flippy said:vruzend is a flawed concept with no regard for safety. that is simply the end of the story.
anything less then spotwelding is a compromise in safety and reliabliity.
flippy said:your packs are not friction fit wich is a plus compared to vruzend, but is also suseptible to corrosion, even worse then welding.
and many people that fix or build batteries onyl see the busted ones, otherwise they would not go to a battery supplier.
BlueSwordM said:Wait, why would AG's design be prone to corrosion?
I mean, nickel-zinc/tin plated copper has excellent resistance to corrosion.
As he mentioned, only the steel bolts have been corroded, and that could be fixed with a zinc, then nickel, plating.