Post by MrBeeeeee » Sep 11 2020 8:47pm

Hey guys,

This is in Oakland, CA.

I'm trying to offset the cost of my own EV build by over-buying batteries direct from the factory in Guangdong. I still have about a hundred cells left from this buy. They're all 60Ah. I've been capacity testing some of them with a Turnigy Reaktor charger, by discharging down to 3.0v and recharging them using the internal setting for LiFePo4 cells. So far out of ten, they've all been over 58Ah using this methodology. The charging leads I'm using are simple Amazon jobs and I'm sure that's affecting my accuracy.

I'm asking $60 per cell on Craigslist, but I'll sell to Endless Sphere members at $50 per cell as long as I don't have to ship them.
In any case, here's the Craigslist ad:

https://sfbay.craigslist.org/eby/mat/d/ ... 77562.html


Size (mm): 173x102x40
Mass (lb): 3.03
Nominal Voltage: 3.2v
Discharge Cut-off: 2.50v
Recommended SOC 5%-95%
Capacity 60Ah
Charging Cut-off: 3.65v
Internal Resistance: <0.6 mOhm
Stud size: M5
Max Discharge Current: 180A (3c)

Cycle Life
Residual capacity: ≥80%(25±2℃, 1C/1C, 100%DOD, 1500cycles)

0~50°C(Charging Temperature)
-20~60°C(Discharging Temperature)

Storage Temperature and Humidity
-15°C ~45°C, ≤80%RH
-10°C ~ + 35°C, ≤80%RH

Charging Temperature Range
0~50℃

Discharging Temperature Range
-20~60℃

Discharging Capacity at 25℃
≥60.0Ah

Discharging Capacity at 55℃
≥60.0Ah

Discharging Capacity at -20℃
≥42Ah

Cycle Life
Residual capacity: ≥80%(25±2℃, 1C/1C, 100%DOD, 1500cycles)
00c0c_eoFMHRW0kEI_0CI0t2_1200x900.jpg
00c0c_eoFMHRW0kEI_0CI0t2_1200x900.jpg (186.77 KiB) Viewed 525 times
00K0K_3Zdx2t11Vyc_0CI0t2_1200x900.jpg
00K0K_3Zdx2t11Vyc_0CI0t2_1200x900.jpg (177.97 KiB) Viewed 525 times
00m0m_akJMNzueVxC_0CI0t2_1200x900.jpg
00m0m_akJMNzueVxC_0CI0t2_1200x900.jpg (97.77 KiB) Viewed 525 times
00N0N_bjJOO0FCugN_0CI0t2_1200x900.jpg
00N0N_bjJOO0FCugN_0CI0t2_1200x900.jpg (257.13 KiB) Viewed 525 times

john61ct   100 GW

100 GW
Posts: 7454
Joined: Dec 18 2018 2:06pm

Re: LiFePo4 Cells 60Ah New from the Factory in SF Bay Area

Post by john61ct » Sep 11 2020 9:57pm

Any indication of the maker? or can you link to the seller?

MrBeeeeee   10 mW

10 mW
Posts: 22
Joined: Nov 09 2018 2:27am

Re: LiFePo4 Cells 60Ah New from the Factory in SF Bay Area

Post by MrBeeeeee » Sep 11 2020 10:10pm

Sure, the maker was Shenzhen Xuba. I dealt with Amy. She was very nice.

https://szxuba.en.alibaba.com/

Jazzman56   100 mW

100 mW
Posts: 38
Joined: Sep 07 2014 12:47am
Location: Australia, NSW

Re: LiFePo4 Cells 60Ah New from the Factory in SF Bay Area

Post by Jazzman56 » Feb 14 2021 8:06am

Did these XUBA 60ah cells test to capacity? Any issues with them ? How tall are they with the studs ?

MrBeeeeee   10 mW

10 mW
Posts: 22
Joined: Nov 09 2018 2:27am

Re: LiFePo4 Cells 60Ah New from the Factory in SF Bay Area

Post by MrBeeeeee » Feb 14 2021 1:27pm

Every battery I tested was slightly less than the stated capacity. Most were just shy of 59Ah with a few in the 57Ah range. The internal resistivity was very consistent, but I was only measuring with a simple hobby charger.

One guy I did sell to was a material science researcher and he performed some more rigorous tests with proper equipment. He expressed that he was quite pleased with how they performed.

It's been several months since I've sold them and no one has had an experience negative enough to let me know about it, sonI consider that quite good.

I couldn't tell you about the terminal dimensions though as I don't have anymore.