Contactor Failure

Things that fly
Post Reply
User avatar
methods   10 GW

10 GW
Posts: 4401
Joined: Aug 08 2008 12:08pm
Location: Santa Cruz CA
Contact:

Contactor Failure

Post by methods » Jul 05 2017 10:23am

I will write it up once root cause for the entire system is determined.
contactor failure.jpg
contactor failure.jpg (38.29 KiB) Viewed 893 times
This was during a bench test shake down.
Parts pedigree
Procedure and pre-flight checkout

We are working on basic precheck
One test is measuring contactor resistance
The contactor is to be instrumented such that during a run-up the contacts can be read like a shunt. GO or NO GO.

We can do a simple Red Light, Green Light for this. Visual.
It can be as complicated as an interlock... but... keep it simple yes?
The complicated version measures contactor resistance and latches the contactor open

Meh... Visual only.
No electronics which are not needed.

Contactor contacts must be measured under load to present.

-methods
Increasing battery voltage and controller current limit will result in a non linear experience

User avatar
bigmoose   100 MW

100 MW
Posts: 2653
Joined: Aug 06 2009 3:05pm
Location: North coast USA
Contact:

Re: Contactor Failure

Post by bigmoose » Jul 05 2017 2:48pm

That thing arc under load disconnect? ... then weld under subsequent turn on?
"Live simply. Love generously. Care deeply. Speak kindly. Leave the rest to God..." all the best, Dave

User avatar
methods   10 GW

10 GW
Posts: 4401
Joined: Aug 08 2008 12:08pm
Location: Santa Cruz CA
Contact:

Re: Contactor Failure

Post by methods » Jul 05 2017 2:53pm

Investigating.
Increasing battery voltage and controller current limit will result in a non linear experience

User avatar
liveforphysics   100 GW

100 GW
Posts: 14005
Joined: Oct 29 2008 1:48am
Location: Santa Cruz, CA, USA

Re: Contactor Failure

Post by liveforphysics » Jul 05 2017 4:28pm

Single non-complete pre-charge make event welds them pretty reliably.

Or like Dave mentioned, any operation that damages the surfaces can lead to welding once it's taken current on damaged contact pads.
Each carcinogen vapor exposure includes a dice roll for cancer.

Each mutagen vapor exposure includes a dice roll for reproductive genetic defects in your children.

Each engine start sprays them into a shared atmosphere which includes beings not offered an opportunity to consent accepting these cancer experiences and defective genetics life experiences.

Every post is a free gift to the collective of minds composing the living bleeding edge of LEV development on our spaceship.

User avatar
methods   10 GW

10 GW
Posts: 4401
Joined: Aug 08 2008 12:08pm
Location: Santa Cruz CA
Contact:

Re: Contactor Failure

Post by methods » Jul 05 2017 6:46pm

It was strapped with a 2K 25W Precharge resistor - permanent strap no button.

The system was recently reconfigured tho... Perhaps the contactor coil was inadvertently powered during the cable swap, the precharge resistor failed, or some other issue revolving around reconfig.


-methods
Increasing battery voltage and controller current limit will result in a non linear experience

User avatar
fechter   100 GW

100 GW
Posts: 13185
Joined: Dec 31 2006 3:23pm
Location: California Bay Area, USA

Re: Contactor Failure

Post by fechter » Jul 05 2017 7:10pm

Hard to see in the picture. Are the contacts damaged? The coil looks toasted. Measuring the voltage across the contacts is a good way to verify contact. If the controller was drawing current, then the precharge resistor would not get the caps up to full charge.

I've been real impressed with the ability of FETs to handle large current spikes, like my battery spot welder. A solid state contactor should be able to just slam on fast without blowing anything up. I've been looking into that as an alternative to the soft-start, constant dv/dt precharge circuit I designed before. I also have a precharge circuit that drives a relay coil once the precharge is completed.
"One test is worth a thousand opinions"

User avatar
methods   10 GW

10 GW
Posts: 4401
Joined: Aug 08 2008 12:08pm
Location: Santa Cruz CA
Contact:

Re: Contactor Failure

Post by methods » Jul 06 2017 4:51pm

One of our primary suspicions is a heavy load on the Kelly leading to the precharge not being able to keep up. Major change was Battery voltage from 80V to 100V... Which may have been enough to weld... Then heat.

-methods
Increasing battery voltage and controller current limit will result in a non linear experience