kWeld - "Next level" DIY battery spot welder

Batteries, Chargers, and Battery Management Systems.
User avatar
tatus1969   1 kW

1 kW
Posts: 349
Joined: Mar 17 2017 7:36am
Location: Germany
Contact:

Re: low cost DIY battery spot welder

Post by tatus1969 » Jul 09 2017 10:54am

This started as a one-off, but my solution has some unique features (apart from being very robust - I will explain those in the upcoming video), so I am planning to sell it in form of a kit. It depends on you makers and builders how that kit should look like. My idea is to only sell assembled/tested/programmed PCBs and the mechanical parts in raw form. This means (apart from things like bolts, nuts, cable lugs, ...) brass blocks cut to length, copper rod, and enough AWG8 wire. You would need to drill and cut the brass pieces, cut and form the copper rod into electrodes, and cut / crimp the cables. The other extreme would be supplying complete systems, but this involves considerable machining work and would make everything much more expensive. I need some feedback from you folks... And if someone is interested in a kit, just send me a PM.
Resistance is futile - We Are The Watt.

User avatar
mxer   1 kW

1 kW
Posts: 350
Joined: May 15 2011 9:01am
Location: United Kindom

Re: low cost DIY battery spot welder

Post by mxer » Jul 09 2017 1:47pm

Pm'ed definitely interested in the raw materials to have a play, great project and thanks for sharing.

:D

User avatar
spinningmagnets   100 GW

100 GW
Posts: 11824
Joined: Dec 21 2007 10:27pm
Location: Ft Riley, NE Kansas

Re: low cost DIY battery spot welder

Post by spinningmagnets » Jul 09 2017 6:44pm

I can't speak for anyone else, but...here's what I would want the seller to do at a minimum.

Image

I like the board in the pic above, all of the tiny electronic components are all in one place (instead of me needing to order them from three different vendors), and they are all soldered in the proper location on the board.

What I most want is for the brain-chip to be pre-programmed by the seller before I get it. It may be quick and easy for you, but I will pay for someone else to make sure that it is done right.

What I can easily do without screwing it up:
Cut square bar into proper lengths, drill seven holes in each, bolt bars to their proper place.
Make the four cables (I can source all the components for the cables locally)
Attach fuse
solder-in the large single capacitor (too easy, just make sure the positive hole is clearly marked?)
Make all the tube standoffs (brass, plastic?...either is easy). I can also source stand-off tubes locally without any wait
Attach screen read-out
solder-in the adjustment dial into place
plug-in and solder that 6-pin "segger" device

If you add the raw square bar to the kit, that's fine, I can finish it off. However, you can make the shipping a little lighter because I can source the square bar from a local metals supplier (since you are shipping around the world). I just need the dimensions, and I can be working on it while I wait for your kit to arrive...You can have the cables as a purchase option, either a loose-part kit or complete, but...I can make those too, quite easily.

Sooo...is that all I have to do to take the kit from the first pic to end up like the second pic below?

[edit: I now think I would definitely recommend that you make the square-bars and cables available on your website as a completed product (cut and drilled), separate from the basic kit. However, charge a high price for those, because most DIY guys can buy those by themselves using local materials...no need for you to try to be competitive and get headaches over the easy-to-get stuff. The square bar can be found at onlinemetals.com, and you need to focus on the tech stuff, not brass bars and cables. I just bought a 3/4-inch diameter copper rod a foot long for $20, arrived in four days.]

Image

12-C   100 W

100 W
Posts: 185
Joined: Oct 14 2016 9:22pm

Re: low cost DIY battery spot welder

Post by 12-C » Jul 09 2017 10:44pm

+1 spinning magments

The reflow work for SMT is well beyond another project that I want to undertake. And forget about programming.

soldering through hole components is simple enough and rather fun...

It would be great if it was a "all components included- build most yourself" type product.

Looks really impressive!

Any idea if you anticipate it handling thicker ribbon, aluminum or copper?

Thanks!

User avatar
tatus1969   1 kW

1 kW
Posts: 349
Joined: Mar 17 2017 7:36am
Location: Germany
Contact:

Re: low cost DIY battery spot welder

Post by tatus1969 » Jul 10 2017 1:11am

The video is online!

If you like it, you can help me by sharing the video via Facebook etc.

https://youtu.be/Ceos88VO6p4
Resistance is futile - We Are The Watt.

User avatar
spinningmagnets   100 GW

100 GW
Posts: 11824
Joined: Dec 21 2007 10:27pm
Location: Ft Riley, NE Kansas

Re: low cost DIY battery spot welder

Post by spinningmagnets » Jul 10 2017 1:26am

All I can say is...WOW!

I like it even more now that I have seen the video. Please save one for me, and PM me your paypal email address.

As I stated above, I do not need the cables, the probes or the square bars, but I will need everything else.

User avatar
mxer   1 kW

1 kW
Posts: 350
Joined: May 15 2011 9:01am
Location: United Kindom

Re: low cost DIY battery spot welder

Post by mxer » Jul 10 2017 4:00am

+1 above

Video is great! Thanks. Pm me your details, cheers

User avatar
TheBeastie   10 MW

10 MW
Posts: 2172
Joined: Jul 28 2012 12:31am
Location: Melbourne Australia

Re: low cost DIY battery spot welder

Post by TheBeastie » Jul 10 2017 1:06pm

Wow amazing job. Really looks awesome.
That really is a truly next-gen DIY spot welder. We can't ever have enough projects like this.
I really like the LCD display with a joule output reading with the variable knob.
And the auto-mode without footswitch is cool.
But then I saw the self-calibration and auto milliohm resistance reporting,
just wow.
subscribed.
Speed Kills Range, 10mph = 46 miles range, 20mph = 20 miles, 30mph = 8 miles rangehttps://goo.gl/1JNL53
Over Charging Kills ur battery bit.ly/1hzWKl4
Consider PAS as your only throttle https://goo.gl/Kg1F8F
Fuel-Cell is the ultimate battery coupled with 4th-gen Nuclear
https://goo.gl/TcKtHs https://goo.gl/ZhFFot https://goo.gl/gfa215
10 Square Miles of solar panels = 0.12GW average power! https://goo.gl/Ub1S39

User avatar
fechter   100 GW

100 GW
Posts: 15098
Joined: Dec 31 2006 3:23pm
Location: California Bay Area, USA

Re: low cost DIY battery spot welder

Post by fechter » Jul 10 2017 2:10pm

Gets my seal of approval. Nice work.
"One test is worth a thousand opinions"

User avatar
mauimart   100 W

100 W
Posts: 216
Joined: Nov 10 2009 2:08pm
Location: maui

Re: low cost DIY battery spot welder

Post by mauimart » Jul 10 2017 2:39pm

Simple sophistication. Brilliant! Have you tried to weld 0.2mm nickel strip with the 5Ah battery?

User avatar
tatus1969   1 kW

1 kW
Posts: 349
Joined: Mar 17 2017 7:36am
Location: Germany
Contact:

Re: low cost DIY battery spot welder

Post by tatus1969 » Jul 10 2017 4:50pm

spinningmagnets wrote:
Thanks a lot for your helpful thoughts. (No, you haven't forgotten anything.)

I will go ahead and make these items available:
1) PCB with all SMT components soldered and microcontroller programmed
2) set of through-hole components like capacitor, connectors, LCD, potentiometer, etc
3) fully assembled and programmed PCB
4) cable assembly for those who don't have a suitable crimp tool
5) set of mechanical components like bolts and nuts, excluding the parts that need machining
5a) the foot switch
6) set of raw brass and copper parts, cut to length
7) set of finished brass and copper parts
8 ) programmer for firmware updates that plugs into USB (the Segger tool is a full debugger and too costly), plus an update tool (Windows)
Last edited by tatus1969 on Jul 10 2017 5:55pm, edited 2 times in total.
Resistance is futile - We Are The Watt.

User avatar
tatus1969   1 kW

1 kW
Posts: 349
Joined: Mar 17 2017 7:36am
Location: Germany
Contact:

Re: low cost DIY battery spot welder

Post by tatus1969 » Jul 10 2017 4:51pm

spinningmagnets wrote:All I can say is...WOW!

I like it even more now that I have seen the video. Please save one for me, and PM me your paypal email address.

As I stated above, I do not need the cables, the probes or the square bars, but I will need everything else.
Thanks :D Did you receive my last PM's?
Resistance is futile - We Are The Watt.

User avatar
tatus1969   1 kW

1 kW
Posts: 349
Joined: Mar 17 2017 7:36am
Location: Germany
Contact:

Re: low cost DIY battery spot welder

Post by tatus1969 » Jul 10 2017 5:00pm

mauimart wrote: Simple sophistication. Brilliant!
Thanks, usability was my first priority. This made me opt against fancy push buttons as well, even tough they are cheaper. I recently had to work with a Weller WX2 soldering station. Setting the temperature with its touch keys takes ages and is a real headache.
mauimart wrote: Have you tried to weld 0.2mm nickel strip with the 5Ah battery?
I've just tried to weld five layers of 0.1mm nickel strip. The two bottom layers are welded but can easily be separated. The top three layers stick together. Just yesterday I have ordered 0.1mm copper foil and some of these, these are 0.3mm nickel.

Image
Resistance is futile - We Are The Watt.

User avatar
spinningmagnets   100 GW

100 GW
Posts: 11824
Joined: Dec 21 2007 10:27pm
Location: Ft Riley, NE Kansas

Re: low cost DIY battery spot welder

Post by spinningmagnets » Jul 10 2017 6:41pm

I like how long the slots are on those nickel strips. I believe that those slots will help make the spot-welds more consistent.

12-C   100 W

100 W
Posts: 185
Joined: Oct 14 2016 9:22pm

Re: low cost DIY battery spot welder

Post by 12-C » Jul 10 2017 11:04pm

Great product!

Can you quote a price and how long until delivery? I sent a PM.

I really liked the video.

Do you anticipate it being able to weld copper, aluminum, or any others?

Thanks!

User avatar
tomjasz   10 GW

10 GW
Posts: 4314
Joined: Mar 29 2014 1:45pm
Location: Out riding, MN USA
Contact:

Re: low cost DIY battery spot welder

Post by tomjasz » Jul 10 2017 11:11pm

Website listed at end of video..
Thanks Justin_le we're here thanks to you. All the best to the mods for their tireless work keeping it on an even keel.

User avatar
tatus1969   1 kW

1 kW
Posts: 349
Joined: Mar 17 2017 7:36am
Location: Germany
Contact:

Re: low cost DIY battery spot welder

Post by tatus1969 » Jul 11 2017 2:16am

12-C wrote: Can you quote a price and how long until delivery?
I am busy doing the calculations, but that is not yet finished (almost). I will order assembled PCBs from a professional service, expect around 3 wks for that. Then give me a few days for testing/programming/packing/shipping.
12-C wrote: Do you anticipate it being able to weld copper, aluminum, or any others?
It certainly does 0.3mm nickel, but a lot depends on the power source. The welder circuit contributes only 140 micro (!) ohms. The MOSFETs are rated 40V and I have programmed a current limit of 2000A for 200ms, so there should be enough headroom for thicker materials.
Last edited by tatus1969 on Jul 11 2017 2:23am, edited 1 time in total.
Resistance is futile - We Are The Watt.

User avatar
tatus1969   1 kW

1 kW
Posts: 349
Joined: Mar 17 2017 7:36am
Location: Germany
Contact:

Re: low cost DIY battery spot welder

Post by tatus1969 » Jul 11 2017 2:19am

I made a video where I am doing robustnes testing:

edit: this time the correct link:
https://youtu.be/fWXphoDE_H8
Resistance is futile - We Are The Watt.

User avatar
tatus1969   1 kW

1 kW
Posts: 349
Joined: Mar 17 2017 7:36am
Location: Germany
Contact:

Re: low cost DIY battery spot welder

Post by tatus1969 » Jul 11 2017 2:53pm

Okay, I'll continue finishing the release design and send an RFQ to my PCB assembly company, but I wanted to share this one with you first. It's rather crazy (and educational?), please don't take it too seriously - I am a quality minded professional EE despite of what you see there :wink:

https://youtu.be/JR3GJYScquc
Resistance is futile - We Are The Watt.

12-C   100 W

100 W
Posts: 185
Joined: Oct 14 2016 9:22pm

Re: low cost DIY battery spot welder

Post by 12-C » Jul 11 2017 11:20pm

tatus1969 wrote:Okay, I'll continue finishing the release design and send an RFQ to my PCB assembly company, but I wanted to share this one with you first. It's rather crazy (and educational?), please don't take it too seriously - I am a quality minded professional EE despite of what you see there :wink:

https://youtu.be/JR3GJYScquc
hahaha that was great, I actually jumped lol scared me as much as you lol

would it be possible to program a sensing feature to prevent autofire if the electrodes are in contact?

User avatar
mxer   1 kW

1 kW
Posts: 350
Joined: May 15 2011 9:01am
Location: United Kindom

Re: low cost DIY battery spot welder

Post by mxer » Jul 12 2017 5:23am

HaHaha, very educational.

Made me jump too, interesting to see the extreme :D

User avatar
fechter   100 GW

100 GW
Posts: 15098
Joined: Dec 31 2006 3:23pm
Location: California Bay Area, USA

Re: low cost DIY battery spot welder

Post by fechter » Jul 12 2017 10:32am

Maybe some heat-shrink tubing around the electrodes with only the tip exposed might help with the accidental firing. :wink: I could imagine using a foot pedal in conjunction with the auto fire as well. Use the foot pedal to disable firing when not pressed. I didn't really like using a foot pedal for firing as the thing had a bad tendency to move around on the floor, but I could see just holding it down to enable auto-fire.

Pretty impressive it welds those slotted tabs with the electrodes on the same side of the slot. With the electrodes on opposite sides of the slot, it should take much less current to get a good weld.
"One test is worth a thousand opinions"

User avatar
tatus1969   1 kW

1 kW
Posts: 349
Joined: Mar 17 2017 7:36am
Location: Germany
Contact:

Re: low cost DIY battery spot welder

Post by tatus1969 » Jul 12 2017 2:39pm

12-C wrote: would it be possible to program a sensing feature to prevent autofire if the electrodes are in contact?
That is not easily possible. I need to fire a pulse in order to measure the resistance between the electrodes, it cannot distinguish a dead short from a nickel strip before that. If what I did in the video were a dead short. But I had a different idea, the video showing it is already rendering 8)

What would probably be convenient is to integrate the switch into one of the electrode holder, and make it spring loaded, but that definitely exceeds my mechanical skills. Not to speak of how to maintain low resistance...
fechter wrote: Maybe some heat-shrink tubing around the electrodes with only the tip exposed might help with the accidental firing. :wink:
You bet what I did right after the video :wink:
fechter wrote: I could imagine using a foot pedal in conjunction with the auto fire as well. Use the foot pedal to disable firing when not pressed. I didn't really like using a foot pedal for firing as the thing had a bad tendency to move around on the floor, but I could see just holding it down to enable auto-fire.
Me too, for the same reason. But that is an interesting idea, I will keep that in mind. Please watch my next video and tell me what you think about my improvement idea.
fechter wrote: Pretty impressive it welds those slotted tabs with the electrodes on the same side of the slot.
You probably don't believe me that I already knew how to use these tabs before making that video...
Last edited by tatus1969 on Jul 12 2017 3:07pm, edited 1 time in total.
Resistance is futile - We Are The Watt.

User avatar
tatus1969   1 kW

1 kW
Posts: 349
Joined: Mar 17 2017 7:36am
Location: Germany
Contact:

Re: low cost DIY battery spot welder

Post by tatus1969 » Jul 12 2017 3:06pm

There goes the next video, showing some improvements:
https://youtu.be/9-CQd02EDIs
Resistance is futile - We Are The Watt.

12-C   100 W

100 W
Posts: 185
Joined: Oct 14 2016 9:22pm

Re: low cost DIY battery spot welder

Post by 12-C » Jul 13 2017 11:52pm

Nice features!

Post Reply