG_2960 (Small).JPG
IMG_2960 (Small).JPG (41.86 KiB) Viewed 4920 times
IMG_2963 (Small).JPG
IMG_2963 (Small).JPG (40.7 KiB) Viewed 4920 times
IMG_2962 (Small).JPG
IMG_2962 (Small).JPG (54.73 KiB) Viewed 4920 times
IMG_2969 (Small).JPG
IMG_2969 (Small).JPG (51.47 KiB) Viewed 4920 times
IMG_2949 (Small).JPG
IMG_2949 (Small).JPG (58.34 KiB) Viewed 4920 times
IMG_2971 (Small).JPG
IMG_2971 (Small).JPG (33.37 KiB) Viewed 4920 times
IMG_2979 (Small).JPG
IMG_2979 (Small).JPG (35.52 KiB) Viewed 4920 times

User avatar
izeman   100 GW

100 GW
Posts: 5072
Joined: Jun 21 2011 8:25am
Location: Vienna, Austria
Contact:

Re: Custom aluminum frame with 2.8kwh capacity

Post by izeman » Sep 26 2016 3:27am

that's a really deep cut. sending shivers down my spine. :(
but the result will be great. i still love those 20Ah cells. they perform so nicely, and are so easy to handle.

Im_Getting_Better   1 mW

1 mW
Posts: 10
Joined: Aug 02 2016 10:02am
Location: Perth, Australia

Re: Custom aluminum frame with 2.8kwh capacity

Post by Im_Getting_Better » Sep 26 2016 5:00am

Well that looks painful.
Really glad I saw this thread, looking forward to seeing how it ends up.

User avatar
Ratking   1 kW

1 kW
Posts: 499
Joined: May 20 2010 5:27am
Location: Norway

Re: Custom aluminum frame with 2.8kwh capacity

Post by Ratking » Sep 26 2016 5:17am

izeman wrote:that's a really deep cut. sending shivers down my spine. :(
but the result will be great. i still love those 20Ah cells. they perform so nicely, and are so easy to handle.
It was not that painful before the doctor used a ordinary toothbrush to scrub out the dirt. But that did not help the pain :D I am glad it worked out, because I worked with the wound open for 12h before i went to the hospital. I did not want to ruin a day at the workshop, but in hindsight I should have gone straight there, because the wound can dry up and make it harder to sew and heal. Live and learn

I hope the result will be good, I do feel the plan I have now will secure the batteries in place for good. I want this bike to be a work horse that I can use without any worry for a long time

whereswally606   100 kW

100 kW
Posts: 1149
Joined: Jun 19 2011 2:11pm
Location: Cheshire, UK

Re: Custom aluminum frame with 2.8kwh capacity

Post by whereswally606 » Sep 26 2016 5:37am

Ratking wrote: because I worked with the wound open for 12h before i went to the hospital.
makes me think of the black knight sketch in the monty python's holy grail. Ah tis but a flesh wound.

I think id have downed tools and washed it out, gone and got some pain killers. anyway hope it heals well.
Distributing "Lebowski" FOC Controller PCB (Through hole) since 2016
Moped: Emax 110s 2009

User avatar
izeman   100 GW

100 GW
Posts: 5072
Joined: Jun 21 2011 8:25am
Location: Vienna, Austria
Contact:

Re: Custom aluminum frame with 2.8kwh capacity

Post by izeman » Sep 26 2016 7:57am

"we call it a draw ... i'll bite your legs off ... love it ... :)