Re: Battery Advice Needed For Middle School Competition

Post by DrkAngel » Nov 11 2017 2:46pm

Sonas @ $150 per 100 cells = 4 x 24 cell battery builds
A little learning is a dangerous thing;
Drink deep, or taste not the Pierian spring:
There, shallow draughts intoxicate the brain,
And drinking largely, sobers us again.

I enjoy enlightening ... and enlivening the spirit of the innovators.

New & Improved - Acronym Definitions

Index - Homemade Battery Packs - Updated - December 2019

EBike Toolbox - Bargains! $

Endless Sphere Wiki - Lost?

BlueBell   10 W

10 W
Posts: 74
Joined: Sep 28 2017 2:52am

Re: Battery Advice Needed For Middle School Competition

Post by BlueBell » Nov 11 2017 4:08pm

DrkAngel wrote:Sonas @ $150 per 100 cells = 4 x 24 cell battery builds
OMG, you should see what I get when Googling this!
Can't seem to find Sonas lipo's on-line...

User avatar
DrkAngel   100 GW

100 GW
Posts: 5435
Joined: Dec 15 2010 11:14am
Location: Upstate-Western-Southern Tier NY. USA

Re: Battery Advice Needed For Middle School Competition

Post by DrkAngel » Nov 12 2017 4:49pm

BlueBell wrote:
DrkAngel wrote:Sonas @ $150 per 100 cells = 4 x 24 cell battery builds
OMG, you should see what I get when Googling this!
Can't seem to find Sonas lipo's on-line...
Can't confirm Sona cells as 2000mAh ...
Not sure of replacement candidates.

Need:
180Wh ÷ 3.6V cells = 50Ah
12s2p (≤ 2080mAh cells) 43.2V 2000 or 2050mAh
13s2p (≤ 1923mAh cells) 46.8V
14s2p (≤ 1785mAh cells) 50.4V best ... if available
15s2p (≤ 1666mAh cells) 54V 1650mAh cells max recommended
16s2p (≤ 1562mAh cells)57.6V


180Wh ÷ 3.7V cells = 48.64Ah
12s2p (≤ 2026mAh cells) 44.4V
13s2p (≤ 1870mAh cells) 48.1V best ... if available
14s2p (≤ 1737mAh cells) 51.8V
15s2p (≤ 1621mAh cells) 55.5V 1600mAh cells max recommended
16s2p (≤ 1529mAh cells) 59.2V

Reputable possibilities:

Image

Lipo ...
.
A little learning is a dangerous thing;
Drink deep, or taste not the Pierian spring:
There, shallow draughts intoxicate the brain,
And drinking largely, sobers us again.

I enjoy enlightening ... and enlivening the spirit of the innovators.

New & Improved - Acronym Definitions

Index - Homemade Battery Packs - Updated - December 2019

EBike Toolbox - Bargains! $

Endless Sphere Wiki - Lost?

User avatar
DrkAngel   100 GW

100 GW
Posts: 5435
Joined: Dec 15 2010 11:14am
Location: Upstate-Western-Southern Tier NY. USA

Re: Battery Advice Needed For Middle School Competition

Post by DrkAngel » Nov 12 2017 5:18pm

Hobbyking!

11.1V 3200mAh Turnigy LiPo - $20

3s 11.1V x 3.2Ah =35.52Wh x 5 = 177.6Wh

15s LiPo 55.5V 3.2Ah = 177.6Wh


3s 11.1V 4000mAh LiPo

3s 11.1V x 4.0Ah = 44.4Wh x 4 = 177.6Wh

12s LiPo 44.4V 4.0Ah = 177.6Wh
A little learning is a dangerous thing;
Drink deep, or taste not the Pierian spring:
There, shallow draughts intoxicate the brain,
And drinking largely, sobers us again.

I enjoy enlightening ... and enlivening the spirit of the innovators.

New & Improved - Acronym Definitions

Index - Homemade Battery Packs - Updated - December 2019

EBike Toolbox - Bargains! $

Endless Sphere Wiki - Lost?

BlueBell   10 W

10 W
Posts: 74
Joined: Sep 28 2017 2:52am

Re: Battery Advice Needed For Middle School Competition

Post by BlueBell » Nov 12 2017 9:52pm

DrkAngel,

I'm really starting to feel like an idiot here.
Not really sure what you're trying to beat me over the head with.
It looks like four different battery options...?
Is that right?
Is the C-number relevent here or are they all the same?
Knowing our requirements, is there one combination you would recommend over another?
If it's all the same then I would think the fewer number of pieces the fewer connections we'd have to make.
And what about charging?
The IMax B6?
Does that go between the panels and the battery?
What A/C charger were you thinking of or should we just use the panels leading up to the race?
I'm starting to get discouraged here, it seems like I'm missing something... something obvious.
<sigh>

User avatar
DrkAngel   100 GW

100 GW
Posts: 5435
Joined: Dec 15 2010 11:14am
Location: Upstate-Western-Southern Tier NY. USA

Re: Battery Advice Needed For Middle School Competition

Post by DrkAngel » Nov 12 2017 11:54pm

Sona 18650 cells may not qualify due to lack of documentation-verification of capacity.

2 different Lipo possibilities.
Higher C rate provides less sag but very high C rate tends to sacrifice reliability-durability.
Under your planned discharge C rate will be less than 3 C, so possibly 20-30C might be optimal.

iMax B6 is for testing, charging and balancing (equalizing) individual 3s LiPo, 4 individual charges for 3s LiPo packs.
Use panels to "top off" battery.
I recommend the 4 x 4000mAh as best choices. 5 x 3200mAh pushes charged voltage to 63V which is the probable controllers capacitor rating-limit. I don't recommend pushing to limit.
A little learning is a dangerous thing;
Drink deep, or taste not the Pierian spring:
There, shallow draughts intoxicate the brain,
And drinking largely, sobers us again.

I enjoy enlightening ... and enlivening the spirit of the innovators.

New & Improved - Acronym Definitions

Index - Homemade Battery Packs - Updated - December 2019

EBike Toolbox - Bargains! $

Endless Sphere Wiki - Lost?

markz   100 GW

100 GW
Posts: 11986
Joined: Jan 09 2014 11:38pm
Location: Alberta Canada

Re: Battery Advice Needed For Middle School Competition

Post by markz » Nov 13 2017 12:21am

High Ah trades off Discharge in 18650 format, so 3.5Ah is the highest these days, best guess is 10A discharge. But them 2.0-2.5Ah's can get 25A-30A discharge.

I have not looked at pouches or other formats.
Last edited by markz on Nov 14 2017 2:38pm, edited 1 time in total.

999zip999   100 GW

100 GW
Posts: 9878
Joined: Jan 10 2010 1:40pm
Location: Dana Point So. Cal

Re: Battery Advice Needed For Middle School Competition

Post by 999zip999 » Nov 13 2017 11:35am

I know it takes a lot of energy to get the prop started
So what is the amp draw of the controller and add a few ? So 12s 2p of Samsung 25r cells 25amp cell. Price is going down. Maybe 3.75- 4.00 usd each.

BlueBell   10 W

10 W
Posts: 74
Joined: Sep 28 2017 2:52am

Re: Battery Advice Needed For Middle School Competition

Post by BlueBell » Nov 14 2017 2:24pm

"Sona 18650 cells may not qualify due to lack of documentation-verification of capacity."
Yes, you hit the nail on the head there.
They require documentation of battery specs.
Max 180 Watt-hours

Not sure which Turnigy 4000 you meant.
This one:
https://hobbyking.com/en_us/turnigy-bat ... xt-60.html

How will we ensure 25 minutes out of this set-up?
If we fall short by even 20 seconds we are disqualified!


"I know it takes a lot of energy to get the prop started"
Not really, especially considering the high torque of electric motors on start up.
It takes considerable more power at speed, ~8 - 10 knots ( ~4.5 m/s ).

User avatar
DrkAngel   100 GW

100 GW
Posts: 5435
Joined: Dec 15 2010 11:14am
Location: Upstate-Western-Southern Tier NY. USA

Re: Battery Advice Needed For Middle School Competition

Post by DrkAngel » Nov 14 2017 3:43pm

Not sure on the 4Ah RC LiPo.
1. Median C rate, (20-30C for better consistency-reliability)
2. good brand name. Ask others about "good brand name".

Watt meter has watt function.
... think I figured this for you already ...
DrkAngel wrote:2. Watt-watt Hour meters are fairly accurate and inexpensive. If a throttle is used, maximum safe battery output can be regulated fairly precisely!
180wh x 60/25 min = 432w
Should maintain 400w+ battery output for 25 minutes
Important to test drive before actual race.
Keep throttle positioned for determined watt usage (400W?) battery output.
A little learning is a dangerous thing;
Drink deep, or taste not the Pierian spring:
There, shallow draughts intoxicate the brain,
And drinking largely, sobers us again.

I enjoy enlightening ... and enlivening the spirit of the innovators.

New & Improved - Acronym Definitions

Index - Homemade Battery Packs - Updated - December 2019

EBike Toolbox - Bargains! $

Endless Sphere Wiki - Lost?

BlueBell   10 W

10 W
Posts: 74
Joined: Sep 28 2017 2:52am

Re: Battery Advice Needed For Middle School Competition

Post by BlueBell » Nov 14 2017 4:59pm

Ah, yes indeed, you did show me that, thank you and my apologies for overlooking it.
I've just read through the thread a few times and believe I'm getting a firm grasp on reality, finally.

So, 25C constant with 50C burst isn't okay?
You pick one. :)

BlueBell   10 W

10 W
Posts: 74
Joined: Sep 28 2017 2:52am

Re: Battery Advice Needed For Middle School Competition

Post by BlueBell » Nov 14 2017 5:04pm


User avatar
DrkAngel   100 GW

100 GW
Posts: 5435
Joined: Dec 15 2010 11:14am
Location: Upstate-Western-Southern Tier NY. USA

Re: Battery Advice Needed For Middle School Competition

Post by DrkAngel » Nov 14 2017 6:08pm

Either look good!
If budget allows, might recommend 2 sets of batteries or at least 1 spare, in case of accident or failure?
Graphene is newer tech with greater reputed lifespan.
A little learning is a dangerous thing;
Drink deep, or taste not the Pierian spring:
There, shallow draughts intoxicate the brain,
And drinking largely, sobers us again.

I enjoy enlightening ... and enlivening the spirit of the innovators.

New & Improved - Acronym Definitions

Index - Homemade Battery Packs - Updated - December 2019

EBike Toolbox - Bargains! $

Endless Sphere Wiki - Lost?

BlueBell   10 W

10 W
Posts: 74
Joined: Sep 28 2017 2:52am

Re: Battery Advice Needed For Middle School Competition

Post by BlueBell » Nov 14 2017 7:41pm

Yes, we are advised to have a second battery in case of poor weather and the solar-only heats will run on battery instead.

But I thought you didn't like the first one, the HobbyKing R/C one.
Graphene you say. Perhaps that has something to do with the differing three letter abbreviation associated with the different lipo listings.

Come on, stick your neck out and recommend one... please.
Or your two top picks, then you're not on the hook.
Is the heavier battery, of the same rating, the better way to go?

Thanks again.

User avatar
DrkAngel   100 GW

100 GW
Posts: 5435
Joined: Dec 15 2010 11:14am
Location: Upstate-Western-Southern Tier NY. USA

Re: Battery Advice Needed For Middle School Competition

Post by DrkAngel » Nov 14 2017 7:53pm

A little learning is a dangerous thing;
Drink deep, or taste not the Pierian spring:
There, shallow draughts intoxicate the brain,
And drinking largely, sobers us again.

I enjoy enlightening ... and enlivening the spirit of the innovators.

New & Improved - Acronym Definitions

Index - Homemade Battery Packs - Updated - December 2019

EBike Toolbox - Bargains! $

Endless Sphere Wiki - Lost?

BlueBell   10 W

10 W
Posts: 74
Joined: Sep 28 2017 2:52am

Re: Battery Advice Needed For Middle School Competition

Post by BlueBell » Nov 14 2017 8:00pm

Lol, ok, graphene it is... even though it's lighter.

markz   100 GW

100 GW
Posts: 11986
Joined: Jan 09 2014 11:38pm
Location: Alberta Canada

Re: Battery Advice Needed For Middle School Competition

Post by markz » Nov 15 2017 1:39pm

With them RC lipo its just like lego, you plug whatever you want together, making sure to pay very very very very close attention to what you are doing. Buying or making a parallel adapter, I used a 5.5mm connector with 10awg that split into six 4mm 12 or 14awg wire, then I bought some 5.5mm bullets and some wire to solder the main wire. Its pretty simple to learn. Then you got to take care in charging and discharging. One day I will buy LiPo again.

BlueBell   10 W

10 W
Posts: 74
Joined: Sep 28 2017 2:52am

Re: Battery Advice Needed For Middle School Competition

Post by BlueBell » Nov 16 2017 11:26am

999zip999 wrote:I know it takes a lot of energy to get the prop started
So what is the amp draw of the controller and add a few ? So 12s 2p of Samsung 25r cells 25amp cell. Price is going down. Maybe 3.75- 4.00 usd each.
Did you mean it takes a lot to get the motor going?
I've been told we may have a problem when running on panels only getting the motor turning due to it's high start-up draw. The panels may drop below the min voltage cut off in the controller.

BlueBell   10 W

10 W
Posts: 74
Joined: Sep 28 2017 2:52am

Re: Battery Advice Needed For Middle School Competition

Post by BlueBell » Nov 16 2017 11:40am

DrkAngel,

I noticed the upper limit on the motor controller is 42.5 +/- 0.5 Volts.
Is this going to be a problem at 44.4V?
This is printed on the controller, the spec sheet differs, same for LVC.

User avatar
DrkAngel   100 GW

100 GW
Posts: 5435
Joined: Dec 15 2010 11:14am
Location: Upstate-Western-Southern Tier NY. USA

Re: Battery Advice Needed For Middle School Competition

Post by DrkAngel » Nov 16 2017 12:59pm

.
...
Edited!

Better contact seller to confirm!
States 36-48V capable! ... ?
Very often 36V controllers have no HVC (High Voltage Cutoff) 42.5V might be hypothetical?

42.5V upper limit would be bad for 44.4V or from panels!
~31V LVC with 44.4V ≥ 50.4V charged capability required.
Last edited by DrkAngel on Nov 18 2017 9:42am, edited 3 times in total.
A little learning is a dangerous thing;
Drink deep, or taste not the Pierian spring:
There, shallow draughts intoxicate the brain,
And drinking largely, sobers us again.

I enjoy enlightening ... and enlivening the spirit of the innovators.

New & Improved - Acronym Definitions

Index - Homemade Battery Packs - Updated - December 2019

EBike Toolbox - Bargains! $

Endless Sphere Wiki - Lost?

999zip999   100 GW

100 GW
Posts: 9878
Joined: Jan 10 2010 1:40pm
Location: Dana Point So. Cal

Re: Battery Advice Needed For Middle School Competition

Post by 999zip999 » Nov 17 2017 11:20pm

42 volt is 10s fully charged.
Ok srill guessing 42v fully charged x 42,000mah equals 176 wh ?

User avatar
DrkAngel   100 GW

100 GW
Posts: 5435
Joined: Dec 15 2010 11:14am
Location: Upstate-Western-Southern Tier NY. USA

Re: Battery Advice Needed For Middle School Competition

Post by DrkAngel » Nov 18 2017 9:03am

Volts x Amps = Watts
Volts x Amp hours= Watt hours
V x Ah = Wh

"V" (Volts) is based on the average discharge voltage during a full discharge.
EG. 4.2V >> 3.2V MFG rated @ 3.7V
Wh is based on Ah x V averaged

Wh is rated at mfg rating of average voltage at modest discharge rate 11.1V (3x cell 3.7V) x mfg rated mAh (4000mAh) = 44.4Wh
(12s) 44.4V x 4Ah = 177.6Wh (180Wh limit)

edited previous post ... clarified expanded.
Last edited by DrkAngel on Nov 19 2017 2:40pm, edited 1 time in total.
A little learning is a dangerous thing;
Drink deep, or taste not the Pierian spring:
There, shallow draughts intoxicate the brain,
And drinking largely, sobers us again.

I enjoy enlightening ... and enlivening the spirit of the innovators.

New & Improved - Acronym Definitions

Index - Homemade Battery Packs - Updated - December 2019

EBike Toolbox - Bargains! $

Endless Sphere Wiki - Lost?

999zip999   100 GW

100 GW
Posts: 9878
Joined: Jan 10 2010 1:40pm
Location: Dana Point So. Cal

Re: Battery Advice Needed For Middle School Competition

Post by 999zip999 » Nov 18 2017 4:12pm

Aren't we stuck at 42.5 volts because the upper limit of his controller or 10s ?

BlueBell   10 W

10 W
Posts: 74
Joined: Sep 28 2017 2:52am

Re: Battery Advice Needed For Middle School Competition

Post by BlueBell » Nov 22 2017 1:24pm

Can we pick the direction of rotation on this motor or is it predetermined?
We are proposing to thread an aluminum tube onto the shaft threads of the motor.
If it turns counterclockwise, it will tend to unscrew our propeller shaft!

User avatar
DrkAngel   100 GW

100 GW
Posts: 5435
Joined: Dec 15 2010 11:14am
Location: Upstate-Western-Southern Tier NY. USA

Re: Battery Advice Needed For Middle School Competition

Post by DrkAngel » Nov 22 2017 3:18pm

Youtube search shows motor turns clockwise, facing gear.

BM1418ZXF(BLDC)

Brushless motors, typically, are not reversible, without special controller.
A little learning is a dangerous thing;
Drink deep, or taste not the Pierian spring:
There, shallow draughts intoxicate the brain,
And drinking largely, sobers us again.

I enjoy enlightening ... and enlivening the spirit of the innovators.

New & Improved - Acronym Definitions

Index - Homemade Battery Packs - Updated - December 2019

EBike Toolbox - Bargains! $

Endless Sphere Wiki - Lost?

Post Reply