Sanyo 25Ah nmc Voltage Drop

Batteries, Chargers, and Battery Management Systems.
Pota   100 W

100 W
Posts: 140
Joined: May 15 2017 8:27am

Re: Sanyo 25Ah nmc Voltage Drop

Post by Pota » Nov 08 2018 3:19pm

Okay, ill try explain it, thanks alot btw :D

First off, we have the same motor. Prestolite MTY4001 36v stock.

Just look at these two videos
https://www.youtube.com/watch?v=BGwtqgN_7no
https://www.youtube.com/watch?v=KObUDN7pMcE

the first is with EXTREMLY grippy wide tires.
the second is with normal gokart tires.
he is running 1.16:1

Same setup in both videos, only different tires. He is running 110v 500amp open revolt controller. In other words, yes more volt than mine, ive tested 84v, but again. today i tested 48v, and the burnout WITHOUT me in the cart is the same, just less high rpm wheel spin. (spun the tires at 480amp+ with the test yesterday @ 84v and today @48v, so seems the volt doesent make any different in when it starts to spin, both at 480amp+)

I did a test today with 48v. Pushing it against the wall, i wasent in the cart, so it only had around 60-70kg load at the back tires (motor and frame). Still same gear ratio 1:1. I added a clamp meter to be sure that the data from the controller wasent wrong, and yes, they was correct, i peaked 662amp @ 48v.
It started to spin the wheels at around 480amp+.

With me in the cart it would NEVER do any kind of burnout, and the wheels wouldent spin.

The motor is wired in this way
Plus to S-1
S-2 to A-1
Ground to A-2

Brush picture. I got 8 of these.
Attachments
45651734_2169983906601469_722118099926515712_n.jpg
45665132_2095268840525446_906543510285451264_n.jpg
45805286_1111024775739379_6829954799094464512_n.jpg
45642400_2254525871259391_5428584507454259200_n.jpg
45693898_2179296282311914_3457719853220102144_n.jpg
45754828_297086650904107_5660137296872079360_n.jpg
45793320_708988116167105_5758517096199749632_n.jpg
Last edited by Pota on Nov 08 2018 3:53pm, edited 2 times in total.

User avatar
neptronix   100 GW

100 GW
Posts: 14109
Joined: Jun 15 2010 5:56pm
Location: California refugee living in Utah, USA
Contact:

Re: Sanyo 25Ah nmc Voltage Drop

Post by neptronix » Nov 08 2018 3:51pm

Punx0r wrote:
Nov 08 2018 11:55am
If motor is the same and motor current is the same (or better) then your motor torque will be the same (or better) regardless of battery voltage. If gearing is the same (or lower) then axle torque will be the same (or better).
Unfortunately not the case with BLDC motors. You will see a jump in torque with voltage because the total wattage converted back down to phase amperage can be much higher.

You can even check this on the ebikes.ca motor simulator. Take this link and change the battery to the 66v dewalt battery. You'll see a ~20% boost in torque.

https://www.ebikes.ca/tools/simulator.h ... t=B3623_GA

But we need motor speed to make burnouts, which comes mostly from voltage, not amperage in this case. OP does not have the same motor speed because of a combination of huge battery sag and lower battery voltage to begin with.
"Love and compassion are necessities, not luxuries. Without them, humanity cannot survive." - Dalai Lama

My first major build: 1.6kW 8T MAC motor on a Trek 4500.
The new all-arounder: Leafmotor 1500w @ 4kW on a Turner O2 full suspension.
The monster scooter: 20" eZee on a Cannondale Semi Recumbent.
Whipper-snapper: ? on a lightweight BikeE Semi Recumbent

Pota   100 W

100 W
Posts: 140
Joined: May 15 2017 8:27am

Re: Sanyo 25Ah nmc Voltage Drop

Post by Pota » Nov 08 2018 4:22pm

Btw. This is brushed to brushless.

999zip999   100 GW

100 GW
Posts: 8986
Joined: Jan 10 2010 1:40pm
Location: Dana Point So. Cal

Re: Sanyo 25Ah nmc Voltage Drop

Post by 999zip999 » Nov 08 2018 5:56pm

3p...

Punx0r   100 GW

100 GW
Posts: 5311
Joined: May 03 2012 8:16am
Location: England

Re: Sanyo 25Ah nmc Voltage Drop

Post by Punx0r » Nov 08 2018 6:05pm

Wow, that's some torque he has! :shock:

Neptronix, I think this the motor both karts have:

http://vi.vipr.ebaydesc.com/ws/eBayISAP ... cureDesc=0

AFAIK on anything brushed, motor current = battery current. The controller simply chops the supply with PWM to deliver reduced voltage & current to the motor.


I'm running out of guesses and my knowledge of non-PM DC motors is pretty thin, but since this motor has separate connections for field and armature and I'm not sure what systems both your controllers use, are you sure both motors are connected in the same configuration RE: series/sepex/compound? I'm wondering if maybe he's accidentally or deliberately miss-wired his motor and is putting way more current through the field winding than intended?
Pota wrote:
Nov 06 2018 7:57pm
This guy is running about 100v. 1:1 gear ratio and 500amp controller. He does INSANE burnout.
Im having 600amp, and have been running 82v. with 1:2 gear ratio. 1 on motor and 2 on axle. But im NOWHERE near that kind of burnout.
Probably a silly question, but just to check when you say "1 on motor, 2 on axle" I assume that's twice the number of teeth on the axle sprocket and not 1 revolution on motor = 2 revolutions on axle? I.e. your motor is geared DOWN not UP. I appreciate you said you also tested it at 1:1 and there's not much room for confusion there...

Punx0r   100 GW

100 GW
Posts: 5311
Joined: May 03 2012 8:16am
Location: England

Re: Sanyo 25Ah nmc Voltage Drop

Post by Punx0r » Nov 08 2018 6:17pm

999zip999 wrote:
Nov 08 2018 5:56pm
3p...
The OP is delivering 600A to his motor on a 1P VW e-up pack

The other guy is delivering 500A to his identical motor from (according to Youtube comments) a Leaf & VW pack


600A @ 1P on the e-up cells is 24C which is leaning pretty hard on them but what is the other guy's pack like? I can't tell from image of the battery at the end of the video if it's 1P or 2P. Either way, Leaf cells are good for, what, 10C?

Pota   100 W

100 W
Posts: 140
Joined: May 15 2017 8:27am

Re: Sanyo 25Ah nmc Voltage Drop

Post by Pota » Nov 08 2018 6:21pm

Punx0r wrote:
Nov 08 2018 6:05pm
Wow, that's some torque he has! :shock:

Neptronix, I think this the motor both karts have:

http://vi.vipr.ebaydesc.com/ws/eBayISAP ... cureDesc=0

AFAIK on anything brushed, motor current = battery current. The controller simply chops the supply with PWM to deliver reduced voltage & current to the motor.


I'm running out of guesses and my knowledge of non-PM DC motors is pretty thin, but since this motor has separate connections for field and armature and I'm not sure what systems both your controllers use, are you sure both motors are connected in the same configuration RE: series/sepex/compound? I'm wondering if maybe he's accidentally or deliberately miss-wired his motor and is putting way more current through the field winding than intended?
Pota wrote:
Nov 06 2018 7:57pm
This guy is running about 100v. 1:1 gear ratio and 500amp controller. He does INSANE burnout.
Im having 600amp, and have been running 82v. with 1:2 gear ratio. 1 on motor and 2 on axle. But im NOWHERE near that kind of burnout.
Probably a silly question, but just to check when you say "1 on motor, 2 on axle" I assume that's twice the number of teeth on the axle sprocket and not 1 revolution on motor = 2 revolutions on axle? I.e. your motor is geared DOWN not UP. I appreciate you said you also tested it at 1:1 and there's not much room for confusion there...
Correct. THATS the motor i have, i bought from that guy, but a newer one :)

Yes, thats what ive been thinking aswell, maybe the wiring is different. I think ive done it right, but there may be another way to increase the torque alot.

Correct, example. 18teeth on motor, 36 on the axle :)

I mean, it wont help me with the amp going from 1p to 2p. Because 1p already gives me 662amp at peak :) And you know, it actualy is around 600amp for maybe 5sec!

User avatar
eee291   10 kW

10 kW
Posts: 995
Joined: Nov 05 2015 4:35pm
Location: Austria, Burgenland

Re: Sanyo 25Ah nmc Voltage Drop

Post by eee291 » Nov 08 2018 6:28pm

Do you have the same sized tires as that guy?

Pota   100 W

100 W
Posts: 140
Joined: May 15 2017 8:27am

Re: Sanyo 25Ah nmc Voltage Drop

Post by Pota » Nov 08 2018 6:35pm

eee291 wrote:
Nov 08 2018 6:28pm
Do you have the same sized tires as that guy?
Yes, but thats not the problem, even with car tires. I have WAAAAAAYYYY lower torque. There are other things that make mine alot weaker.

User avatar
neptronix   100 GW

100 GW
Posts: 14109
Joined: Jun 15 2010 5:56pm
Location: California refugee living in Utah, USA
Contact:

Re: Sanyo 25Ah nmc Voltage Drop

Post by neptronix » Nov 08 2018 7:22pm

Punx0r wrote:
Nov 08 2018 6:05pm
AFAIK on anything brushed, motor current = battery current. The controller simply chops the supply with PWM to deliver reduced voltage & current to the motor.
He said it was brushed to brushless..

Anyway, wheel RPM data from both karts is missing and i suggested speed is the main factor here.



As i demonstrate here, wheel speed makes smoke, and all you need is enough torque to start the reaction..
Crystalyte 3548 ( fastest winding available ) spinning at ~950rpm on a very soft tire.

See how much smoke i made in just a few seconds from all that friction? it's the wheel speed that causes the tire to get hot enough to vaporize.
"Love and compassion are necessities, not luxuries. Without them, humanity cannot survive." - Dalai Lama

My first major build: 1.6kW 8T MAC motor on a Trek 4500.
The new all-arounder: Leafmotor 1500w @ 4kW on a Turner O2 full suspension.
The monster scooter: 20" eZee on a Cannondale Semi Recumbent.
Whipper-snapper: ? on a lightweight BikeE Semi Recumbent

Pota   100 W

100 W
Posts: 140
Joined: May 15 2017 8:27am

Re: Sanyo 25Ah nmc Voltage Drop

Post by Pota » Nov 09 2018 2:23am

Mine make INSANE smoke at 84v With noone in the gokart. But With me sitting in it, its a different story, it wont spin.

Punx0r   100 GW

100 GW
Posts: 5311
Joined: May 03 2012 8:16am
Location: England

Re: Sanyo 25Ah nmc Voltage Drop

Post by Punx0r » Nov 09 2018 3:31am

There's definitely something weird going on as it looks like an apples-to-apples comparison between your karts but he is clearly making way more torque at the axle than you despite you have a bit more motor current and shorter gearing :?

It would be great if one of the guys knowledgeable on non-PM brushed motors could comment.

Pota   100 W

100 W
Posts: 140
Joined: May 15 2017 8:27am

Re: Sanyo 25Ah nmc Voltage Drop

Post by Pota » Nov 09 2018 3:56am

Some say it may be my brushes advancement. @ DIYElectricCar they say im loosing 80% torque if its 30% Advanced.

redline2097   100 W

100 W
Posts: 165
Joined: Jun 18 2015 1:43am

Re: Sanyo 25Ah nmc Voltage Drop

Post by redline2097 » Nov 09 2018 4:51am

Whats the total weight of Kart + You?

Pota   100 W

100 W
Posts: 140
Joined: May 15 2017 8:27am

Re: Sanyo 25Ah nmc Voltage Drop

Post by Pota » Nov 09 2018 6:04am

150-200kg

Joachim   1 kW

1 kW
Posts: 433
Joined: Jul 30 2015 1:02pm
Contact:

Re: Sanyo 25Ah nmc Voltage Drop

Post by Joachim » Nov 09 2018 2:50pm

try 18S 2p :lowbatt:

Punx0r   100 GW

100 GW
Posts: 5311
Joined: May 03 2012 8:16am
Location: England

Re: Sanyo 25Ah nmc Voltage Drop

Post by Punx0r » Nov 12 2018 8:27am

Pota wrote:
Nov 09 2018 3:56am
Some say it may be my brushes advancement. @ DIYElectricCar they say im loosing 80% torque if its 30% Advanced.
I was going to suggest the DIYElectricCar forum as those guys are much more experienced with large brushed motors.

Looking at the news photos above I'd guess your motor is wired in a series configuration. I was thinking if it was intended to be shunt or sepex this might restrict power by placing a relatively high-resistance field winding in series with the armature, but your measurements show this isn't the case. As with the suggestions of increasing the battery to 2P or 3P, your motor is drawing plenty of current, it's just not using it to make torque like the other guy's is. Presumably it's wasting it as heat instead, so maybe you're onto something with the brush timing. Maybe someone monkeyed around with the motor before it got into your hands?

Pota   100 W

100 W
Posts: 140
Joined: May 15 2017 8:27am

Re: Sanyo 25Ah nmc Voltage Drop

Post by Pota » Nov 13 2018 1:42pm

Punx0r wrote:
Nov 12 2018 8:27am
Pota wrote:
Nov 09 2018 3:56am
Some say it may be my brushes advancement. @ DIYElectricCar they say im loosing 80% torque if its 30% Advanced.
I was going to suggest the DIYElectricCar forum as those guys are much more experienced with large brushed motors.

Looking at the news photos above I'd guess your motor is wired in a series configuration. I was thinking if it was intended to be shunt or sepex this might restrict power by placing a relatively high-resistance field winding in series with the armature, but your measurements show this isn't the case. As with the suggestions of increasing the battery to 2P or 3P, your motor is drawing plenty of current, it's just not using it to make torque like the other guy's is. Presumably it's wasting it as heat instead, so maybe you're onto something with the brush timing. Maybe someone monkeyed around with the motor before it got into your hands?
True, but no, the brush timing was good.

But i havent tried reversing the motor.

Post Reply