Firedog,
Do you do any type of protection between the packs in series as described by this post here:
viewtopic.php?f=14&t=99279#p1453668
Tool battery (Makita) mounts for ebikes
-
- Posts: 289
- Joined: Apr 23 2008 3:53pm
Re: Tool battery (Makita) mounts for ebikes
I have made Makita rebuildable battery. Uses the top cover with a latch and screws.
Bought a trimmer and was not satisfied with run time. I can build 2 to 8P packs. Here is 3P 9.6AH:
https://cults3d.com/en/3d-model/gadget/ ... ita-module
Bought a trimmer and was not satisfied with run time. I can build 2 to 8P packs. Here is 3P 9.6AH:
https://cults3d.com/en/3d-model/gadget/ ... ita-module
-
- Posts: 59
- Joined: Apr 06 2018 3:53pm
Re: Tool battery (Makita) mounts for ebikes
Seriously awesome work there. I'd love to see a build thread on your custom power tool batteries.
For folks that have a few toys and don't rely on them for commuting, I still think having swappable power tool brick batteries is a great option. Not to mention you can rely on your tools to last much longer without worrying about going to the hardware store and finding out they don't make the ones in the proper shape to fit your tool anymore.
For folks that have a few toys and don't rely on them for commuting, I still think having swappable power tool brick batteries is a great option. Not to mention you can rely on your tools to last much longer without worrying about going to the hardware store and finding out they don't make the ones in the proper shape to fit your tool anymore.
Re: Tool battery (Makita) mounts for ebikes
I have files on cults3d. You can print everything at home. Its for older type pcb without bms but i have design for new bms boards too.MorbidlyObeseKoala wrote: ↑Feb 04 2021 11:10amSeriously awesome work there. I'd love to see a build thread on your custom power tool batteries.
For folks that have a few toys and don't rely on them for commuting, I still think having swappable power tool brick batteries is a great option. Not to mention you can rely on your tools to last much longer without worrying about going to the hardware store and finding out they don't make the ones in the proper shape to fit your tool anymore.
https://cults3d.com/en/3d-model/gadget/ ... ita-module