Bosch Active Line 3 mid-drive motor tear down

Electric Motors and Controllers
Post Reply
User avatar
avandalen   10 W

10 W
Posts: 96
Joined: Oct 02 2010 10:40am
Location: Maastricht, The Netherlands
Contact:

Bosch Active Line 3 mid-drive motor tear down

Post by avandalen » Sep 08 2018 9:50am

For my solar powered bicycle, the Maxun One, I designed a very powerful and lightweight mid-drive motor. I also wanted to investigate whether I could use a Bosch Active Line 3 motor. The Bosch motor weight is 2975g, this is relatively lightweight for a mid-drive motor, but it is still too heavy for my solar bike.

So, I wanted to investigate if the Bosch motor can be reduced in weight, so I disassembled the motor. This is also a great opportunity to see how it works and which electronic parts are used.

See the whole article here:
http://www.avdweb.nl/solar-bike/hub-mot ... ine-3.html

What is striking after opening the motor is that there are only a few parts inside, that is a great achievement of the Bosch engineers:Image
Image
Image

See the whole article here:
http://www.avdweb.nl/solar-bike/hub-mot ... ine-3.html

User avatar
robbie   1 W

1 W
Posts: 50
Joined: Sep 28 2012 3:09pm

Re: Bosch Active Line 3 mid-drive motor tear down

Post by robbie » Sep 09 2018 12:59pm

A great tear down, and fantastic website by the way.

Have you figured out where you can remove any material to lighten the product up?

SlowCo   100 kW

100 kW
Posts: 1339
Joined: Jan 05 2015 5:43pm
Location: The Netherlands

Re: Bosch Active Line 3 mid-drive motor tear down

Post by SlowCo » Sep 09 2018 7:17pm

Beautiful engineering from Bosch and a nice tear down from you.
Some other light weight mid drives:
viewtopic.php?f=28&t=95704
https://www.gngebike.com/ultralight-300w-kit

And please show your own design here also.

casainho   1.21 GW

1.21 GW
Posts: 3845
Joined: Feb 14 2011 2:43pm

Re: Bosch Active Line 3 mid-drive motor tear down

Post by casainho » Sep 13 2018 4:56am

avandalen, thanks for sharing!!

Really good to see the Bosch technology and compare to cheap chinese options like TSDZ2 mid drive motor: https://github.com/OpenSource-EBike-fir ... _wiki/wiki

Sure Bosch technology is more advanced but from the perspective of using the motor to other applications like hand bicycles, repair, DIY and having/owning knowledge about motor technology, cheap chinese like TSDZ2 mid drive motor is the way to go!!
- TSDZ2 FAQ: issues and repairs, etc
- TSDZ2 OpenSource firmware

Developer of the Flexible OpenSource firmware for EBikes: TSDZ2 mid drive motor, KT motor controllers and displays: Bafang 850C color, SW102 Bluetooth and KT-LCD3.

If you like my work, please consider making a donation. I am being using the donations to buy needed resources for my developments. My paypal: casainho AT gmail.com.

User avatar
avandalen   10 W

10 W
Posts: 96
Joined: Oct 02 2010 10:40am
Location: Maastricht, The Netherlands
Contact:

Re: Bosch Active Line 3 mid-drive motor tear down

Post by avandalen » Sep 21 2018 9:51am

robbie wrote:
Sep 09 2018 12:59pm
A great tear down, and fantastic website by the way.

Have you figured out where you can remove any material to lighten the product up?
No it is not possible.
I will switch to a Shimano Steps E8000 (2.88kg) or Brose mid drive motor (2.9kg in 2019)

User avatar
avandalen   10 W

10 W
Posts: 96
Joined: Oct 02 2010 10:40am
Location: Maastricht, The Netherlands
Contact:

Re: Bosch Active Line 3 mid-drive motor tear down

Post by avandalen » May 21 2019 7:45am

See the article about the motor graph here:
Image
https://endless-sphere.com/forums/viewt ... 0&t=100180

Post Reply