Yes, i have rewelded the sidepods and using larger tube that goes over the frame.

- sidebars.jpg (447.68 KiB) Viewed 813 times
And i used 5mm aluminium sheets so I could place my first battery cells "winston 60Ah lifepo" 16pcs in left and right.

- sidebumperholders.jpg (226.64 KiB) Viewed 813 times
With my lighter 37kg small lifepo4 pack left and right side are the same as I have in the right ~23kg motor with mounts and ~10kg controller with cooling.
If I would start with a new frame I would do i differently. I think some round or sqare aluminium tubes that sits on the frame and go from left to right under the seat. And connect with some clamps. It would be lighter and still allow frame to bend in corners.
But still i would use battery in left and controller and motor in right.
Also my current setup is to low and i have to replace some intube nuts because they worn out as seen in this picture (do not look at red circles, I have an old frame and it was worn in that places so I had to reinforce it).