Hi all,
New member here. Trying to see if anyone can help me out.
We repair hybrid battery packs in Milwaukee and recently we signed a contract with a local junk yard to remove the hybrid battery pack out of 650 Ford Escape hybrids. It will probably take 6 months to complete but we started already and I can see a storage issue will occur for our facility
I will include photos of what I am talking about but our customer simply wants to crush the cars to get the scrap metal but until the battery is remove they cannot send it thru the crusher. So we take out the packs complete. We have opened some up to take photos of the cells to see if there are people that needs them. The cells are automotive grade NiMh D size cells. They are 1.2v nominal and 5,500mah capacity from the factory. We have not performed any significant tests other than to measure standing voltage which shows that all the cells are holding charge and since they all came out of running and driving vehicles we can assume they still have decent capacity.
Our thoughts was someone can use these cells for solar energy storage. As of right now we have all the injection molded holding trays, BMS and cooling fans and wiring harness and sensor wires. But to save space we plan on taking the cells out and selling the fans and other electronics separately on ebay. Apparently the fans are highly desirable.
If you have ideas of how these cells can be repurposed please feel free to respond or mesaage me.
Our website is WWW.HYBRIDHEROMKE.COM
My personal cell is 414-614-4258. Feel free to text or call.
Thank you
Andy
What do you do with 650 Ford Escape hybrid battery packs?
-
- Posts: 3
- Joined: Dec 17 2019 11:38am
What do you do with 650 Ford Escape hybrid battery packs?
- Attachments
-
- 20210406_141111.jpg (4.34 MiB) Viewed 127 times
-
- 20210402_143806.jpg (3.36 MiB) Viewed 127 times
-
- 20210402_143629.jpg (5.34 MiB) Viewed 127 times
-
- 20210402_144618.jpg (5.25 MiB) Viewed 127 times
-
- 20210402_140443.jpg (3.83 MiB) Viewed 127 times
- amberwolf 100 GW
- Posts: 32116
- Joined: Aug 17 2009 6:43am
- Location: Phoenix, AZ, USA, Earth, Sol, Local Bubble, Orion Arm, Milky Way, Local Group
- Contact:
Re: What do you do with 650 Ford Escape hybrid battery packs?
Dunno if the batteries are useful, but you should take the motor and controller systems out and sell *those* cheap. 

This post has been moved to the items for sale section as well, because it advertises your business, and presumably you wish to sell the things discussed in the post.

Nope. You've been here almost a year and a half, with a post for other items for sale in the used section, in which you also said you were a "new member here".

This post has been moved to the items for sale section as well, because it advertises your business, and presumably you wish to sell the things discussed in the post.
If you found this advice helpful, supporting contributions are accepted here.
"if it ain't broke, improve it till it is"----Dog-Hauler Cargo eTrike SB Cruiser----The HI-Lebowski: a Lebowski SMD brain running a zombified Honda IMA Inverter: a HOW-TO guide----Cargo eBike CrazyBike2----General Blog
"if it ain't broke, improve it till it is"----Dog-Hauler Cargo eTrike SB Cruiser----The HI-Lebowski: a Lebowski SMD brain running a zombified Honda IMA Inverter: a HOW-TO guide----Cargo eBike CrazyBike2----General Blog
-
- Posts: 3
- Joined: Dec 17 2019 11:38am
What do you do with 650 Ford Escape hybrid battery packs?
Hi all,
Trying to see if anyone can help me out.
We repair hybrid battery packs in Milwaukee and recently we signed a contract with a local junk yard to remove the hybrid battery pack out of 650 Ford Escape hybrids. It will probably take 6 months to complete but we started already and I can see a storage issue will occur for our facility
I will include photos of what I am talking about but our customer simply wants to crush the cars to get the scrap metal but until the battery is remove they cannot send it thru the crusher. So we take out the packs complete. We have opened some up to take photos of the cells to see if there are people that needs them. The cells are automotive grade NiMh D size cells. They are 1.2v nominal and 5,500mah capacity from the factory. We have not performed any significant tests other than to measure standing voltage which shows that all the cells are holding charge and since they all came out of running and driving vehicles we can assume they still have decent capacity.
Our thoughts was someone can use these cells for solar energy storage. As of right now we have all the injection molded holding trays, BMS and cooling fans and wiring harness and sensor wires. But to save space we plan on taking the cells out and selling the fans and other electronics separately on ebay. Apparently the fans are highly desirable.
If you have ideas of how these cells can be repurposed please feel free to respond or mesaage me.
Our website is WWW.HYBRIDHEROMKE.COM
My personal cell is 414-614-4258. Feel free to text or call.
Thank you
Andy
Trying to see if anyone can help me out.
We repair hybrid battery packs in Milwaukee and recently we signed a contract with a local junk yard to remove the hybrid battery pack out of 650 Ford Escape hybrids. It will probably take 6 months to complete but we started already and I can see a storage issue will occur for our facility
I will include photos of what I am talking about but our customer simply wants to crush the cars to get the scrap metal but until the battery is remove they cannot send it thru the crusher. So we take out the packs complete. We have opened some up to take photos of the cells to see if there are people that needs them. The cells are automotive grade NiMh D size cells. They are 1.2v nominal and 5,500mah capacity from the factory. We have not performed any significant tests other than to measure standing voltage which shows that all the cells are holding charge and since they all came out of running and driving vehicles we can assume they still have decent capacity.
Our thoughts was someone can use these cells for solar energy storage. As of right now we have all the injection molded holding trays, BMS and cooling fans and wiring harness and sensor wires. But to save space we plan on taking the cells out and selling the fans and other electronics separately on ebay. Apparently the fans are highly desirable.
If you have ideas of how these cells can be repurposed please feel free to respond or mesaage me.
Our website is WWW.HYBRIDHEROMKE.COM
My personal cell is 414-614-4258. Feel free to text or call.
Thank you
Andy
- Attachments
-
- 20210406_141111.jpg (4.34 MiB) Viewed 65 times
-
- 20210402_143648.jpg (4.51 MiB) Viewed 65 times
-
- 20210402_144538.jpg (5.16 MiB) Viewed 65 times
-
- 20210402_140426.jpg (4.52 MiB) Viewed 65 times
-
- Posts: 17
- Joined: Aug 09 2019 5:24pm
Re: What do you do with 650 Ford Escape hybrid battery packs?
Here is a website that sells lithium batteries, it appears to me that they try to put the least amount of manpower hours into selling the batteries. They don't take the packs apart and give as much information about each individual battery that are in the packs and give info about how the final purchaser can take the batteries apart, recycle wire, copper, etc. and use the individual cells to make ebike battery packs or power wall packs for solar energy houses.
https://batteryhookup.com/
The one big cost for the batteries is the shipping cost and a hazard fee on some kinds of batteries, a business can get into real trouble if all the rules and regulations in regards to shipping are not followed.
The pictures that you have do not show any information about the individual cells, here is an article about taking a Ford Escape battery apart, the article is from 2014 and mentions that the batteries are NiMH, which are not as desirable as are lithium batteries.
https://300mpg.org/2014/10/13/deconstru ... otorcycle/
https://batteryhookup.com/
The one big cost for the batteries is the shipping cost and a hazard fee on some kinds of batteries, a business can get into real trouble if all the rules and regulations in regards to shipping are not followed.
The pictures that you have do not show any information about the individual cells, here is an article about taking a Ford Escape battery apart, the article is from 2014 and mentions that the batteries are NiMH, which are not as desirable as are lithium batteries.
https://300mpg.org/2014/10/13/deconstru ... otorcycle/
- amberwolf 100 GW
- Posts: 32116
- Joined: Aug 17 2009 6:43am
- Location: Phoenix, AZ, USA, Earth, Sol, Local Bubble, Orion Arm, Milky Way, Local Group
- Contact:
Re: What do you do with 650 Ford Escape hybrid battery packs?
Your new thread for the same thing has been merged with the first one you made for it.
Please don't make multiple threads for the same thing.
Please don't make multiple threads for the same thing.
If you found this advice helpful, supporting contributions are accepted here.
"if it ain't broke, improve it till it is"----Dog-Hauler Cargo eTrike SB Cruiser----The HI-Lebowski: a Lebowski SMD brain running a zombified Honda IMA Inverter: a HOW-TO guide----Cargo eBike CrazyBike2----General Blog
"if it ain't broke, improve it till it is"----Dog-Hauler Cargo eTrike SB Cruiser----The HI-Lebowski: a Lebowski SMD brain running a zombified Honda IMA Inverter: a HOW-TO guide----Cargo eBike CrazyBike2----General Blog