deronmoped
10 kW
- Joined
- Oct 6, 2008
- Messages
- 706
I have a RC LiPo pack that I want to make charging easier. The way I have been charging it now, is alternating between a bulk charger and charging the cells individually with a balance charger. I would like to use the bulk charger most of the time, but cells go out of balance very quickly. It's a pain charging, so for that reason, it limits my use of the bike. The pack is 10S2P. The question is, can I install a BMS to just balance the pack? I would not be using the output function or discharge limit function. I would still be using my existing ESC for output to the motor. I have a low voltage alarm.