FalconEV 36v10a Discharge Graph

Post by oatnet » Sep 01 2007 10:00pm

Below is a discharge curve showing the first two full cycles on the FalconEV pack, on a CBA-II.

Before the first cycle, I used .6ah from the as-shipped charge, re-charged it, and discharged @ 2.37amps (.237c, restricted to under 100 watts by CBA II) to 34v. 2nd cycle I discharged to 33v. Both yielded @ 10.7 ah without engaging the BMS low-voltage cutoff, I think the 'recharge' on the first cycle burped in a few extra watts.

After much disappointment with NiMh ratings, I think 10.71ah on a battery rated for 10ah is pretty refreshing. I can't wait to see what it yields at a 30a discharge. I am a little sketchy on the charge time, I believe it was about 8 hours using the supplied 1.5a chargers.

The factory Andy buys from is so concerned about the other pack (damaged in shipping) that they are paying to ship it back to China to inspect it. That sounds like an organization with resources, and a commitment to quality. Andy has shipped me a replacement battery, he happened to have an extra 15ah LiMn pack, I paid extra for the 50% capacity increase.

Andy reported that the 10ah pack has a 30a BMS , but the 15ah pack has a 50a bms, and he highly recommends the 15ah pack as a minimum. I foolishly insisted that 30a would be plenty, as my Tidalforce runs at 30a in 'turbo' - which it does, except for that irksome little .2 second 47a spike on WOT that trips the 30ah BMS.

So the 15ah replacement pack will allow me to test on my TF, and the 10ah and 15ah packs can combine serial for 72v10ah@30a for my other motors. Either way, not much real-world testing I can do until the 15ah pack arrives!

-JD
Attachments
FalconEVLiMn36v10ah_2.37a discharge cycles 1 + 2.jpg
FalconEVLiMn36v10ah_2.37a discharge cycles 1 + 2.jpg (142.9 KiB) Viewed 1318 times
Last edited by oatnet on Sep 03 2007 2:17pm, edited 2 times in total.

User avatar
xyster   1 GW

1 GW
Posts: 3089
Joined: Jan 02 2007 8:39pm
Location: Visualize Rural Sheep

Post by xyster » Sep 01 2007 10:52pm

Cool -- did you just get the CBA?

The legend says "12 li-ion cells". Unless something has recently changed radically, a 36 volt LiMn pack should be 10 cells; a 36 volt LiFePO4 pack should be 12 cells.
Ebike: 5304/20", 72V 35A controller, 33AH 80V 20s15p (18650 sized cells) DIY lithium-ion pack
http://endless-sphere.com/forums/viewto ... 47&start=0
Scooter: '06 Stealth s1000, 48V 30A, 4x10ah SLA
http://endless-sphere.com/forums/viewtopic.php?t=148
Ebike: '06 Currie Mongoose, 32V 35A, 32V 22AH hybrid SLA/Li-ion pack
http://endless-sphere.com/forums/viewtopic.php?t=1010

User avatar
oatnet   10 MW

10 MW
Posts: 2341
Joined: Apr 26 2007 3:03pm
Location: SoCal, USA

OATNET Table Of Contents

Post by oatnet » Sep 02 2007 1:03am


====================================
OATNET Table Of Contents
====================================
In 2007, after lurking for many months, I became the 117th person to join endless-sphere, which now boasts a membership of over 14,000. Thanks to the teachings of smarter folks on E:S, I have experienced a lot in my time here and I wanted to post links to highlights in my signature. Unfortunately we can only have (6) URL's in our signature, so I put 5 links for favorite projects there, and pointed the 6th at this page. There are far more links here than I would have put into a signature, so now it is more of a table of contents. I would prefer it if people do not post on this thread, and instead leave it buried in the distant past. PICTURES from my favorite builds follow, including a time-lapse VIDEO of a Vectrix pack build.


Builds: Technical: Battery Firsts: Random: ===================================================================================
Vectrix Pack Replacement:

This VIDEO shows a few still photos of the old pack coming out, then a time-lapse of the entire battery being built.
  • (5) blue cells are arranged side-by-side to parallel them into a 50ah "supercell", and a capped with orange cell-holders.
    (5) of these supercells are laid end-to-end to connect them in series, giving a 5s5p "row" of cells.
    (9) of these rows are stacked on top of each other to form a pack with 45s5p / 175v50ah / 8kw capacity /250a continious.


However, because of the overhang in the front of the bike, I could only squeeze the first 6 rows of cells through the opening. Accordingly, you will see the first (6) rows built outside the bike, then hoisted into the bike. Next you see the remaining (3) rows being installed on top of the pack, installed directly inside the bike itself. In the end, I show the 46.5 mile range I got on my aggressive maiden voyage, with the resting voltage still above 3v/cell so there was more capacity to be had. Note that the orange cell-holders hold 2 rows worth of cells, so I am actually building two rows at a time.

http://endless-sphere.com/forums/viewto ... 75#p571231






===================================================================================
Here are some duplicate links I fleshed out with pictures for one of Justin's threads:



Norco A-line/xlyte 5403:
http://www.endless-sphere.com/forums/vi ... 95#p659513
Image
Image




Specialized Enduro Comp/BMC V2-T:
http://www.endless-sphere.com/forums/vi ... =6&t=24329
Image
Image




TF-IO/BMC V3, and the birth of the front-mounted pack as a handling IMPROVEMENT:
http://endless-sphere.com/forums/viewto ... 60#p281372
Image
Image




Kepler Friction-Drive outrunner:
http://endless-sphere.com/forums/viewto ... 28&t=21309
Image
Image




x5tracycle links:
Upgrade http://endless-sphere.com/forums/viewto ... =3&t=10201
Build http://endless-sphere.com/forums/viewto ... f=6&t=3514
Image
Image




TF/X5 wheelie machine:
Image
Image
http://endless-sphere.com/forums/viewto ... f=6&t=3205




My first build, circa 2007:
http://endless-sphere.com/forums/viewto ... ?f=6&t=848
Image
Image




===================================================================================
Finally, the original post I pirated/edited to add this TOC:


I bought my CBA last May
Now it helps me Every Day,
Recommend it, I would Say.

:oops:
/dork mode off

You are correct about the cell count, wise one. The CBA doesn't have a LiMn selection so I chose LiPo and the application gueses how many cells are in the pack, and force feeds that into the title, like it or not.

The only parameters that affect the test are cutoff voltage, cutoff temp, and drain rate. The battery type and cell count just happy fluff, ineffective ingenuity.

Drain rate on the CBA II is limited to 125 watts up to 12v (I think) and under 100w up to 36v, although I have had it overheat/shudown near 100w so I leave a little headroom.