What battery chem did they sell me?

Batteries, Chargers, and Battery Management Systems.
Post Reply
slippman   100 µW

100 µW
Posts: 9
Joined: Nov 01 2011 12:51pm

What battery chem did they sell me?

Post by slippman » Mar 26 2012 3:59am

Hi guys, after much agony I finally bought a 48v 10ah battery, the "frog" case model from conhis. http://conhismotor.com/ProductShow.asp?id=210
When it arrived I was shocked that it weighed so little 3,4kg (7.5lb) so I opened it up. It is supposed to be 5p13s, and I thought it to be a Li-Ion NiCoMn chemistry... but, at this weight, it has to be lipo right? Haven't checked how many amp hours it actually holds.

I opened the case, and it's a pack of greyish pouches with a a bms bundled in with heatshrunk plastic, you cant see much unless you cut the plastic...
Photo1(2).jpg

stewrobb   1 W

1 W
Posts: 58
Joined: Aug 30 2011 4:38pm
Location: Toronto, Canada

Re: What battery chem did they sell me?

Post by stewrobb » Mar 26 2012 4:12am

Whats the final voltage on the charge, and how many cells in series, that will definitely help, may not be definite depending on voltage though.
Gio 500+ scooter - @72v 50A X8M06 Greentime Controller
Delta/Wye - Regen - 20s3p 20c Turnigy hardcase
- Drove until the end, bent frame retired it

Current Build:
Ironhorse Hardtail frame, 120mm Suspension
Front Hayes Hydro Disc, Rear cable Disc
18 FET 4110 60A (for now) Controller
1000w Rear Motor - 420rpm@48v
20s3p Turnigy 5Ah

amigafan2003   1 kW

1 kW
Posts: 460
Joined: Jul 14 2011 10:05am
Location: UK

Re: What battery chem did they sell me?

Post by amigafan2003 » Mar 26 2012 5:29am

It's using Li-Ion NiCoMn pouches. Pouches weight less that cylindical cells.

You basically have one of these but the 10 AH version.

slippman   100 µW

100 µW
Posts: 9
Joined: Nov 01 2011 12:51pm

Re: What battery chem did they sell me?

Post by slippman » Mar 26 2012 5:45am

Thanks amigafan, that is most likely it! Seems to be the right weight etc. Kinda happy if they are not lipo, I live in an apartment and dont really have a safe place to charge them... btw, It's supposed to be 13s, but it's hard to see. The charger is supposed to cut off at 54.6v per it's markings, but when I measure I get 52.5v. Not sure what to make of that, it could be my multimeter that's off a bit I hope? Guess the only way to know for sure how many amp hours its holding would be to do a discharge test with a known load. Want to put some cycles on it first before bringing it all the way down to lvc...

As long as it performs well, it seems like a nice pack - lightweight, not too expensive, good mounting solution. Sure, you dont want to pull 1000+ watts out of it, but with my ecrazyman controller 48v/500w it should be a good match.

User avatar
neptronix   100 GW

100 GW
Posts: 15678
Joined: Jun 15 2010 5:56pm
Location: Utah, USA
Contact:

Re: What battery chem did they sell me?

Post by neptronix » Mar 26 2012 7:32am

Btw, lipo is not a chemistry, it is a cell form factor and it refers to a pouch style cell.. just FYI.

The potentially 'splodey chemistry you're referring to when you say 'lipo' is lithium cobalt, or li-co.
"Love and compassion are necessities, not luxuries. Without them, humanity cannot survive." - Dalai Lama

My first major build: 1.6kW 8T MAC motor on a Trek 4500 MTB.
Monster MTB: Leafmotor 1500w @ 4kW on a Turner O2 full suspension.
The monster scooter: Heavy duty Cannondale semi recumbent - under construction.
Blue Dream: Maxaraya FS semi recumbent and high efficiency mid-drive - under construction.

cwah   10 GW

10 GW
Posts: 4228
Joined: Jul 24 2011 5:42am
Location: Between paris and london

Re: What battery chem did they sell me?

Post by cwah » Mar 26 2012 12:52pm

Yeah, chemistry very similar to the one from BMSBattery. It's LiMN2O4 battery.

I've the 36V version that weight 3 kg.

However, it has lost 33% of its total capacity in 5 months. Not sure if it's the weather (around 11C),but that's annoying.

User avatar
dogman dan   100 GW

100 GW
Posts: 36021
Joined: May 17 2008 12:53pm
Location: Las Cruces New Mexico USA

Re: What battery chem did they sell me?

Post by dogman dan » Mar 27 2012 6:50am

Hopefully at least some of that capacity will return when temps are more warm. I lose about 20% capacity on pingbattery if the weather is very cold. That improves if you insulate it.

slippman   100 µW

100 µW
Posts: 9
Joined: Nov 01 2011 12:51pm

Re: What battery chem did they sell me?

Post by slippman » Mar 27 2012 8:55am

Didn't know that about lipo/lico, thanks. Don't like the sound of that capacity reduction... hmm, I guess time will tell, I hope mine holds up OK. loving the power to weight rato!

dnmun   100 GW

100 GW
Posts: 16190
Joined: Jun 09 2008 1:32pm
Location: portland, or and loveland, co

Re: What battery chem did they sell me?

Post by dnmun » Mar 27 2012 11:16am

lipo is lithium polymer. the cathode is an organic structure that holds the ions.

lifepo4 is lithium iron phosphate, the cathodic structure is a spinel, a crystalline structure that retains its physical strength when depleted of lithium ions which it stores in the voids inside the crystal. it is not the same as lipo.

limn2o4 is lithium manganese oxide, a crystalline structure which holds the lithium ions when they are stored in the cathode. again, not the same as lipo.

lipo is an organic polymer which will not hold the oxygen atoms from the chemical reaction when heated. lifepo4 has the oxygen locked into a structure which does not release the oxygen until it is heated to over 600 degrees C. this is why lifepo4 is safe when over charged and lipo is not.

999zip999   100 GW

100 GW
Posts: 10084
Joined: Jan 10 2010 1:40pm
Location: Dana Point So. Cal

Re: What battery chem did they sell me?

Post by 999zip999 » Mar 27 2012 1:05pm

Thanks Dnmun

User avatar
liveforphysics   100 GW

100 GW
Posts: 14163
Joined: Oct 29 2008 1:48am
Location: Long Beach, CA, USA

Re: What battery chem did they sell me?

Post by liveforphysics » Mar 27 2012 1:38pm

dnmun wrote:lipo is lithium polymer. the cathode is an organic structure that holds the ions.
Both anode and cathode hold ions...
dnmun wrote: lifepo4 is lithium iron phosphate, the cathodic structure is a spinel, a crystalline structure that retains its physical strength when depleted of lithium ions which it stores in the voids inside the crystal. it is not the same as lipo.
No. Lithium Iron cathodes are not spinel, they are olivine structures. Manganese chemistries, and a couple others (that aren't used because they don't make sense) have spinel structures. They also use a polymer seperator containing the electrolyte, the very same polyethyleneoxide or polyvinylidene difluoride film as RC LiCoO2 LiPo and NMC LiPo etc.
dnmun wrote: limn2o4 is lithium manganese oxide, a crystalline structure which holds the lithium ions when they are stored in the cathode. again, not the same as lipo.
All cathode material is crystalline (unless I'm forgetting one?)... Manganese oxide is arranged in a spinel formation. They also almost always use a polymer seperator containing the electrolyte.
dnmun wrote: lipo is an organic polymer which will not hold the oxygen atoms from the chemical reaction when heated. lifepo4 has the oxygen locked into a structure which does not release the oxygen until it is heated to over 600 degrees C. this is why lifepo4 is safe when over charged and lipo is not.
LiFePO4 burns and explodes impressively just like everything else that stores energy if you do enough of the wrong thing to it. LiFePO4 just has a much stronger bond to break before liberating the O2. A123/headways/thundersag cells blow up nicely with enough over-charge, just like everything else that you cause to take in more energy than it's able to shed after it's saturated it's ability to store energy.
Each carcinogen vapor exposure includes a dice roll for cancer.

Each mutagen vapor exposure includes a dice roll for reproductive genetic defects in your children.

Each engine start sprays them into a shared atmosphere which includes beings not offered an opportunity to consent accepting these cancer experiences and defective genetics life experiences.

Every post is a free gift to the collective of minds composing the living bleeding edge of LEV development on our spaceship.

Post Reply