I've been using a few packs from Unit Pack Power (UPP) lately and I've been having some bad experiences.
I do Uber eats with my ebike, so I need a lot of energy to get me through the day. I have a 35 Ah pack (not UPP), a 14Ah pack (from UPP) and more recently a 7 Ah pack (also UPP). I've been able to work all day without having to schedule charging sessions between shifts.
I was pretty happy with my set up that I went to buy a second 14 Ah pack as a spare.
Prior to my second purchase of the 14 Ah pack, I did have the nickel strip that connected the red positive along with the first bms wire to the pack snap on me. I managed to patch that to get it working again but upon examination and research, I discovered that the strips used are nickel plated steel and susceptible to corrosion. There are definitely some rust marks that I'll probably have to deal with in the future. I've had this pack since January and used it everyday from full to empty through to October.
After receiving the spare pack, I decided to swap out the 10 month old one. It performed well up until today, when I discovered the bms burned out on me. When I started my day, it didn't quite fully charge and when I came home the charger wouldn't work at all. It wasn't until I was about to change my charging connector that I noticed a hole burnt through the bottom of the bag and some tiny sparks happening. There was also some dampness on the cardboard insulator. And yes it had the blue heat shrink over it. And this pack was inside a seemingly strong water proof bag.
I just reinstalled the previous pack but now I'm nervous of having to rely on it for the long term, so I'll be searching for a reputable brand that also meets the form factor requirements of my frame. I have this pack strapped on the down tube. This is a full suspension frame, so there is a little more clearance from the front wheel.
I'll be attaching several pics in the next posts.
I've been using a few packs from Unit Pack Power (UPP) lately and I've been having some bad experiences.
I do Uber eats with my ebike, so I need a lot of energy to get me through the day. I have a 35 Ah pack (not UPP), a 14Ah pack (from UPP) and more recently a 7 Ah pack (also UPP). I've been able to work all day without having to schedule charging sessions between shifts.
I was pretty happy with my set up that I went to buy a second 14 Ah pack as a spare.
Prior to my second purchase of the 14 Ah pack, I did have the nickel strip that connected the red positive along with the first bms wire to the pack snap on me. I managed to patch that to get it working again but upon examination and research, I discovered that the strips used are nickel plated steel and susceptible to corrosion. There are definitely some rust marks that I'll probably have to deal with in the future. I've had this pack since January and used it everyday from full to empty through to October.
After receiving the spare pack, I decided to swap out the 10 month old one. It performed well up until today, when I discovered the bms burned out on me. When I started my day, it didn't quite fully charge and when I came home the charger wouldn't work at all. It wasn't until I was about to change my charging connector that I noticed a hole burnt through the bottom of the bag and some tiny sparks happening. There was also some dampness on the cardboard insulator. And yes it had the blue heat shrink over it. And this pack was inside a seemingly strong water proof bag.
I just reinstalled the previous pack but now I'm nervous of having to rely on it for the long term, so I'll be searching for a reputable brand that also meets the form factor requirements of my frame. I have this pack strapped on the down tube. This is a full suspension frame, so there is a little more clearance from the front wheel.
I'll be attaching several pics in the next posts.
Re: What the heck is wrong with UPP packs!?
Here's some images of the fried bms.
As you can see, it just totally cooked on the left.
As you can see, it just totally cooked on the left.
- Attachments
-
- IMG20201109012649_compressed.jpg (64.89 KiB) Viewed 1140 times
-
- IMG20201109013502_compressed.jpg (200.47 KiB) Viewed 1140 times
-
- IMG20201109015718_compressed.jpg (67.22 KiB) Viewed 1140 times
Re: What the heck is wrong with UPP packs!?
Thanks Justin_le we're here thanks to you. All the best to the mods for their tireless work keeping it on an even keel.
Re: What the heck is wrong with UPP packs!?
I'd agree with you except, I've had a pretty good experience with keeping water out with various packs. And I ride through some potent rains.
No, I have a different theory. I think that the hole burned through first and then I rode through some sprinklers and puddles recently that may have flicked up into that opening. As I said, I have this pack strapped on the downtube. The front wheel probably flicked some of that moisture.
Re: What the heck is wrong with UPP packs!?
Yeah, I saw that video.
Re: What the heck is wrong with UPP packs!?
Wouldn't you know it. My 10 month old pack that I swapped in last night wouldn't work today. When I plugged her in, my throttle indicator had it sitting on 4.3v. which happened to me a couple of days ago with the recently fried pack but I assumed it was my connector. It was back to normal when I ensured proper contact them. I had no such luck this time. Wouldn't resume charging either.
When I opened her up, nothing looked physically damaged (except for the corrosion on the strips). However, when I went to volt test each series, the first one was at 0.2v while the rest were at a healthy 41.v. I'll post more pics when I get home.
When I opened her up, nothing looked physically damaged (except for the corrosion on the strips). However, when I went to volt test each series, the first one was at 0.2v while the rest were at a healthy 41.v. I'll post more pics when I get home.
Re: What the heck is wrong with UPP packs!?
Here are some pics of the 10 month old pack. I checked each series' voltage. There all around 4.1v except for that first one by the court wire bodging. It is on 0.33v
The month old pack is around 3.6v with the first series at 1.36v
The month old pack is around 3.6v with the first series at 1.36v
- Attachments
-
- You'll see that I had to bodge a copper wire attached by spade connectors
- IMG20201110011158_compressed.jpg (126.98 KiB) Viewed 1058 times
-
- Here is a hole in the strip from an earlier wire that I didn't strip the whole way. It concentrated all the best there
- IMG20201110011433_compressed.jpg (82.89 KiB) Viewed 1058 times
-
- Here's a shot from the other side with sing of that corrosion I was talking about
- IMG20201110011213_compressed.jpg (149.46 KiB) Viewed 1058 times
Re: What the heck is wrong with UPP packs!?
Here's a shot of the "new" pack after I ripped open the packaging.
I suspect that the cardboard insulator used acts as a sponge and only serves to spread any moisture that happens to get in. I prefer it when they use the hard plastic like insulator.
I suspect that the cardboard insulator used acts as a sponge and only serves to spread any moisture that happens to get in. I prefer it when they use the hard plastic like insulator.
- Attachments
-
- Corrosion set in fast this time
- IMG20201110013650_compressed.jpg (190.9 KiB) Viewed 1056 times
Re: What the heck is wrong with UPP packs!?
The autopsy continues. Here a shot the bms that didn't burn. Well I guess it did.
- Attachments
-
- From the underneath. It's quite scorched at the ground discharge wire.
- IMG20201110015358_compressed.jpg (443.77 KiB) Viewed 1053 times
Re: What the heck is wrong with UPP packs!?
And on the top side of the bms, I noticed 5 modules with the first 3 looking singed at the back. What are those things? This is my first bms autopsy.
- Attachments
-
- IMG20201110020056_compressed.jpg (159.08 KiB) Viewed 1053 times
- www.recumbents.com 10 kW
- Posts: 942
- Joined: May 26 2008 8:42pm
- Location: Chicago area
- Contact:
Re: What the heck is wrong with UPP packs!?
Those are the power FETs. It looks like you are putting a higher continuous load on the BMS than the FETs can handle without overheating. Sometime you can add a heat sink to resolve that but the better resolution is to use a higher power BMS. What amperage is the pack rated at?
E-bike projects - http://www.recumbents.com/wisil/e-bent
Re: What the heck is wrong with UPP packs!?
I was wondering about that but I'm using a 35A max controller with a 17A continuous. The bms is supposed to be fit for 30A continuous and 90A max.www.recumbents.com wrote: ↑Nov 09 2020 4:00pmThose are the power FETs. It looks like you are putting a higher continuous load on the BMS than the FETs can handle without overheating. Sometime you can add a heat sink to resolve that but the better resolution is to use a higher power BMS. What amperage is the pack rated at?
Re: What the heck is wrong with UPP packs!?
looks like you get to try and salvage some cells and make a new pack. i use cell holders and plasti-dip to waterproof
30Q test viewtopic.php?f=14&t=108547
40T test viewtopic.php?f=14&t=106550
Sony VTC6 viewtopic.php?f=14&t=108661
mnke 26650 test viewtopic.php?f=14&t=107191
Battery magnets viewtopic.php?f=14&t=106190&hilit=magne ... 5#p1563730
40T test viewtopic.php?f=14&t=106550
Sony VTC6 viewtopic.php?f=14&t=108661
mnke 26650 test viewtopic.php?f=14&t=107191
Battery magnets viewtopic.php?f=14&t=106190&hilit=magne ... 5#p1563730
Re: What the heck is wrong with UPP packs!?
i usually roll the nickel strip off the cells, kind of like how you open a can of spam. on the negative end some batteries have weak metal and it rips a hole in the bottom where the spot welds are, try rolling the strip off the dead cells to see.
you might be able to cut the packs in half and connect the two good halves together in series to get up and going right away
you might be able to cut the packs in half and connect the two good halves together in series to get up and going right away
30Q test viewtopic.php?f=14&t=108547
40T test viewtopic.php?f=14&t=106550
Sony VTC6 viewtopic.php?f=14&t=108661
mnke 26650 test viewtopic.php?f=14&t=107191
Battery magnets viewtopic.php?f=14&t=106190&hilit=magne ... 5#p1563730
40T test viewtopic.php?f=14&t=106550
Sony VTC6 viewtopic.php?f=14&t=108661
mnke 26650 test viewtopic.php?f=14&t=107191
Battery magnets viewtopic.php?f=14&t=106190&hilit=magne ... 5#p1563730
Re: What the heck is wrong with UPP packs!?
I have a question about the UPP's BMS compatibility with my controller/motor setup.
The BMS in these 14Ah packs are rated at 30A continuous and 90A peak.
My controller is rated at 17A continuous and 35A peak.
And my motor is 500 watts. I don't know what that means in terms of how many amps it can take or whether it pulls any additional itself (I had an experience with a1200 watt motor pulling my controller's peak as continuous for some reason, still can't wrap my head around that one)
My question is, even though the continuous ratings of 30A of the BMS exceeds that of my controller's continuous 17A, is it still likely that the fewer times I might hit peak (30-35A) can lead to the type of failure I experienced here?
The BMS in these 14Ah packs are rated at 30A continuous and 90A peak.
My controller is rated at 17A continuous and 35A peak.
And my motor is 500 watts. I don't know what that means in terms of how many amps it can take or whether it pulls any additional itself (I had an experience with a1200 watt motor pulling my controller's peak as continuous for some reason, still can't wrap my head around that one)
My question is, even though the continuous ratings of 30A of the BMS exceeds that of my controller's continuous 17A, is it still likely that the fewer times I might hit peak (30-35A) can lead to the type of failure I experienced here?
Re: What the heck is wrong with UPP packs!?
motor wattage continuous
not peak rating
never seen 30a bms peak 90a
more like 40-50a if that
multiple problems here
overloading is bad as evidenced here
water only makes things worse
not peak rating
never seen 30a bms peak 90a
more like 40-50a if that
multiple problems here
overloading is bad as evidenced here
water only makes things worse
In 2013 an ad appears on Russia social networks: Интернет-операторы хотели! Работа в шикарном офисе в Ольгино !!!, зарплата 25960 рублей в месяц
Re: What the heck is wrong with UPP packs!?
Saw this not too long ago which completely turned me off to UPP, not that I wasn't already skeptical.
https://youtu.be/JCaDz_2YcGQ
https://youtu.be/JCaDz_2YcGQ
Re: What the heck is wrong with UPP packs!?
A quick update on my experience. The vendor for one of the packs sent me a replacement. This was the pack that started sparking up and burning a hole through its bag. I've been riding with it for only 20 days and already, it just started to not get a full charge. It stops charging at 53v, whereas it normally charges fully to 54.6. I've even been extra careful to avoid draining it right down to the bottom this time.
Re: What the heck is wrong with UPP packs!?
Bank out of balance and shiit bms not doing its job, just the regular.ClintBX wrote: ↑Dec 29 2020 2:28amA quick update on my experience. The vendor for one of the packs sent me a replacement. This was the pack that started sparking up and burning a hole through its bag. I've been riding with it for only 20 days and already, it just started to not get a full charge. It stops charging at 53v, whereas it normally charges fully to 54.6. I've even been extra careful to avoid draining it right down to the bottom this time.
Re: What the heck is wrong with UPP packs!?
Just email them.. they'll send a new one out.... I've had 6 packs from them all awesome...
Re: What the heck is wrong with UPP packs!?
UPP sucks. Very poor quality builds, using nickel-coated steel connections rather than pure nickel. And low ball cheap featureless BMS.