Epic 7kw+ 12 fet controller...or there abouts :)

Get real world experience and user feedback on the electric bicycle products.
John in CR   100 GW

100 GW
Posts: 14568
Joined: May 20 2008 12:58am
Location: Paradise

Re: Epic 7kw+ 12 fet controller...or there abouts :)

Post by John in CR » Mar 10 2019 4:36pm

Even just one on that back end plate would do a lot of good just by getting the hot air out of the controller. Since there was nothing to get hot on the bottom of my boards, I blocked that off as a path for air to flow to help focus flow where it was needed most. These days, since I use 6 phase motors, I don't need super powerful controllers, so I run them stock and at conservative settings. 100A each from the battery with less than 2:1 phase/batt current limits at voltages from 74V nominal to 115V nominal is typically plenty...especially since I have the modded MadAss running at 30kw+ peak input for thrills.

shaman   1 kW

1 kW
Posts: 336
Joined: Dec 10 2018 7:03pm
Location: Fort Worth, TX, USA

Re: Epic 7kw+ 12 fet controller...or there abouts :)

Post by shaman » Mar 10 2019 6:58pm

John in CR wrote:
Mar 10 2019 4:36pm
I use 6 phase motors
Where does one get those 6 phase motors?
if all you know is theory, then you're only theoretically intelligent

User avatar
ElectricGod   1 GW

1 GW
Posts: 3404
Joined: Nov 01 2015 5:24pm
Location: 3 OH 3

Re: Epic 7kw+ 12 fet controller...or there abouts :)

Post by ElectricGod » Mar 11 2019 12:25am

shaman wrote:
Mar 10 2019 6:58pm
John in CR wrote:
Mar 10 2019 4:36pm
I use 6 phase motors
Where does one get those 6 phase motors?
Depends on the power you want...

John is talking about hubmonsters. He has several of them, but they are not cheap. I have 2 of them. It took looking in local for sale sites a long time to find them on existing electric mopeds.

Just about all Motenergy axial flux motors are dual stator or 6 phases. Again not inexpensive.

You can take any outrunner and wind it for 6 phases. I have an Alien Power 12090 that's burnt out. I'll eventually get around to winding it for 6 phases.
XB-502: viewtopic.php?f=10&t=83302&p=1222730#p1222730

Currie scooter: viewtopic.php?f=35&t=83830&p=1227407#p1227407

Benjamin Franklin - "Any fool can criticize, condemn and complain and most fools do."

Philaphlous   1 kW

1 kW
Posts: 431
Joined: Mar 28 2017 7:17am

Re: Epic 7kw+ 12 fet controller...or there abouts :)

Post by Philaphlous » Mar 12 2019 12:28pm

Well it's definitely not going to be waterproof or water tight with those fans... After a 14mi ride on my controller pulling anywhere from 600-1500w...more around 650W consistently I had absolutely no heat from my controller. Pretty amazing! Well see what happens when it's 90F out but I'm not worried at all pulling 2K through mine. I also added new thermal paste to the mosfet heatsink block.

I better be seeing wheelies from this controller!

User avatar
ElectricGod   1 GW

1 GW
Posts: 3404
Joined: Nov 01 2015 5:24pm
Location: 3 OH 3

Re: Epic 7kw+ 12 fet controller...or there abouts :)

Post by ElectricGod » Mar 12 2019 4:06pm

I posted back a few pages in this thread about losing a few mosfets in the controller. I was running an Alien Power 12090 when it happened.

A couple of days ago, I connected that exact same motor again and sure enough, popped mosfets again. Grrr!

Back a few months, I assumed there was a couple of weak mosfets...it happens form time to time.

I took the 12090 apart and found I have a partial phase short to the stator. The motor is effectively brand new as it's never seen more than bench use. This is why I'm blowing mosfets. There's no evidence that a motor phase is damaged.
XB-502: viewtopic.php?f=10&t=83302&p=1222730#p1222730

Currie scooter: viewtopic.php?f=35&t=83830&p=1227407#p1227407

Benjamin Franklin - "Any fool can criticize, condemn and complain and most fools do."

Philaphlous   1 kW

1 kW
Posts: 431
Joined: Mar 28 2017 7:17am

Re: Epic 7kw+ 12 fet controller...or there abouts :)

Post by Philaphlous » Mar 20 2019 4:08pm

So from your extensive experience with modding the controller where do you see the weakest link to be? I'm considering adding a little more solder to the shunt for 55-60A on mine... Im thinking the 14-16awg phase wires going into the motor that are only about 6" long won't like those phase amps...

User avatar
ElectricGod   1 GW

1 GW
Posts: 3404
Joined: Nov 01 2015 5:24pm
Location: 3 OH 3

Re: Epic 7kw+ 12 fet controller...or there abouts :)

Post by ElectricGod » Mar 21 2019 8:14am

Philaphlous wrote:
Mar 20 2019 4:08pm
So from your extensive experience with modding the controller where do you see the weakest link to be? I'm considering adding a little more solder to the shunt for 55-60A on mine... Im thinking the 14-16awg phase wires going into the motor that are only about 6" long won't like those phase amps...
Are you talking about the 12 fet PV controller or something else? No PV controller uses 14 or 16 awg wires anywhere.

Adding solder to the shunts...
just don't. If you want more amperage do it right and use better shunts.
Also, if you are using a PV controller, this is the wrong way to go about doing things. These controllers are fully programmable.
"buttering up" shunts is what you do to cheap Chinese dumb controllers that you buy on ebay for $40.
XB-502: viewtopic.php?f=10&t=83302&p=1222730#p1222730

Currie scooter: viewtopic.php?f=35&t=83830&p=1227407#p1227407

Benjamin Franklin - "Any fool can criticize, condemn and complain and most fools do."

Philaphlous   1 kW

1 kW
Posts: 431
Joined: Mar 28 2017 7:17am

Re: Epic 7kw+ 12 fet controller...or there abouts :)

Post by Philaphlous » Mar 26 2019 4:09am

ElectricGod wrote:
Mar 21 2019 8:14am
Philaphlous wrote:
Mar 20 2019 4:08pm
So from your extensive experience with modding the controller where do you see the weakest link to be? I'm considering adding a little more solder to the shunt for 55-60A on mine... Im thinking the 14-16awg phase wires going into the motor that are only about 6" long won't like those phase amps...
Are you talking about the 12 fet PV controller or something else? No PV controller uses 14 or 16 awg wires anywhere.

Adding solder to the shunts...
just don't. If you want more amperage do it right and use better shunts.
Also, if you are using a PV controller, this is the wrong way to go about doing things. These controllers are fully programmable.
"buttering up" shunts is what you do to cheap Chinese dumb controllers that you buy on ebay for $40.
Yea I got one of those cheap ass controllers your talking about. It does have soldering points for a plug to program it but those aren't used at all.
It's kinda strange though that the controller doesn't really even get warm... Maybe it's just in such a great location on my bike? It's behind the downtube between the rear wheel and downtube. It gets airflow from the front and I believe also some from the wheel.

j bjork   10 kW

10 kW
Posts: 668
Joined: Aug 31 2018 3:01pm
Location: Linköping, Sweden

Re: Epic 7kw+ 12 fet controller...or there abouts :)

Post by j bjork » May 08 2019 4:57am

Interesting thred :wink:

Has there been any progress with this project?

User avatar
ElectricGod   1 GW

1 GW
Posts: 3404
Joined: Nov 01 2015 5:24pm
Location: 3 OH 3

Re: Epic 7kw+ 12 fet controller...or there abouts :)

Post by ElectricGod » May 12 2019 4:49pm

j bjork wrote:
May 08 2019 4:57am
Interesting thred :wink:

Has there been any progress with this project?
No much...until a couple of days ago. The AP 12090 with the shorted phase blew up the controller. I've had many things on my plate recently so this just sat. I got it pulled apart a couple of days ago and found that 10 of the 12 mosfets are cooked. I've replaced all of them, but need to test it out now.

That was a lot of money on new top end mosfets that lasted just minutes! GRRR!
XB-502: viewtopic.php?f=10&t=83302&p=1222730#p1222730

Currie scooter: viewtopic.php?f=35&t=83830&p=1227407#p1227407

Benjamin Franklin - "Any fool can criticize, condemn and complain and most fools do."

User avatar
ElectricGod   1 GW

1 GW
Posts: 3404
Joined: Nov 01 2015 5:24pm
Location: 3 OH 3

Re: Epic 7kw+ 12 fet controller...or there abouts :)

Post by ElectricGod » May 14 2019 12:45am

Well that controller is a lost cause...
Not only were the mosfets toast, but the control electronics were fried too. That Alien Power motor really messed things up badly!

I have another of the 12 fet PV controllers. Last night, I got it mostly modded. The 8 awg wires and big shunts are added. The phase busses still need some beefing up. I'm going to rework my copper heat spreader a little before installing it in the beefed up shell.
XB-502: viewtopic.php?f=10&t=83302&p=1222730#p1222730

Currie scooter: viewtopic.php?f=35&t=83830&p=1227407#p1227407

Benjamin Franklin - "Any fool can criticize, condemn and complain and most fools do."

User avatar
ElectricGod   1 GW

1 GW
Posts: 3404
Joined: Nov 01 2015 5:24pm
Location: 3 OH 3

Re: Epic 7kw+ 12 fet controller...or there abouts :)

Post by ElectricGod » Jan 08 2020 1:28pm

It's been a very long time since I worked on this project.

I had to shelve it for a while and over the weekend got back to it.
You could call this a failure or a success...depending on point of view.
I'd say it is a success...I got 7kw and the controller held up quite nicely with the added cooling.

I was measuring 100 battery amps at 82v...so 8kw.
No idea about phase amps. I was about to check that when the controller blew up.
I think I've found the maximum limits I can achieve with this controller!
As you can see all I changed in it is the mosfets and added larger shunts and wires.
7kw was working pretty nicely with the added heat sinking.
8kw exceeded the limits of the board and mosfets.
I was already thinking 7kw was pretty impressive!

I'm not going to try and repair this controller!
There's circuit traces burnt off the board.
I have no idea how many mosfets are cooked, but many exploded.
Probably the MCU and driver components are fried too.
You will notice that I'm not using ceramic insulators.
I had a few of them break so I stuck with kapton for this test.
I had a temp sensor on a mosfet tab and another outside the case on the heat spreader.
Temps on the mosfet spiked suddenly and then this happened.
7kw...doable...8kw...no...not really.

Image

Image

Image

Image
XB-502: viewtopic.php?f=10&t=83302&p=1222730#p1222730

Currie scooter: viewtopic.php?f=35&t=83830&p=1227407#p1227407

Benjamin Franklin - "Any fool can criticize, condemn and complain and most fools do."

redmouse   1 W

1 W
Posts: 61
Joined: Aug 03 2017 7:16pm

Re: Epic 7kw+ 12 fet controller...or there abouts :)

Post by redmouse » Jan 08 2020 8:02pm

This has been an epic journey, thanks for sharing it with us!

Would you do a short recap of the mods, and what configuration worked best? And shunt mod, how did you get to 7kW specifically?

User avatar
fechter   100 GW

100 GW
Posts: 14957
Joined: Dec 31 2006 3:23pm
Location: California Bay Area, USA

Re: Epic 7kw+ 12 fet controller...or there abouts :)

Post by fechter » Jan 14 2020 10:53pm

That's some impressive toast there. I'd guess one of the FETs shorted, but sort of hard to see with all the carbon. Looks like it blew one trace off the board. It's remotely possible the trace blew first then things cascaded.
"One test is worth a thousand opinions"

User avatar
madin88   1 GW

1 GW
Posts: 3075
Joined: May 27 2013 2:02am
Location: Austria

Re: Epic 7kw+ 12 fet controller...or there abouts :)

Post by madin88 » Jan 15 2020 6:42am

fechter wrote:
Jan 14 2020 10:53pm
Looks like it blew one trace off the board. It's remotely possible the trace blew first then things cascaded.
It could have happended that way.
When i repaird my two 12F back then, i noticed the issue and beefed up those traces. They supply batt minus to one of the two low-side FET's so it has to carry around 50% of the phase current.