ossivirt said:How to best describe the difference
I did multiple welds to 0.15mm nickel with sunko and prayed afterwards that even one of then would hold. With kweld every single one is constantly strong and I need pliers to rip off the nickel and it tears of around the weld points leaving the welds and rest of the nickel still attached to the cell.
I have the cheapest possible sunko welder so I had it at maximum settings and kweld beats it even at very low energy levels. (10j)
Headrc said:Ossivirt ...so 50j and you got good welds for .1MM nickle plated copper? With the regular electrodes? I now have some .15mm nickel plated copper so it sounds like I would have to even use a higher setting .....
I noticed this also. Nickel plating got burned black and maybe little vapor too.ridethelightning said:i think he was talking about straight 0.15 nickel. if you find 0.15 nickleplated copper, let us know!
i have doubts about it though. its used in power tool packs, but when i tried welding it, i think the nickle skin vapourises causing issues, as you need so much current for the copper, the nickle has high resistance and poof!
I think you need at least 75j depending on your battery amps and other things likely even more..Headrc said:I do have a sample of some .15 nickel plated copper ....and it is available but not cheap. But useless to me unless I can get good welds with it ...which is why I asked. I tried some at 25j with the stock electrodes and the welds were not good. I will have to try a higher setting or different electrode material to see if I can get good welds. Which is why I asked if anyone has done it to see if they could suggest the proper setting.
When electrolyte comes out and air gets in the cell should be disposed of. It might hold voltage but likely it will have lower capacity and it will age quickly. There is also concern about fire-safety..Compoundbike said:Quick update I received my K-Weld after few welds liquid came out. First i thought this was Water from previous use but turned out it came from the "Lanzhd" Cell.
I had the setting on 9.5 Joule automatic
However i reduced up to 2.5 Joule and worked better.
I measured the Cell voltage and still seem to be good, should i be careful with the leaked Cells?
Compoundbike said:Is that normal that the K-Weld can burn through the Battery that Electrolyte comes out? Probably Not.
So has this happened to Someone else?
Compoundbike said:Is that normal that the K-Weld can burn through the Battery that Electrolyte comes out? Probably Not.
So has this happened to Someone else?
Compoundbike said:Okay how should I say.. First there's a touch with some sparkles after that there's a good weld with nickel plate melting, but at the same time liquid is coming out. :?
*edit* also twice a small flame came out.
that is not 2J, that looks like 200J+.Compoundbike said:Okay how should I say.. First there's a touch with some sparkles after that there's a good weld with nickel plate melting, but at the same time liquid is coming out. :?
*edit* also twice a small flame came out.
https://i.ibb.co/sqVjjyQ/IMG-20190609-121130.jpg