Post by garolittle » Nov 14 2019 1:13pm

Background: I have a 14S/20P pack of LG HG2 cells and need to measure the internal resistance of each cell string. Can I use the process discussed at the 4-minute mark of the YouTube link below except use a 20-olm resistor instead of a 1-olm resistor? Thanks!

https://youtu.be/av38iBxcOgQ
VenomKarts, LLC
VenomKarts.com
Augusta, GA

User avatar
PaulD   100 W

100 W
Posts: 298
Joined: Aug 28 2008 5:42pm
Location: Ashland, OR, USA
Contact:

Re: Internal Resistance for pack of LG HG2 cells

Post by PaulD » Nov 14 2019 2:41pm

To be clear, you want to measure the resistance of each 14S1P string? Or each 1S20P group? Not sure how your pack is configured. Basically, you can estimate current using I = V/R. I usually use 2C current for measuring DC resistance. If your current is too low, the voltage drop is too low and your accuracy isn't great. Obviously you don't want the current to be too high for your test equipment either.

User avatar
garolittle   1 kW

1 kW
Posts: 350
Joined: Mar 03 2018 1:06pm
Location: Augusta, GA U.S.A

Re: Internal Resistance for pack of LG HG2 cells

Post by garolittle » Nov 14 2019 2:49pm

PaulD wrote:
Nov 14 2019 2:41pm
To be clear, you want to measure the resistance of each 14S1P string? Or each 1S20P group? Not sure how your pack is configured.
My apologies. Since the 20 in parallel act as a single cell in terms of voltage, I want to measure the internal resistance of each sting of 20
VenomKarts, LLC
VenomKarts.com
Augusta, GA

docware   100 W

100 W
Posts: 293
Joined: Sep 16 2018 5:36am

Re: Internal Resistance for pack of LG HG2 cells

Post by docware » Nov 14 2019 5:51pm

garolittle,what is purpose of this pack measurement ?

User avatar
garolittle   1 kW

1 kW
Posts: 350
Joined: Mar 03 2018 1:06pm
Location: Augusta, GA U.S.A

Re: Internal Resistance for pack of LG HG2 cells

Post by garolittle » Nov 14 2019 5:57pm

docware wrote:
Nov 14 2019 5:51pm
garolittle,what is purpose of this pack measurement ?
I want to verify the BMS data regarding the internal resistance. I have an Orion jr. BMS and it is showing a higher reading than normal. Typical IR for this pack has been .8 to .9 but the recent reading was 2.8.
Attachments
DF2C1EDD-7C7C-480B-8910-C0C346EFA53A.jpeg
DF2C1EDD-7C7C-480B-8910-C0C346EFA53A.jpeg (196.32 KiB) Viewed 1331 times
VenomKarts, LLC
VenomKarts.com
Augusta, GA

User avatar
garolittle   1 kW

1 kW
Posts: 350
Joined: Mar 03 2018 1:06pm
Location: Augusta, GA U.S.A

Re: Internal Resistance for pack of LG HG2 cells

Post by garolittle » Nov 14 2019 5:58pm

I do not believe the 2.81 is correct but I want to double check to be sure. Thanks for any ideas. Gary
VenomKarts, LLC
VenomKarts.com
Augusta, GA

docware   100 W

100 W
Posts: 293
Joined: Sep 16 2018 5:36am

Re: Internal Resistance for pack of LG HG2 cells

Post by docware » Nov 14 2019 6:08pm

Measurement on the video has an error about 30 %. New fresh LG HG2 cell should have about 21 - 22 miliohm at 25 °C and 3,85 V, at 4 V may be even little bit higher. I assume that such accuracy is not acceptable for you.

docware   100 W

100 W
Posts: 293
Joined: Sep 16 2018 5:36am

Re: Internal Resistance for pack of LG HG2 cells

Post by docware » Nov 14 2019 6:36pm

Got an idea. If you can measure charging current or if you know the charging current, you can calculate internal resistance from the charging current value and voltage difference on the cell. You just need to have DMM with resolution mV or better 0,1 mV and connect to any cell´s balance wiring.

User avatar
garolittle   1 kW

1 kW
Posts: 350
Joined: Mar 03 2018 1:06pm
Location: Augusta, GA U.S.A

Re: Internal Resistance for pack of LG HG2 cells

Post by garolittle » Nov 14 2019 8:13pm

docware wrote:
Nov 14 2019 6:36pm
Got an idea. If you can measure charging current or if you know the charging current, you can calculate internal resistance from the charging current value and voltage difference on the cell. You just need to have DMM with resolution mV or better 0,1 mV and connect to any cell´s balance wiring.
Hey Sir. Thanks for the great responses. I will try your idea and let you know the results. I have to show my ignorance now ..... What is “DMM”. Also, in the screenshot above, what does 2.81 mean? Miliolms? It is normally .8 - .9. I could not find the unit of measure in the Orion JR manual. Thanks again for all of your help.
VenomKarts, LLC
VenomKarts.com
Augusta, GA

john61ct   1.21 GW

1.21 GW
Posts: 3621
Joined: Dec 18 2018 2:06pm

Re: Internal Resistance for pack of LG HG2 cells

Post by john61ct » Nov 14 2019 8:21pm

DMM is a Digital Multi-Meter

Getting IR for benchmarking changes from now vs later is very useful.

However, requires using the same calibrated instrumentation, voltage delta, current levels, SoC and temperature in order to be usefully comparable.

In theory it's a single number, but

______
In theory there is no difference between theory and practice. In practice there is.
— Yogi Berra


User avatar
garolittle   1 kW

1 kW
Posts: 350
Joined: Mar 03 2018 1:06pm
Location: Augusta, GA U.S.A

Re: Internal Resistance for pack of LG HG2 cells

Post by garolittle » Nov 14 2019 8:32pm

john61ct wrote:
Nov 14 2019 8:21pm
DMM is a Digital Multi-Meter

Getting IR for benchmarking changes from now vs later is very useful.
Roger that and thanks!
VenomKarts, LLC
VenomKarts.com
Augusta, GA

docware   100 W

100 W
Posts: 293
Joined: Sep 16 2018 5:36am

Re: Internal Resistance for pack of LG HG2 cells

Post by docware » Nov 15 2019 1:48am

Yes, as john61ct mentioned, tracing of the internal resistance is useful, however requires using still the same conditions (temperature, SOC) and method. Using precise equipment is a must.

2,81 probably means miliohms, 20p LG HG2 should have about 1 miliohm per one paralel group (new fresh cells). Values 0,8 – 0,9 are telling us that inaccuracy of this BMS measurement was 10 – 20 %.

If you want to copy resistor method from video, you need to get at least 1A per cell which is 20A total. 4 V per cell means 56 V total for 14s battery. To get 20 A you need precise resistor 2,8 Ohm, power dissipated on resistor would be 1 120 W !!! Moreover, as temperature of the resistor will go up, the resistance will go up also and real current will be smaller. That is one reason of inaccuracy on the video, unsufficient DMM resolution is another, unsufficient resistor accuracy another, ………

As 1 kW precise cooled resistor is little bit a problem, I suggested method of cell´s voltage difference measurement during charging. I assume that charging current is about 1A per cell.

Resulting accuracy will depends on the current measurement accuracy and voltmeter resolution.
Even if total inaccuracy will be suppose 10 – 20 %, for checking of sudden 300 % rise of IR measurement such method could be sufficient.
Maybe you can borrow DMM with enough resolution and clamp meter or precise shunt for current mesurement.

Hillhater   100 GW

100 GW
Posts: 10670
Joined: Aug 03 2010 10:33pm
Location: Sydney ..(Hilly part !) .. Australia/ Down under !

Re: Internal Resistance for pack of LG HG2 cells

Post by Hillhater » Nov 15 2019 2:03am

Remember, this is a “group” of 20 cells in parallel.
Whilst they stay connected in parallel, you cannot get any IR data for individual cells...only the “group” result
And that can be affected by many other things such as connection integrity (40+ connections per group !) and individual bad cells corrupting the results of measurements
This forum owes its existence to Justin of ebikes.ca

docware   100 W

100 W
Posts: 293
Joined: Sep 16 2018 5:36am

Re: Internal Resistance for pack of LG HG2 cells

Post by docware » Nov 15 2019 2:11am

We are not speaking about IR for idividual cells. garolittle wants to verify BMS internal resistance measurement, because it is showing 3 x higher readig than normal.

User avatar
garolittle   1 kW

1 kW
Posts: 350
Joined: Mar 03 2018 1:06pm
Location: Augusta, GA U.S.A

Re: Internal Resistance for pack of LG HG2 cells

Post by garolittle » Nov 15 2019 9:12am

I really appreciate all of the responses. I have learned many things and will use the “charger method” references above. Good point about the individual cells. Also, it is true I am only looking for the IR of the cell string (with 20 in parallel). Either way, I appreciate the responses from both of you. Gary
VenomKarts, LLC
VenomKarts.com
Augusta, GA

john61ct   1.21 GW

1.21 GW
Posts: 3621
Joined: Dec 18 2018 2:06pm

Re: Internal Resistance for pack of LG HG2 cells

Post by john61ct » Nov 15 2019 12:15pm

Cells connected in parallel can be referred to as a Group

A String always refers to cells or groups connected in **series**

Bank is the highest level, usually a fixed location or tied to a boat or vehicle, at a specific useful/standard voltage, for some reason often not used for propulsion use cases.

"Pack" is widely used for EV / propulsion, can be like "modules" as a physical unit, but can also signify the whole bank, so I generally avoid if that makes things ambiguous. But, OK to use packs to mean "portable bank", as in powerpak, and also "pack-level" charging rather than bulk charging, to distinguish from balance charging or node-style charging via cell-level balance leads.

I use "Modules" for standalone functional units
usually portable, physically self-contained
at a specific useful/standard voltage
usually can be used / charged separately
and/or wired in series or parallel to comprise
the main bank, even rotated in and out

Otherwise sub-banks or sub-packs, when xPyS units are further joined in parallel or series to comprise the full Bank or Pack.

john61ct   1.21 GW

1.21 GW
Posts: 3621
Joined: Dec 18 2018 2:06pm

Re: Internal Resistance for pack of LG HG2 cells

Post by john61ct » Nov 15 2019 12:16pm

can you link to where you bought that pack?

docware   100 W

100 W
Posts: 293
Joined: Sep 16 2018 5:36am

Re: Internal Resistance for pack of LG HG2 cells

Post by docware » Nov 15 2019 3:54pm

garolittle wrote:
Nov 15 2019 9:12am
I really appreciate all of the responses. I have learned many things and will use the “charger method” references above. Good point about the individual cells. Also, it is true I am only looking for the IR of the cell string (with 20 in parallel). Either way, I appreciate the responses from both of you. Gary
Let us know the outcome Gary.

User avatar
garolittle   1 kW

1 kW
Posts: 350
Joined: Mar 03 2018 1:06pm
Location: Augusta, GA U.S.A

Re: Internal Resistance for pack of LG HG2 cells

Post by garolittle » Nov 15 2019 4:00pm

Yes sir. I will run the test on Sunday and post the results by Sunday night or Monday morning. Thank you again for all of your ideas.
VenomKarts, LLC
VenomKarts.com
Augusta, GA

User avatar
garolittle   1 kW

1 kW
Posts: 350
Joined: Mar 03 2018 1:06pm
Location: Augusta, GA U.S.A

Re: Internal Resistance for pack of LG HG2 cells

Post by garolittle » Nov 16 2019 2:25pm

john61ct wrote:
Nov 15 2019 12:16pm
can you link to where you bought that pack?
www.allcelltech.com.
VenomKarts, LLC
VenomKarts.com
Augusta, GA

User avatar
garolittle   1 kW

1 kW
Posts: 350
Joined: Mar 03 2018 1:06pm
Location: Augusta, GA U.S.A

Re: Internal Resistance for pack of LG HG2 cells

Post by garolittle » Nov 16 2019 3:55pm

docware wrote:
Nov 14 2019 6:36pm
Got an idea. If you can measure charging current or if you know the charging current, you can calculate internal resistance from the charging current value and voltage difference on the cell. You just need to have DMM with resolution mV or better 0,1 mV and connect to any cell´s balance wiring.
So my DMM is very basic. See below. Any recommendations for a good one I can buy to perform this test? Thanks.
5612F86D-4C0B-4E28-89DB-E8B0BCF58689.png
5612F86D-4C0B-4E28-89DB-E8B0BCF58689.png (194.1 KiB) Viewed 1209 times
VenomKarts, LLC
VenomKarts.com
Augusta, GA

john61ct   1.21 GW

1.21 GW
Posts: 3621
Joined: Dec 18 2018 2:06pm

Re: Internal Resistance for pack of LG HG2 cells

Post by john61ct » Nov 16 2019 3:59pm

Hmm interesting. I've thought of using potting compound that is thermally conductive with aluminum shell.

But phase changing sure takes things to another level.

Of course best practice is to prevent heat from rising significantly, but some people / use cases just require /accept that.

User avatar
garolittle   1 kW

1 kW
Posts: 350
Joined: Mar 03 2018 1:06pm
Location: Augusta, GA U.S.A

Re: Internal Resistance for pack of LG HG2 cells

Post by garolittle » Nov 16 2019 4:23pm

john61ct wrote:
Nov 16 2019 3:59pm


But phase changing sure takes things to another level.

We strongly recommend AllCell Technologies. Great product and excellent customer service. 8)
VenomKarts, LLC
VenomKarts.com
Augusta, GA

User avatar
garolittle   1 kW

1 kW
Posts: 350
Joined: Mar 03 2018 1:06pm
Location: Augusta, GA U.S.A

Re: Internal Resistance for pack of LG HG2 cells

Post by garolittle » Nov 18 2019 1:33pm

Ok. Part of the mystery was solved. When I use the OrionJr. BMS “Setup Wizard”, I have to select a battery type. Since the LG HG2 was not listed, I chose the other LG cell. That is what caused the “2.81” reading for Internal Resistance”. Last night, I changed it to the Panasonic cell and the reading returned to a more normal IR reading of .96. Apparently, the LC cell that I selected previously was a different chemistry.
3DD5DBFA-3B14-4269-A703-B8AA4FF829A6.png
3DD5DBFA-3B14-4269-A703-B8AA4FF829A6.png (483.02 KiB) Viewed 971 times
VenomKarts, LLC
VenomKarts.com
Augusta, GA

john61ct   1.21 GW

1.21 GW
Posts: 3621
Joined: Dec 18 2018 2:06pm

Re: Internal Resistance for pack of LG HG2 cells

Post by john61ct » Nov 18 2019 2:08pm

What does the BMS use those data for?

I'm surprised it doesn't read them directly in order to tell the user, rather than the other way around.

Do they update the "library" as new cells come on the market?