12v battery liquid

Talk about anything and everything here within reason.
Post Reply
rami   1 µW

1 µW
Posts: 2
Joined: Dec 06 2019 5:49am

12v battery liquid

Post by rami » Dec 06 2019 6:13am

Hello;

I have 120AH 12v battery, the liquid inside was brown, so I emptied the liquid, filtered it, and put it back in the battery. The battery before that process was reading 12.4v, now it is not accepting any charge, I have 3 chargers and tried to use them, the charger is giving 14v but the amp is staying on the zero mark. Moreover I haven't wash the inside of the battery or clean it, all I have done emptying, filtering, then put it back.

Please can anyone direct me what should I do to bring it back to life.

Regards.

User avatar
LeftieBiker   100 kW

100 kW
Posts: 1165
Joined: Nov 06 2012 1:33am
Location: Upstate NY, United States

Re: 12v battery liquid

Post by LeftieBiker » Dec 06 2019 6:38am

You removed much or most of the electrolyte. That was not a good idea, as you have found.
2018 Nissan Leaf SL with Pro Pilot
2009 Vectrix VX-1 Maxi Scooter W/ 18 Leaf modules
2018 Magnum Metro with noisy motor
2019 GreenBike folder
2019 3 wheel 36 volt scooter

rami   1 µW

1 µW
Posts: 2
Joined: Dec 06 2019 5:49am

Re: 12v battery liquid

Post by rami » Dec 06 2019 6:48am

Hi Leftibiker;

Thanks for your reply. I didn't understand, I returned the same amount of original liquid back to the battery.

Please explain so I would know what went wrong, also what should I do next to revive it, should I put 30% acid with new 70% distilled water?

User avatar
LeftieBiker   100 kW

100 kW
Posts: 1165
Joined: Nov 06 2012 1:33am
Location: Upstate NY, United States

Re: 12v battery liquid

Post by LeftieBiker » Dec 07 2019 2:47am

I don't know the exact composition of the battery, but you obviously filtered out one or more of the electrolyte components, along with any dirt that was there. If I were to try anything, it would be to drain the electrolyte again, and try to find a new bottle of replacement electrolyte for a new battery. You would probably only be able to add about 75% of it. Frankly, I'd just dispose of the battery.
2018 Nissan Leaf SL with Pro Pilot
2009 Vectrix VX-1 Maxi Scooter W/ 18 Leaf modules
2018 Magnum Metro with noisy motor
2019 GreenBike folder
2019 3 wheel 36 volt scooter

Voltron   1 GW

1 GW
Posts: 3089
Joined: May 02 2013 4:53pm
Location: Santa Barbara CA

Re: 12v battery liquid

Post by Voltron » Dec 07 2019 5:01am

Or you stirred up crud at the bottom that's been shed off the plates, and it's internally shorting. Also, did you use a hydrometer on it yet?

goatman   100 MW

100 MW
Posts: 2666
Joined: Jun 23 2019 6:50pm
Location: Surrey, B.C.

Re: 12v battery liquid

Post by goatman » Dec 25 2019 3:11pm

in Canada you can go to Lordco and buy battery acid, its not cheap. in batteries I don't care about that are dead and just need to get another summers use, I would dump out the acid in a 5 gallon bucket,neutralise with lots of baking soda, be careful. little soda at a time.
id put a tablespoon of soda in each cell and flush with water to clean the cells and dump that out. then just fill with water and charge.i might of added a teaspoon of baking soda to each cell before charging, cant remember exactly. I did that for my 1976 gmc 4x4 bush truck. I was never left stranded in the middle of nowhere but come fall when it gets cold the battery was done.
theres lots of youtube videos on it. some people use pickling salt for electrolyte but sometimes your lead plates are toast.

Post Reply