Boeing Dreamliner Battery Fire

Batteries, Chargers, and Battery Management Systems.
Bamboo   10 mW

10 mW
Posts: 34
Joined: Aug 08 2011 6:27am
Location: Where 38% of traffic is by bicycles (250k+ town)

Re: Boeing Dreamliner Battery Fire

Post by Bamboo » Jan 17 2013 6:54am

amberwolf wrote:probable spec sheet for the cells:
http://www.s399157097.onlinehome.us/Spe ... P10-65.pdf
Thanks for that link, Amberwolf!

A company like Boeing wants a reliable supplier, no doubt, but looking at the specs it would amaze me if they did choose that Yuasa LiCo battery, only 87 - 101 Wh/kg? Even the much safer A123 pouch LiFePos have 130Wh/kg...

ebent   10 kW

10 kW
Posts: 556
Joined: Jan 19 2010 6:11pm
Location: Stuart, Florida

Re: Boeing Dreamliner Battery Fire

Post by ebent » Jan 17 2013 6:57am

My understanding of lithium cobalt. Please correct me. L. cobalt is used in stuff like phones. It is the most dense of the chemistries. Which allows the most talk time, and a very high discharge rate. Because the demand of discharge from small devices they get warm but no fire or explosion. But if we used it on our ebikes, we would have lots of fires and worse. Is that the idea?
2005 catrike pocket trike, sold 2013
750 watt hub motor
48v 18ah Lifepo4 electrified 1/2010
2014 HP Scorpion fs 26 April 2015 owned
electrified 6/6/2015 ride till you die...don't die riding
48v 20 ah LiMn2O4

User avatar
bigmoose   100 MW

100 MW
Posts: 2682
Joined: Aug 06 2009 3:05pm
Location: North coast USA
Contact:

Re: Boeing Dreamliner Battery Fire

Post by bigmoose » Jan 17 2013 7:32am

neptronix wrote:I'm laughing my fraggin' ass off over here reading this article.
I can point out at least a dozen people on this forum who could have designed a better battery pack.
Me too, on many levels! First, it is so ironic that all our transport restrictions on Li batteries was to prevent a mishap on an aircraft... now Boeing designs large format Li into their premier airframe, and what happens, and aircraft system initiated Li fire...

Next, to solve their problems perhaps we should send them a few rolls of Mil-Spec Chinese sourced, grey duct tape!! :mrgreen:
"Live simply. Love generously. Care deeply. Speak kindly. Leave the rest to God..." all the best, Dave

etriker   100 kW

100 kW
Posts: 1078
Joined: May 27 2012 8:21am
Location: Florida USA

Re: Boeing Dreamliner Battery Fire

Post by etriker » Jan 17 2013 8:07am

bigmoose wrote:
neptronix wrote:I'm laughing my fraggin' ass off over here reading this article.
I can point out at least a dozen people on this forum who could have designed a better battery pack.
Me too, on many levels! First, it is so ironic that all our transport restrictions on Li batteries was to prevent a mishap on an aircraft... now Boeing designs large format Li into their premier airframe, and what happens, and aircraft system initiated Li fire...

Next, to solve their problems perhaps we should send them a few rolls of Mil-Spec Chinese sourced, grey duct tape!! :mrgreen:
I would rather have you design my ebike battery than the people that designed the ones for the jets. That is for sure.

I bet it was young, well paid, college trained engineers that text a lot and goof off on the computer at work, that designed those jet battery packs ?

SamTexas   100 MW

100 MW
Posts: 2714
Joined: Dec 29 2010 5:34am
Location: Houston, Texas

Re: Boeing Dreamliner Battery Fire

Post by SamTexas » Jan 17 2013 8:16am

ebent wrote:My understanding of lithium cobalt. Please correct me. L. cobalt is used in stuff like phones. It is the most dense of the chemistries. Which allows the most talk time, and a very high discharge rate. Because the demand of discharge from small devices they get warm but no fire or explosion. But if we used it on our ebikes, we would have lots of fires and worse. Is that the idea?
The RC LiCo (aka HobbyKing LiPo) is not used in a single consumer product that I'm aware of.
The "Consumer" LiCo is found in almost every consumer products: Laptop, GPS, camera, cell phone, etc... They are also used in commercially available ebike battery packs. They are also used the Tesla battery pack.

RC LiCo has a lower energy density than Consumer LiCo but a much higher discharge rate.
Consumer LiCo has a higher energy density but a much lower discharge rate.

Both of them are Lithium Cobalt Oxide (LiCo).

ebent   10 kW

10 kW
Posts: 556
Joined: Jan 19 2010 6:11pm
Location: Stuart, Florida

Re: Boeing Dreamliner Battery Fire

Post by ebent » Jan 17 2013 8:37am

Thanks Sam. Every time I hear lipo I thought that was the chemistry. One more sliver of knowledge. On a relative basis lipo is volatile compared to most other chemistries. How much weight and space and ah would be lost if LiFePO4 was used instead? Isn't that the better solution?
2005 catrike pocket trike, sold 2013
750 watt hub motor
48v 18ah Lifepo4 electrified 1/2010
2014 HP Scorpion fs 26 April 2015 owned
electrified 6/6/2015 ride till you die...don't die riding
48v 20 ah LiMn2O4

etriker   100 kW

100 kW
Posts: 1078
Joined: May 27 2012 8:21am
Location: Florida USA

Re: Boeing Dreamliner Battery Fire

Post by etriker » Jan 17 2013 8:42am

ebent wrote:Thanks Sam. Every time I hear lipo I thought that was the chemistry. One more sliver of knowledge. On a relative basis lipo is volatile compared to most other chemistries. How much weight and space and ah would be lost if LiFePO4 was used instead? Isn't that the better solution?
Surely those bozos that designed that pack and put it in a jet could have designed and built a LiFePO4 pack that could burn up too ?

Jason27   10 kW

10 kW
Posts: 643
Joined: Apr 17 2011 8:10pm
Location: San Francisco, CA

Re: Boeing Dreamliner Battery Fire

Post by Jason27 » Jan 17 2013 8:50am

Boeing 787= outsourcing lesson from hell
My ebike:
Diamondback with WE 800 watt hub motor with AllCell 48V 20AH Lithium Manganese battery pack.

Jason27   10 kW

10 kW
Posts: 643
Joined: Apr 17 2011 8:10pm
Location: San Francisco, CA

Re: Boeing Dreamliner Battery Fire

Post by Jason27 » Jan 17 2013 8:52am

Takes notes all you MBA students and future CEO's.. Good case study here on globalization.
My ebike:
Diamondback with WE 800 watt hub motor with AllCell 48V 20AH Lithium Manganese battery pack.

SamTexas   100 MW

100 MW
Posts: 2714
Joined: Dec 29 2010 5:34am
Location: Houston, Texas

Re: Boeing Dreamliner Battery Fire

Post by SamTexas » Jan 17 2013 8:54am

ebent wrote:Thanks Sam. Every time I hear lipo I thought that was the chemistry. One more sliver of knowledge. On a relative basis lipo is volatile compared to most other chemistries. How much weight and space and ah would be lost if LiFePO4 was used instead? Isn't that the better solution?
You're welcome.

This HobbyKing popular pack
http://www.hobbyking.com/hobbyking/stor ... _pack.html
has 74Wh (3.7 * 4 * 5) and weighs 528g, so 140Wh/kg.

The LiFePo4 A123 20Ah pouch has 65Wh and weighs 496g, so 131Wh/kg

The Consumer LiCo Panasonic 18650 3.4Ah cell has 12.95Wh and weighs 45g, so 288Wh/kg.

etriker   100 kW

100 kW
Posts: 1078
Joined: May 27 2012 8:21am
Location: Florida USA

Re: Boeing Dreamliner Battery Fire

Post by etriker » Jan 17 2013 9:00am

Jason27 wrote:Takes notes all you MBA students and future CEO's.. Good case study here on globalization.
http://www.urbandictionary.com/define.p ... id=4877142

Generation Z is taking over. They are hooked on asian porn. We are screwed ! ! !

User avatar
bigmoose   100 MW

100 MW
Posts: 2682
Joined: Aug 06 2009 3:05pm
Location: North coast USA
Contact:

Re: Boeing Dreamliner Battery Fire

Post by bigmoose » Jan 17 2013 9:20am

Jason27 wrote:Boeing 787= outsourcing lesson from hell
Amen to that. Have to spread around the fabrication pie to all the countries that are purchasers. Second fact that cannot be denied is the personal impact in past years of Alan Mulally. He was probably the best manager of complex aerospace systems since Warner Von Braun. He worked on the 777 program first as director of engineering and, from September 1992, as vice-president and general manager. The 777 as you know came in close to on time, and had a pretty good record. Alan is now CEO of Ford Motor Company, and I say proudly, the only american car company that did not need, nor take any bailout money.

The dreamliner has been a bust on schedule, I think it is 3 or 4 years late. Now problems with fuel leaks and major systems. Boeing has clearly lost something with Alan leaving.

I have never been an advocate of composite systems for high reliability, civilian systems. I guess we will see with the dreamliner as the years unfold. Our constant quest for efficiency is going to be our Achilles heel.
"Live simply. Love generously. Care deeply. Speak kindly. Leave the rest to God..." all the best, Dave

Jason27   10 kW

10 kW
Posts: 643
Joined: Apr 17 2011 8:10pm
Location: San Francisco, CA

Re: Boeing Dreamliner Battery Fire

Post by Jason27 » Jan 17 2013 9:26am

The thought that you can't make things in house is not true.

I just watched an interview on YouTube with the CEO of Tesla Elon Musk saying he found it cheaper to make the Tesla roadster and model S parts in house in California rather than outsource the parts. Obviously Boeing did the opposite.
My ebike:
Diamondback with WE 800 watt hub motor with AllCell 48V 20AH Lithium Manganese battery pack.

Harold in CR   1 MW

1 MW
Posts: 1651
Joined: Feb 01 2010 7:19pm
Location: Costa Rica

Re: Boeing Dreamliner Battery Fire

Post by Harold in CR » Jan 17 2013 9:27am

Our constant quest for efficiency is going to be our Achilles heel
Well stated, Bigmoose. 8)
Thanks to Justin, the forum is open source and NON-commercialized.

etriker   100 kW

100 kW
Posts: 1078
Joined: May 27 2012 8:21am
Location: Florida USA

Re: Boeing Dreamliner Battery Fire

Post by etriker » Jan 17 2013 9:28am

bigmoose wrote:
Jason27 wrote:Boeing 787= outsourcing lesson from hell
Amen to that. Have to spread around the fabrication pie to all the countries that are purchasers. Second fact that cannot be denied is the personal impact in past years of Alan Mulally. He was probably the best manager of complex aerospace systems since Warner Von Braun. He worked on the 777 program first as director of engineering and, from September 1992, as vice-president and general manager. The 777 as you know came in close to on time, and had a pretty good record. Alan is now CEO of Ford Motor Company, and I say proudly, the only american car company that did not need, nor take any bailout money.

The dreamliner has been a bust on schedule, I think it is 3 or 4 years late. Now problems with fuel leaks and major systems. Boeing has clearly lost something with Alan leaving.

I have never been an advocate of composite systems for high reliability, civilian systems. I guess we will see with the dreamliner as the years unfold. Our constant quest for efficiency is going to be our Achilles heel.
Our Achilles heel really is our workers goofing off at work texting and playing on the computers.

The younger workers do it so much. Half the day their face is looking at an I Phone texting. Boys and girls.

Those I phones are taking us down ?

The kids can't focus at work.

They are getting harder to train to do hi tech work that needs a lot of focus.

Those I Phones got their brains all over the place.

flathill   100 kW

100 kW
Posts: 1273
Joined: Jul 06 2010 9:26pm

Re: Boeing Dreamliner Battery Fire

Post by flathill » Jan 17 2013 9:35am

just waiting for the Tesla scare once the chemistry is connected
then I can buy back in
all stocks should be down if the longshoreman strike at the end of the month

The breakthrough with lithium-ion batteries was in the electrolyte material. Up until 1990 batteries were water-based. Researchers at Berkeley found that using an organic electrolyte led to dramatic increases in energy density, or the amount of energy in the package.
Lithium-ion batteries such as those used on the 787 have safeguards, such as controllers that trigger a shut-off if temperatures rise too much; vent built-up pressure; and prevent the batteries from bursting into flame.
A Boeing executive said the 787 has a redundant safety system with four controllers on the batteries, although that’s apparently not enough to prevent incidents and satisfy regulators.
Research continues into improving lithium-ion batteries, but the technology is now mature, said Jonathan Posner, associate professor of mechanical engineering at the University of Washington, who called the technology “a logical choice” for the 787.
“I don’t think Boeing would have used it if it wasn’t mature,” he said.
Posner said Boeing seems to have “an engineering issue that just has to be resolved. But I would be surprised if they don’t continue to use lithium-ion batteries in the 787.”
Different materials can be used in these batteries, some safer than others. Based on information posted on its website, Boeing supplier GS Yuasa appears to be using lithium cobalt oxide cathode material, which is the original material used by Sony.
“From a safety point of view, that’s not the best,” said Ji-Guang Zhang, a researcher at the Pacific Northwest National Laboratory in Richland. He said cobalt oxide batteries ignite at lower temperature than batteries made with other materials, such as lithium ion phosphate.
Supplier GS Yuasa declined to discuss whether the batteries in question use cobalt oxide and referred questions to its partner Thales Group, which didn’t promptly respond.
Still, it’s all relative.
“Theoretically, it is safe,” Zhang said. “I think it is not less safe than a gasoline-powered engine. ... Gas is much easier to burn than batteries.”
Battaglia said lithium-ion phosphate “has been known to sort of be safer.” But he added that “nothing is safe — you’ve still got a lot of energy and an electrolyte in there that’s flammable.”

etriker   100 kW

100 kW
Posts: 1078
Joined: May 27 2012 8:21am
Location: Florida USA

Re: Boeing Dreamliner Battery Fire

Post by etriker » Jan 17 2013 9:52am

Dogman would have suggested they make the pack easy to get to in case of a fire ?

Heck, that should be the #1 lipo rule.

They had to hack a hole in the jet and it took 40 mins to put out the fire ?

I would rather Dogman design my battery pack than the bozos that designed that jet pack.

Dogman, Boeing needs you.

etriker   100 kW

100 kW
Posts: 1078
Joined: May 27 2012 8:21am
Location: Florida USA

Re: Boeing Dreamliner Battery Fire

Post by etriker » Jan 17 2013 10:01am

Their biggest mistake was they thought their battery packs were safe and would not burn.

ES is more advanced in that we believe all battery packs can burn and should be treated as such.

That pack could have burned when that jet was in the air loaded with people.

hydro-one   10 kW

10 kW
Posts: 866
Joined: Dec 19 2008 2:02pm
Location: winipeg Canada

Re: Boeing Dreamliner Battery Fire

Post by hydro-one » Jan 17 2013 10:36am

Yeah it should have been dumpable like a shit brick onto the runway. or onto a tether away from the plane if in flight. or at least designed where all fire was contained, and all smoke was vented to exterior of plane. All batteries can burn, lipo is just highly exothermic with huge toxic smoke. and i mean huge. and flames.

very ironic though with lithium shipping regs an all that.
Pro ebiker
28s hk lipo
3ooA kelly/cromotor 17"
sana cruz bullit

User avatar
fizzit   10 kW

10 kW
Posts: 737
Joined: Mar 10 2010 10:14pm
Location: Seattle, WA

Re: Boeing Dreamliner Battery Fire

Post by fizzit » Jan 17 2013 11:09am

Jason27 wrote:The thought that you can't make things in house is not true.

I just watched an interview on YouTube with the CEO of Tesla Elon Musk saying he found it cheaper to make the Tesla roadster and model S parts in house in California rather than outsource the parts. Obviously Boeing did the opposite.
Tesla does not make their batteries in house.
-Colin

User avatar
neptronix   100 GW

100 GW
Posts: 14247
Joined: Jun 15 2010 5:56pm
Location: California refugee living in Utah, USA
Contact:

Re: Boeing Dreamliner Battery Fire

Post by neptronix » Jan 17 2013 11:32am

hydro-one wrote:Yeah it should have been dumpable like a shit brick onto the runway. or onto a tether away from the plane if in flight. or at least designed where all fire was contained, and all smoke was vented to exterior of plane. All batteries can burn, lipo is just highly exothermic with huge toxic smoke. and i mean huge. and flames.

very ironic though with lithium shipping regs an all that.
Right? shipping dangerous lithium batteries is apparently only OK when they're a critical part of the airplane. :lol:
"Love and compassion are necessities, not luxuries. Without them, humanity cannot survive." - Dalai Lama

My first major build: 1.6kW 8T MAC motor on a Trek 4500.
The new all-arounder: Leafmotor 1500w @ 4kW on a Turner O2 full suspension.
The monster scooter: 20" eZee on a Cannondale Semi Recumbent.
Whipper-snapper: ? on a lightweight BikeE Semi Recumbent

User avatar
knoxie   10 MW

10 MW
Posts: 2431
Joined: Jan 03 2007 5:54pm
Location: UK
Contact:

Dreamliner Lithium Ion Battery fires

Post by knoxie » Jan 17 2013 5:17pm

Well publicised fires on board Boeing dreamliner planes, pretty serious and I would bet this is more down to how they are being charged and supported rather than the cells themselves.

I had to laugh though, on the news they showed a picture of the burnt batter box and said, this is the battery in question, its about the size of a shoebox, now this battery doesnt actually power the planes engines :lol: :lol: you dont say ha ha, its funny I said to the missus no a box of lipo that size just about powers my ebike :lol:

Its funny that the airlines for a long while have clamped down on the transportation of lipo in the cargo hold but seem to accept that its safe to use in the plane? bit of a double standard.

This is going to cost someone their job and a lot of money for sure.

Image
Electric KMX 72V Lipo, USPD drive unit. BMX 72V, Puma BMC,
Raleigh 26 inch MTB Puma 50V Turnigy 25C Lipo 10AH, Trek MTB, X5 48V NIMH. Electric BMX
http://tinyurl.com/4vrmc8 http://tinyurl.com/3umm4n

aroundqube   1 kW

1 kW
Posts: 483
Joined: Mar 12 2012 9:58pm

Re: Boeing Dreamliner Battery Fire

Post by aroundqube » Jan 17 2013 10:30pm

Just wondering if cabin pressure could have anything to do with this. What if these lost pressure at altitude?

Joseph C.   1 MW

1 MW
Posts: 1797
Joined: Feb 03 2011 8:43am
Location: Ireland
Contact:

Re: Boeing Dreamliner Battery Fire

Post by Joseph C. » Jan 17 2013 10:43pm

aroundqube wrote:Just wondering if cabin pressure could have anything to do with this. What if these lost pressure at altitude?
Surely that would have been known though? They would have instruments to detect any loss in pressure.

There seems to be other problems with the 787 besides the batteries - cabin windows breaking, electrical problems, fuel leaks. The Toulousains must be delighted with Boeing's problems.

The batteries are getting most of the attention because they are exotic but there seems to be a widespread systems failure across unrelated areas. Something is seriously wrong. You can't easily imagine Boeing workers being so careless and their work would have to pass multiple checks - so that leaves design and manufacture.
Yellow Magpie - Home Of The Talented And The Interesting

http://yellowmagpie.com

User avatar
fizzit   10 kW

10 kW
Posts: 737
Joined: Mar 10 2010 10:14pm
Location: Seattle, WA

Re: Boeing Dreamliner Battery Fire

Post by fizzit » Jan 17 2013 11:00pm

Joseph C. wrote:
Surely that would have been known though? They would have instruments to detect any loss in pressure.

There seems to be other problems with the 787 besides the batteries - cabin windows breaking, electrical problems, fuel leaks. The must be delighted with Boeing's problems.

The batteries are getting most of the attention because they are exotic but there seems to be a widespread systems failure across unrelated areas. Something is seriously wrong. You can't easily imagine Boeing workers being so careless and their work would have to pass multiple checks - so that leaves design and manufacture.
Yeah cabin pressure was definitely not lost. But I don't think that the "Toulousains" can laugh after their problems with the A380 :P
-Colin

Post Reply