40T, neodymium magnets, plasti dip cycle test

Batteries, Chargers, and Battery Management Systems.
john61ct   100 GW

100 GW
Posts: 7579
Joined: Dec 18 2018 2:06pm

Re: 40T, neodymium magnets, plasti dip cycle test

Post by john61ct » Apr 26 2021 12:45pm

Also for a mobile application the possibly extreme, and certainly constant shock and vibration needs to be taken into account

goatman   100 MW

100 MW
Posts: 2910
Joined: Jun 23 2019 6:50pm
Location: Surrey, B.C.

Re: 40T, neodymium magnets, plasti dip cycle test

Post by goatman » May 03 2021 7:12pm

need to finish a battery
have scrap nickel strip
IMG_20210503_105500.jpg
IMG_20210503_105500.jpg (4.25 MiB) Viewed 221 times
wrong dimension
IMG_20210503_111005.jpg
IMG_20210503_111005.jpg (3.87 MiB) Viewed 221 times
time to mickey mouse it
IMG_20210503_112831.jpg
IMG_20210503_112831.jpg (3.34 MiB) Viewed 221 times
1/8 x 3/8 magnets are strong
IMG_20210503_113349.jpg
IMG_20210503_113349.jpg (3.29 MiB) Viewed 221 times
10mmx1mm not so much
IMG_20210503_113627.jpg
IMG_20210503_113627.jpg (3.21 MiB) Viewed 221 times
10mm x 1mm will hold the cell at this angle
IMG_20210503_113942.jpg
IMG_20210503_113942.jpg (3.88 MiB) Viewed 221 times
trace onto foil
IMG_20210503_115953.jpg
IMG_20210503_115953.jpg (4.03 MiB) Viewed 221 times
IMG_20210503_122405.jpg
IMG_20210503_122405.jpg (4.06 MiB) Viewed 221 times
shouldve made all like this
IMG_20210503_144619.jpg
IMG_20210503_144619.jpg (3.71 MiB) Viewed 221 times
10 gauge
IMG_20210503_152052.jpg
IMG_20210503_152052.jpg (3.95 MiB) Viewed 221 times
IMG_20210503_152341.jpg
IMG_20210503_152341.jpg (3.9 MiB) Viewed 221 times
IMG_20210503_152658.jpg
IMG_20210503_152658.jpg (3.73 MiB) Viewed 221 times
twist crimped with 20 gauge
IMG_20210503_155631.jpg
IMG_20210503_155631.jpg (4 MiB) Viewed 221 times
dont really like that, want more contact for amps, decided to wrap with copper strand
IMG_20210503_155658.jpg
IMG_20210503_155658.jpg (4.02 MiB) Viewed 221 times
IMG_20210503_155736.jpg
IMG_20210503_155736.jpg (3.9 MiB) Viewed 221 times
IMG_20210503_162214.jpg
IMG_20210503_162214.jpg (4.03 MiB) Viewed 221 times
IMG_20210503_184039.jpg
IMG_20210503_184039.jpg (4.06 MiB) Viewed 214 times
using 7.5mm magnets and a 10mm to help keep everything in place while i caulk it in place
IMG_20210503_190602.jpg
IMG_20210503_190602.jpg (3.82 MiB) Viewed 214 times
IMG_20210503_191525.jpg
IMG_20210503_191525.jpg (3.47 MiB) Viewed 214 times

Pajda   1 kW

1 kW
Posts: 406
Joined: Jan 24 2016 3:45am
Location: Czech Republic

Re: 40T, neodymium magnets, plasti dip cycle test

Post by Pajda » May 04 2021 8:54am

I must say that I like to follow your inventive approach :)

goatman   100 MW

100 MW
Posts: 2910
Joined: Jun 23 2019 6:50pm
Location: Surrey, B.C.

Re: 40T, neodymium magnets, plasti dip cycle test

Post by goatman » May 04 2021 10:45am

ya :D amazon lost my 0.1mm copper in shipping and im moving June.01 so i didnt want to order anything til end of the month
im low on everything, magnets, cell holders, big battery wrap, 18 pin connectors....


in the meantime. the nickel is 0.15mm and 3 layers of foil is about 0.1mm for total of 0.25mm

5mm square magnet has 0.6lbs pull at 0.1mm
https://www.indigoinstruments.com/magne ... 222-1.html

to equal the pull of 1-10mm magnet 1.2 lb pull
i used 1-7.5mm ring and 1-5mm square, 1.4lb pull
IMG_20210305_230857.jpg
IMG_20210305_230857.jpg (3.37 MiB) Viewed 197 times
IMG_20210504_082717.jpg
IMG_20210504_082717.jpg (4.17 MiB) Viewed 197 times
time for plast dip

Ianhill   10 MW

10 MW
Posts: 2391
Joined: Sep 25 2015 5:55pm

Re: 40T, neodymium magnets, plasti dip cycle test

Post by Ianhill » May 04 2021 6:32pm

Thats perseverance for you got there in the end.
IMG_20210505_002903747.jpg
IMG_20210505_002903747.jpg (175.33 KiB) Viewed 181 times
Only one bit i spot is that little overhang would be ideally rounded on the corners so it stays within the tabs boundarys to guarantee no foul play later on but otherwise that a real nice bit of progress you got by there and looking forward to seeing how it performs thermally under load i think it should do quite well.

goatman   100 MW

100 MW
Posts: 2910
Joined: Jun 23 2019 6:50pm
Location: Surrey, B.C.

Re: 40T, neodymium magnets, plasti dip cycle test

Post by goatman » May 04 2021 8:49pm

yes i scrunched up the copper foil before spraying
IMG_20210504_164228.jpg
IMG_20210504_164228.jpg (4.12 MiB) Viewed 172 times
this is plasti dip when first sprayed
itll sit there and bubble like this til it settles down and give another coat in 30 minutes


IMG_20210504_184008.jpg
IMG_20210504_184008.jpg (4.58 MiB) Viewed 172 times

Hummina Shadeeba   100 MW

100 MW
Posts: 2669
Joined: Apr 25 2014 10:26pm
Location: sausalito cali..up the hill in front of the cruising club.

Re: 40T, neodymium magnets, plasti dip cycle test

Post by Hummina Shadeeba » May 04 2021 11:16pm

How does potting effect the safety release valves on cells? I don’t know how but the A123 26650 cells will somehow disconnect when shorted for long enough and then magically come back. (Current will drop drastically but same voltage somehow, then later string current). It’s a pretty safe cell to begin with but what if u jam up the pid or whatever it’s called on some other cells? Maybe be a fun experiment

If going for maximum pull with small magnets maybe worth adding a back iron. Cheaper than a bigger magnet.

goatman   100 MW

100 MW
Posts: 2910
Joined: Jun 23 2019 6:50pm
Location: Surrey, B.C.

Re: 40T, neodymium magnets, plasti dip cycle test

Post by goatman » May 05 2021 1:01am

dont need back iron, theres enough in the can
bigger/heavier the magnet, the more lbs of pull required to keep the weight of the magnet in place

been trying to go as small and light as possible

7.5mm magnets with 0.1mm copper ill do a test when i get it to see how many amps it can do before the connection goes bad

7.5 mm magnets and foil will do 15amps, i run those on the trike at 7amps max with no issues
my 14 gauge battery leads were warmer than the batteries so im switching everything to 10awg

im putting this 5mm magnet battery build in the trike because they can handle 7 amps and putting the 7.5mm magnet battery build in the other bike because they can do 15 amps

i just dont know how the smoothness of 0.1mm copper will effect the connection but thats what i want to use for the terminal connections

theres no shorting out happening, plasti dip is an electrical insulator, i used the pour on plasti dip that comes in a can and covered the whole side of a 17s battery, i was kind of nervous thinking it might short out and blow up but nothing happened

as far as blowing up, im using 30Qs and 25Rs i havent seen them blow up from shorting them out
30Q
https://www.youtube.com/watch?v=Ys5wwUJOz58

25r
https://www.youtube.com/watch?v=oBlac5gWLfI

User avatar
nicobie   1 GW

1 GW
Posts: 3287
Joined: Aug 07 2008 1:48pm
Location: Central Coast CA, USA

Re: 40T, neodymium magnets, plasti dip cycle test

Post by nicobie » May 05 2021 1:23am

That's unconventional and probably why I like it. Strapped on well, I would think it should work fine. :thumb:
Take it easy... but take it. (Woody Guthrie)

my eTownie build thread: http://endless-sphere.com/forums/viewto ... =6&t=23701
Magazine article https://www.electricbike.com/nicks-etownie/

Ianhill   10 MW

10 MW
Posts: 2391
Joined: Sep 25 2015 5:55pm

Re: 40T, neodymium magnets, plasti dip cycle test

Post by Ianhill » May 05 2021 1:24am

Back iron on the rear of the magnet would guide the field lines on the reverse to give a higher surface tesla on the magnet 🧲 so it should increase pull strength.

I wonder if theres small enough magnets available to create a hallbach array no back iton needed it could double the pull to the cell and have less than half the field strength away from the pack where its not needed.

goatman   100 MW

100 MW
Posts: 2910
Joined: Jun 23 2019 6:50pm
Location: Surrey, B.C.

Re: 40T, neodymium magnets, plasti dip cycle test

Post by goatman » May 05 2021 9:22am

Ianhill wrote:
May 05 2021 1:24am
Back iron on the rear of the magnet would guide the field lines on the reverse to give a higher surface tesla on the magnet 🧲 so it should increase pull strength.

I wonder if theres small enough magnets available to create a hallbach array no back iton needed it could double the pull to the cell and have less than half the field strength away from the pack where its not needed.
you guys lost me, had to go google back iron and hallback array.

try to figure it out later :D

MorbidlyObeseKoala   1 W

1 W
Posts: 63
Joined: Apr 06 2018 3:53pm

Re: 40T, neodymium magnets, plasti dip cycle test

Post by MorbidlyObeseKoala » May 05 2021 9:22am

Wouldn't a back iron also provide a short path for current for the whole battery? Or was the idea to place that back iron over the layered plastidip?

A pull strength test might be interesting to compare crappy spot welds to the magnets but if goatman is getting repeatable amperage results, then this seems to be a novel approach with no specialized tools to me. My limited experience with plastidip on my car, I would say monitor it after a year or so for any flakes or tears. Tends to dry out and be painful to remove in one piece when it's fresh.

Just have to make sure your scissors or crap from the messy workbench don't get pulled into the magnets and short the whole thing out before you get it dipped.

goatman   100 MW

100 MW
Posts: 2910
Joined: Jun 23 2019 6:50pm
Location: Surrey, B.C.

Re: 40T, neodymium magnets, plasti dip cycle test

Post by goatman » May 05 2021 9:36am

been using plasti dip on my 25r packs for over a year

if you put it on thick it peels off clean
71ZGHae.jpg
71ZGHae.jpg (17.15 KiB) Viewed 137 times
after handling them every day i gave them another coat about a month ago

going to order shrink for the packs and just shrink wrap them once all wired up

Ianhill   10 MW

10 MW
Posts: 2391
Joined: Sep 25 2015 5:55pm

Re: 40T, neodymium magnets, plasti dip cycle test

Post by Ianhill » May 05 2021 11:12am

Back iron in this case could be as simple as a metal button sat on top of each magnet so it wouldn't be part of the electrical circuit only magnetic.

Ive had a look for some small magnets that might be suitable to make an array but theres no chance from what i can find anything small enough.

User avatar
nicobie   1 GW

1 GW
Posts: 3287
Joined: Aug 07 2008 1:48pm
Location: Central Coast CA, USA

Re: 40T, neodymium magnets, plasti dip cycle test

Post by nicobie » May 05 2021 3:10pm

I've been using these on cabinet doors for years.

https://www.leevalley.com/en-us/shop/ha ... asher-sets

Canadian company too.
Take it easy... but take it. (Woody Guthrie)

my eTownie build thread: http://endless-sphere.com/forums/viewto ... =6&t=23701
Magazine article https://www.electricbike.com/nicks-etownie/

goatman   100 MW

100 MW
Posts: 2910
Joined: Jun 23 2019 6:50pm
Location: Surrey, B.C.

Re: 40T, neodymium magnets, plasti dip cycle test

Post by goatman » May 05 2021 7:22pm

took that 5mm pack to the hill i test the batteries on and pulled 47amps (almost 12 amps/cell) no problems then paralleled to the 7.5mm battery went for a 8km ride. the trike is set to 3000 watts, 8p means less volt sag so the max amps were 44 (5.5amps) packs were the same temp and no issues

goatman   100 MW

100 MW
Posts: 2910
Joined: Jun 23 2019 6:50pm
Location: Surrey, B.C.

Re: 40T, neodymium magnets, plasti dip cycle test

Post by goatman » May 14 2021 9:14pm

have about 500km's/15 charge cycles on the 7.5mm magnet build
its been nice out with temps around 20 celcius
wrapped the battery in cardboard and stuck it in my tank bag so it stays warm
they only see about 6.25 amps max most of the time about 4amps
packs fine, no issues
IMG_20210514_185357 (1).jpg
IMG_20210514_185357 (1).jpg (2.7 MiB) Viewed 45 times

Hummina Shadeeba   100 MW

100 MW
Posts: 2669
Joined: Apr 25 2014 10:26pm
Location: sausalito cali..up the hill in front of the cruising club.

Re: 40T, neodymium magnets, plasti dip cycle test

Post by Hummina Shadeeba » May 14 2021 10:03pm

It seems with the magnets you don’t have to worry about rough riding stressing connections, and the rubber holding it all in place is nice.


You could get the least resistance of any connections I’d think. I guess you didn’t get a precision resistance meter for the battery and I didn’t read about comparing it to other packs or how it ages which would be nice.

goatman   100 MW

100 MW
Posts: 2910
Joined: Jun 23 2019 6:50pm
Location: Surrey, B.C.

Re: 40T, neodymium magnets, plasti dip cycle test

Post by goatman » May 14 2021 10:42pm

the ca3 shows resistance but i dont know what its measuring
my load tester shows resistance but i dont know what its measuring

i could hook up my 25r pack that was spot welded then i soldered 14 gauge copper wire to all the series connections and compare to the 30Q but i dont think that will prove anything its just different cells
i have those pics somewhere here

someone would have to spotweld 2 new cells in series with nickel and do a test and do the same with another 2 new cells in series with the copper, i dont have a spotwelder

Post Reply