Norco Aline and Kevlar/carbon tank

Show off your E-bike creation here.
User avatar
Samd   1.21 GW

1.21 GW
Posts: 3667
Joined: Jun 28 2011 11:08pm
Location: Ballarat, AU
Contact:

Norco Aline and Kevlar/carbon tank

Post by Samd » Jun 10 2016 6:20pm

I collect these frames now. The rear end far surpasses a single swinger offroad and is protected by a patent.

I've converted a few with aluminium but figured it was time to get my composite on.

Carbon is conductive so I'm thinking Kevlar inside (flame retardant too) and carbon external. Image


Sent from my iPhone using Tapatalk
http://ballaratebikes.com/

ImageImageImage
"Knowledge is knowing that a tomato is a fruit. Wisdom is knowing that a 165mm rear shock can't deliver 220mm of rear swingarm travel." - Oprah Winfrey.

User avatar
Samd   1.21 GW

1.21 GW
Posts: 3667
Joined: Jun 28 2011 11:08pm
Location: Ballarat, AU
Contact:

Re: Norco Aline and Kevlar/carbon tank

Post by Samd » Jun 10 2016 6:22pm

I can fit a couple of kwhr of 18650ga and the width will be so narrow. Image


Sent from my iPhone using Tapatalk
http://ballaratebikes.com/

ImageImageImage
"Knowledge is knowing that a tomato is a fruit. Wisdom is knowing that a 165mm rear shock can't deliver 220mm of rear swingarm travel." - Oprah Winfrey.

User avatar
Samd   1.21 GW

1.21 GW
Posts: 3667
Joined: Jun 28 2011 11:08pm
Location: Ballarat, AU
Contact:

Re: Norco Aline and Kevlar/carbon tank

Post by Samd » Jun 10 2016 6:23pm

3D printing a form for the composite layup. I have a box of dp810 to bond the final result to the ally. Image


Sent from my iPhone using Tapatalk
http://ballaratebikes.com/

ImageImageImage
"Knowledge is knowing that a tomato is a fruit. Wisdom is knowing that a 165mm rear shock can't deliver 220mm of rear swingarm travel." - Oprah Winfrey.

User avatar
Samd   1.21 GW

1.21 GW
Posts: 3667
Joined: Jun 28 2011 11:08pm
Location: Ballarat, AU
Contact:

Re: Norco Aline and Kevlar/carbon tank

Post by Samd » Jun 10 2016 6:25pm

The joy of these frames is the 68mm bottom bracket and the 150mm rear which can have 8mm Waterjet plates inserted inside to take a 135mm hub.

I have two frames. Might build a mid and a hub. :)


Sent from my iPhone using Tapatalk
http://ballaratebikes.com/

ImageImageImage
"Knowledge is knowing that a tomato is a fruit. Wisdom is knowing that a 165mm rear shock can't deliver 220mm of rear swingarm travel." - Oprah Winfrey.

User avatar
macribs   1.21 GW

1.21 GW
Posts: 3612
Joined: Jul 22 2014 5:59pm

Re: Norco Aline and Kevlar/carbon tank

Post by macribs » Jun 11 2016 7:48pm

Sweet samd! Those bikes will be fantastic. Stealth looking. Light weight and nimble.
Looking forward to see the bikes completed.

Really like your style of building, and now with a bullet proof kevlar/carbon tank. 8)

User avatar
Kepler   1 GW

1 GW
Posts: 3239
Joined: Nov 08 2009 9:22pm
Location: Eastern suburbs Melbourne Australia

Re: Norco Aline and Kevlar/carbon tank

Post by Kepler » Jun 11 2016 8:20pm

I am liking this project a lot. Sub'd
Current Rides

Lightest true ebike on the planet: ON ROAD viewtopic.php?f=6&t=74269
eBoost on facebook: http://www.facebook.com/pages/Eboost/200306283342024/

User avatar
Samd   1.21 GW

1.21 GW
Posts: 3667
Joined: Jun 28 2011 11:08pm
Location: Ballarat, AU
Contact:

Re: Norco Aline and Kevlar/carbon tank

Post by Samd » Jun 17 2016 4:07am

My first layup on cardboard was flimsy. So I've waterjetted up a 2mm ally subframe. Kevlar liner and carbon outer. Then I'll Waterjet up a 1mm outer layer exoskeleton style other some funky Voronoi cutouts to suit the lithe shape of the donor frame.

It's flat pack ikea meets champagne ebiking.


Sent from my iPhone using Tapatalk
http://ballaratebikes.com/

ImageImageImage
"Knowledge is knowing that a tomato is a fruit. Wisdom is knowing that a 165mm rear shock can't deliver 220mm of rear swingarm travel." - Oprah Winfrey.

User avatar
Samd   1.21 GW

1.21 GW
Posts: 3667
Joined: Jun 28 2011 11:08pm
Location: Ballarat, AU
Contact:

Re: Norco Aline and Kevlar/carbon tank

Post by Samd » Jun 17 2016 4:07am

Image


Sent from my iPhone using Tapatalk
http://ballaratebikes.com/

ImageImageImage
"Knowledge is knowing that a tomato is a fruit. Wisdom is knowing that a 165mm rear shock can't deliver 220mm of rear swingarm travel." - Oprah Winfrey.

User avatar
Samd   1.21 GW

1.21 GW
Posts: 3667
Joined: Jun 28 2011 11:08pm
Location: Ballarat, AU
Contact:

Re: Norco Aline and Kevlar/carbon tank

Post by Samd » Jun 17 2016 4:18pm

Image


Sent from my iPhone using Tapatalk
http://ballaratebikes.com/

ImageImageImage
"Knowledge is knowing that a tomato is a fruit. Wisdom is knowing that a 165mm rear shock can't deliver 220mm of rear swingarm travel." - Oprah Winfrey.

User avatar
Sean9002   1 kW

1 kW
Posts: 345
Joined: Jun 16 2013 7:57am
Location: Australia

Re: Norco Aline and Kevlar/carbon tank

Post by Sean9002 » Jun 19 2016 5:22pm

Samd wrote:Image


Sent from my iPhone using Tapatalk
Nice work boots boss! :lol:
OSET 20+ - Custom frame and swingarm, Motorims - 66V
Ruff Cycles Porucho - MXUS 3000w - whitewalls - Gloss black/Pearl blue/copper leaf - custom tanks - bobber saddle
Giant Glory 00 - Clyte X5404 - Hubsinks - 18FET Sinewave
Fuji Nevada S - MXUS 35mm- Hubsinks - 12FET Sinewave
39inch longboard Dual 50mm, 12s lipo

User avatar
Samd   1.21 GW

1.21 GW
Posts: 3667
Joined: Jun 28 2011 11:08pm
Location: Ballarat, AU
Contact:

Re: Norco Aline and Kevlar/carbon tank

Post by Samd » Jun 19 2016 5:23pm

I like to throw something in there for the aussies. :mrgreen:
http://ballaratebikes.com/

ImageImageImage
"Knowledge is knowing that a tomato is a fruit. Wisdom is knowing that a 165mm rear shock can't deliver 220mm of rear swingarm travel." - Oprah Winfrey.

r3volved   100 kW

100 kW
Posts: 1452
Joined: Jul 24 2013 4:01pm
Location: Waterloo, Ontario, Canada

Re: Norco Aline and Kevlar/carbon tank

Post by r3volved » Jun 20 2016 9:01am

That looks great!
There's one of those frames near me for $60 right now...if you didn't live on the other side of the bloody planet I would scoop it and get you to do it up!

User avatar
Samd   1.21 GW

1.21 GW
Posts: 3667
Joined: Jun 28 2011 11:08pm
Location: Ballarat, AU
Contact:

Re: Norco Aline and Kevlar/carbon tank

Post by Samd » Jun 20 2016 6:53pm

Sixty dollars! Jesus in a sundress! There's people here who'd jump at 300!
I could send you the flat sheet and a tube of dp810 for very little indeed. Then you just fold it up and sand and glue it. I could probably get it there for under $150CAD all up..
http://ballaratebikes.com/

ImageImageImage
"Knowledge is knowing that a tomato is a fruit. Wisdom is knowing that a 165mm rear shock can't deliver 220mm of rear swingarm travel." - Oprah Winfrey.

User avatar
Samd   1.21 GW

1.21 GW
Posts: 3667
Joined: Jun 28 2011 11:08pm
Location: Ballarat, AU
Contact:

Re: Norco Aline and Kevlar/carbon tank

Post by Samd » Jun 20 2016 11:26pm

I'm amazed at the lack of expense in waterjetting. Before I glue it all up I am going to get some outer plates made up (shown in red below) as well as a base door (in grey) to make the shape interesting and increase the torsional rigidity.
Attachments
New Picture.jpg
http://ballaratebikes.com/

ImageImageImage
"Knowledge is knowing that a tomato is a fruit. Wisdom is knowing that a 165mm rear shock can't deliver 220mm of rear swingarm travel." - Oprah Winfrey.

User avatar
Samd   1.21 GW

1.21 GW
Posts: 3667
Joined: Jun 28 2011 11:08pm
Location: Ballarat, AU
Contact:

Re: Norco Aline and Kevlar/carbon tank

Post by Samd » Jun 21 2016 9:52pm

Image

Sides done


Sent from my iPhone using Tapatalk
http://ballaratebikes.com/

ImageImageImage
"Knowledge is knowing that a tomato is a fruit. Wisdom is knowing that a 165mm rear shock can't deliver 220mm of rear swingarm travel." - Oprah Winfrey.

User avatar
spinningmagnets   100 GW

100 GW
Posts: 11527
Joined: Dec 21 2007 10:27pm
Location: Ft Riley, NE Kansas

Re: Norco Aline and Kevlar/carbon tank

Post by spinningmagnets » Jun 21 2016 10:14pm

Fantastic work, Sam. I'd be curious to add a few more Ah by fattening the bottom of the battery case a little, but...of course everyone has an opinion, and you on the other hand are actually doing something. Thanks for posting for everyones benefit.

$60 is an awesome deal. My immediate interest in these frames is that they can also take a mid drive well, so the builder has a choice between middie and hubbie...

The newer Norco alines seem to have an "S"-curved downtube, and the older ones have a straighter downtube. I assume from what I've read that they are built like a tank.

User avatar
Samd   1.21 GW

1.21 GW
Posts: 3667
Joined: Jun 28 2011 11:08pm
Location: Ballarat, AU
Contact:

Re: Norco Aline and Kevlar/carbon tank

Post by Samd » Jun 22 2016 12:29am

Yes like all high end DH frames they are built to take huge drops Ron.

I've got two so might fit the internal rear plates to one for a hub and the other a bbs HD.

I've kept the tank about 85mm wide so I can sling an Infineon sine wave off the bottom.

Did you see the cell layout photo above? From memory my plan took about 110 cells. That's about 1400 watthours of 18650ga.

I gotta keep the weight down for jumps. My days of riding 50kg washing machine clones are over mate ;)


Sent from my iPhone using Tapatalk
http://ballaratebikes.com/

ImageImageImage
"Knowledge is knowing that a tomato is a fruit. Wisdom is knowing that a 165mm rear shock can't deliver 220mm of rear swingarm travel." - Oprah Winfrey.

User avatar
Samd   1.21 GW

1.21 GW
Posts: 3667
Joined: Jun 28 2011 11:08pm
Location: Ballarat, AU
Contact:

Re: Norco Aline and Kevlar/carbon tank

Post by Samd » Jun 22 2016 12:34am

Hey Ron for the other frame shape keep an eye on this one.

https://endless-sphere.com/forums/viewt ... 5#p1191458


Sent from my iPhone using Tapatalk
http://ballaratebikes.com/

ImageImageImage
"Knowledge is knowing that a tomato is a fruit. Wisdom is knowing that a 165mm rear shock can't deliver 220mm of rear swingarm travel." - Oprah Winfrey.

User avatar
Samd   1.21 GW

1.21 GW
Posts: 3667
Joined: Jun 28 2011 11:08pm
Location: Ballarat, AU
Contact:

Re: Norco Aline and Kevlar/carbon tank

Post by Samd » Jun 22 2016 12:51am

A bit of dp810 on the corner joins. Image


Sent from my iPhone using Tapatalk
http://ballaratebikes.com/

ImageImageImage
"Knowledge is knowing that a tomato is a fruit. Wisdom is knowing that a 165mm rear shock can't deliver 220mm of rear swingarm travel." - Oprah Winfrey.

User avatar
macribs   1.21 GW

1.21 GW
Posts: 3612
Joined: Jul 22 2014 5:59pm

Re: Norco Aline and Kevlar/carbon tank

Post by macribs » Jun 22 2016 3:41am

I tried to look at the earlier pics to see the joints of the alubox but no luck. Very clever way to fold the box, now that is origami for everyone :)
What I was trying to figure out from the pics is if there is any overlapping of the sheet metal in the joints, or if sheet metal meets in a 90 degree corner?

Trying to understand what kind of surface area is needed for the dp810 to work properly.
Folding sheet metal then gluing for bonding is über cool.

You will weld the box onto the frame or glue it in place?

User avatar
Samd   1.21 GW

1.21 GW
Posts: 3667
Joined: Jun 28 2011 11:08pm
Location: Ballarat, AU
Contact:

Re: Norco Aline and Kevlar/carbon tank

Post by Samd » Jun 22 2016 5:29am

No overlapping with metal. I did dremel the fold lines about 1mm. Took maybe 3mins.

Yes not metal behind. But with Kevlar as below. Dp810 specialises in slippery surfaces.

I'll glue it in place. Image


Sent from my iPhone using Tapatalk
http://ballaratebikes.com/

ImageImageImage
"Knowledge is knowing that a tomato is a fruit. Wisdom is knowing that a 165mm rear shock can't deliver 220mm of rear swingarm travel." - Oprah Winfrey.

User avatar
Samd   1.21 GW

1.21 GW
Posts: 3667
Joined: Jun 28 2011 11:08pm
Location: Ballarat, AU
Contact:

Re: Norco Aline and Kevlar/carbon tank

Post by Samd » Jun 23 2016 6:47pm

Sent from my iPhone using Tapatalk
http://ballaratebikes.com/

ImageImageImage
"Knowledge is knowing that a tomato is a fruit. Wisdom is knowing that a 165mm rear shock can't deliver 220mm of rear swingarm travel." - Oprah Winfrey.

User avatar
Samd   1.21 GW

1.21 GW
Posts: 3667
Joined: Jun 28 2011 11:08pm
Location: Ballarat, AU
Contact:

Re: Norco Aline and Kevlar/carbon tank

Post by Samd » Jun 24 2016 10:43pm

External carbon layer and Kevlar lining is making the box really sturdy. Happy so far with my experiment. Image


Sent from my iPhone using Tapatalk
http://ballaratebikes.com/

ImageImageImage
"Knowledge is knowing that a tomato is a fruit. Wisdom is knowing that a 165mm rear shock can't deliver 220mm of rear swingarm travel." - Oprah Winfrey.

User avatar
Samd   1.21 GW

1.21 GW
Posts: 3667
Joined: Jun 28 2011 11:08pm
Location: Ballarat, AU
Contact:

Re: Norco Aline and Kevlar/carbon tank

Post by Samd » Jun 29 2016 5:33pm

Really snug. Almost ready to bond it in. Will enamel the outer ladder brace first to stop corrosion. ImageImage


Sent from my iPhone using Tapatalk
http://ballaratebikes.com/

ImageImageImage
"Knowledge is knowing that a tomato is a fruit. Wisdom is knowing that a 165mm rear shock can't deliver 220mm of rear swingarm travel." - Oprah Winfrey.

User avatar
IanM   100 W

100 W
Posts: 144
Joined: Jun 08 2015 3:56am
Location: Canberra Australia

Re: Norco Aline and Kevlar/carbon tank

Post by IanM » Jun 30 2016 2:47am

This would be a good candidate for a BBSHD. I just stuck one on my 2009 trance X1 today and like it a lot. This frame shouldn't have the clearance issues I anticipate with the trance. I'm worried I will smash the motor on a rock or log. It is nice not having 15kg of weight in my back wheel but then it sucks that I can't do power wheelies at 40kmh like I can on th FLX. Keep up the good work Sam I am keen to see how this turns out, should be a cracker.

Post Reply