Panosonic 25ah Prismatic cells for sale $28

Have extra parts that need a good home? Post it up here and see if anyone else is searching for what you are selling.
Joachim   1 kW

1 kW
Posts: 435
Joined: Jul 30 2015 1:02pm
Contact:

Re: Panosonic 25ah Prismatic cells for sale $22

Post by Joachim » Jun 01 2018 6:16am

Image
Image

eric1565   10 W

10 W
Posts: 96
Joined: Feb 28 2015 4:50pm

Re: Panosonic 25ah Prismatic cells for sale $22

Post by eric1565 » Jun 03 2018 2:04pm

Update on the 12V car battery.

These cells do not take much to squash them down. All these bolt as hand tight. I have used the original bus bars as gages to make sure they are all good.

Still need to trim the all threads, and to put in a bottom supporting structure.

IMG_20180603_135607546.jpg
IMG_20180603_135607546.jpg (237.34 KiB) Viewed 2052 times

dafex   1 mW

1 mW
Posts: 15
Joined: Oct 06 2014 10:08am

Re: Panosonic 25ah Prismatic cells for sale $22

Post by dafex » Jun 03 2018 5:10pm

Hi Eric,

why you didn't reuse the original brackets? Cut the brackets apart and weld them together to fit the length of the new batterie.

I have done this with 12s batteries to build 14s batteries.
VW Batterie 1.jpg
Old and new Batterie
VW Batterie 2.jpg
During disassembling
VW Batterie 3.jpg
Welded brackets

eric1565   10 W

10 W
Posts: 96
Joined: Feb 28 2015 4:50pm

Re: Panosonic 25ah Prismatic cells for sale $22

Post by eric1565 » Jun 04 2018 12:26pm

I thought about that, but I was in a hurry to make this. Also didn't have easy access to a welder :( I still have the brackets, and can still do that. But what I am currently doing is planning on making custom aluminum cases to hold the batteries.

The other reason why I didn't do it was because I still was not sure what size I needed it to be. Now that I have built up this 4S2P battery I know what it needs to be. I've now cad'ed it all up and have exact sizes.

Eric

User avatar
parabellum   10 MW

10 MW
Posts: 2085
Joined: Nov 19 2010 9:55am
Location: Dominican Republic, north.

Re: Panosonic 25ah Prismatic cells for sale $22

Post by parabellum » Jun 12 2018 11:05pm

Hi Eric.

1.13"/cell looks right, where array starts to hold in 1 peace without cells sliding on each other, thanks.

Can you suggest a charge rate and max. charge rate for those cells?

P.S. I think it will not harm to add all new findings in the first post, like compression width, DCR and all relevant to the buyer information.

eric1565   10 W

10 W
Posts: 96
Joined: Feb 28 2015 4:50pm

Re: Panosonic 25ah Prismatic cells for sale $22

Post by eric1565 » Jun 14 2018 5:50pm

Charge rate of .3C to 1C. I have not check to see what the cmax regens at.

The 3.3kwh charger charges at .3C

I know for Tesla cells we recommend .3C charge rate and these can handle much more.

I will update the first post shortly

Eric

eric1565   10 W

10 W
Posts: 96
Joined: Feb 28 2015 4:50pm

Re: Panosonic 25ah Prismatic cells for sale $22

Post by eric1565 » Jul 04 2018 11:41pm

I gave a friend of mine the 12V pack I made. He has a 2500 watt audio system in his car. He had 2 car lead batteries in his car, and when he turned it up the voltage sagged to 11.2V. He added the lithium battery, and the voltage dropped to 13.2 when he turned it up. So significant improvement. He has yes to remove the 2nd lead battery to give me data on that.

I'm in the process of making an enclosure for the battery, and well sell 50, 75, and 100 ah "12v" batteries. They would run a bit better if the voltage on the alternator was increased up to 15V or so. The batteries will also have a 4S BMS installed.

Eric

eric1565   10 W

10 W
Posts: 96
Joined: Feb 28 2015 4:50pm

Re: Panosonic 25ah Prismatic cells for sale $22

Post by eric1565 » Jul 08 2018 10:18pm

I got the 12V car audio battery together. I put in plastic spacers between all the aluminum parts.

I ran out of aluminum bar stock so I used some of the OEM buss bars.
IMG_20180708_214610178_small.jpg
IMG_20180708_214610178_small.jpg (152.28 KiB) Viewed 1838 times
IMG_20180708_214626127_small.jpg
IMG_20180708_214626127_small.jpg (183.13 KiB) Viewed 1838 times
IMG_20180708_214723029_HDR_small.jpg
IMG_20180708_214723029_HDR_small.jpg (99.14 KiB) Viewed 1838 times
IMG_20180708_214733796s.jpg
IMG_20180708_214733796s.jpg (228.68 KiB) Viewed 1838 times

User avatar
parabellum   10 MW

10 MW
Posts: 2085
Joined: Nov 19 2010 9:55am
Location: Dominican Republic, north.

Re: Panosonic 25ah Prismatic cells for sale $22

Post by parabellum » Jul 08 2018 10:55pm

That looks really cool. Nice CNC.
Why are you using aluminium for connectors?
My first thought was copper, I used it finally as well with some contact grease on (aluminium will need some oxide breaking compound to).

eric1565   10 W

10 W
Posts: 96
Joined: Feb 28 2015 4:50pm

Re: Panosonic 25ah Prismatic cells for sale $22

Post by eric1565 » Jul 09 2018 10:22am

I guess I can get copper. Aluminum is easy to get. And has decent current carrying capabilities.

Was thinking of making a nickle solution to coat the aluminum with... If going to do that I guess I should just use copper.

I was a bit worried about the oxide, but they use aluminum for wires, well for a while untill houses started to burn down. But that was a function of creep. Not an issue with bars.

Still perfecting the design. I will look into copper.

If u have any other suggestions or questions let me know

Eric
Last edited by eric1565 on Aug 27 2018 1:31pm, edited 1 time in total.

999zip999   100 GW

100 GW
Posts: 9934
Joined: Jan 10 2010 1:40pm
Location: Dana Point So. Cal

Re: Panosonic 25ah Prismatic cells for sale $22

Post by 999zip999 » Jul 09 2018 10:54pm

Can you put a lighter or a ruler in those pictures so we can get a idea what size these packs are ? Thank you

eric1565   10 W

10 W
Posts: 96
Joined: Feb 28 2015 4:50pm

Re: Panosonic 25ah Prismatic cells for sale $22

Post by eric1565 » Jul 10 2018 9:52pm

Here are some pics of the model.

I'm sorry they are not of the real part, but i'm lazy :(

You can hand calc it out pretty easy. Each cell is 1.13 thick, so if you add up the cells X 1.13 and then add on .375" for the 2 end pieces * 2 (.75" total) you should get the lenght of the pack. Yeah pretty close... calc says 9.79, actual is 9.7ish.

Weight is about 13 lbs.(about 1.6 lbs per cell) you can hold with one hand no problem... about 800Wh (each cell is like 93wh, I rounded) I can do any size up to 3 or 4' long. 10" is the longest so far, and I am sure there is a learning process for the longer ones... 20" is no problem, but I would guess longer than that gets to be trickly to assemble.
cad_pics_of_packs_1.JPG
cad_pics_of_packs_1.JPG (102.55 KiB) Viewed 1775 times
cad_pics_of_packs_2.JPG
cad_pics_of_packs_2.JPG (86.96 KiB) Viewed 1775 times
cad_pics_of_packs_3.JPG
cad_pics_of_packs_3.JPG (77.38 KiB) Viewed 1775 times

999zip999   100 GW

100 GW
Posts: 9934
Joined: Jan 10 2010 1:40pm
Location: Dana Point So. Cal

Re: Panosonic 25ah Prismatic cells for sale $22

Post by 999zip999 » Jul 11 2018 4:00pm

Thanks for the answer I will mock something up to check fit.

eric1565   10 W

10 W
Posts: 96
Joined: Feb 28 2015 4:50pm

Re: Panosonic 25ah Prismatic cells for sale $22

Post by eric1565 » Jul 11 2018 9:54pm

Pic of the prototype with the 3D printed terminal caps.
IMG_20180711_084117139.jpg
IMG_20180711_084117139.jpg (125.87 KiB) Viewed 1747 times

999zip999   100 GW

100 GW
Posts: 9934
Joined: Jan 10 2010 1:40pm
Location: Dana Point So. Cal

Re: Panosonic 25ah Prismatic cells for sale $22

Post by 999zip999 » Jul 12 2018 3:04pm

That looks much better than the illustration

eric1565   10 W

10 W
Posts: 96
Joined: Feb 28 2015 4:50pm

Re: Panosonic 25ah Prismatic cells for sale $22

Post by eric1565 » Jul 24 2018 10:18pm

Ok, still working on the car audio battery. But it could be anything depending on how the cell layout. This is a 100ah battery I am making for a guy. I am redesigning it to be beefier, because I think it is a bit wimpy.

4S4P_100ah_1small.jpg
4S4P_100ah_2small.jpg
4S4P_100ah_3small.jpg
4S4P_100ah_4Small.jpg
Eric

KD5ZXG   10 W

10 W
Posts: 87
Joined: Jul 13 2018 10:02pm

Re: Panosonic 25ah Prismatic cells for sale $22

Post by KD5ZXG » Jul 25 2018 2:12am

So, how many would I need to buy from you to get them in an original frame?
I'm not even sure how many different sized frames you might have collected.

I'm on the north side of Dallas. How best might they get here from Houston
without the delivery man setting himself on fire? Even Greyhound won't ship
Lithium.

eric1565   10 W

10 W
Posts: 96
Joined: Feb 28 2015 4:50pm

Re: Panosonic 25ah Prismatic cells for sale $22

Post by eric1565 » Jul 25 2018 11:24am

I don't fully understand the question so here are multiple answers
1. In the stock OEM frame there are 21 - this is the cheapest way to get cells. U buy 21 and I'll sell them for $410 plus shipping
2. I can make any size frame any voltage any capacity range. The frames COST me about $100 to make so I sell them for $125. If I can lower that cost over time prices will reflect that. I would not do more that 16-20 cells... It started to be difficult to compress.
3. I have 2 assys for sale on eBay. Prices on ES are 10% less. I have a 50 ah and a 100ah.

I am scrapping all the current frames due to lack or size. I am beefing them up. Current end plates bend slightly, new style will not bend.

coleasterling   100 W

100 W
Posts: 292
Joined: Sep 21 2010 3:37am

Re: Panosonic 25ah Prismatic cells for sale $22

Post by coleasterling » Jul 25 2018 12:36pm

You clearly have CNC capability of some sort, but if you wanted to have someone else do it, I own and run a full CNC shop in College Station and would be interested in quoting your parts. I like your solution for these cells, overall. Looked at using them several times myself, but the form factor isn't quite right for my application.

81forest   100 W

100 W
Posts: 105
Joined: Jun 11 2018 12:14pm
Location: Issaquah, WA

Re: Panosonic 25ah Prismatic cells for sale $22

Post by 81forest » Aug 11 2018 1:16pm

Pm sent, are these still available?

User avatar
marty3d   1 µW

1 µW
Posts: 1
Joined: Aug 11 2018 6:25pm

Re: Panosonic 25ah Prismatic cells for sale $28

Post by marty3d » Jan 13 2019 12:42am

Are any of these still available?
E-Bike, rear hub motor, Grin CA & controller, 16S batteries
Fat tire scooter - Cushman 2hp brushed motor, Curtis 300A controller, 10S lipo, Arduino control conditioner.