kWeld - "Next level" DIY battery spot welder
Re: low cost DIY battery spot welder
This started as a one-off, but my solution has some unique features (apart from being very robust - I will explain those in the upcoming video), so I am planning to sell it in form of a kit. It depends on you makers and builders how that kit should look like. My idea is to only sell assembled/tested/programmed PCBs and the mechanical parts in raw form. This means (apart from things like bolts, nuts, cable lugs, ...) brass blocks cut to length, copper rod, and enough AWG8 wire. You would need to drill and cut the brass pieces, cut and form the copper rod into electrodes, and cut / crimp the cables. The other extreme would be supplying complete systems, but this involves considerable machining work and would make everything much more expensive. I need some feedback from you folks... And if someone is interested in a kit, just send me a PM.
Resistance is futile - We Are The Watt.
Re: low cost DIY battery spot welder
Pm'ed definitely interested in the raw materials to have a play, great project and thanks for sharing.


- spinningmagnets 100 GW
- Posts: 11824
- Joined: Dec 21 2007 10:27pm
- Location: Ft Riley, NE Kansas
Re: low cost DIY battery spot welder
I can't speak for anyone else, but...here's what I would want the seller to do at a minimum.

I like the board in the pic above, all of the tiny electronic components are all in one place (instead of me needing to order them from three different vendors), and they are all soldered in the proper location on the board.
What I most want is for the brain-chip to be pre-programmed by the seller before I get it. It may be quick and easy for you, but I will pay for someone else to make sure that it is done right.
What I can easily do without screwing it up:
Cut square bar into proper lengths, drill seven holes in each, bolt bars to their proper place.
Make the four cables (I can source all the components for the cables locally)
Attach fuse
solder-in the large single capacitor (too easy, just make sure the positive hole is clearly marked?)
Make all the tube standoffs (brass, plastic?...either is easy). I can also source stand-off tubes locally without any wait
Attach screen read-out
solder-in the adjustment dial into place
plug-in and solder that 6-pin "segger" device
If you add the raw square bar to the kit, that's fine, I can finish it off. However, you can make the shipping a little lighter because I can source the square bar from a local metals supplier (since you are shipping around the world). I just need the dimensions, and I can be working on it while I wait for your kit to arrive...You can have the cables as a purchase option, either a loose-part kit or complete, but...I can make those too, quite easily.
Sooo...is that all I have to do to take the kit from the first pic to end up like the second pic below?
[edit: I now think I would definitely recommend that you make the square-bars and cables available on your website as a completed product (cut and drilled), separate from the basic kit. However, charge a high price for those, because most DIY guys can buy those by themselves using local materials...no need for you to try to be competitive and get headaches over the easy-to-get stuff. The square bar can be found at onlinemetals.com, and you need to focus on the tech stuff, not brass bars and cables. I just bought a 3/4-inch diameter copper rod a foot long for $20, arrived in four days.]

I like the board in the pic above, all of the tiny electronic components are all in one place (instead of me needing to order them from three different vendors), and they are all soldered in the proper location on the board.
What I most want is for the brain-chip to be pre-programmed by the seller before I get it. It may be quick and easy for you, but I will pay for someone else to make sure that it is done right.
What I can easily do without screwing it up:
Cut square bar into proper lengths, drill seven holes in each, bolt bars to their proper place.
Make the four cables (I can source all the components for the cables locally)
Attach fuse
solder-in the large single capacitor (too easy, just make sure the positive hole is clearly marked?)
Make all the tube standoffs (brass, plastic?...either is easy). I can also source stand-off tubes locally without any wait
Attach screen read-out
solder-in the adjustment dial into place
plug-in and solder that 6-pin "segger" device
If you add the raw square bar to the kit, that's fine, I can finish it off. However, you can make the shipping a little lighter because I can source the square bar from a local metals supplier (since you are shipping around the world). I just need the dimensions, and I can be working on it while I wait for your kit to arrive...You can have the cables as a purchase option, either a loose-part kit or complete, but...I can make those too, quite easily.
Sooo...is that all I have to do to take the kit from the first pic to end up like the second pic below?
[edit: I now think I would definitely recommend that you make the square-bars and cables available on your website as a completed product (cut and drilled), separate from the basic kit. However, charge a high price for those, because most DIY guys can buy those by themselves using local materials...no need for you to try to be competitive and get headaches over the easy-to-get stuff. The square bar can be found at onlinemetals.com, and you need to focus on the tech stuff, not brass bars and cables. I just bought a 3/4-inch diameter copper rod a foot long for $20, arrived in four days.]
Re: low cost DIY battery spot welder
+1 spinning magments
The reflow work for SMT is well beyond another project that I want to undertake. And forget about programming.
soldering through hole components is simple enough and rather fun...
It would be great if it was a "all components included- build most yourself" type product.
Looks really impressive!
Any idea if you anticipate it handling thicker ribbon, aluminum or copper?
Thanks!
The reflow work for SMT is well beyond another project that I want to undertake. And forget about programming.
soldering through hole components is simple enough and rather fun...
It would be great if it was a "all components included- build most yourself" type product.
Looks really impressive!
Any idea if you anticipate it handling thicker ribbon, aluminum or copper?
Thanks!
Re: low cost DIY battery spot welder
The video is online!
If you like it, you can help me by sharing the video via Facebook etc.
https://youtu.be/Ceos88VO6p4
If you like it, you can help me by sharing the video via Facebook etc.
https://youtu.be/Ceos88VO6p4
Resistance is futile - We Are The Watt.
- spinningmagnets 100 GW
- Posts: 11824
- Joined: Dec 21 2007 10:27pm
- Location: Ft Riley, NE Kansas
Re: low cost DIY battery spot welder
All I can say is...WOW!
I like it even more now that I have seen the video. Please save one for me, and PM me your paypal email address.
As I stated above, I do not need the cables, the probes or the square bars, but I will need everything else.
I like it even more now that I have seen the video. Please save one for me, and PM me your paypal email address.
As I stated above, I do not need the cables, the probes or the square bars, but I will need everything else.
Re: low cost DIY battery spot welder
+1 above
Video is great! Thanks. Pm me your details, cheers
Video is great! Thanks. Pm me your details, cheers
- TheBeastie 10 MW
- Posts: 2172
- Joined: Jul 28 2012 12:31am
- Location: Melbourne Australia
Re: low cost DIY battery spot welder
Wow amazing job. Really looks awesome.
That really is a truly next-gen DIY spot welder. We can't ever have enough projects like this.
I really like the LCD display with a joule output reading with the variable knob.
And the auto-mode without footswitch is cool.
But then I saw the self-calibration and auto milliohm resistance reporting,
just wow.
subscribed.
That really is a truly next-gen DIY spot welder. We can't ever have enough projects like this.
I really like the LCD display with a joule output reading with the variable knob.
And the auto-mode without footswitch is cool.
But then I saw the self-calibration and auto milliohm resistance reporting,
just wow.
subscribed.
Speed Kills Range, 10mph = 46 miles range, 20mph = 20 miles, 30mph = 8 miles rangehttps://goo.gl/1JNL53
Over Charging Kills ur battery bit.ly/1hzWKl4
Consider PAS as your only throttle https://goo.gl/Kg1F8F
Fuel-Cell is the ultimate battery coupled with 4th-gen Nuclear
https://goo.gl/TcKtHs https://goo.gl/ZhFFot https://goo.gl/gfa215
10 Square Miles of solar panels = 0.12GW average power! https://goo.gl/Ub1S39
Over Charging Kills ur battery bit.ly/1hzWKl4
Consider PAS as your only throttle https://goo.gl/Kg1F8F
Fuel-Cell is the ultimate battery coupled with 4th-gen Nuclear
https://goo.gl/TcKtHs https://goo.gl/ZhFFot https://goo.gl/gfa215
10 Square Miles of solar panels = 0.12GW average power! https://goo.gl/Ub1S39
Re: low cost DIY battery spot welder
Gets my seal of approval. Nice work.
"One test is worth a thousand opinions"
Re: low cost DIY battery spot welder
Simple sophistication. Brilliant! Have you tried to weld 0.2mm nickel strip with the 5Ah battery?
Re: low cost DIY battery spot welder
Thanks a lot for your helpful thoughts. (No, you haven't forgotten anything.)spinningmagnets wrote:
I will go ahead and make these items available:
1) PCB with all SMT components soldered and microcontroller programmed
2) set of through-hole components like capacitor, connectors, LCD, potentiometer, etc
3) fully assembled and programmed PCB
4) cable assembly for those who don't have a suitable crimp tool
5) set of mechanical components like bolts and nuts, excluding the parts that need machining
5a) the foot switch
6) set of raw brass and copper parts, cut to length
7) set of finished brass and copper parts
8 ) programmer for firmware updates that plugs into USB (the Segger tool is a full debugger and too costly), plus an update tool (Windows)
Last edited by tatus1969 on Jul 10 2017 5:55pm, edited 2 times in total.
Resistance is futile - We Are The Watt.
Re: low cost DIY battery spot welder
Thanksspinningmagnets wrote:All I can say is...WOW!
I like it even more now that I have seen the video. Please save one for me, and PM me your paypal email address.
As I stated above, I do not need the cables, the probes or the square bars, but I will need everything else.

Resistance is futile - We Are The Watt.
Re: low cost DIY battery spot welder
Thanks, usability was my first priority. This made me opt against fancy push buttons as well, even tough they are cheaper. I recently had to work with a Weller WX2 soldering station. Setting the temperature with its touch keys takes ages and is a real headache.mauimart wrote: Simple sophistication. Brilliant!
I've just tried to weld five layers of 0.1mm nickel strip. The two bottom layers are welded but can easily be separated. The top three layers stick together. Just yesterday I have ordered 0.1mm copper foil and some of these, these are 0.3mm nickel.mauimart wrote: Have you tried to weld 0.2mm nickel strip with the 5Ah battery?

Resistance is futile - We Are The Watt.
- spinningmagnets 100 GW
- Posts: 11824
- Joined: Dec 21 2007 10:27pm
- Location: Ft Riley, NE Kansas
Re: low cost DIY battery spot welder
I like how long the slots are on those nickel strips. I believe that those slots will help make the spot-welds more consistent.
Re: low cost DIY battery spot welder
Great product!
Can you quote a price and how long until delivery? I sent a PM.
I really liked the video.
Do you anticipate it being able to weld copper, aluminum, or any others?
Thanks!
Can you quote a price and how long until delivery? I sent a PM.
I really liked the video.
Do you anticipate it being able to weld copper, aluminum, or any others?
Thanks!
Re: low cost DIY battery spot welder
Website listed at end of video..
Thanks Justin_le we're here thanks to you. All the best to the mods for their tireless work keeping it on an even keel.
Re: low cost DIY battery spot welder
I am busy doing the calculations, but that is not yet finished (almost). I will order assembled PCBs from a professional service, expect around 3 wks for that. Then give me a few days for testing/programming/packing/shipping.12-C wrote: Can you quote a price and how long until delivery?
It certainly does 0.3mm nickel, but a lot depends on the power source. The welder circuit contributes only 140 micro (!) ohms. The MOSFETs are rated 40V and I have programmed a current limit of 2000A for 200ms, so there should be enough headroom for thicker materials.12-C wrote: Do you anticipate it being able to weld copper, aluminum, or any others?
Last edited by tatus1969 on Jul 11 2017 2:23am, edited 1 time in total.
Resistance is futile - We Are The Watt.
Re: low cost DIY battery spot welder
I made a video where I am doing robustnes testing:
edit: this time the correct link:
https://youtu.be/fWXphoDE_H8
edit: this time the correct link:
https://youtu.be/fWXphoDE_H8
Resistance is futile - We Are The Watt.
Re: low cost DIY battery spot welder
Okay, I'll continue finishing the release design and send an RFQ to my PCB assembly company, but I wanted to share this one with you first. It's rather crazy (and educational?), please don't take it too seriously - I am a quality minded professional EE despite of what you see there
https://youtu.be/JR3GJYScquc

https://youtu.be/JR3GJYScquc
Resistance is futile - We Are The Watt.
Re: low cost DIY battery spot welder
hahaha that was great, I actually jumped lol scared me as much as you loltatus1969 wrote:Okay, I'll continue finishing the release design and send an RFQ to my PCB assembly company, but I wanted to share this one with you first. It's rather crazy (and educational?), please don't take it too seriously - I am a quality minded professional EE despite of what you see there![]()
https://youtu.be/JR3GJYScquc
would it be possible to program a sensing feature to prevent autofire if the electrodes are in contact?
Re: low cost DIY battery spot welder
HaHaha, very educational.
Made me jump too, interesting to see the extreme
Made me jump too, interesting to see the extreme

Re: low cost DIY battery spot welder
Maybe some heat-shrink tubing around the electrodes with only the tip exposed might help with the accidental firing.
I could imagine using a foot pedal in conjunction with the auto fire as well. Use the foot pedal to disable firing when not pressed. I didn't really like using a foot pedal for firing as the thing had a bad tendency to move around on the floor, but I could see just holding it down to enable auto-fire.
Pretty impressive it welds those slotted tabs with the electrodes on the same side of the slot. With the electrodes on opposite sides of the slot, it should take much less current to get a good weld.

Pretty impressive it welds those slotted tabs with the electrodes on the same side of the slot. With the electrodes on opposite sides of the slot, it should take much less current to get a good weld.
"One test is worth a thousand opinions"
Re: low cost DIY battery spot welder
That is not easily possible. I need to fire a pulse in order to measure the resistance between the electrodes, it cannot distinguish a dead short from a nickel strip before that. If what I did in the video were a dead short. But I had a different idea, the video showing it is already rendering12-C wrote: would it be possible to program a sensing feature to prevent autofire if the electrodes are in contact?

What would probably be convenient is to integrate the switch into one of the electrode holder, and make it spring loaded, but that definitely exceeds my mechanical skills. Not to speak of how to maintain low resistance...
You bet what I did right after the videofechter wrote: Maybe some heat-shrink tubing around the electrodes with only the tip exposed might help with the accidental firing.![]()

Me too, for the same reason. But that is an interesting idea, I will keep that in mind. Please watch my next video and tell me what you think about my improvement idea.fechter wrote: I could imagine using a foot pedal in conjunction with the auto fire as well. Use the foot pedal to disable firing when not pressed. I didn't really like using a foot pedal for firing as the thing had a bad tendency to move around on the floor, but I could see just holding it down to enable auto-fire.
You probably don't believe me that I already knew how to use these tabs before making that video...fechter wrote: Pretty impressive it welds those slotted tabs with the electrodes on the same side of the slot.
Last edited by tatus1969 on Jul 12 2017 3:07pm, edited 1 time in total.
Resistance is futile - We Are The Watt.
Re: low cost DIY battery spot welder
There goes the next video, showing some improvements:
https://youtu.be/9-CQd02EDIs
https://youtu.be/9-CQd02EDIs
Resistance is futile - We Are The Watt.
Re: low cost DIY battery spot welder
Nice features!