Hi

I have made a custom hub motor dropout for Scott high Octane, voltage and Gambler. Those models have the same removable drop-out.
this made the conversion for to Ebike easier. Made from 6061 aluminium CNC
this is a time consuming process so the price is set at 250$ for the set.

Pm me for any questions
Attachments
scott drop-out 2.jpg
scott drop-out 2.jpg (147.26 KiB) Viewed 978 times
scott drop-out.jpg
scott drop-out.jpg (153.19 KiB) Viewed 978 times

whereswally606   100 kW

100 kW
Posts: 1106
Joined: Jun 19 2011 2:11pm
Location: Cheshire, UK

Re: Scott High Octane, Voltage and Gambler Hub Motor Drop-ou

Post by whereswally606 » Aug 31 2017 6:34am

I think I've been waiting about 8 years for someone to do this. I've got 3 frames (ransoms) but 250 dollars is beyond my budget. do you have the STL cause I'm building a mpcnc and might roll my own too. Check out my thread on bikes with removable dropouts you might find a market if you could do any bike to order.

Sent from my ALE-L02 using Tapatalk
Distributing "Lebowski" FOC Controller PCB (Through hole) since 2016
Moped: Emax 110s 2009

leffex   100 W

100 W
Posts: 192
Joined: Apr 08 2012 4:39pm
Location: Sweden

Re: Scott High Octane, Voltage and Gambler Hub Motor Drop-ou

Post by leffex » Sep 01 2017 6:00am

awesome. I like your style. If I needed I'd buy from you but not right now. I love ebike creativeity and work/jobs coming out of this and especially it's very cool to se actual success, though, even smal :D
5kw, dh, 85v/65a system.

straby187   1 mW

1 mW
Posts: 14
Joined: Nov 05 2015 12:02pm

Re: Scott High Octane, Voltage and Gambler Hub Motor Drop-ou

Post by straby187 » Sep 01 2017 12:03pm

voltagedeopout.jpg
voltagedeopout.jpg (48.57 KiB) Viewed 910 times
Real nice!! I had to hand mill my voltage dropouts and wasted a lot of aluminum..



User avatar
boisrondevens   100 W

100 W
Posts: 205
Joined: Jul 11 2011 11:30am
Location: Canada
Contact:

Re: Scott High Octane, Voltage and Gambler Hub Motor Drop-out

Post by boisrondevens » Feb 28 2018 5:55pm

New built with custom drop-out
Attachments
IMG_Feb282018at55316PM.jpg
IMG_Feb282018at55316PM.jpg (129.23 KiB) Viewed 519 times
IMG_Feb282018at64335PM.jpg
IMG_Feb282018at64335PM.jpg (102.04 KiB) Viewed 504 times
IMG_Feb282018at64308PM.jpg
IMG_Feb282018at64308PM.jpg (61.43 KiB) Viewed 504 times

whereswally606   100 kW

100 kW
Posts: 1106
Joined: Jun 19 2011 2:11pm
Location: Cheshire, UK

Re: Scott High Octane, Voltage and Gambler Hub Motor Drop-out

Post by whereswally606 » Mar 01 2018 7:30am

they look so sweet. loving the colour scheme.
Distributing "Lebowski" FOC Controller PCB (Through hole) since 2016
Moped: Emax 110s 2009

Post Reply