I tried 2 aliexpress stores and 3-4 Serbian local stores and no luck.
Is there any place where i can buy PURE nickel?

Thanks!
 
I bought this one twice, it's legit:
https://www.aliexpress.com/item/Pure-Nickel-Strip-for-Scientific-research-18650-battery-welding-Size-0-2-8mm/32739610924.html
Scratched and left it in saltwater over night, no rust.
Also soft and doesn't break after bending it often.

The seller also has other sizes.
 
Like wise did the same to this H strip from Annbattery, have bought 3 times now.
https://www.aliexpress.com/item/18650-battery-pure-nickel-strip-LiFePo4-LiMn2O4-LiCoO2-cell-connect-the-nickel-belt-Cylindrical-batteries-nickel/32721800824.html?spm=a2g0s.9042311.0.0.27424c4dbujdYt


Waiting for this to arrive so I can test it.
https://www.aliexpress.com/item/5-m-roll-0-15mm-25mm-5000mm-Quality-low-resistance-99-96-pure-nickel-Strip-Sheets/32816830002.html?spm=a2g0s.9042311.0.0.31ab4c4dt7xCRK
 
Perhaps some of these will help?

https://endless-sphere.com/forums/search.php?keywords=pure+nickel+strip&terms=all&author=&sc=1&sf=titleonly&sr=topics&sk=t&sd=d&st=0&ch=300&t=0&submit=Search

https://endless-sphere.com/forums/search.php?keywords=pure+nickel+strip&terms=all&author=&sc=1&sf=msgonly&sr=posts&sk=t&sd=d&st=0&ch=300&t=0&submit=Search
 
amberwolf said:
Perhaps some of these will help?

https://endless-sphere.com/forums/search.php?keywords=pure+nickel+strip&terms=all&author=&sc=1&sf=titleonly&sr=topics&sk=t&sd=d&st=0&ch=300&t=0&submit=Search

https://endless-sphere.com/forums/search.php?keywords=pure+nickel+strip&terms=all&author=&sc=1&sf=msgonly&sr=posts&sk=t&sd=d&st=0&ch=300&t=0&submit=Search

Yeah i used search option but those threads are old and some links are dead. I wanted to have some fresh informations.
 
I have tested this one by deep grinding the surface and a saline solution, no rust deposits or discolouring to Nickel or solution.

https://www.aliexpress.com/item/5-m-roll-0-15mm-25mm-5000mm-Quality-low-resistance-99-96-pure-nickel-Strip-Sheets/32816830002.html?spm=a2g0s.9042311.0.0.31ab4c4dt7xCRK
 
I ordered from here https://annpower.aliexpress.com/store/623665?spm=2114.10010108.0.0.76db12f7q56eiF
Lets hope this is pure.
 
BotoXbz said:
I bought this one twice, it's legit:
https://www.aliexpress.com/item/Pure-Nickel-Strip-for-Scientific-research-18650-battery-welding-Size-0-2-8mm/32739610924.html
Scratched and left it in saltwater over night, no rust.
Also soft and doesn't break after bending it often.

The seller also has other sizes.

holy shait, tha stuff is expensive.

just order from here, you can buy by the kilo.

https://www.aliexpress.com/item/1kg-roll-Thickness-0-2mm-High-Quality-low-resistance-99-96-pure-nickel-Strip-Sheets-for/32864774543.html
 
flippy said:
BotoXbz said:
I bought this one twice, it's legit:
https://www.aliexpress.com/item/Pure-Nickel-Strip-for-Scientific-research-18650-battery-welding-Size-0-2-8mm/32739610924.html
Scratched and left it in saltwater over night, no rust.
Also soft and doesn't break after bending it often.

The seller also has other sizes.

holy shait, tha stuff is expensive.

just order from here, you can buy by the kilo.

https://www.aliexpress.com/item/1kg-roll-Thickness-0-2mm-High-Quality-low-resistance-99-96-pure-nickel-Strip-Sheets-for/32864774543.html

It's cheaper for me to buy that than paying import tax and processing fees in EU on the bigger one...
 
BotoXbz said:
It's cheaper for me to buy that than paying import tax and processing fees in EU on the bigger one...


never had to pay import tax with this one, they mark it with a value of 10 bucks or something like that. and its just a roll of metal, customs dont care about that.
 
Go cheap like big battery rebuild company do en get this crap :shock: this is a real joke and i see this al the time :twisted:
iq8swi.jpg

2i106ea.jpg
 
Joachim said:
Go cheap like big battery rebuild company do en get this crap :shock: this is a real joke and i see this al the time :twisted:
iq8swi.jpg

2i106ea.jpg

I tried to find pure nickel in Serbia - no luck. 3 "serious companies" who works with batteries (cells reparation and similar) have "nickel" in their shops. All 3 nickel plated steel. Total amaterism!
 
thats not so bad, i got way worse batteries i needed to rebuild in the past years due to crappy stuff like this
some even got their entire strips rusted away due to water ingress.

for battery builders that shit is inexcusable.
 
krlenjuska said:
I ordered from here https://annpower.aliexpress.com/store/623665?spm=2114.10010108.0.0.76db12f7q56eiF
Lets hope this is pure.

I recieved this nickel strip and its pure.
 
krlenjuska said:
krlenjuska said:
I ordered from here https://annpower.aliexpress.com/store/623665?spm=2114.10010108.0.0.76db12f7q56eiF
Lets hope this is pure.

I recieved this nickel strip and its pure.

I buy from these guys too and can recommend. Also they have it in pretty much whatever thickness you want.
 