Crash Machine
100 W
I've got two 48v Ping V2.5s. One 10Ah and one 15Ah. Maybe 30 cycles on the 10 Ah and about 15 cycles on the 15Ah. Ping even sent me some diodes to parellel them together. I used them for a while but the batteries balanced out so close to each other that I quit using the diodes. What can I say these batteries ROCK. Ping is a wonder to deal with and had them to me within 10 days I believe. The leds are such a great idea I'm sure we'll see them on other batteries.It's very reassuring to see those little lights come on. Plus they're kinda' mezmerizing. Like a Dead show I saw one time...